ASTM A36 C and MC steel channels are carbon structural C-shapes or MC-shapes with 36 ksi minimum yield and 58–80 ksi tensile strength. Dimensions follow the ASTM A6/A6M C and MC series. This page covers A36 channels only, not W-shapes or plates. SHH STEEL reviews grade, designation, edition and certificate requirements before quoting.
Keywords
ASTM A36 C and MC Steel Channels, ASTM A36 Steel Channel, A36 C channel, A36 MC channel, ASTM A6 C channel
Equivalent Grades:
Near-equivalents only, not automatic substitutes: A36 W-shapes use the same grade, not the same section; A572 Grade 50 channel is a higher-strength grade; Q235B; S235JR; SS400.
Share:
General Description
Material Specification
Available Sizes of A36 C and MC Steel Channels
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why Source A36 Steel Channels from SHH STEEL
FAQ
Conclusion

What are ASTM A36 C and MC Steel Channels?

ASTM A36 steel channel is a hot-rolled C-shape or MC-shape in carbon structural steel A36. The material standard is ASTM A36/A36M. Dimensions, mass and general requirements for the rolled section are those of ASTM A6/A6M. The 36 ksi [250 MPa] minimum yield is the same figure used for A36 plates and for A36 wide-flange beams, but this page is for the channel, not for a W-shape, an angle, or a plate.

American Standard channels are designated C, for example C 6×8.2 or C 15×50, where the second number is theoretical mass in pounds per foot. Miscellaneous channels are designated MC, for example MC 12×10.6 or MC 18×58. An MC is not a C of the same depth: the flange width, web thickness and mass are those of the MC series, not a substitute C 12 or C 18. Neither series is a European UPN or UPE, and neither is a Chinese or Japanese channel of a similar millimetre depth.

These channels are filed under ASTM A36 steel channel profiles in the steel channel profiles category of steel structural profiles. The same grade in plate form is listed separately as ASTM A36 steel plate and ASME SA-36 steel plate. Do not use those plate pages as a channel data sheet.

A36 channels are used for building frames, bracing, stair stringers and general industrial work when the specification names this carbon grade in a C or MC section. The grade is not a pressure-vessel or nuclear safety material, and it is not a substitute for ASTM A572 Grade 50 when a 50 ksi yield is what the order requires.

This page covers C and MC Steel Channels in ASTM A36. The American Standard (C) and miscellaneous (MC) series follow ASTM A6/A6M; the material specification does not by itself define the dimensions.

Material, Dimensions and Tolerances for A36 Channels

The order and the inspection certificate should keep material, dimensions and tolerances distinct:

  • ASTM A36/A36M is the material standard. This article uses chemistry and tensile values for A36 shapes from ASTM A36/A36M-19. The edition named on the order governs acceptance.
  • ASTM A6/A6M is the general-requirements and dimensional standard for these rolled channels. The size tables below are reference dimensions and theoretical masses for the standard C and MC series, not a mill rolling list. The edition of A6/A6M named on the order governs dimensional acceptance.

A documented special combination — for example A36 on a UPN, or a C-shape certified to a different material standard — is only valid if every requirement of each named standard is met. Matching a nominal 6 in or 150 mm depth is not a substitution.

A36 Channel Sizes: Standard C and MC Series

The tables list designation, depth, flange width, web and flange thickness, and theoretical mass, in inch-pound and SI units, for the standard American Standard (C) and miscellaneous (MC) series under ASTM A6/A6M. Use them to identify and estimate, not as a rolling programme for A36. Mid-range C 6 to C 12 sizes are the usual enquiry core; the lightest C 3 rows and the MC 18 range should be confirmed size by size.

C 6×8.2 and C 6×13 share a 6 in depth but not a web or a mass: 8.2 lb/ft is the light web in that group, 13 lb/ft the heavy one. MC 12×10.6 is a miscellaneous 12 in channel, not a C 12×20.7. C 15×50, the heaviest standard C, has a 0.65 in flange, still far below the 3 in flange thickness at which A36 changes its manganese and silicon rule.

American Standard channels (C series)

32 sizes, from C 3×3.5 to C 15×50.

Swipe horizontally to view all dimensions.

Designation d (in) bf (in) tw (in) tf (in) d (mm) bf (mm) tw (mm) tf (mm) Mass (lb/ft) Mass (kg/m)
C 3×3.5 3 1.37 0.132 0.273 76.2 34.8 3.35 6.93 3.5 5.2
C 3×4.1 3 1.41 0.17 0.273 76.2 35.8 4.32 6.93 4.1 6.1
C 3×5 3 1.5 0.258 0.273 76.2 38.1 6.55 6.93 5 7.4
C 3×6 3 1.6 0.356 0.273 76.2 40.6 9.04 6.93 6 8.9
C 4×4.5 4 1.52 0.125 0.296 102 38.6 3.18 7.52 4.5 6.7
C 4×5.4 4 1.58 0.184 0.296 102 40.1 4.67 7.52 5.4 8
C 4×6.25 4 1.65 0.247 0.296 102 41.9 6.27 7.52 6.25 9.3
C 4×7.25 4 1.72 0.321 0.296 102 43.7 8.15 7.52 7.25 10.8
C 5×6.7 5 1.75 0.19 0.32 127 44.5 4.83 8.13 6.7 10.4
C 5×9 5 1.89 0.325 0.32 127 48 8.26 8.13 9 13
C 6×8.2 6 1.92 0.2 0.343 152 48.8 5.08 8.71 8.2 12.2
C 6×10.5 6 2.03 0.314 0.343 152 51.6 7.98 8.71 10.5 15.6
C 6×13 6 2.16 0.437 0.343 152 54.9 11.1 8.71 13 19.3
C 7×9.8 7 2.09 0.21 0.366 178 53.1 5.33 9.3 9.8 14.6
C 7×12.25 7 2.19 0.314 0.366 178 55.6 7.98 9.3 12.25 18.2
C 7×14.75 7 2.3 0.419 0.366 178 58.4 10.6 9.3 14.75 22
C 8×11.5 8 2.26 0.22 0.39 203 57.4 5.59 9.91 11.5 17.1
C 8×13.75 8 2.34 0.303 0.39 203 59.4 7.7 9.91 13.75 20.5
C 8×18.75 8 2.53 0.487 0.39 203 64.3 12.4 9.91 18.75 27.9
C 9×13.4 9 2.43 0.233 0.413 229 61.7 5.92 10.5 13.4 19.9
C 9×15 9 2.49 0.285 0.413 229 63.2 7.24 10.5 15 22
C 9×20 9 2.65 0.448 0.413 229 67.3 11.4 10.5 20 30
C 10×15.3 10 2.6 0.24 0.436 254 66 6.1 11.1 15.3 22.8
C 10×20 10 2.74 0.379 0.436 254 69.6 9.63 11.1 20 30
C 10×25 10 2.89 0.526 0.436 254 73.4 13.4 11.1 25 37
C 10×30 10 3.03 0.673 0.436 254 77 17.1 11.1 30 45
C 12×20.7 12 2.94 0.282 0.501 305 74.7 7.16 12.7 20.7 30.8
C 12×25 12 3.05 0.387 0.501 305 77.5 9.83 12.7 25 37
C 12×30 12 3.17 0.51 0.501 305 80.5 13 12.7 30 45
C 15×33.9 15 3.4 0.4 0.65 381 86.4 10.2 16.5 33.9 50.4
C 15×40 15 3.52 0.52 0.65 381 89.4 13.2 16.5 40 60
C 15×50 15 3.72 0.716 0.65 381 94.5 18.2 16.5 50 74

Miscellaneous channels (MC series)

40 sizes, from MC 3×7.1 to MC 18×58.

Swipe horizontally to view all dimensions.

Designation d (in) bf (in) tw (in) tf (in) d (mm) bf (mm) tw (mm) tf (mm) Mass (lb/ft) Mass (kg/m)
MC 3×7.1 3 1.94 0.312 0.351 76.2 49.3 7.92 8.92 7.1 10.6
MC 4×13.8 4 2.5 0.5 0.5 102 63.5 12.7 12.7 13.8 20.5
MC 6×6.5 6 1.85 0.155 0.291 152 47 3.94 7.39 6.5 9.7
MC 6×7 6 1.88 0.179 0.291 152 47.8 4.55 7.39 7 10.4
MC 6×12 6 2.5 0.31 0.375 152 63.5 7.87 9.53 12 17.9
MC 6×15.1 6 2.94 0.316 0.475 152 74.7 8.03 12.1 15.1 22.5
MC 6×15.3 6 3.5 0.34 0.385 152 88.9 8.64 9.78 15.3 22.8
MC 6×16.3 6 3 0.375 0.475 152 76.2 9.53 12.1 16.3 24.3
MC 6×18 6 3.5 0.379 0.475 152 88.9 9.63 12.1 18 26.8
MC 7×19.1 7 3.45 0.352 0.5 178 87.6 8.94 12.7 19.1 28.4
MC 7×22.7 7 3.6 0.503 0.5 178 91.4 12.8 12.7 22.7 33.8
MC 8×8.5 8 1.87 0.179 0.311 203 47.5 4.55 7.9 8.5 12.6
MC 8×18.7 8 2.98 0.353 0.5 203 75.7 8.97 12.7 18.7 27.8
MC 8×20 8 3.03 0.4 0.5 203 77 10.2 12.7 20 29.8
MC 8×21.4 8 3.45 0.375 0.525 203 87.6 9.53 13.3 21.4 31.8
MC 8×22.8 8 3.5 0.427 0.525 203 88.9 10.8 13.3 22.8 33.9
MC 9×23.9 9 3.45 0.4 0.55 229 87.6 10.2 14 23.9 35.6
MC 9×25.4 9 3.5 0.45 0.55 229 88.9 11.4 14 25.4 37.8
MC 10×6.5 10 1.17 0.152 0.202 254 29.7 3.86 5.13 6.5 9.7
MC 10×8.4 10 1.5 0.17 0.28 254 38.1 4.32 7.11 8.4 12.5
MC 10×22 10 3.32 0.29 0.575 254 84.3 7.37 14.6 22 33
MC 10×25 10 3.41 0.38 0.575 254 86.6 9.65 14.6 25 37
MC 10×28.5 10 3.95 0.425 0.575 254 100 10.8 14.6 28.5 42.4
MC 10×33.6 10 4.1 0.575 0.575 254 104 14.6 14.6 33.6 50
MC 10×41.1 10 4.32 0.796 0.575 254 110 20.2 14.6 41.1 61.2
MC 12×10.6 12 1.5 0.19 0.309 305 38.1 4.83 7.85 10.6 15.8
MC 12×14.3 12 2.12 0.25 0.313 305 53.8 6.35 7.95 14.3 21.3
MC 12×31 12 3.67 0.37 0.7 305 93.2 9.4 17.8 31 46
MC 12×35 12 3.77 0.465 0.7 305 95.8 11.8 17.8 35 52
MC 12×40 12 3.89 0.59 0.7 305 98.8 15 17.8 40 60
MC 12×45 12 4.01 0.71 0.7 305 102 18 17.8 45 67
MC 12×50 12 4.14 0.835 0.7 305 105 21.2 17.8 50 74
MC 13×31.8 13 4 0.375 0.61 330 102 9.53 15.5 31.8 47.3
MC 13×35 13 4.07 0.447 0.61 330 103 11.4 15.5 35 52
MC 13×40 13 4.19 0.56 0.61 330 106 14.2 15.5 40 60
MC 13×50 13 4.41 0.787 0.61 330 112 20 15.5 50 74
MC 18×42.7 18 3.95 0.45 0.625 457 100 11.4 15.9 42.7 63.5
MC 18×45.8 18 4 0.5 0.625 457 102 12.7 15.9 45.8 68.2
MC 18×51.9 18 4.1 0.6 0.625 457 104 15.2 15.9 51.9 77.2
MC 18×58 18 4.2 0.7 0.625 457 107 17.8 15.9 58 86

S-shapes and other bar-size or special channels can be reviewed when they are named on the enquiry. Complete tables for those series are not reproduced here. European UPN or UPE, and Chinese or Japanese channel designations, belong to their own dimensional standards, not to these C and MC rows.

A36 Chemical Composition for Channels (Shapes Column)

The figures below are heat-analysis limits for A36 shapes from Table 3 of ASTM A36/A36M-19. They are the “All” thicknesses shapes column. They must not be copied from a plate-width column, and they are limits, not typical heat results.

Element Heat analysis, shapes, all thicknesses Notes for A36 channels
C, max (%) 0.26 From the shapes column of Table 3, not a plate-width column.
Mn No specified requirement The heat analysis for manganese shall be determined and reported in accordance with A6/A6M.
P, max (%) 0.04 —
S, max (%) 0.05 —
Si, max (%) 0.40 For shapes with flange thickness over 3 in [75 mm], manganese shall be 0.85–1.35% and silicon 0.15–0.40%. None of the standard C or MC rows in the size tables below has a flange that thick.
Cu, min (%) 0.20 when copper steel is specified This minimum applies only when copper steel is specified on the order.

A36 Channel Mechanical Properties: Yield, Tensile and Elongation

Tensile properties of A36 channels follow the shapes requirements in Table 2 of ASTM A36/A36M-19. The 32 ksi [220 MPa] yield that applies to plates over 8 in does not apply to these sections. The footnote that removes the 80 ksi tensile maximum and lowers the 2 in elongation to 19% applies only to wide-flange shapes with flange thickness over 3 in, not to C or MC channels.

Property Requirement for A36 shapes
Minimum yield point 36 ksi [250 MPa]
Tensile strength 58–80 ksi [400–550 MPa]
Minimum elongation in 8 in [200 mm] 20%
Minimum elongation in 2 in [50 mm] 21%

Charpy V-notch testing is not a default A36 requirement. Supplementary requirements such as S5 or S30 apply only when they are named on the order. All of the standard C and MC rows tabulated above have a cross-sectional area of at least 1.09 in², so the small-shape tension-test waiver in clause 8.2 does not apply to this list.

Delivery Conditions, Inspection and Identification

A36 channels are commonly supplied as-rolled. The inspection document should show ASTM A36/A36M and its edition, the grade A36, the A6/A6M designation (C or MC), the heat number, the heat analysis (including reported manganese), and the tensile results. If copper steel, a Charpy supplementary, or a particular A6/A6M finish is required, that must appear on the order and on the certificate. An A36 W-shape certificate does not, by itself, identify a C or MC section.

An EN 10204 type 3.1 document, or the mill’s equivalent inspection certificate, is the usual export request; type 3.2 or nominated third-party attendance can be added when the specification requires it. Identification follows the mill’s marking practice. Length is a matter for the rolling programme and the order, often in the region of 20–40 ft or 6–12 m.

Weldability and Surface Condition of A36 Channels

A36 is a weldable carbon structural steel when thickness, joint design and hydrogen control are taken into account. The specification does not table a carbon-equivalent limit for the grade. Procedure should be set from the certificate analysis and the applicable welding specification, not from an invented CEV figure. This page does not prescribe a procedure or a preheat chart.

The as-rolled surface is mill scale. Blast, paint or galvanizing is an order option. Cutting, punching, forming or coating can be reviewed when that specification is sent with the enquiry. They are not assumed for every size.

A6/A6M Shape Tolerances and Theoretical Mass

Dimensional and mass tolerances for these C and MC sections are those of ASTM A6/A6M, not of A36/A36M itself. This article does not reproduce the inch or millimetre tolerance tables; acceptance is against the edition named on the order.

A delivered C 6×13 will measure close to the tabulated depth, flange and thicknesses within those tolerances, not as a set of exact advertised inches. Out-of-square and flange tilt matter for connections. Settlement on theoretical or weighed mass should follow the contract.

Applications and Service Limits

A36 steel channels are used where a 36 ksi carbon grade and a C or MC section are specified:

  • Building and industrial frames, bracing, purlins, stair stringers and general fabrications whose specification names A36 channel rather than Grade 50 or a non-American channel series.
  • Export packages that compare the grade with Q235B or with S235JR, provided each line keeps its own material standard and shape system.

It is not specified here for pressure equipment, for nuclear safety-related components, or for members that actually require A572 Grade 50 or a tabulated impact test. Durability comes from the coating or fire-protection system, not from the A36 designation.

A36 Channel Compared with A36 Beams, Grade 50 and Q235B

A36 wide-flange beams share the same material standard and the same 36 ksi yield, but they are W-shapes, not C or MC sections. An A572 Grade 50 channel can use the same C and MC series at a higher yield and with a different chemistry table. Q235B and S235JR are useful lower-strength comparisons only if chemistry, toughness and the shape standard are also satisfied.

Dual certification requires every requirement of each named standard to be met on the delivered piece. The A36 steel angle page in this series will be linked here once it is published.

Near-Equivalents: Not Automatic Substitutes

The comparisons below are for orientation. They are not a licence to substitute one grade or one shape for another on a contract or an inspection certificate.

Grade / designation Standard Relationship to A36 channel Caution
A36 W-shape ASTM A36/A36M; dimensions ASTM A6/A6M The same material specification, usually as wide-flange beams. A W-shape and a C or MC of similar depth are different sections, with different flanges, mass and connection details.
A572 Grade 50 channel ASTM A572/A572M; dimensions ASTM A6/A6M A higher-strength low-alloy channel that can use the same C and MC series. Grade 50 has its own chemistry, a 50 ksi yield, and no 80 ksi tensile cap. It is not an A36 certificate.
Q235B / SS400 / S235JR GB/T 700 or JIS G 3101 or EN 10025-2; different shape standards Common lower-strength comparisons in export enquiries. Each has its own chemistry and shape system (GB, JIS or UPN/UPE). A shared 36 ksi or 235 MPa discussion is not a substitution method.

Sourcing A36 Steel Channels from SHH STEEL

SHH STEEL supplies A36 steel channels as an export trading house, coordinating mill production and project procurement. For this product the useful work is to keep C and MC designations from being mixed, to keep the A36 shapes chemistry and tensile table from being fulfilled with a plate certificate, and to align the A6/A6M size, the material edition and the inspection document before a rolling programme is committed.

Sections can be sourced from mills that SHH STEEL buys from, including Masteel, Rizhao Steel, Laiwu (Shandong Steel Laiwu) and Tung Ho Steel, among others when the programme matches the order. Those mills do not each roll every C or MC size in A36. Mid-range C sizes are the usual core; MC 18 rows and uncommon light C 3 variants are confirmed per line.

The same enquiry can also cover W-shapes, angles, or Chinese, Japanese or European designations, provided each line states its material standard, shape standard and size. If cutting, punching, forming or a coating system is required, include that specification for review. Export packing and container loading can be arranged to the packing list agreed for the shipment.

A36 C and MC Steel Channel FAQs

Is a C-shape the same as an MC of the same depth?
No. C designations are American Standard channels; MC designations are miscellaneous channels. MC 12×10.6 is not a C 12, and the flange, web and mass are those of the MC series. The order should use the designation that the specification actually names.
Does the 32 ksi yield for thick plate apply to A36 channels?
No. The 32 ksi [220 MPa] yield in ASTM A36/A36M is for plates over 8 in thick. A36 channels are shapes, with a 36 ksi [250 MPa] minimum yield and a 58–80 ksi tensile range.
Are A36 channels and A36 W-shapes interchangeable?
They may be certified to the same material standard, but they are different sections under A6/A6M. A W-shape certificate and a W depth do not identify a C or MC channel.
Is a Charpy test required for A36 channel?
Not by default. Charpy supplementary requirements such as S5 or S30 apply only when they are named on the order.
Which standards should appear on the inspection document?
At least ASTM A36/A36M and its edition, the grade A36, the C or MC designation to A6/A6M, the heat number, heat analysis including reported manganese, and tensile results. Any copper-steel or impact supplementary should also appear if it was ordered.

Request a Quotation for ASTM A36 C and MC Steel Channels

ASTM A36 C and MC steel channels are carbon structural C-shapes or MC-shapes with 36 ksi [250 MPa] minimum yield. Nominate the C or MC size to ASTM A6/A6M and the material to ASTM A36/A36M-19 (or the edition on the order). The tables are reference dimensions, not a rolling list. Send the designation list, edition, certificate type and any processing notes; SHH STEEL will review the package and quote accordingly.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X