ASME SA240 UNS N08811 Stainless Steel Plate at SHH STEEL warehouse

ASME SA240 UNS N08811 Stainless Steel Plate

ASME SA240 UNS N08811 Stainless Steel Plate: iron-nickel-chromium heat-resistant grade to ASME SA-240/SA-240M, hot-rolled plate from stock in China. SHH STEEL supplies mill-direct material with EN 10204 3.1/3.2 certificates, third-party inspection and cutting to size.
Keywords
SA240 UNS N08811 plate, N08811 plate, N08811 stainless plate supplier, ASME SA-240/SA-240M N08811, N08811 plate stock China
Equivalent Grades:
EN 1.4959 X8NiCrAlTi32-21 (nearest); EN 1.4876 X10NiCrAlTi32-21 (nearest)
Share:
Overview
Specification
Chemical Composition
Mechanical Properties
Performance
Grade Selection
Heat Treatment
Surface Finishes
Tolerances
Stock
Equivalent Grades
Related Grades
Applications and Fabrication
Testing and Inspection
Specification Mistakes
Buyer Concerns
How to Order
FAQ
Conclusion

What is ASME SA240 UNS N08811 Stainless Steel Plate?

Technical reviewer: Jack · Updated: 2026-10-21

Equivalent grades: UNS N08811 ≈ EN 1.4959 X8NiCrAlTi32-21 (nearest) ≈ EN 1.4876 X10NiCrAlTi32-21 (nearest).

UNS N08811 is a iron-nickel-chromium heat-resistant grade. N08811 is the high-temperature version of the 32Ni-21Cr Fe-Ni-Cr family (N08800 / N08810 / N08811). Its carbon range of 0.06–0.10 %, Al + Ti of 0.85–1.20 % and a coarse grain from a high solution-anneal temperature give the highest creep-rupture strength of the three, for service above about 600 °C.

ASME SA-240 is the Boiler and Pressure Vessel Code version of ASTM A240, published in Section II Part A. It is ordered when plate will be used in Code construction such as Section VIII pressure vessels, Section I boilers or B31.3 piping components made from plate. Chemistry and tensile limits are the same as in A240, but the certificate and marking must state SA-240 so the Authorized Inspector can accept the material.

This page sets out the ASME SA-240/SA-240M requirements for UNS N08811 plate: specification summary, chemistry, mechanical properties, high-temperature behaviour, heat treatment, finishes and tolerances, current stock, equivalents, fabrication and testing. SHH STEEL supplies it mill-direct from China with EN 10204 3.1 certificates, optional third-party inspection and in-house cutting.

UNS N08811 plate: specification summary

Item UNS N08811 data
Standard ASME BPVC Section II Part A, SA-240/SA-240M (identical with or adapted from ASTM A240/A240M)
General requirements SA-480/SA-480M
Product form plate 5.00 mm (3/16 in.) and over; sheet and strip also covered
Typical thickness 5–80 mm hot-rolled; heavier by mill enquiry
Widths 1500, 2000, 2500 mm; wider by enquiry
Lengths 6000 mm standard; up to 12000 mm or cut to size
Finish No.1 (hot-rolled, annealed and pickled)
Marking SA-240 with grade, heat and plate number; dual A240/SA-240 marking common
Certificates EN 10204 3.1 stating SA-240; 3.2 with third-party or AI witness on request
Grade family heat-resistant

Size range. Plate is produced on Steckel or reversing mills from about 5 mm up to 80–100 mm depending on grade, with widths of 1500–2500 mm and lengths up to 12 m; thinner plate of 3–12 mm is often cut from hot-rolled coil. Very heavy or wide plates, and plates with tight flatness, should be confirmed before ordering. UNS N08811 is a specialty grade made by a limited number of mills in campaign rolling. Stock covers the common sizes listed below; for project quantities or unusual sizes, plan for a mill campaign and reserve the heat early.

Chemical composition of UNS N08811 (ASME SA-240/SA-240M)

Element wt %
C 0.06–0.10
Si 1.00 max
Mn 1.50 max
P 0.040 max
S 0.015 max
Cr 19.0–23.0
Ni 30.0–35.0
Cu 0.75 max
Ti 0.25–0.60
Al 0.25–0.60
Fe 39.5 min

Single values are maximums unless marked min. Ranges are heat (cast) analysis limits.

For heat-resistant grades the key elements are chromium (oxide scale), nickel (austenite stability, carburisation resistance) and silicon, aluminium or rare earths where present (scale adhesion). Sulfur and phosphorus are kept low to protect hot ductility and weldability.

Mechanical properties of UNS N08811 plate

Condition / thickness Tensile strength, min Yield strength 0.2 %, min Elongation in 50 mm, min Hardness, max
all thicknesses 450 MPa (65 ksi) 170 MPa (25 ksi) 30 % —

The minimum proof strength is 170 MPa. For high-temperature design, room-temperature values are only an acceptance check; use creep and stress-rupture data from the standard’s informative annexes or the ASME allowable stresses where Code rules apply. Tension tests are taken in the direction stated in the standard; where a hardness limit is given, it is a maximum that confirms correct annealing.

High-temperature behaviour of UNS N08811

This is a heat-resistant grade: it is selected for oxidation resistance, strength and structural stability at high temperature rather than for wet corrosion. Chromium forms the protective oxide, nickel stabilises the austenite against thermal cycling and carburisation, and silicon, rare earths or nitrogen, where present, improve scale adhesion or creep strength. The maximum useful temperature in air depends on atmosphere, thermal cycling and load, so published scaling temperatures are a guide, not a design value.

Sulfur-bearing gases attack high-nickel alloys, while carburising or nitriding atmospheres favour higher nickel; vanadium-bearing ash and molten salts need special evaluation. Long exposure in the 600–900 °C range can form sigma phase in high-chromium grades and reduce room-temperature toughness, which matters for parts that are cleaned or repaired cold. Creep-rupture values are given in the standard’s informative annexes or by the mill and should be used for design instead of room-temperature strength.

How UNS N08811 compares with related grades

Grade Cr Ni Mo N PREN (min) YS / Rp0.2 min, MPa
UNS N08811 19.0–23.0 30.0–35.0 — — — 170
UNS S30815 20.0–22.0 10.0–12.0 — 0.14–0.20 — 310
UNS S30900 22.0–24.0 12.0–15.0 — — — 205
UNS S31000 24.0–26.0 19.0–22.0 — — — 205
UNS N08330 17.0–20.0 34.0–37.0 — — — 205

Choose UNS N08811 when oxidation resistance and strength at temperature drive the selection. For wet corrosion at room temperature, a low-carbon corrosion-resistant grade is usually a better choice, and in sulfur-rich gases a lower-nickel grade may outperform a high-nickel one.

The table uses specification limits, not typical mill values, so it shows the guaranteed position of each grade. Final selection should also consider product availability in the thickness you need, welding consumables, and the inspection requirements of your project.

Heat treatment and delivery condition of UNS N08811

Heat treatment: 1150 °C min, rapid cooling; grain size ASTM 5 or coarser.

Heat-resistant plate is supplied solution annealed. For high-temperature service, a coarser grain size improves creep strength, while a finer grain improves fatigue and room-temperature ductility; where it matters, state the grain-size requirement on the order. Stress relief is not normally needed.

Surface finishes for UNS N08811 plate

Plate to SA-240 is normally supplied with a No.1 finish: hot rolled, solution annealed and pickled, with a matt grey surface. Shot-blasted and pickled surfaces are the norm on heavy plate. Ground or polished faces, and plates with protective film for the process side, can be produced after delivery in our workshop. Surface defects are judged against the A480/SA-480 workmanship clause; for vessel internals the purchaser may add surface-roughness or cleanliness requirements.

Dimensions, tolerances and flatness

Thickness, width, length, flatness and camber tolerances follow SA-480/A480 tables for hot-rolled plate; ordered thickness is a minimum unless the order states nominal. For pressure parts, the thickness at any point must not fall below the ordered minimum, so heavy plate is often ordered with a small plus allowance. Flatness of thin plate cut from coil should be checked after cutting. Mill edge, sheared, plasma or waterjet-cut edges and bevelling for welding are available.

Code use of SA-240 plate. Before welding, the manufacturer must identify the P-Number and group number of N08811 from ASME Section IX (QW/QG-422) for the welding procedure qualification, and the designer takes allowable stresses from Section II Part D. Impact-test exemptions for austenitic and duplex plate are given in Section VIII Division 1 (UHA-51) and depend on grade, thickness and minimum design metal temperature, so cryogenic or low-temperature duty should be stated when you order. For heavy plate, ultrasonic examination to SA-578 and PMI of each plate are common supplementary requirements. Ask for the plate number to be hard-stamped or stencilled so traceability survives cutting.

UNS N08811 plate stock in China

Thickness (mm) Width (mm) Length (mm) Finish Approx. quantity Location
6 1500 / 2000 6000 No.1 100+ t China
8 1500 / 2000 6000 No.1 100+ t China
10 2000 6000 No.1 100+ t China
12 2000 6000 No.1 100+ t China
16 2000 / 2500 6000 No.1 100+ t China
20 2000 / 2500 6000 / 8000 No.1 100+ t China
30 2000 / 2500 6000 No.1 100+ t China

Quantities are approximate and stock changes daily. Send your size list for current availability; other thicknesses, widths and cut sizes can be supplied from mill production.

Packing and logistics. Plate is bundled on steel or wooden skids with steel bands and edge protection, typically 3–8 t per bundle, and marked with heat and plate numbers. Cut pieces are crated. Heavy and wide plate ships in open-top or flat-rack containers or by break-bulk; we send loading photos with the shipping documents.

UNS N08811 equivalents in other standards

Standard Designation Comment
EN 1.4959 X8NiCrAlTi32-21 nearest grade only; limits differ, check before substituting
EN 1.4876 X10NiCrAlTi32-21 nearest grade only; limits differ, check before substituting

Equivalents are close, not identical. When a project names one standard, order to that standard or ask for multiple certification and check every limit on the certificate.

Related grades by alloy family

Heat-resistant

Heat-resistant grades ranked by chromium, nickel and silicon: SA-240 S30908, SA-240 S31008, SA-240 S30909, SA-240 S31009, 1.4948 (EN 10028-7), 1.4950 (EN 10028-7), 1.4951 (EN 10028-7), SA-240 S30815, SA-240 S30900, SA-240 S31000, SA-240 N08330, 1.4845 (EN 10095).

Same grade, other specification

A240 N08811.

Applications, forming and welding of UNS N08811

Typical uses: ethylene and steam-methane reformer furnace parts, pigtails and headers, heat-treatment equipment, and high-temperature heat exchangers.

Heat-resistant plate is usually cut by plasma or waterjet, formed hot or cold, and welded with matching heat-resistant consumables. Cut by plasma, laser or waterjet and remove heat tint by pickling or grinding. For welding use a matching heat-resistant filler such as ER309, ER310 or ERNiCr-3 according to the service temperature. Keep the weld area clean and free of carbon-steel contamination, and pickle and passivate after welding where corrosion resistance matters.

Fabrication at temperature. Design furnace parts to allow for thermal expansion, which is about 1.5 times that of carbon steel, and avoid sharp corners where scale can spall. Welds should be full penetration where they carry load at temperature. For high-silicon grades, use low heat input to limit hot cracking. After long service, high-chromium plate may be embrittled by sigma phase, so repair welding of old parts needs care and sometimes a solution anneal first.

Certificates, testing and receiving inspection

Every delivery carries a mill certificate to ASME SA-480/SA-480M with heat analysis, tensile results and hardness, and the grade and standard as ordered. Supplementary tests we can arrange: PMI, grain-size measurement (ASTM E112) where the grade requires it, elevated-temperature tensile tests by agreement, and ultrasonic testing of heavy plate. Third-party witness by SGS, BV, TÜV, DNV, ABS or LR is available with EN 10204 3.2 certificates.

On receipt, check marking and heat number against the certificate, measure thickness at several points and confirm the finish and edge condition before cutting.

Common mistakes when specifying UNS N08811

  • Selecting by room-temperature strength instead of creep data.
  • Substituting a low-carbon corrosion grade (for example 310S for 310) without checking creep strength.
  • Ignoring the atmosphere: sulfur, carburising gas and vanadium ash change the ranking of grades.

Each of these can be avoided by writing the requirement into the purchase order and checking it on the certificate before the material is cut.

Sourcing UNS N08811: buyer concerns and SHH STEEL solutions

Concern How SHH STEEL handles it
Wrong grade substitution (for example 304 for 309/310) PMI of every plate before dispatch
Distortion of large furnace panels levelled plate and cut-to-size blanks with low-stress cutting
Small quantities across many sizes mixed thicknesses and grades combined in one shipment
Cutting and edge preparation in-house shearing, plasma, laser and waterjet cutting, bevelling
Delivery delays weekly production and shipping updates with photos

How to order UNS N08811 plate

State the standard and edition (ASME SA-240/SA-240M), the grade (UNS N08811), thickness, width and length or coil, finish, quantity, tolerance class, any added chemistry limits, the supplementary tests and acceptance values from your specification, the certificate type and inspection agency, and packing. Send the list to SHH STEEL and we will reply with price, available stock and lead time.

FAQ

What is the difference between SA-240 and A240 for N08811?
The chemistry and tensile requirements are the same. SA-240 is the ASME Code edition, so plate for pressure vessels must be certified and marked SA-240; dual-certified A240/SA-240 plate covers both.
Is UNS N08811 equivalent to EN 1.4959 X8NiCrAlTi32-21?
They are the nearest match, but limits differ; check each element and the property table before substituting.
What is the maximum service temperature of UNS N08811?
It depends on the atmosphere, thermal cycling and load. Published scaling temperatures are a guide for oxidation in air only; for load-bearing parts use creep-rupture data.
Can I order small quantities or cut sizes?
Yes. We combine mixed thicknesses and grades into one shipment and cut plate and sheet to size in our workshop.
Which certificates and tests can you provide?
Every order ships with a mill certificate (EN 10204 3.1 type) showing heat analysis and mechanical tests. Supplementary tests and 3.2 certificates with SGS, BV, TÜV or another agency are available by agreement.

Conclusion

UNS N08811 plate should be ordered with the points the standard leaves open written into the contract: finish, tolerance class, any extra chemistry limits and the supplementary tests your application needs. With those fixed, stock material from China is a fast and reliable route.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X