ASME SA240 UNS N08904 (Type 904L) stainless steel plate at SHH STEEL warehouse

ASME SA240 UNS N08904 Stainless Steel Plate

ASME SA240 UNS N08904 stainless steel plate: UNS N08904 (Type 904L) is a high-alloy austenitic grade with copper, supplied as plate, sheet and strip to ASME SA-240 / ASTM A240 (C ≤ 0.020 %, Cr 19.0–23.0 %, Ni 23.0–28.0 %, Mo 4.00–5.00 %; minimum yield 220 MPa). SHH STEEL advises on grade selection and dual certification and supplies mill-direct plate with third-party inspection, small-lot consolidation and in-house processing.
Keywords
ASME SA240 UNS N08904, SA240 N08904 plate, UNS N08904 stainless steel plate, SA-240 Type 904L plate, N08904 sheet supplier
Equivalent Grades:
EN 1.4539 X1NiCrMoCu25-20-5; JIS SUS890L; GB/T 015Cr21Ni26Mo5Cu2 (S39042) (nearest; limits differ)
Share:
Overview
Specification
Chemical Composition
Mechanical Properties
Heat Treatment
Key Characteristics
Equivalent Grades
Related Grades
Applications
Sizes and Supply Forms
Fabrication
Testing and Certificates
Buyer Concerns
Supply Notes
FAQ
Conclusion

What is ASME SA240 UNS N08904 stainless steel plate?

UNS N08904 (Type 904L) is a high-alloy austenitic steel with 19.0–23.0 % Cr, 23.0–28.0 % Ni, 4.00–5.00 % Mo and 1.00–2.00 % Cu, with carbon ≤ 0.020 %. Copper and high nickel give good resistance to sulfuric acid, and molybdenum gives pitting resistance well above 316L. Its high nickel content puts it in the UNS N08 series used for high-nickel iron-base alloys, but it is ordered as plate under SA-240 like the 300-series grades. The fully austenitic structure is tough at low temperature and essentially non-magnetic. For buyers, the practical point is that UNS N08904 (Type 904L) is ordered, tested and certified as SA-240 / A240 plate, so the purchase order, the mill test report and the plate marking must all show the UNS number and the specification edition.

This page sets out the SA-240 and A480 requirements for UNS N08904 (Type 904L) plate, sheet and strip: specification data, heat and product analysis limits, mechanical properties, heat treatment, the nearest EN, JIS and GB/T grades, sizes, testing and the documents that come with each shipment. SHH STEEL supplies N08904 plate mill-direct from long-term mill partners and advises buyers on grade selection, dual certification and inspection before the order is placed.

Every value on this page is taken from the specification named in each table; where a standard leaves a point to agreement, the page says so. SHH STEEL engineers can check a drawing or tender requirement against these limits before quotation.

UNS N08904 (Type 904L) specification data

UNS N08904 (Type 904L) appears in Table 1 (chemistry) and Table 2 (mechanical properties) of the specification. For ASME Code construction, order and certify to SA-240 for the Code edition named in the design; most mills issue dual ASTM A240 / ASME SA-240 certificates. Allowable stresses are not part of SA-240 and come from ASME Section II, Part D.

The table summarises how UNS N08904 (Type 904L) is specified and supplied:

Item Requirement / supply information
Product specification ASME SA-240/SA-240M (ASME BPVC Section II, Part A), the Code adoption of ASTM A240/A240M
General requirements ASTM A480/A480M (ASME SA-480): ordering, heat treatment, product analysis, tolerances, finish, testing, marking and certification
UNS designation UNS N08904
Type Type 904L
Steel family High-alloy austenitic stainless steel
Product forms (A480 definitions) Plate: 5.00 mm and over in thickness and over 250 mm wide. Sheet: under 5.00 mm thick and 600 mm and over wide. Strip: cold-rolled, under 5.00 mm thick and under 600 mm wide
Typical supply range Hot rolled plate 3–50 mm and cold rolled sheet 0.5–6 mm.
Width / length (typical) 1000–2000 mm wide (wider plate by mill campaign); 2000–6000 mm long, coil, or cut to size
Heat-treatment condition 1095 °C [2000 °F] minimum, then quenched in water or rapidly cooled by other means (A480 Table A1.2)
Finish Plate: hot-rolled, heat treated and pickled (essentially No. 1). Sheet: No. 1, 2D, 2B or bright annealed; polished No. 3 / No. 4 on request
Mandatory tests Heat analysis; tension test (tensile, 0.2 % yield, elongation), hardness
Optional tests (when ordered) PMI, ultrasonic testing, Charpy impact (S1), 1 % offset yield (S3), intergranular corrosion to A262 Practice E
Dimensional tolerances A480 Annex A2 (inch-pound) or Annex A3 (A480M, SI), by production route and product width
Marking Specification, type or UNS designation, material identification (heat) number and manufacturer’s name or mark (A480 25.1)
Certificates Material test report to A480 Section 8; EN 10204 3.1 as standard; EN 10204 3.2 with third-party witness on request

Under A480 1.2, the product specification prevails over A480 when the two conflict, and a more stringent purchase-order requirement prevails over both. The purchase order cannot waive a test or relax a requirement of either specification. State the unit system (A240 or A240M) on the order.

UNS N08904 chemical composition: heat analysis and product analysis

The heat analysis limits for UNS N08904 (Type 904L) are below, in percent by mass (maximum unless a range or minimum is shown), from A240/SA-240 Table 1:

Grade C Mn P S Si Cr Ni Mo N Cu
UNS N08904 0.020 2.00 0.045 0.035 1.00 19.0–23.0 23.0–28.0 4.00–5.00 0.10 1.00–2.00

Heat analysis versus product analysis. The heat (melt or ladle) analysis is made by the steel producer on a sample taken during pouring or from in-process product (A480 6.2). It must meet the Table 1 limits exactly, and it is the analysis reported on the mill test report. A product (check) analysis is an analysis of the finished plate, which the purchaser may make to verify its identity (A480 7.1). Because of segregation and sampling, it is allowed to fall slightly outside the Table 1 limits by the tolerances of A480 Table A1.1. These tolerances do not apply to the heat analysis. The comparison below applies them to N08904:

Element Heat (melt/ladle) analysis, % — A240/SA-240 Table 1 Product analysis tolerance — A480/SA-480 Table A1.1 Permitted product (check) analysis, %
Carbon (C) 0.020 max 0.005 over max ≤ 0.025
Manganese (Mn) 2.00 max 0.04 over max ≤ 2.04
Phosphorus (P) 0.045 max 0.010 over max ≤ 0.055
Sulfur (S) 0.035 max 0.005 over max ≤ 0.040
Silicon (Si) 1.00 max 0.05 over max ≤ 1.05
Chromium (Cr) 19.0–23.0 0.25 under min / 0.25 over max 18.75–23.25
Nickel (Ni) 23.0–28.0 0.20 under min / 0.20 over max 22.80–28.20
Molybdenum (Mo) 4.00–5.00 0.10 under min / 0.10 over max 3.90–5.10
Nitrogen (N) 0.10 max 0.01 over max ≤ 0.11
Copper (Cu) 1.00–2.00 0.10 under min / 0.10 over max 0.90–2.10

How to read the table: the tolerance band is chosen by the specified limit, or by the maximum of a specified range, and is applied below the minimum and above the maximum. Under A480 7.2, several determinations of one element in a heat must show the same tendency; they may not fall both above and below the range. Where a requirement is a ratio, such as Ti ≥ 5×(C+N), the ratio found by product analysis must be at least 0.90× the specified minimum (A480 A1.1).

A480 6.3.1 also sets allowances for unspecified copper, molybdenum, titanium and niobium (Cu 0.75 %, Mo 0.75 %, Ti 0.10 %, Nb 0.10 %). These prevent one grade being certified when it actually meets another grade’s composition. Handheld XRF PMI confirms alloy identity but cannot measure carbon or nitrogen. When an L, H or nitrogen-controlled grade must be proven, a laboratory or spark-OES product analysis is needed.

What the main elements do in N08904:

  • Carbon ≤ 0.020 %: low carbon limits chromium carbide precipitation in weld heat-affected zones.
  • Chromium 19.0–23.0 %: forms the passive film that makes the steel stainless; higher chromium improves resistance to corrosion and oxidation.
  • Nickel 23.0–28.0 %: stabilises the austenite and improves toughness and ductility.
  • Molybdenum 4.00–5.00 %: improves resistance to pitting and crevice corrosion in chloride media.
  • Copper 1.00–2.00 %: improves resistance in reducing acids such as sulfuric acid.

Indicative PREN (Cr + 3.3 Mo + 16 N) calculated by SHH STEEL from the minimum Table 1 values is about 32.2. This is not a specification requirement; the PREN of a given heat is calculated from its actual analysis and is usually higher.

UNS N08904 mechanical properties (annealed)

Room-temperature tensile and hardness requirements for UNS N08904 (Type 904L) in the annealed condition (ASTM A240/A240M Table 2):

Condition / thickness Tensile strength, min Yield strength 0.2 %, min Elongation in 50 mm, min Hardness, max Cold bend
All thicknesses 490 MPa [71 ksi] 220 MPa [31 ksi] 35 % 90 HRBW not required

Yield strength is the 0.2 % offset value; 1 % offset yield can be reported when ordered under Supplementary Requirement S3, and Charpy impact tests under Supplementary Requirement S1.

Bend tests are not required for austenitic or duplex grades.

Tension specimens are taken from finished material and tested to ASTM A370 (A480 17.1). For cut-length plate, A480 16.1.2 requires one tension test and one or more hardness tests for each 100 pieces or fewer of the same heat and nominal thickness heat treated together; coil product is tested from each coil. Retests follow A370 and A480 Section 20.

The values in Table 2 are room-temperature minimums for acceptance. Design strength at temperature, including allowable stresses for ASME Code calculations, comes from ASME Section II, Part D and the construction code, not from SA-240.

Heat treatment of UNS N08904 plate

Heat treatment for UNS N08904 (Type 904L): 1095 °C [2000 °F] minimum, then quenched in water or rapidly cooled by other means (A480 Table A1.2).

A480 15.1 requires the heat treatment to be a separate thermal cycle; in-process thermal cycles may not replace the annealing cycle. Material that fails a test may be re-heat-treated and resubmitted (A480 20.5).

Key characteristics of UNS N08904 (Type 904L)

UNS N08904 (Type 904L) is a high-alloy austenitic grade with copper. The points that matter most when specifying it:

  • Minimum tensile 490 MPa and yield 220 MPa; elongation 35 %.
  • A240 lists 904L as a common name, not a trademark.
  • High nickel gives good resistance to chloride stress-corrosion cracking.
  • Weld with over-alloyed or matching fillers under controlled heat input.

High nickel, molybdenum and copper give strong resistance to sulfuric and phosphoric acid and much better resistance to chloride pitting and stress-corrosion cracking than 316L. Low carbon limits sensitization during welding. Because the alloy is highly alloyed, segregation in welds matters, so low heat input and over-alloyed filler metals are usual.

UNS N08904 equivalent grades: ASTM/ASME, EN, JIS and GB/T compared

Equivalent grades are cross-references, not interchangeable specifications. Each standard sets its own element ranges, minimum properties, test methods and product-form rules, so a plate certified to one standard is only certified to another when the same heat has been tested against both and the certificate says so. SHH STEEL checks every dual- or multi-standard request against each standard line by line before confirming the order.

System Standard Designation Closeness What to check
ASME / ASTM SA-240 / A240 with A480 / SA-480 UNS N08904 (Type 904L) reference grade Specification edition required by the code or contract
EN EN 10088-2 / EN 10028-7 1.4539 X1NiCrMoCu25-20-5 nearest equivalent; not identical Steel number and name; proof strengths Rp0.2/Rp1.0 depend on product form (C, H or P) and thickness; elongation is measured on a different gauge length
JIS JIS G4304 (hot-rolled) / G4305 (cold-rolled) SUS890L commonly cross-referenced; not identical SUS designation; chemistry ranges set independently; check carbon, nitrogen and nickel against the A240 row
GB/T GB/T 4237 (hot-rolled) / GB/T 3280 (cold-rolled) 015Cr21Ni26Mo5Cu2 (S39042) commonly cross-referenced; not identical GB/T 20878 name and numeric code; the numeric code is not a UNS number even when it looks similar

European standards. EN 10088-2 covers corrosion-resisting stainless steel sheet, plate and strip for general purposes. EN 10028-7 covers flat stainless products for pressure purposes and is the flat-product standard normally used for pressure equipment in Europe. Both use a steel number (1.4xxx) and a steel name built from the composition, and many steel numbers appear in both, but confirm that the steel number is listed in the edition you need. EN values for 0.2 % and 1 % proof strength depend on product form (cold-rolled strip C, hot-rolled strip H, hot-rolled plate P) and thickness. EN elongation is measured on proportional or 80 mm gauge lengths, so it cannot be compared directly with the A240 elongation in 50 mm.

Japanese standards. JIS G4304 covers hot-rolled and JIS G4305 cold-rolled stainless plate, sheet and strip, both with SUS designations. JIS chemistry ranges are close to the AISI-type grades but are set independently, so carbon, nitrogen and nickel limits should be checked against the A240 row whenever a heat must meet both.

Chinese standards. GB/T 4237 covers hot-rolled and GB/T 3280 cold-rolled stainless plate, sheet and strip, using GB/T 20878 grade names such as 06Cr19Ni10 and numeric codes such as S30408. The numeric code is a Chinese designation and is not a UNS number, even where the digits look similar. Always state the standard next to the code on purchase orders and certificates.

Related ASTM and ASME specifications. A240 and SA-240 share the same technical content; ASME adopts a specific A240 edition for each Code edition, so Code work should name SA-240. General requirements come from A480 / SA-480. Clad plate with this cladding is ordered to A264 (Cr-Ni steel-clad plate). A666 covers annealed or cold-worked austenitic sheet, strip, plate and flat bar for structural and architectural uses; check whether the grade is listed there. Other product forms use their own specifications (pipe, forgings, bar), so check that the UNS number is listed in each one before ordering a matching set.

In practice, SHH STEEL offers dual-certified plate (for example A240 / EN 10088-2) when a mill heat is designed to meet both standards. When it cannot be, we recommend ordering to the single standard the design code requires and treating the others as reference only.

UNS N08904 (Type 904L) compared with related grades

Grades buyers most often compare with UNS N08904 (Type 904L):

The site also has pages organised by type designation for the same or closely related material: ASTM A240 Type 904L stainless steel sheet & plate, ASME SA240 904L stainless steel plate. This page is the UNS-number reference for SA-240 orders; the material is the same where the grade is the same.

All grades in this series are listed under ASME SA240/SA240M stainless steel plate and ASTM A240/A240M stainless steel plate.

Applications of SA240 UNS N08904 plate

Typical uses of UNS N08904 (Type 904L) plate, sheet and strip:

  • Sulfuric and phosphoric acid plant equipment
  • Pulp and paper bleach plant
  • Seawater-cooled heat exchangers and condensers
  • Pharmaceutical and fine-chemical vessels

The final choice should always be checked against the service medium, temperature and design code; SHH STEEL can share mill corrosion data and reference projects on request.

This grade is chosen when 316L or 317L is not resistant enough but a nickel-base alloy would cost too much. Common uses are acid service, seawater-cooled equipment and pollution-control plant. Duplex grades are a frequent alternative where their temperature limits and fabrication needs are acceptable.

UNS N08904 (Type 904L) sizes, finishes and supply forms

Size ranges below are typical mill capabilities for UNS N08904 (Type 904L), not limits set by the specification; actual availability depends on the mill campaign and is confirmed at quotation.

Item Typical supply range
Product forms Hot rolled plate 3–50 mm and cold rolled sheet 0.5–6 mm.
Width 1000, 1219, 1250, 1500, 1800, 2000 mm; wider plate by mill
Length 2000, 2438, 3000, 6000 mm, coil, or cut to size
Surface finish No.1 (hot rolled, annealed and pickled) for plate; 2B, 2D or BA for cold rolled sheet; No.4 / HL polishing on request
Tolerances ASTM A480/A480M, or tighter by agreement

For weight estimates, plate weight (kg) ≈ thickness (mm) × width (m) × length (m) × density, with density about 8.0 g/cm³ for this grade family. The mill certificate weight governs invoicing.

Plate finishes under A480 Section 13 range from heat treated with scale left on, which is used for heat-resisting service because scale impairs corrosion resistance, to blast-cleaned or pickled, which is essentially a No. 1 finish and the usual choice for corrosion service. Sheet finishes under Section 11 include No. 1, 2D (dull, good for deep drawing), 2B (smooth, moderately reflective), bright annealed, and polished No. 3, 4, 6, 7 and 8. Thickness should be ordered as a decimal or fractional dimension, not a gauge number (A480 4.1.7).

Forming, welding and heat treatment of UNS N08904

High-alloy austenitic plate forms well but work-hardens; use adequate press capacity.

Weld with low, controlled heat input and a matching or over-alloyed filler to keep corrosion resistance in the weld; avoid contamination with carbon steel.

Solution annealing follows ASTM A480/A480M; pickle and passivate after fabrication.

Repair of plate surface defects by welding is permitted unless prohibited by other specifications or the order (A480 Section 21). Defect depth may not exceed one-third of nominal thickness, and the total repaired area may not exceed 1 % of the plate surface, without the purchaser’s prior approval. Welding procedures and welders must be qualified to ASME Section IX, consumables must suit the plate, and the repaired area must be ground smooth. Buyers who do not accept weld repairs should say so on the order.

Cutting is normally by plasma, waterjet or abrasive saw; avoid oxy-fuel cutting on stainless steel. Keep stainless plate away from carbon-steel dust and tools during handling and fabrication, because embedded iron causes rust staining. Pickling and passivation after fabrication restore the passive surface.

Testing, inspection and certificates for N08904 plate

Each heat is tested to SA-240 / A240 and ASTM A480/A480M: heat analysis, tension tests and hardness, plus the surface and dimensional checks for the product form.

Mill test certificates to EN 10204 3.1 are standard. EN 10204 3.2 certificates with third-party witness (TUV, ABS, CCS, BV, DNV, LR or an inspector named by the buyer) can be arranged, together with optional tests such as PMI, intergranular corrosion, ultrasonic testing and Charpy impact (Supplementary Requirement S1).

Under A480 18.2.1, the intergranular corrosion test (Practice E of A262) is run only when the order specifies it, although all non-H austenitic chromium-nickel types are expected to pass it. Low-carbon and stabilised types are tested on sensitised specimens, other types in the as-shipped condition.

Plate is marked in two places near the ends, or line-marked along one edge, with the specification, type or UNS number, heat number and manufacturer; material under 6.4 mm is not die-stamped (A480 25.1). The supplier must pass on a copy of the original mill test report (A480 8.4), and test-based rejections must be reported within 60 working days of receipt (A480 23.1).

Common buyer concerns and SHH STEEL solutions

The concerns below come up most often when buyers source UNS N08904 (Type 904L) plate from China, together with how SHH STEEL deals with each one.

Buyer Concern SHH STEEL Solution
Fake material or certificates Each heat can be checked by TUV, ABS, CCS or another class society as third-party witness, and partner laboratories run PMI, chemical and mechanical tests against the order. Third-party witness and EN 10204 3.2 certificates available.
Unsafe deposit TT and LC are both accepted, including TT + LC combinations. For large projects the buyer can sign directly with the mill, and SHH STEEL handles coordination and documents for a small service fee.
Small orders below mill MOQ Small quantities are consolidated with other customers’ orders of the same grade and thickness, so even lots below the mill MOQ are rolled as genuine mill production with full traceability.
Slow delivery Dedicated staff chase the mill delivery schedule and report progress at melting, rolling, heat treatment, testing and packing, so delays are seen early.
Processing needs Our own workshop provides cutting, bevelling, machining to drawings and surface pretreatment as value-added services, so plates arrive ready for fabrication.

How to order UNS N08904 plate from SHH STEEL

A480 4.1 makes the purchaser responsible for stating every requirement. A complete enquiry for N08904 plate should include:

  • Quantity (weight and number of pieces).
  • Specification and edition: ASME SA-240 or ASTM A240 (with edition) and A480; add “M” for SI units.
  • Type or UNS designation: UNS N08904 (Type 904L).
  • Condition (hot-rolled or cold-rolled, annealed or heat treated) and finish; for polished finishes, one or both sides.
  • Form (plate, sheet or strip) and dimensions (thickness, width and length, in the same units).
  • Supplementary requirements and special tests (Charpy, intergranular corrosion, phase tests, UT, PMI).
  • Inspection document (EN 10204 3.1 or 3.2), third-party inspector, marking and packing requirements.

SHH STEEL works as a sourcing and supply partner with long-term mill relationships. We help select the grade, check dual-certification options, consolidate small lots, follow production at the mill and process plates in our own workshop before shipment. Payment by TT or LC is accepted.

For N08904, the SHH STEEL team can also share recent mill test reports for reference, confirm which thicknesses are in the current rolling campaign and propose a cutting plan that reduces scrap. Send your enquiry with drawings or a cutting list and we will reply with a quotation, lead time and inspection plan.

FAQ

Is 904L a stainless steel or a nickel alloy?
N08904 carries a UNS N number because of its high nickel, but A240 lists it with the austenitic stainless steels. It is iron-based, with 23.0–28.0 % nickel.
Is 904L better than 316L?
In sulfuric acid, phosphoric acid and chloride environments, yes. N08904 has 4.00–5.00 % Mo, 1.00–2.00 % Cu and much more nickel than S31603, so it costs more but lasts longer in these media.
What is the EN equivalent of N08904?
EN 1.4539 (X1NiCrMoCu25-20-5) is the nearest EN grade. Its ranges overlap with A240 but are not identical, so dual certification needs a heat that meets both.
Where can I buy ASME SA240 UNS N08904 plate in small quantities?
SHH STEEL consolidates small orders of N08904 with other customers’ orders of the same grade, so lots below the mill MOQ can still be placed against mill production. Cut-to-size pieces can be supplied from our workshop.
What certificates come with N08904 stainless steel plate?
Plates are supplied with EN 10204 3.1 mill test certificates to SA-240 / A240. Third-party witness and EN 10204 3.2 certificates available, issued with TUV, ABS, CCS or another nominated inspector.
What is the lead time for N08904 plate from China?
Lead time depends on the mill rolling schedule, thickness and the tests ordered, and is confirmed with the quotation. Dedicated SHH STEEL staff follow the mill schedule and report progress until shipment.

Conclusion

ASME SA240 UNS N08904 Stainless Steel Plate is ordered as UNS N08904 (Type 904L), a high-alloy austenitic grade with copper. Specify the standard and edition, the UNS number, the inspection document and any supplementary tests on the order so the certificate can be checked line by line. SHH STEEL supports the order from grade check to delivery, and you can contact SHH STEEL for a quotation, mill-direct supply and processing to your drawings.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X