EN 10095 X10NiCrAlTi32-21 1.4876 Heat Resistant Steel Plate at SHH STEEL warehouse

EN 10095 X10NiCrAlTi32-21 1.4876 Heat Resistant Steel Plate

EN 10095 X10NiCrAlTi32-21 1.4876 Heat Resistant Steel Plate: heat-resistant grade to EN 10095, hot-rolled plate from stock in China. SHH STEEL supplies mill-direct material with EN 10204 3.1/3.2 certificates, third-party inspection and cutting to size.
Keywords
1.4876 heat resistant plate, 1.4876 plate, 1.4876 stainless plate supplier, EN 10095 1.4876, 1.4876 plate stock China
Equivalent Grades:
UNS N08800 (close); UNS N08810 (close)
Share:
Overview
Specification
Chemical Composition
Mechanical Properties
Performance
Grade Selection
Heat Treatment
Surface Finishes
Tolerances
Stock
Equivalent Grades
Related Grades
Applications and Fabrication
Testing and Inspection
Specification Mistakes
Buyer Concerns
How to Order
FAQ
Conclusion

What is EN 10095 X10NiCrAlTi32-21 1.4876 Heat Resistant Steel Plate?

Technical reviewer: Jack · Updated: 2026-10-21

Equivalent grades: 1.4876 X10NiCrAlTi32-21 ≈ UNS N08800 (close) ≈ UNS N08810 (close).

1.4876 X10NiCrAlTi32-21 is a heat-resistant grade. 1.4876 is the EN designation of the 32Ni-21Cr-Al-Ti iron-nickel-chromium alloy family. It resists oxidation and carburisation up to about 1100 °C and keeps a stable austenitic structure without sigma formation, so it is used for long-term high-temperature service.

EN 10095 is the European standard for heat-resisting steels and nickel alloys. Unlike EN 10088-2, which is aimed at corrosion resistance, EN 10095 covers grades chosen for oxidation resistance and strength above about 550 °C, and gives informative scaling temperatures and creep data. Plate is supplied solution annealed and descaled.

This page sets out the EN 10095 requirements for 1.4876 X10NiCrAlTi32-21 plate: specification summary, chemistry, mechanical properties, high-temperature behaviour, heat treatment, finishes and tolerances, current stock, equivalents, fabrication and testing. SHH STEEL supplies it mill-direct from China with EN 10204 3.1 certificates, optional third-party inspection and in-house cutting.

1.4876 X10NiCrAlTi32-21 plate: specification summary

Item 1.4876 X10NiCrAlTi32-21 data
Standard EN 10095:1999, heat resisting steels and nickel alloys
Product forms hot-rolled plate, hot- and cold-rolled strip and sheet, bars and sections
Delivery condition solution annealed (austenitic) or annealed (ferritic), descaled
Typical thickness 0.5–6 mm cold rolled; 3–80 mm hot-rolled plate
Dimensions and tolerances EN 10029, EN 10051, EN ISO 9445
Required tests cast analysis, tensile test at room temperature
Inspection documents EN 10204 3.1 or 3.2
Grade family heat-resistant

Size range. Plate is produced on Steckel or reversing mills from about 5 mm up to 80–100 mm depending on grade, with widths of 1500–2500 mm and lengths up to 12 m; thinner plate of 3–12 mm is often cut from hot-rolled coil. Very heavy or wide plates, and plates with tight flatness, should be confirmed before ordering. 1.4876 X10NiCrAlTi32-21 is a specialty grade made by a limited number of mills in campaign rolling. Stock covers the common sizes listed below; for project quantities or unusual sizes, plan for a mill campaign and reserve the heat early.

Chemical composition of 1.4876 X10NiCrAlTi32-21 (EN 10095)

Element wt %
C 0.12 max
Si 1.00 max
Mn 2.00 max
P 0.030 max
S 0.015 max
Cr 19.0–23.0
Ni 30.0–34.0
Ti 0.15–0.60
Al 0.15–0.60

Single values are maximums unless marked min. Ranges are heat (cast) analysis limits.

For heat-resistant grades the key elements are chromium (oxide scale), nickel (austenite stability, carburisation resistance) and silicon, aluminium or rare earths where present (scale adhesion). Sulfur and phosphorus are kept low to protect hot ductility and weldability.

Mechanical properties of 1.4876 X10NiCrAlTi32-21 plate

Product form / thickness Rp0.2 min, MPa Rm, MPa A min, % (flat products, a > 3 mm)
flat products ≤ 75 mm, +AT 170 450–680 30

The minimum proof strength is 170 MPa. For high-temperature design, room-temperature values are only an acceptance check; use creep and stress-rupture data from the standard’s informative annexes or the ASME allowable stresses where Code rules apply. Tension tests are taken in the direction stated in the standard; where a hardness limit is given, it is a maximum that confirms correct annealing.

High-temperature behaviour of 1.4876 X10NiCrAlTi32-21

This is a heat-resistant grade: it is selected for oxidation resistance, strength and structural stability at high temperature rather than for wet corrosion. Chromium forms the protective oxide, nickel stabilises the austenite against thermal cycling and carburisation, and silicon, rare earths or nitrogen, where present, improve scale adhesion or creep strength. The maximum useful temperature in air depends on atmosphere, thermal cycling and load, so published scaling temperatures are a guide, not a design value.

Sulfur-bearing gases attack high-nickel alloys, while carburising or nitriding atmospheres favour higher nickel; vanadium-bearing ash and molten salts need special evaluation. Long exposure in the 600–900 °C range can form sigma phase in high-chromium grades and reduce room-temperature toughness, which matters for parts that are cleaned or repaired cold. Creep-rupture values are given in the standard’s informative annexes or by the mill and should be used for design instead of room-temperature strength.

How 1.4876 X10NiCrAlTi32-21 compares with related grades

Grade Cr Ni Mo N PREN (min) YS / Rp0.2 min, MPa
1.4876 X10NiCrAlTi32-21 19.0–23.0 30.0–34.0 — — — 170
1.4845 X8CrNi25-21 24.0–26.0 19.0–22.0 — 0.11 max — 210
1.4828 X15CrNiSi20-12 19.0–21.0 11.0–13.0 — 0.11 max — 230
1.4833 X12CrNi23-13 22.0–24.0 12.0–14.0 — 0.11 max — 210
1.4835 X9CrNiSiNCe21-11-2 20.0–22.0 10.0–12.0 — 0.12–0.20 — 310

Choose 1.4876 X10NiCrAlTi32-21 when oxidation resistance and strength at temperature drive the selection. For wet corrosion at room temperature, a low-carbon corrosion-resistant grade is usually a better choice, and in sulfur-rich gases a lower-nickel grade may outperform a high-nickel one.

The table uses specification limits, not typical mill values, so it shows the guaranteed position of each grade. Final selection should also consider product availability in the thickness you need, welding consumables, and the inspection requirements of your project.

Heat treatment and delivery condition of 1.4876 X10NiCrAlTi32-21

Heat treatment: 1050–1150 °C (+AT), water or air.

Heat-resistant plate is supplied solution annealed. For high-temperature service, a coarser grain size improves creep strength, while a finer grain improves fatigue and room-temperature ductility; where it matters, state the grain-size requirement on the order. Stress relief is not normally needed.

Surface finishes for 1.4876 X10NiCrAlTi32-21 plate

Heat-resistant plate is supplied hot rolled, solution annealed and pickled (1D), or mechanically descaled (1E). Thin gauges are available cold rolled in 2D or 2B. Because the steel is used in furnaces, surface finish matters less than flatness and edge condition; ask for levelled plate when parts will be laser cut or welded into large panels.

Dimensions, tolerances and flatness

Dimensional tolerances follow EN 10029 for plate, EN 10051 for hot-rolled strip and sheet, and EN ISO 9445 for cold-rolled material. Large furnace panels are sensitive to residual stress and flatness; specify flatness class S (special) on EN 10029 plate where needed.

Design data in EN 10095. The room-temperature properties in the standard are acceptance values. For design, EN 10095 gives informative data: the scaling temperature in air, typical elevated-temperature strength and creep-rupture values. These are useful for selecting a grade, but the standard does not guarantee them, so for load-bearing furnace parts the designer should apply safety factors and, where available, use mill test data at temperature. For pressure equipment, EN 10028-7 lists some creep-resistant austenitic grades with guaranteed elevated-temperature properties.

1.4876 X10NiCrAlTi32-21 plate stock in China

Thickness (mm) Width (mm) Length (mm) Finish Approx. quantity Location
6 1500 / 2000 6000 1D 100+ t China
8 1500 / 2000 6000 1D 100+ t China
10 2000 6000 1D 100+ t China
12 2000 6000 1D 100+ t China
16 2000 / 2500 6000 1D 100+ t China
20 2000 / 2500 6000 / 8000 1D 100+ t China
30 2000 / 2500 6000 1D 100+ t China

Quantities are approximate and stock changes daily. Send your size list for current availability; other thicknesses, widths and cut sizes can be supplied from mill production.

Packing and logistics. Plate is bundled on steel or wooden skids with steel bands and edge protection, typically 3–8 t per bundle, and marked with heat and plate numbers. Cut pieces are crated. Heavy and wide plate ships in open-top or flat-rack containers or by break-bulk; we send loading photos with the shipping documents.

1.4876 X10NiCrAlTi32-21 equivalents in other standards

Standard Designation Comment
ASTM / UNS UNS N08800 close match; one or more limits (usually C, Si or N) differ
ASTM / UNS UNS N08810 close match; one or more limits (usually C, Si or N) differ

Equivalents are close, not identical. When a project names one standard, order to that standard or ask for multiple certification and check every limit on the certificate.

Related grades by alloy family

Applications, forming and welding of 1.4876 X10NiCrAlTi32-21

Typical uses: petrochemical furnace components, heat-treatment equipment, steam generators, heat-exchanger parts, and sheathing.

Heat-resistant plate is usually cut by plasma or waterjet, formed hot or cold, and welded with matching heat-resistant consumables. Cut by plasma, laser or waterjet and remove heat tint by pickling or grinding. For welding use a matching heat-resistant filler such as ER309, ER310 or ERNiCr-3 according to the service temperature. Keep the weld area clean and free of carbon-steel contamination, and pickle and passivate after welding where corrosion resistance matters.

Fabrication at temperature. Design furnace parts to allow for thermal expansion, which is about 1.5 times that of carbon steel, and avoid sharp corners where scale can spall. Welds should be full penetration where they carry load at temperature. For high-silicon grades, use low heat input to limit hot cracking. After long service, high-chromium plate may be embrittled by sigma phase, so repair welding of old parts needs care and sometimes a solution anneal first.

Certificates, testing and receiving inspection

Every delivery carries a mill certificate to EN 10095 with heat analysis, tensile results and hardness, and the grade and standard as ordered. Supplementary tests we can arrange: PMI, grain-size measurement (ASTM E112) where the grade requires it, elevated-temperature tensile tests by agreement, and ultrasonic testing of heavy plate. Third-party witness by SGS, BV, TÜV, DNV, ABS or LR is available with EN 10204 3.2 certificates.

On receipt, check marking and heat number against the certificate, measure thickness at several points and confirm the finish and edge condition before cutting.

Common mistakes when specifying 1.4876 X10NiCrAlTi32-21

  • Selecting by room-temperature strength instead of creep data.
  • Substituting a low-carbon corrosion grade (for example 310S for 310) without checking creep strength.
  • Ignoring the atmosphere: sulfur, carburising gas and vanadium ash change the ranking of grades.

Each of these can be avoided by writing the requirement into the purchase order and checking it on the certificate before the material is cut.

Sourcing 1.4876 X10NiCrAlTi32-21: buyer concerns and SHH STEEL solutions

Concern How SHH STEEL handles it
Wrong grade substitution (for example 304 for 309/310) PMI of every plate before dispatch
Distortion of large furnace panels levelled plate and cut-to-size blanks with low-stress cutting
Small quantities across many sizes mixed thicknesses and grades combined in one shipment
Cutting and edge preparation in-house shearing, plasma, laser and waterjet cutting, bevelling
Delivery delays weekly production and shipping updates with photos

How to order 1.4876 X10NiCrAlTi32-21 plate

State the standard and edition (EN 10095), the grade (1.4876 X10NiCrAlTi32-21), thickness, width and length or coil, finish, quantity, tolerance class, any added chemistry limits, the supplementary tests and acceptance values from your specification, the certificate type and inspection agency, and packing. Send the list to SHH STEEL and we will reply with price, available stock and lead time.

FAQ

Why order 1.4876 to EN 10095 instead of EN 10088-2?
EN 10095 is the standard for heat-resisting steels. It defines the chemistry and properties used for high-temperature design and gives informative scaling and creep data; 1.4876 is a heat-resisting grade and is ordered to EN 10095.
Is 1.4876 X10NiCrAlTi32-21 equivalent to UNS N08800?
They are close; one or more limits differ, so check the certificate against both standards or order dual certification.
What is the maximum service temperature of 1.4876 X10NiCrAlTi32-21?
It depends on the atmosphere, thermal cycling and load. Published scaling temperatures are a guide for oxidation in air only; for load-bearing parts use creep-rupture data.
Can I order small quantities or cut sizes?
Yes. We combine mixed thicknesses and grades into one shipment and cut plate and sheet to size in our workshop.
Which certificates and tests can you provide?
Every order ships with a mill certificate (EN 10204 3.1 type) showing heat analysis and mechanical tests. Supplementary tests and 3.2 certificates with SGS, BV, TÜV or another agency are available by agreement.

Conclusion

1.4876 X10NiCrAlTi32-21 plate should be ordered with the points the standard leaves open written into the contract: finish, tolerance class, any extra chemistry limits and the supplementary tests your application needs. With those fixed, stock material from China is a fast and reliable route.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X