ASME SA516 GRADE 65 | ASME SA516GR65 Carbon Steel Plates
General Description
What is ASME SA516 GRADE 65?
As an expert at SHH STEEL, I’m excited to highlight our ASME SA516 Grade 65 Carbon Steel Plates, also known as ASME SA516GR65 or ASME SA516 GR 65. This grade is a reliable workhorse for pressure vessels and boilers, providing a tensile strength of 450-585 MPa and a minimum yield strength of 240 MPa.
It’s engineered for moderate-temperature service up to 450°C and pressures to 500 bar, making it perfect for applications where toughness and weldability are key. SHH STEEL, a leading carbon steel exporter, supplies these plates in thicknesses from 5mm to 500mm, with widths up to 4600mm and lengths to 12000mm, catering to the demands of large-scale industrial projects.
The normalized condition of ASME SA 516 GR 65 plates refines the grain structure, boosting ductility and impact resistance to handle welded constructions in challenging environments. For buyers looking for ASME SA516 Gr.65 properties or equivalents, this grade shines with its cost-effectiveness and adherence to ASME Section VIII Division 1, the code for pressure-containing equipment. SHH STEEL’s ASME SA516 GR.65 plates are thoroughly tested for ultrasonic inspection and Charpy impact, delivering defect-free performance that meets global standards.
With a balanced carbon equivalent (CE ≤0.41 per AWS D1.1), these plates facilitate seamless welding, reducing the risk of hydrogen-induced cracking. The material’s ability to retain properties after heat treatment makes it ideal for multi-pass welding in vessel fabrication. SHH STEEL’s dedication to quality means every plate comes with mill test certificates, giving buyers confidence in critical applications like oil & gas storage and power generation.
Material Specification
As an production expert at SHH STEEL, I can confirm that ASME SA516 Grade 65 carbon steel plates are governed by ASME SA-516/SA-516M, the ASME Boiler and Pressure Vessel Code Section II Part A adaptation of ASTM A516/A516M-17. This specification outlines requirements for carbon steel plates for moderate and lower temperature service, ensuring suitability for welded pressure vessels and boilers.
SHH STEEL complies fully with this standard, providing plates in normalized or stress-relieved conditions to optimize mechanical properties. The specification supports thicknesses from 5mm to 500mm, widths up to 4600mm, and lengths to 12000mm, with custom dimensions available for large-diameter vessel designs.
Ultrasonic examination per ASME SA-20 or ASTM A435 Class 1 detects laminations, guaranteeing defect-free material, while dual certification with EN 10028-2 or GB/T 713 is offered for international compatibility.
This makes our ASME SA516 GR 65 plates a reliable choice for global buyers, supported by mill test certificates for complete traceability.
| Specification Element | Requirement | SHH STEEL Compliance | Keywords |
| Primary Standard | ASME SA-516/SA-516M | ASME Section VIII | SA516 Gr.65 specification |
| Thickness Range | 5mm-500mm (custom) | Mill Test Certificate | SA516 Gr.65 dimensions |
| Width/Length | Up to 4600mm / 12000mm | Custom fabrication available | SA516 Gr.65 size options |
| Ultrasonic Testing | No laminations >0.25% thickness | Class 1 per ASME SA-20 | SA516 Gr.65 inspection |
| Heat Treatment | Normalized or stress-relieved | 900-950°C furnace control | SA516 Gr.65 heat treat |
Chemical Composition
At SHH STEEL, we ensure the chemical composition of ASME SA516 Grade 65 is tightly controlled per ASME SA-516/SA-516M to guarantee weldability and toughness.
The maximum carbon content is 0.23%, preventing brittleness, while manganese (0.60-1.20%) boosts strength. Phosphorus and sulfur are capped at 0.035% each to minimize cracking, and silicon (0.15-0.40%) supports deoxidation during steelmaking.
Optional vanadium (≤0.02%) refines grains, improving low-temperature impact resistance. Our testing per ASME SA-350 maintains a Carbon Equivalent (CE) ≤0.40 per AWS D1.1, making ASME SA516 GR 65 plates a reliable choice for buyers searching for “ASME SA516 GR 65 chemical composition.”
| Element | Content (%) | Standard Limit | Test Method | Role | Keywords |
| Carbon (C) | ≤0.23 | 0.23 max | ASME SA-350 | Strength without brittleness | SA516 Gr.65 carbon |
| Manganese (Mn) | 0.60-1.20 | 0.60-1.20 | ASME SA-350 | Toughness, hardenability | SA516 Gr.65 manganese |
| Phosphorus (P) | ≤0.035 | 0.035 max | ASME SA-350 | Reduces brittleness | SA516 Gr.65 phosphorus |
| Sulfur (S) | ≤0.035 | 0.035 max | ASME SA-350 | Improves weldability | SA516 Gr.65 sulfur |
| Silicon (Si) | 0.15-0.40 | 0.15-0.40 | ASME SA-350 | Deoxidation, fluidity | SA516 Gr.65 silicon |
| Vanadium (V) | ≤0.02 | 0.02 max | ASME SA-350 | Grain refinement | SA516 Gr.65 vanadium |
Mechanical Properties
As an expert at SHH STEEL, I can assure you that ASME SA516 Grade 65 carbon steel plates deliver strong mechanical properties, tested per ASME SA-8 for tensile/yield, ASME SA-23 for impact, and ASME SA-466 for fatigue.
With a minimum yield strength of 240 MPa and tensile range of 450-585 MPa, these plates support high load-bearing capacity, while 19% elongation ensures ductility for forming.
The impact energy of 27J at -20°C prevents brittle failure, and the modulus of elasticity (200 GPa per ASME SA-111) provides structural stability. The fatigue limit (240 MPa est. per ASME SA-466) varies with surface finish, optimized by our grinding process.
This makes ASME SA516 GR.65 plates a reliable choice for buyers searching for “ASME SA516 GR 65 mechanical properties.”
| Property | Value | Test Method | Temperature (°C) | Thickness Effect | Keywords |
| Tensile Strength | 450-585 MPa | ASME SA-8 | Ambient | -5% >100mm | SA516 Gr.65 tensile |
| Yield Strength | 240 MPa (min) | ASME SA-8 | Ambient | Stable to 200mm | SA516 Gr.65 yield |
| Elongation | 19% (min) | ASME SA-8 | Ambient | 15-20% (5-25mm) | SA516 Gr.65 elongation |
| Impact Energy | 27J @ -20°C (min) | ASME SA-23 | -20 | 27J all thicknesses | SA516 Gr.65 impact |
| Modulus of Elasticity | 200 GPa | ASME SA-111 | Ambient | Constant | SA516 Gr.65 modulus |
| Fatigue Limit | 240 MPa (est.) | ASME SA-466 | Ambient | Varies with surface | SA516 Gr.65 fatigue |
Delivery Conditions
SHH STEEL ensures ASME SA516 GR 65 carbon steel plates are delivered in optimal conditions to suit pressure vessel needs.
We offer as-rolled, normalized (900-950°C), or stress-relieved (620-650°C) options per ASME SA-20, with quenched and tempered conditions available for enhanced toughness.
Normalized plates refine grain structure for improved impact resistance, ideal for boilers up to 400°C.
Stress-relieved reduce residual stresses for welded structures, while quenched and tempered (870-900°C quench, 650°C temper) suits wear applications.
Heat numbers provide traceability, and our global transit time, especially 3-7 days to Asia, ensures timely delivery.
| Condition | Temperature (°C) | Duration (hours/inch) | Standard | Keywords |
| As-Rolled | Ambient | N/A | ASME SA-20 | SA516 Gr.65 delivery |
| Normalized | 900-950 | 1 | ASME SA-20 | SA516 Gr.65 normalized |
| Stress-Relieved | 620-650 | 1 | ASME SA-20 | SA516 Gr.65 stress relief |
| Quenched & Tempered | Quench 870-900, Temper 650 | 0.5-1 | ASME SA-20 | SA516 Gr.65 tempered |
| Transit Time (Asia) | 3-7 days | N/A | ISO 9001 | SA516 Gr.65 shipping |
Tolerances
Precision is paramount for ASME SA516 GR 65 carbon steel plates, and SHH STEEL maintains strict tolerances per ASME SA-6 to ensure seamless fabrication.
Thickness tolerance is ±1.5mm for plates under 40mm and ±2.0mm for thicker sections up to 200mm (custom 300mm).
Width and length tolerances are ±10mm standard, with ±5mm for precision orders up to 4600mm width and 12000mm length.
Surface flatness is 3mm per meter, per ASME SA-6, preventing warping during welding or heat treatment.
For European projects, EN 10029 Class B tolerances are offered, enhancing compatibility.
| Tolerance Type | Value (mm) | Standard | Applicable Thickness (mm) | Keywords |
| Thickness (<40mm) | ±1.5 | ASME SA-6 | 5-40 | SA516 Gr.65 tolerance |
| Thickness (>40mm) | ±2.0 | ASME SA-6 | 40-200 | SA516 Gr.65 thickness tol |
| Width | ±10 (standard), ±5 (custom) | ASME SA-6, EN 10029 | All | SA516 Gr.65 width tol |
| Length | ±10 (standard), ±5 (custom) | ASME SA-6, EN 10029 | All | SA516 Gr.65 length tol |
| Flatness | 3mm per meter | ASME SA-6 | All | SA516 Gr.65 flatness spec |
Weldability
ASME SA516 GR 65 carbon steel plates are highly weldable due to low carbon (≤0.23%) and CE ≤0.40 per AWS D1.1.
SHH STEEL recommends preheating at 150-200°C for thicknesses over 25mm to prevent hydrogen-induced cracking, with post-weld heat treatment (PWHT) at 620-650°C for stress relief.
Supported processes include GTAW, SMAW, and GMAW with E7018 filler (AWS A5.1), achieving 90-95% joint efficiency per ASME Section IX. Low sulfur (≤0.035%) reduces hot shortness, and 19% elongation ensures ductility.
Testing includes bend tests (ASTM E190) for 3t radius and ultrasonic for weld integrity per ASME SA-435.
| Weldability Factor | Value/Condition | Standard | Recommended Process | Keywords |
| Carbon Equivalent (CE) | ≤0.40 | AWS D1.1 | GTAW, SMAW | SA516 Gr.65 weldability |
| Preheating (°C) | 150-200 (>25mm) | ASME Section IX | GMAW | SA516 Gr.65 welding |
| PWHT (°C) | 620-650 | ASME SA-20 | All | SA516 Gr.65 heat treat |
| Filler Metal | E7018 | AWS A5.1 | SMAW | SA516 Gr.65 welding rod |
| Bend Test Radius (mm) | 3t (t=thickness) | ASTM E190 | All | SA516 Gr.65 bend test |
Equivalent Material Grade
Global equivalents for ASME SA516 Gr.65 facilitate international projects, offering similar tensile and yield properties for pressure vessel use.
For example, P295GH (EN 10028-2) is a European equivalent with 410-570 MPa tensile and 295 MPa yield, suitable for boilers in EU regulations. SPV315 (JIS G3115) serves Japanese applications with 450-570 MPa tensile and 315 MPa yield, ideal for high-toughness vessels.
16MnR/Q245R (GB/T 713) is the Chinese standard equivalent, providing 400-540 MPa tensile and 245 MPa yield for cost-effective pressure equipment in Asian markets.
These equivalents ensure cross-compatibility, allowing buyers to substitute ASME SA516 GR 65 plates seamlessly in global supply chains.
| Grade | Standard | Tensile (MPa) | Yield (MPa) | Elongation (%) | Impact (J @ -20°C) | Keywords |
| SA516 Gr.65 | ASME SA-516/SA-516M | 450-585 | 240 | 19 | 27 | SA516 Gr.65 equivalent |
| P295GH | EN 10028-2 | 410-570 | 295 | 22 | 27 | SA516 Gr.65 EN grade |
| SPV315 | JIS G3115 | 450-570 | 315 | 19 | 27 | SA516 Gr.65 JIS grade |
| 16MnR/Q245R | GB/T 713 | 400-540 | 245 | 21 | 27 | SA516 Gr.65 GB grade |
| A537 Cl.1 | ASTM A537 | 485-620 | 345 | 18 | 41 | SA516 Gr.65 alternative |
| A285 Gr.C | ASTM A285 | 310-450 | 205 | 26 | N/A | SA516 Gr.65 low-cost alt |
Supplementary Requirements
Supplementary requirements for ASME SA516 GR 65 carbon steel plates enhance performance for specialized applications, offering buyers tailored options.
These include ultrasonic testing (Class 1 per ASME SA-435 for no laminations >0.25% thickness), Charpy impact at -50°C (27J min per ASME SA-20 for cold service), and heat analysis per heat number (ASME SA-350 for traceability).
Product analysis allows ±0.02% tolerance on elements, while shot blasting to Sa 2.5 (50-100μm profile per ISO 8501-1) is available for surface preparation.
SHH STEEL provides these to meet stringent needs, as buyers search for “SA516 Gr.65 supplementary requirements.”
| Requirement | Detail | Standard | Test Frequency | Applicable Thickness (mm) | Keywords |
| Ultrasonic Testing | Class 1, no laminations | ASME SA-435 | Full plate | 5-500 | SA516 Gr.65 ultrasonic |
| Charpy Impact | -50°C, 27J min | ASME SA-20 | Per heat | 5-500 | SA516 Gr.65 cold impact |
| Heat Analysis | Per heat number | ASME SA-350 | Each batch | All | SA516 Gr.65 analysis |
| Product Analysis | ±0.02% tolerance | ASME SA-350 | Sample per lot | All | SA516 Gr.65 product test |
| Shot Blasting | Sa 2.5, 50-100μm profile | ISO 8501-1 | On request | 5-100 | SA516 Gr.65 blasting |
Applications
ASME SA516 GR 65 carbon steel plates are versatile for moderate-pressure and temperature environments, with excellent strength and toughness.
| Application | Temperature (°C) | Pressure (bar) | Thickness (mm) | Standard Compliance | Keywords |
| Pressure Vessels | Up to 400 | 300 | 20-100 | ASME Section VIII | SA516 Gr.65 vessels |
| Boilers | Up to 350 | 200 | 10-50 | ASME Section I | SA516 Gr.65 boilers |
| Storage Tanks | Up to 200 | 50 | 5-30 | API 650 | SA516 Gr.65 tanks |
| Oil & Gas Equipment | Up to 300 | 250 | 30-120 | NACE MR0175 | SA516 Gr.65 oil equip |
| Heat Exchangers | Up to 250 | 150 | 10-40 | TEMA Standards | SA516 Gr.65 heat exchange |
Details: Pressure vessels benefit from 450-585 MPa tensile at 400°C, while boilers handle 350°C with 19% elongation for forming. Storage tanks use 5-30mm plates for 50 bar, and oil & gas equipment leverages 30-120mm for 250 bar with NACE compliance. Heat exchangers utilize 10-40mm plates for 150 bar at 250°C, per TEMA standards for efficient heat transfer.
Why Choose SHH STEEL
SHH STEEL offers ASME and ASTM-certified SA516 Gr.65 plates, with custom thicknesses up to 300mm and heat treatments tailored to your project. Our 15-year track record includes zero defect deliveries to 50+ countries, backed by SGS verification and mill test certificates.
| Advantage | Benefit | Keywords |
| Expert Certification | ASME Section VIII compliant | SA516 Gr.65 certified |
| Custom Fabrication | Up to 300mm thickness | SA516 Gr.65 custom |
| Proven Reliability | 50+ countries, zero rejects | SA516 Gr.65 trusted supplier |
FAQ
- What is ASME SA516 Grade 65 used for?
- ASME SA516 Grade 65 is widely used for pressure vessels, boilers, and storage tanks in oil & gas and power generation. It handles moderate temperatures up to 400°C and pressures to 300 bar, with 450-585 MPa tensile strength ensuring reliability. SHH STEEL supplies these for welded constructions per ASME Section VIII Division 1.
- What is the difference between SA516 Gr.65 and SA516 Gr.70?
- SA516 Gr.65 has tensile 450-585 MPa and yield 240 MPa, while Gr.70 offers 485-620 MPa and 260 MPa. Gr.65 is cost-effective for moderate stresses, with 19% elongation for forming, whereas Gr.70 suits higher pressure (500 bar). SHH STEEL recommends Gr.65 for standard applications; see our ASTM A 516 Gr 70 page for comparison.
- What is the chemical composition of SA516 Gr.65?
- The composition includes C ≤0.23%, Mn 0.60-1.20%, P ≤0.035%, S ≤0.035%, Si 0.15-0.40%, tested per ASME SA-350. This low-carbon formula ensures excellent weldability with CE ≤0.40 (AWS D1.1). SHH STEEL provides MTCs with full analysis for traceability.
- Is SA516 Gr.65 weldable
- Yes, SA516 Gr.65 is highly weldable with low carbon (≤0.23%) and preheating at 150-200°C for >25mm thicknesses. Use E7018 filler (AWS A5.1) for 90% joint efficiency per ASME Section IX. PWHT at 620-650°C reduces stress, validated by bend tests per ASTM E190.
- What is the density of SA516 Gr.65?
- The density is 7.85 g/cm³, standard for carbon steel, aiding weight calculations in vessel design. Hardness is 120-170 HB (ASME SA-18), balancing wear resistance for high-pressure use.
- What is the equivalent of SA516 Gr.65 in EN standards?
- The closest EN equivalent is P295GH (EN 10028-2), with 410-570 MPa tensile and 295 MPa yield, suitable for EU boilers. SHH STEEL provides dual-certified plates for seamless transitions.
- What is the difference between SA516 Gr.65 and SA516 Gr.55?
- SA516 Gr.65 has higher tensile (450-585 MPa vs. 380-515 MPa) and yield (240 MPa vs. 205 MPa) than Gr.55. Gr.65 offers better impact (27J at -20°C), while Gr.55 is economical for low-stress. Check our ASTM A 516 Gr 55 page.
- What is the difference between SA516 Gr.65 and SA516 Gr.60?
- SA516 Gr.65 has higher tensile (450-585 MPa vs. 415-550 MPa) and yield (240 MPa vs. 220 MPa) than Gr.60. Gr.65 suits higher pressure (500 bar), while Gr.60 is for moderate use. Visit our ASTM A 516 Gr 60 page.
SHH STEEL SOLUTION
SHH STEEL’s ASME SA516 Gr.65 Carbon Steel Plates provide unmatched strength and reliability for pressure vessels and boilers. With precise tolerances, superior weldability, and global equivalents, we offer customized solutions. Trust SHH STEEL for your steel needs—explore our ASTM A 516 Gr 65 page for more details.
For more other grade, please check in the following: ASME SA 516/SA 516M, ASME SA 516 GR 70, ASME SA 516 GR 65, ASME SA 516 GR 60 and ASME SA 516 gr 55 Steel Plate Grade.