Enquiries named SA-53 for Grade B Type S (seamless) pipe use the same ASME B36.10-2022 Table 2-1 typographical rows as the ASTM A53 Grade B Seamless Steel Pipe page, because the technical basis on this companion is ASTM A53/A53M-22. A53/A53M-22 covers NPS 1/8 to NPS 26. The tables list formula-checked rows from Table 2-1 in that range: outside diameter, nominal wall, schedule or identification (STD, XS, XXS) where the table assigns one, and plain-end mass. Each mass has been recomputed with the B36.10 equations Wpe = 10.69(D − t)t lb/ft and 0.0246615(D − t)t kg/m, and only rows that match the published listing are shown. Intermediate walls that appear in Table 2-1 are included. This is a dimensional reference, not a mill stock list, and it is not a listed ASME BPVC size table. Masses are for plain ends; threaded-and-coupled mass is not used here.
NPS 1/8 through 4 (123 rows).
Swipe horizontally to view all dimensions.
| NPS (DN) |
Schedule / identification |
Outside diameter, in (mm) |
Wall thickness, in (mm) |
Plain-end mass, lb/ft (kg/m) |
| 1/8 (6) |
10 |
0.405 (10.29) |
0.049 (1.24) |
0.19 (0.28) |
| 1/8 (6) |
30 |
0.405 (10.29) |
0.057 (1.45) |
0.21 (0.32) |
| 1/8 (6) |
STD / 40 |
0.405 (10.29) |
0.068 (1.73) |
0.24 (0.37) |
| 1/8 (6) |
XS / 80 |
0.405 (10.29) |
0.095 (2.41) |
0.31 (0.47) |
| 1/8 (6) |
160 |
0.405 (10.29) |
0.124 (3.15) |
0.37 (0.55) |
| 1/8 (6) |
XXS |
0.405 (10.29) |
0.19 (4.83) |
0.44 (0.65) |
| 1/4 (8) |
10 |
0.54 (13.72) |
0.065 (1.65) |
0.33 (0.49) |
| 1/4 (8) |
30 |
0.54 (13.72) |
0.073 (1.85) |
0.36 (0.54) |
| 1/4 (8) |
STD / 40 |
0.54 (13.72) |
0.088 (2.24) |
0.43 (0.63) |
| 1/4 (8) |
XS / 80 |
0.54 (13.72) |
0.119 (3.02) |
0.54 (0.80) |
| 1/4 (8) |
160 |
0.54 (13.72) |
0.145 (3.68) |
0.61 (0.91) |
| 1/4 (8) |
XXS |
0.54 (13.72) |
0.238 (6.05) |
0.77 (1.14) |
| 3/8 (10) |
10 |
0.675 (17.14) |
0.065 (1.65) |
0.42 (0.63) |
| 3/8 (10) |
30 |
0.675 (17.14) |
0.073 (1.85) |
0.47 (0.70) |
| 3/8 (10) |
STD / 40 |
0.675 (17.14) |
0.091 (2.31) |
0.57 (0.84) |
| 3/8 (10) |
XS / 80 |
0.675 (17.14) |
0.126 (3.2) |
0.74 (1.10) |
| 3/8 (10) |
160 |
0.675 (17.14) |
0.158 (4.01) |
0.87 (1.30) |
| 3/8 (10) |
XXS |
0.675 (17.14) |
0.252 (6.4) |
1.14 (1.70) |
| 1/2 (15) |
5 |
0.84 (21.34) |
0.065 (1.65) |
0.54 (0.80) |
| 1/2 (15) |
10 |
0.84 (21.34) |
0.083 (2.11) |
0.67 (1.00) |
| 1/2 (15) |
30 |
0.84 (21.34) |
0.095 (2.41) |
0.76 (1.13) |
| 1/2 (15) |
STD / 40 |
0.84 (21.34) |
0.109 (2.77) |
0.85 (1.27) |
| 1/2 (15) |
XS / 80 |
0.84 (21.34) |
0.147 (3.73) |
1.09 (1.62) |
| 1/2 (15) |
160 |
0.84 (21.34) |
0.188 (4.78) |
1.31 (1.95) |
| 3/4 (20) |
5 |
1.05 (26.67) |
0.065 (1.65) |
0.68 (1.02) |
| 3/4 (20) |
10 |
1.05 (26.67) |
0.083 (2.11) |
0.86 (1.28) |
| 3/4 (20) |
30 |
1.05 (26.67) |
0.095 (2.41) |
0.97 (1.44) |
| 3/4 (20) |
STD / 40 |
1.05 (26.67) |
0.113 (2.87) |
1.13 (1.68) |
| 3/4 (20) |
XS / 80 |
1.05 (26.67) |
0.154 (3.91) |
1.48 (2.19) |
| 3/4 (20) |
160 |
1.05 (26.67) |
0.219 (5.56) |
1.95 (2.89) |
| 3/4 (20) |
XXS |
1.05 (26.67) |
0.308 (7.82) |
2.44 (3.64) |
| 1 (25) |
5 |
1.315 (33.4) |
0.065 (1.65) |
0.87 (1.29) |
| 1 (25) |
10 |
1.315 (33.4) |
0.109 (2.77) |
1.41 (2.09) |
| 1 (25) |
30 |
1.315 (33.4) |
0.114 (2.9) |
1.46 (2.18) |
| 1 (25) |
STD / 40 |
1.315 (33.4) |
0.133 (3.38) |
1.68 (2.50) |
| 1 (25) |
XS / 80 |
1.315 (33.4) |
0.179 (4.55) |
2.17 (3.24) |
| 1 (25) |
160 |
1.315 (33.4) |
0.25 (6.35) |
2.85 (4.24) |
| 1 (25) |
XXS |
1.315 (33.4) |
0.358 (9.09) |
3.66 (5.45) |
| 1-1/4 (32) |
5 |
1.66 (42.16) |
0.065 (1.65) |
1.11 (1.65) |
| 1-1/4 (32) |
10 |
1.66 (42.16) |
0.109 (2.77) |
1.81 (2.69) |
| 1-1/4 (32) |
30 |
1.66 (42.16) |
0.117 (2.97) |
1.93 (2.87) |
| 1-1/4 (32) |
STD / 40 |
1.66 (42.16) |
0.14 (3.56) |
2.27 (3.39) |
| 1-1/4 (32) |
XS / 80 |
1.66 (42.16) |
0.191 (4.85) |
3.00 (4.46) |
| 1-1/4 (32) |
160 |
1.66 (42.16) |
0.25 (6.35) |
3.77 (5.61) |
| 1-1/4 (32) |
XXS |
1.66 (42.16) |
0.382 (9.7) |
5.22 (7.76) |
| 1-1/2 (40) |
5 |
1.9 (48.26) |
0.065 (1.65) |
1.28 (1.90) |
| 1-1/2 (40) |
10 |
1.9 (48.26) |
0.109 (2.77) |
2.09 (3.11) |
| 1-1/2 (40) |
30 |
1.9 (48.26) |
0.125 (3.18) |
2.37 (3.54) |
| 1-1/2 (40) |
STD / 40 |
1.9 (48.26) |
0.145 (3.68) |
2.72 (4.05) |
| 1-1/2 (40) |
XS / 80 |
1.9 (48.26) |
0.2 (5.08) |
3.63 (5.41) |
| 1-1/2 (40) |
160 |
1.9 (48.26) |
0.281 (7.14) |
4.86 (7.24) |
| 1-1/2 (40) |
XXS |
1.9 (48.26) |
0.4 (10.16) |
6.41 (9.55) |
| 2 (50) |
5 |
2.375 (60.32) |
0.065 (1.65) |
1.61 (2.39) |
| 2 (50) |
— |
2.375 (60.32) |
0.083 (2.11) |
2.03 (3.03) |
| 2 (50) |
10 |
2.375 (60.32) |
0.109 (2.77) |
2.64 (3.93) |
| 2 (50) |
30 |
2.375 (60.32) |
0.125 (3.18) |
3.01 (4.48) |
| 2 (50) |
— |
2.375 (60.32) |
0.141 (3.58) |
3.37 (5.01) |
| 2 (50) |
STD / 40 |
2.375 (60.32) |
0.154 (3.91) |
3.66 (5.44) |
| 2 (50) |
— |
2.375 (60.32) |
0.172 (4.37) |
4.05 (6.03) |
| 2 (50) |
— |
2.375 (60.32) |
0.188 (4.78) |
4.40 (6.55) |
| 2 (50) |
XS / 80 |
2.375 (60.32) |
0.218 (5.54) |
5.03 (7.48) |
| 2 (50) |
— |
2.375 (60.32) |
0.25 (6.35) |
5.68 (8.45) |
| 2 (50) |
— |
2.375 (60.32) |
0.281 (7.14) |
6.29 (9.36) |
| 2 (50) |
160 |
2.375 (60.32) |
0.344 (8.74) |
7.47 (11.12) |
| 2 (50) |
XXS |
2.375 (60.32) |
0.436 (11.07) |
9.04 (13.45) |
| 2-1/2 (65) |
5 |
2.875 (73.02) |
0.083 (2.11) |
2.48 (3.69) |
| 2-1/2 (65) |
— |
2.875 (73.02) |
0.109 (2.77) |
3.22 (4.80) |
| 2-1/2 (65) |
10 |
2.875 (73.02) |
0.12 (3.05) |
3.53 (5.26) |
| 2-1/2 (65) |
— |
2.875 (73.02) |
0.125 (3.18) |
3.67 (5.48) |
| 2-1/2 (65) |
— |
2.875 (73.02) |
0.141 (3.58) |
4.12 (6.13) |
| 2-1/2 (65) |
— |
2.875 (73.02) |
0.156 (3.96) |
4.53 (6.74) |
| 2-1/2 (65) |
— |
2.875 (73.02) |
0.172 (4.37) |
4.97 (7.40) |
| 2-1/2 (65) |
30 |
2.875 (73.02) |
0.188 (4.78) |
5.40 (8.04) |
| 2-1/2 (65) |
STD / 40 |
2.875 (73.02) |
0.203 (5.16) |
5.80 (8.64) |
| 2-1/2 (65) |
— |
2.875 (73.02) |
0.216 (5.49) |
6.14 (9.14) |
| 2-1/2 (65) |
— |
2.875 (73.02) |
0.25 (6.35) |
7.02 (10.44) |
| 2-1/2 (65) |
XS / 80 |
2.875 (73.02) |
0.276 (7.01) |
7.67 (11.41) |
| 2-1/2 (65) |
160 |
2.875 (73.02) |
0.375 (9.52) |
10.02 (14.91) |
| 2-1/2 (65) |
XXS |
2.875 (73.02) |
0.552 (14.02) |
13.71 (20.40) |
| 3 (80) |
5 |
3.5 (88.9) |
0.083 (2.11) |
3.03 (4.52) |
| 3 (80) |
— |
3.5 (88.9) |
0.109 (2.77) |
3.95 (5.88) |
| 3 (80) |
10 |
3.5 (88.9) |
0.12 (3.05) |
4.34 (6.46) |
| 3 (80) |
— |
3.5 (88.9) |
0.125 (3.18) |
4.51 (6.72) |
| 3 (80) |
— |
3.5 (88.9) |
0.141 (3.58) |
5.06 (7.53) |
| 3 (80) |
— |
3.5 (88.9) |
0.156 (3.96) |
5.58 (8.30) |
| 3 (80) |
— |
3.5 (88.9) |
0.172 (4.37) |
6.12 (9.11) |
| 3 (80) |
30 |
3.5 (88.9) |
0.188 (4.78) |
6.66 (9.92) |
| 3 (80) |
STD / 40 |
3.5 (88.9) |
0.216 (5.49) |
7.58 (11.29) |
| 3 (80) |
— |
3.5 (88.9) |
0.25 (6.35) |
8.69 (12.93) |
| 3 (80) |
— |
3.5 (88.9) |
0.281 (7.14) |
9.67 (14.40) |
| 3 (80) |
XS / 80 |
3.5 (88.9) |
0.3 (7.62) |
10.26 (15.27) |
| 3 (80) |
160 |
3.5 (88.9) |
0.438 (11.13) |
14.34 (21.35) |
| 3 (80) |
XXS |
3.5 (88.9) |
0.6 (15.24) |
18.60 (27.68) |
| 3-1/2 (90) |
5 |
4 (101.6) |
0.083 (2.11) |
3.48 (5.18) |
| 3-1/2 (90) |
— |
4 (101.6) |
0.109 (2.77) |
4.53 (6.75) |
| 3-1/2 (90) |
10 |
4 (101.6) |
0.12 (3.05) |
4.98 (7.41) |
| 3-1/2 (90) |
— |
4 (101.6) |
0.125 (3.18) |
5.18 (7.72) |
| 3-1/2 (90) |
— |
4 (101.6) |
0.141 (3.58) |
5.82 (8.65) |
| 3-1/2 (90) |
— |
4 (101.6) |
0.156 (3.96) |
6.41 (9.54) |
| 3-1/2 (90) |
— |
4 (101.6) |
0.172 (4.37) |
7.04 (10.48) |
| 3-1/2 (90) |
30 |
4 (101.6) |
0.188 (4.78) |
7.66 (11.41) |
| 3-1/2 (90) |
STD / 40 |
4 (101.6) |
0.226 (5.74) |
9.12 (13.57) |
| 3-1/2 (90) |
— |
4 (101.6) |
0.25 (6.35) |
10.02 (14.92) |
| 3-1/2 (90) |
— |
4 (101.6) |
0.281 (7.14) |
11.17 (16.63) |
| 3-1/2 (90) |
XS / 80 |
4 (101.6) |
0.318 (8.08) |
12.52 (18.64) |
| 4 (100) |
5 |
4.5 (114.3) |
0.083 (2.11) |
3.92 (5.84) |
| 4 (100) |
— |
4.5 (114.3) |
0.109 (2.77) |
5.12 (7.62) |
| 4 (100) |
10 |
4.5 (114.3) |
0.12 (3.05) |
5.62 (8.37) |
| 4 (100) |
— |
4.5 (114.3) |
0.125 (3.18) |
5.85 (8.71) |
| 4 (100) |
— |
4.5 (114.3) |
0.141 (3.58) |
6.57 (9.78) |
| 4 (100) |
— |
4.5 (114.3) |
0.156 (3.96) |
7.24 (10.78) |
| 4 (100) |
— |
4.5 (114.3) |
0.172 (4.37) |
7.96 (11.85) |
| 4 (100) |
30 |
4.5 (114.3) |
0.188 (4.78) |
8.67 (12.91) |
| 4 (100) |
— |
4.5 (114.3) |
0.203 (5.16) |
9.32 (13.89) |
| 4 (100) |
— |
4.5 (114.3) |
0.219 (5.56) |
10.02 (14.91) |
| 4 (100) |
STD / 40 |
4.5 (114.3) |
0.237 (6.02) |
10.80 (16.08) |
| 4 (100) |
— |
4.5 (114.3) |
0.25 (6.35) |
11.36 (16.91) |
| 4 (100) |
— |
4.5 (114.3) |
0.281 (7.14) |
12.67 (18.87) |
| 4 (100) |
— |
4.5 (114.3) |
0.312 (7.92) |
13.97 (20.78) |
| 4 (100) |
XS / 80 |
4.5 (114.3) |
0.337 (8.56) |
15.00 (22.32) |
| 4 (100) |
120 |
4.5 (114.3) |
0.438 (11.13) |
19.02 (28.32) |
| 4 (100) |
160 |
4.5 (114.3) |
0.531 (13.49) |
22.53 (33.54) |
| 4 (100) |
XXS |
4.5 (114.3) |
0.674 (17.12) |
27.57 (41.03) |
NPS 5 through 12 (119 rows).
Swipe horizontally to view all dimensions.
| NPS (DN) |
Schedule / identification |
Outside diameter, in (mm) |
Wall thickness, in (mm) |
Plain-end mass, lb/ft (kg/m) |
| 5 (125) |
5 |
5.563 (141.3) |
0.083 (2.11) |
4.86 (7.24) |
| 5 (125) |
5 |
5.563 (141.3) |
0.109 (2.77) |
6.36 (9.46) |
| 5 (125) |
5 |
5.563 (141.3) |
0.125 (3.18) |
7.27 (10.83) |
| 5 (125) |
10 |
5.563 (141.3) |
0.134 (3.4) |
7.78 (11.56) |
| 5 (125) |
5 |
5.563 (141.3) |
0.156 (3.96) |
9.02 (13.41) |
| 5 (125) |
5 |
5.563 (141.3) |
0.188 (4.78) |
10.80 (16.09) |
| 5 (125) |
5 |
5.563 (141.3) |
0.219 (5.56) |
12.51 (18.61) |
| 5 (125) |
STD / 40 |
5.563 (141.3) |
0.258 (6.55) |
14.63 (21.77) |
| 5 (125) |
5 |
5.563 (141.3) |
0.281 (7.14) |
15.87 (23.62) |
| 5 (125) |
5 |
5.563 (141.3) |
0.312 (7.92) |
17.51 (26.05) |
| 5 (125) |
5 |
5.563 (141.3) |
0.344 (8.74) |
19.19 (28.57) |
| 5 (125) |
XS / 80 |
5.563 (141.3) |
0.375 (9.52) |
20.80 (30.94) |
| 5 (125) |
120 |
5.563 (141.3) |
0.5 (12.7) |
27.06 (40.28) |
| 5 (125) |
160 |
5.563 (141.3) |
0.625 (15.88) |
32.99 (49.12) |
| 5 (125) |
XXS |
5.563 (141.3) |
0.75 (19.05) |
38.59 (57.43) |
| 6 (150) |
— |
6.625 (168.28) |
0.083 (2.11) |
5.80 (8.65) |
| 6 (150) |
5 |
6.625 (168.28) |
0.109 (2.77) |
7.59 (11.31) |
| 6 (150) |
— |
6.625 (168.28) |
0.125 (3.18) |
8.69 (12.95) |
| 6 (150) |
10 |
6.625 (168.28) |
0.134 (3.4) |
9.30 (13.83) |
| 6 (150) |
— |
6.625 (168.28) |
0.141 (3.58) |
9.77 (14.54) |
| 6 (150) |
— |
6.625 (168.28) |
0.156 (3.96) |
10.79 (16.05) |
| 6 (150) |
— |
6.625 (168.28) |
0.172 (4.37) |
11.87 (17.66) |
| 6 (150) |
— |
6.625 (168.28) |
0.188 (4.78) |
12.94 (19.27) |
| 6 (150) |
— |
6.625 (168.28) |
0.203 (5.16) |
13.94 (20.76) |
| 6 (150) |
— |
6.625 (168.28) |
0.219 (5.56) |
15.00 (22.31) |
| 6 (150) |
— |
6.625 (168.28) |
0.25 (6.35) |
17.04 (25.36) |
| 6 (150) |
STD / 40 |
6.625 (168.28) |
0.28 (7.11) |
18.99 (28.26) |
| 6 (150) |
— |
6.625 (168.28) |
0.312 (7.92) |
21.06 (31.32) |
| 6 (150) |
— |
6.625 (168.28) |
0.344 (8.74) |
23.10 (34.39) |
| 6 (150) |
— |
6.625 (168.28) |
0.375 (9.52) |
25.05 (37.27) |
| 6 (150) |
XS / 80 |
6.625 (168.28) |
0.432 (10.97) |
28.60 (42.56) |
| 6 (150) |
— |
6.625 (168.28) |
0.5 (12.7) |
32.74 (48.73) |
| 6 (150) |
120 |
6.625 (168.28) |
0.562 (14.27) |
36.43 (54.20) |
| 6 (150) |
— |
6.625 (168.28) |
0.625 (15.88) |
40.09 (59.68) |
| 6 (150) |
160 |
6.625 (168.28) |
0.719 (18.26) |
45.39 (67.56) |
| 6 (150) |
— |
6.625 (168.28) |
0.75 (19.05) |
47.10 (70.11) |
| 6 (150) |
XXS |
6.625 (168.28) |
0.864 (21.95) |
53.21 (79.21) |
| 6 (150) |
— |
6.625 (168.28) |
0.875 (22.22) |
53.78 (80.04) |
| 8 (200) |
5 |
8.625 (219.08) |
0.109 (2.77) |
9.92 (14.78) |
| 8 (200) |
— |
8.625 (219.08) |
0.125 (3.18) |
11.36 (16.93) |
| 8 (200) |
10 |
8.625 (219.08) |
0.148 (3.76) |
13.41 (19.97) |
| 8 (200) |
— |
8.625 (219.08) |
0.156 (3.96) |
14.12 (21.01) |
| 8 (200) |
— |
8.625 (219.08) |
0.188 (4.78) |
16.96 (25.26) |
| 8 (200) |
— |
8.625 (219.08) |
0.203 (5.16) |
18.28 (27.22) |
| 8 (200) |
— |
8.625 (219.08) |
0.219 (5.56) |
19.68 (29.28) |
| 8 (200) |
20 |
8.625 (219.08) |
0.25 (6.35) |
22.38 (33.31) |
| 8 (200) |
30 |
8.625 (219.08) |
0.277 (7.04) |
24.72 (36.81) |
| 8 (200) |
— |
8.625 (219.08) |
0.312 (7.92) |
27.73 (41.24) |
| 8 (200) |
STD / 40 |
8.625 (219.08) |
0.322 (8.18) |
28.58 (42.55) |
| 8 (200) |
— |
8.625 (219.08) |
0.344 (8.74) |
30.45 (45.34) |
| 8 (200) |
— |
8.625 (219.08) |
0.375 (9.52) |
33.07 (49.20) |
| 8 (200) |
60 |
8.625 (219.08) |
0.406 (10.31) |
35.67 (53.08) |
| 8 (200) |
— |
8.625 (219.08) |
0.438 (11.13) |
38.33 (57.08) |
| 8 (200) |
XS / 80 |
8.625 (219.08) |
0.5 (12.7) |
43.43 (64.64) |
| 8 (200) |
— |
8.625 (219.08) |
0.562 (14.27) |
48.44 (72.08) |
| 8 (200) |
100 |
8.625 (219.08) |
0.594 (15.09) |
51.00 (75.91) |
| 8 (200) |
— |
8.625 (219.08) |
0.625 (15.88) |
53.45 (79.58) |
| 8 (200) |
120 |
8.625 (219.08) |
0.719 (18.26) |
60.77 (90.43) |
| 8 (200) |
— |
8.625 (219.08) |
0.75 (19.05) |
63.14 (93.97) |
| 8 (200) |
140 |
8.625 (219.08) |
0.812 (20.62) |
67.82 (100.92) |
| 8 (200) |
XXS |
8.625 (219.08) |
0.875 (22.22) |
72.49 (107.88) |
| 8 (200) |
160 |
8.625 (219.08) |
0.906 (23.01) |
74.76 (111.26) |
| 8 (200) |
— |
8.625 (219.08) |
1 (25.4) |
81.51 (121.32) |
| 10 (250) |
5 |
10.75 (273) |
0.134 (3.4) |
15.21 (22.61) |
| 10 (250) |
10 |
10.75 (273) |
0.156 (3.96) |
17.67 (26.27) |
| 10 (250) |
10 |
10.75 (273) |
0.165 (4.19) |
18.67 (27.78) |
| 10 (250) |
10 |
10.75 (273) |
0.188 (4.78) |
21.23 (31.62) |
| 10 (250) |
10 |
10.75 (273) |
0.203 (5.16) |
22.89 (34.08) |
| 10 (250) |
10 |
10.75 (273) |
0.219 (5.56) |
24.65 (36.67) |
| 10 (250) |
20 |
10.75 (273) |
0.25 (6.35) |
28.06 (41.76) |
| 10 (250) |
10 |
10.75 (273) |
0.279 (7.09) |
31.23 (46.49) |
| 10 (250) |
30 |
10.75 (273) |
0.307 (7.8) |
34.27 (51.01) |
| 10 (250) |
10 |
10.75 (273) |
0.344 (8.74) |
38.27 (56.96) |
| 10 (250) |
STD / 40 |
10.75 (273) |
0.365 (9.27) |
40.52 (60.29) |
| 10 (250) |
10 |
10.75 (273) |
0.438 (11.13) |
48.28 (71.88) |
| 10 (250) |
XS / 60 |
10.75 (273) |
0.5 (12.7) |
54.79 (81.53) |
| 10 (250) |
10 |
10.75 (273) |
0.562 (14.27) |
61.21 (91.05) |
| 10 (250) |
80 |
10.75 (273) |
0.594 (15.09) |
64.49 (95.98) |
| 10 (250) |
10 |
10.75 (273) |
0.625 (15.88) |
67.65 (100.69) |
| 10 (250) |
100 |
10.75 (273) |
0.719 (18.26) |
77.10 (114.71) |
| 10 (250) |
10 |
10.75 (273) |
0.812 (20.62) |
86.26 (128.34) |
| 10 (250) |
120 |
10.75 (273) |
0.844 (21.44) |
89.38 (133.01) |
| 10 (250) |
10 |
10.75 (273) |
0.875 (22.22) |
92.37 (137.42) |
| 10 (250) |
10 |
10.75 (273) |
0.938 (23.83) |
98.39 (146.43) |
| 10 (250) |
XXS / 140 |
10.75 (273) |
1 (25.4) |
104.23 (155.10) |
| 10 (250) |
160 |
10.75 (273) |
1.125 (28.58) |
115.75 (172.27) |
| 10 (250) |
10 |
10.75 (273) |
1.25 (31.75) |
126.94 (188.90) |
| 10 (250) |
10 |
10.75 (273) |
1.375 (34.92) |
137.80 (205.03) |
| 10 (250) |
10 |
10.75 (273) |
1.438 (36.53) |
143.15 (213.03) |
| 12 (300) |
5 |
12.75 (323.8) |
0.156 (3.96) |
21.00 (31.24) |
| 12 (300) |
— |
12.75 (323.8) |
0.172 (4.37) |
23.13 (34.43) |
| 12 (300) |
10 |
12.75 (323.8) |
0.18 (4.57) |
24.19 (35.98) |
| 12 (300) |
— |
12.75 (323.8) |
0.188 (4.78) |
25.25 (37.61) |
| 12 (300) |
— |
12.75 (323.8) |
0.203 (5.16) |
27.23 (40.55) |
| 12 (300) |
— |
12.75 (323.8) |
0.219 (5.56) |
29.34 (43.64) |
| 12 (300) |
20 |
12.75 (323.8) |
0.25 (6.35) |
33.41 (49.71) |
| 12 (300) |
— |
12.75 (323.8) |
0.281 (7.14) |
37.46 (55.76) |
| 12 (300) |
— |
12.75 (323.8) |
0.312 (7.92) |
41.48 (61.70) |
| 12 (300) |
30 |
12.75 (323.8) |
0.33 (8.38) |
43.81 (65.19) |
| 12 (300) |
— |
12.75 (323.8) |
0.344 (8.74) |
45.62 (67.91) |
| 12 (300) |
STD |
12.75 (323.8) |
0.375 (9.52) |
49.61 (73.79) |
| 12 (300) |
40 |
12.75 (323.8) |
0.406 (10.31) |
53.57 (79.71) |
| 12 (300) |
— |
12.75 (323.8) |
0.438 (11.13) |
57.65 (85.82) |
| 12 (300) |
XS |
12.75 (323.8) |
0.5 (12.7) |
65.48 (97.44) |
| 12 (300) |
60 |
12.75 (323.8) |
0.562 (14.27) |
73.22 (108.93) |
| 12 (300) |
— |
12.75 (323.8) |
0.625 (15.88) |
81.01 (120.59) |
| 12 (300) |
80 |
12.75 (323.8) |
0.688 (17.48) |
88.71 (132.05) |
| 12 (300) |
— |
12.75 (323.8) |
0.75 (19.05) |
96.21 (143.17) |
| 12 (300) |
— |
12.75 (323.8) |
0.812 (20.62) |
103.63 (154.17) |
| 12 (300) |
100 |
12.75 (323.8) |
0.844 (21.44) |
107.42 (159.87) |
| 12 (300) |
— |
12.75 (323.8) |
0.875 (22.22) |
111.08 (165.26) |
| 12 (300) |
— |
12.75 (323.8) |
0.938 (23.83) |
118.44 (176.29) |
| 12 (300) |
XXS / 120 |
12.75 (323.8) |
1 (25.4) |
125.61 (186.92) |
| 12 (300) |
— |
12.75 (323.8) |
1.062 (26.97) |
132.69 (197.43) |
| 12 (300) |
140 |
12.75 (323.8) |
1.125 (28.58) |
139.81 (208.08) |
| 12 (300) |
— |
12.75 (323.8) |
1.25 (31.75) |
153.67 (228.68) |
| 12 (300) |
160 |
12.75 (323.8) |
1.312 (33.32) |
160.42 (238.69) |
| 12 (300) |
— |
12.75 (323.8) |
1.375 (34.92) |
167.20 (248.78) |
| 12 (300) |
— |
12.75 (323.8) |
1.5 (38.1) |
180.39 (268.44) |
NPS 14 through 26 (203 rows).
Swipe horizontally to view all dimensions.
| NPS (DN) |
Schedule / identification |
Outside diameter, in (mm) |
Wall thickness, in (mm) |
Plain-end mass, lb/ft (kg/m) |
| 14 (350) |
5 |
14 (355.6) |
0.156 (3.96) |
23.09 (34.34) |
| 14 (350) |
— |
14 (355.6) |
0.188 (4.78) |
27.76 (41.36) |
| 14 (350) |
— |
14 (355.6) |
0.203 (5.16) |
29.94 (44.59) |
| 14 (350) |
— |
14 (355.6) |
0.21 (5.33) |
30.96 (46.04) |
| 14 (350) |
— |
14 (355.6) |
0.219 (5.56) |
32.26 (48.00) |
| 14 (350) |
10 |
14 (355.6) |
0.25 (6.35) |
36.75 (54.69) |
| 14 (350) |
— |
14 (355.6) |
0.281 (7.14) |
41.21 (61.36) |
| 14 (350) |
20 |
14 (355.6) |
0.312 (7.92) |
45.65 (67.91) |
| 14 (350) |
— |
14 (355.6) |
0.344 (8.74) |
50.22 (74.76) |
| 14 (350) |
STD / 30 |
14 (355.6) |
0.375 (9.52) |
54.62 (81.25) |
| 14 (350) |
— |
14 (355.6) |
0.406 (10.31) |
59.00 (87.79) |
| 14 (350) |
40 |
14 (355.6) |
0.438 (11.13) |
63.50 (94.55) |
| 14 (350) |
— |
14 (355.6) |
0.469 (11.91) |
67.84 (100.95) |
| 14 (350) |
XS |
14 (355.6) |
0.5 (12.7) |
72.16 (107.40) |
| 14 (350) |
— |
14 (355.6) |
0.562 (14.27) |
80.73 (120.12) |
| 14 (350) |
60 |
14 (355.6) |
0.594 (15.09) |
85.13 (126.72) |
| 14 (350) |
— |
14 (355.6) |
0.625 (15.88) |
89.36 (133.04) |
| 14 (350) |
— |
14 (355.6) |
0.688 (17.48) |
97.91 (145.76) |
| 14 (350) |
80 |
14 (355.6) |
0.75 (19.05) |
106.23 (158.11) |
| 14 (350) |
— |
14 (355.6) |
0.812 (20.62) |
114.48 (170.34) |
| 14 (350) |
— |
14 (355.6) |
0.875 (22.22) |
122.77 (182.69) |
| 14 (350) |
100 |
14 (355.6) |
0.938 (23.83) |
130.98 (194.98) |
| 14 (350) |
— |
14 (355.6) |
1 (25.4) |
138.97 (206.84) |
| 14 (350) |
— |
14 (355.6) |
1.062 (26.97) |
146.88 (218.58) |
| 14 (350) |
120 |
14 (355.6) |
1.094 (27.79) |
150.93 (224.66) |
| 14 (350) |
— |
14 (355.6) |
1.125 (28.58) |
154.84 (230.49) |
| 14 (350) |
140 |
14 (355.6) |
1.25 (31.75) |
170.37 (253.58) |
| 14 (350) |
160 |
14 (355.6) |
1.406 (35.71) |
189.29 (281.72) |
| 14 (350) |
— |
14 (355.6) |
2 (50.8) |
256.56 (381.85) |
| 14 (350) |
— |
14 (355.6) |
2.125 (53.98) |
269.76 (401.52) |
| 14 (350) |
— |
14 (355.6) |
2.2 (55.88) |
277.51 (413.04) |
| 14 (350) |
— |
14 (355.6) |
2.5 (63.5) |
307.34 (457.43) |
| 16 (400) |
5 |
16 (406.4) |
0.165 (4.19) |
27.93 (41.56) |
| 16 (400) |
— |
16 (406.4) |
0.188 (4.78) |
31.78 (47.34) |
| 16 (400) |
— |
16 (406.4) |
0.203 (5.16) |
34.28 (51.06) |
| 16 (400) |
— |
16 (406.4) |
0.219 (5.56) |
36.95 (54.96) |
| 16 (400) |
10 |
16 (406.4) |
0.25 (6.35) |
42.09 (62.65) |
| 16 (400) |
— |
16 (406.4) |
0.281 (7.14) |
47.22 (70.30) |
| 16 (400) |
20 |
16 (406.4) |
0.312 (7.92) |
52.32 (77.83) |
| 16 (400) |
— |
16 (406.4) |
0.344 (8.74) |
57.57 (85.71) |
| 16 (400) |
STD / 30 |
16 (406.4) |
0.375 (9.52) |
62.64 (93.18) |
| 16 (400) |
— |
16 (406.4) |
0.406 (10.31) |
67.68 (100.71) |
| 16 (400) |
— |
16 (406.4) |
0.438 (11.13) |
72.86 (108.49) |
| 16 (400) |
— |
16 (406.4) |
0.469 (11.91) |
77.87 (115.87) |
| 16 (400) |
XS / 40 |
16 (406.4) |
0.5 (12.7) |
82.85 (123.31) |
| 16 (400) |
— |
16 (406.4) |
0.562 (14.27) |
92.75 (138.00) |
| 16 (400) |
— |
16 (406.4) |
0.625 (15.88) |
102.72 (152.94) |
| 16 (400) |
60 |
16 (406.4) |
0.656 (16.66) |
107.60 (160.13) |
| 16 (400) |
— |
16 (406.4) |
0.688 (17.48) |
112.62 (167.66) |
| 16 (400) |
— |
16 (406.4) |
0.75 (19.05) |
122.27 (181.98) |
| 16 (400) |
— |
16 (406.4) |
0.812 (20.62) |
131.84 (196.18) |
| 16 (400) |
80 |
16 (406.4) |
0.844 (21.44) |
136.74 (203.54) |
| 16 (400) |
— |
16 (406.4) |
0.875 (22.22) |
141.48 (210.52) |
| 16 (400) |
— |
16 (406.4) |
0.938 (23.83) |
151.03 (224.83) |
| 16 (400) |
— |
16 (406.4) |
1 (25.4) |
160.35 (238.66) |
| 16 (400) |
100 |
16 (406.4) |
1.031 (26.19) |
164.98 (245.57) |
| 16 (400) |
— |
16 (406.4) |
1.062 (26.97) |
169.59 (252.37) |
| 16 (400) |
— |
16 (406.4) |
1.125 (28.58) |
178.89 (266.30) |
| 16 (400) |
— |
16 (406.4) |
1.188 (30.18) |
188.11 (280.01) |
| 16 (400) |
120 |
16 (406.4) |
1.219 (30.96) |
192.61 (286.66) |
| 16 (400) |
— |
16 (406.4) |
1.25 (31.75) |
197.10 (293.35) |
| 16 (400) |
140 |
16 (406.4) |
1.438 (36.53) |
223.85 (333.21) |
| 16 (400) |
160 |
16 (406.4) |
1.594 (40.49) |
245.48 (365.38) |
| 16 (400) |
— |
16 (406.4) |
1.75 (44.45) |
266.58 (396.77) |
| 18 (450) |
5 |
18 (457.2) |
0.165 (4.19) |
31.46 (46.81) |
| 18 (450) |
— |
18 (457.2) |
0.188 (4.78) |
35.80 (53.33) |
| 18 (450) |
— |
18 (457.2) |
0.219 (5.56) |
41.63 (61.93) |
| 18 (450) |
10 |
18 (457.2) |
0.25 (6.35) |
47.44 (70.60) |
| 18 (450) |
— |
18 (457.2) |
0.281 (7.14) |
53.23 (79.25) |
| 18 (450) |
20 |
18 (457.2) |
0.312 (7.92) |
58.99 (87.75) |
| 18 (450) |
— |
18 (457.2) |
0.344 (8.74) |
64.93 (96.66) |
| 18 (450) |
STD |
18 (457.2) |
0.375 (9.52) |
70.65 (105.11) |
| 18 (450) |
— |
18 (457.2) |
0.406 (10.31) |
76.36 (113.63) |
| 18 (450) |
30 |
18 (457.2) |
0.438 (11.13) |
82.23 (122.44) |
| 18 (450) |
— |
18 (457.2) |
0.469 (11.91) |
87.89 (130.79) |
| 18 (450) |
XS |
18 (457.2) |
0.5 (12.7) |
93.54 (139.22) |
| 18 (450) |
40 |
18 (457.2) |
0.562 (14.27) |
104.76 (155.88) |
| 18 (450) |
— |
18 (457.2) |
0.625 (15.88) |
116.09 (172.83) |
| 18 (450) |
— |
18 (457.2) |
0.688 (17.48) |
127.32 (189.56) |
| 18 (450) |
60 |
18 (457.2) |
0.75 (19.05) |
138.30 (205.84) |
| 18 (450) |
— |
18 (457.2) |
0.812 (20.62) |
149.20 (222.01) |
| 18 (450) |
— |
18 (457.2) |
0.875 (22.22) |
160.18 (238.36) |
| 18 (450) |
80 |
18 (457.2) |
0.938 (23.83) |
171.08 (254.68) |
| 18 (450) |
— |
18 (457.2) |
1 (25.4) |
181.73 (270.48) |
| 18 (450) |
— |
18 (457.2) |
1.062 (26.97) |
192.29 (286.15) |
| 18 (450) |
— |
18 (457.2) |
1.125 (28.58) |
202.94 (302.10) |
| 18 (450) |
100 |
18 (457.2) |
1.156 (29.36) |
208.15 (309.78) |
| 18 (450) |
— |
18 (457.2) |
1.188 (30.18) |
213.51 (317.82) |
| 18 (450) |
— |
18 (457.2) |
1.25 (31.75) |
223.82 (333.13) |
| 18 (450) |
120 |
18 (457.2) |
1.375 (34.92) |
244.37 (363.66) |
| 18 (450) |
140 |
18 (457.2) |
1.562 (39.67) |
274.48 (408.48) |
| 18 (450) |
160 |
18 (457.2) |
1.781 (45.24) |
308.79 (459.62) |
| 20 (500) |
5 |
20 (508) |
0.188 (4.78) |
39.82 (59.32) |
| 20 (500) |
20 |
20 (508) |
0.219 (5.56) |
46.31 (68.89) |
| 20 (500) |
10 |
20 (508) |
0.25 (6.35) |
52.78 (78.56) |
| 20 (500) |
20 |
20 (508) |
0.281 (7.14) |
59.23 (88.19) |
| 20 (500) |
20 |
20 (508) |
0.312 (7.92) |
65.66 (97.68) |
| 20 (500) |
20 |
20 (508) |
0.344 (8.74) |
72.28 (107.61) |
| 20 (500) |
STD / 20 |
20 (508) |
0.375 (9.52) |
78.67 (117.03) |
| 20 (500) |
20 |
20 (508) |
0.406 (10.31) |
85.04 (126.54) |
| 20 (500) |
20 |
20 (508) |
0.438 (11.13) |
91.59 (136.38) |
| 20 (500) |
20 |
20 (508) |
0.469 (11.91) |
97.92 (145.71) |
| 20 (500) |
XS / 30 |
20 (508) |
0.5 (12.7) |
104.23 (155.13) |
| 20 (500) |
20 |
20 (508) |
0.562 (14.27) |
116.78 (173.75) |
| 20 (500) |
40 |
20 (508) |
0.594 (15.09) |
123.23 (183.43) |
| 20 (500) |
20 |
20 (508) |
0.625 (15.88) |
129.45 (192.73) |
| 20 (500) |
20 |
20 (508) |
0.688 (17.48) |
142.03 (211.45) |
| 20 (500) |
20 |
20 (508) |
0.75 (19.05) |
154.34 (229.71) |
| 20 (500) |
60 |
20 (508) |
0.812 (20.62) |
166.56 (247.84) |
| 20 (500) |
20 |
20 (508) |
0.875 (22.22) |
178.89 (266.20) |
| 20 (500) |
20 |
20 (508) |
0.938 (23.83) |
191.14 (284.54) |
| 20 (500) |
20 |
20 (508) |
1 (25.4) |
203.11 (302.30) |
| 20 (500) |
80 |
20 (508) |
1.031 (26.19) |
209.06 (311.19) |
| 20 (500) |
20 |
20 (508) |
1.062 (26.97) |
215.00 (319.94) |
| 20 (500) |
20 |
20 (508) |
1.125 (28.58) |
227.00 (337.91) |
| 20 (500) |
20 |
20 (508) |
1.188 (30.18) |
238.91 (355.63) |
| 20 (500) |
20 |
20 (508) |
1.25 (31.75) |
250.55 (372.90) |
| 20 (500) |
100 |
20 (508) |
1.281 (32.54) |
256.34 (381.55) |
| 20 (500) |
20 |
20 (508) |
1.312 (33.32) |
262.10 (390.05) |
| 20 (500) |
20 |
20 (508) |
1.375 (34.92) |
273.76 (407.41) |
| 20 (500) |
120 |
20 (508) |
1.5 (38.1) |
296.65 (441.52) |
| 20 (500) |
140 |
20 (508) |
1.75 (44.45) |
341.41 (508.15) |
| 20 (500) |
160 |
20 (508) |
1.969 (50.01) |
379.53 (564.85) |
| 22 (550) |
5 |
22 (558.8) |
0.188 (4.78) |
43.84 (65.31) |
| 22 (550) |
— |
22 (558.8) |
0.219 (5.56) |
50.99 (75.86) |
| 22 (550) |
10 |
22 (558.8) |
0.25 (6.35) |
58.13 (86.51) |
| 22 (550) |
— |
22 (558.8) |
0.281 (7.14) |
65.24 (97.14) |
| 22 (550) |
— |
22 (558.8) |
0.312 (7.92) |
72.34 (107.60) |
| 22 (550) |
— |
22 (558.8) |
0.344 (8.74) |
79.64 (118.56) |
| 22 (550) |
STD / 20 |
22 (558.8) |
0.375 (9.52) |
86.69 (128.96) |
| 22 (550) |
— |
22 (558.8) |
0.406 (10.31) |
93.72 (139.46) |
| 22 (550) |
— |
22 (558.8) |
0.438 (11.13) |
100.96 (150.33) |
| 22 (550) |
— |
22 (558.8) |
0.469 (11.91) |
107.95 (160.63) |
| 22 (550) |
XS / 30 |
22 (558.8) |
0.5 (12.7) |
114.92 (171.04) |
| 22 (550) |
— |
22 (558.8) |
0.562 (14.27) |
128.79 (191.63) |
| 22 (550) |
— |
22 (558.8) |
0.625 (15.88) |
142.81 (212.62) |
| 22 (550) |
— |
22 (558.8) |
0.688 (17.48) |
156.74 (233.35) |
| 22 (550) |
— |
22 (558.8) |
0.75 (19.05) |
170.37 (253.58) |
| 22 (550) |
— |
22 (558.8) |
0.812 (20.62) |
183.92 (273.68) |
| 22 (550) |
60 |
22 (558.8) |
0.875 (22.22) |
197.60 (294.03) |
| 22 (550) |
— |
22 (558.8) |
0.938 (23.83) |
211.19 (314.39) |
| 22 (550) |
— |
22 (558.8) |
1 (25.4) |
224.49 (334.12) |
| 22 (550) |
— |
22 (558.8) |
1.062 (26.97) |
237.70 (353.73) |
| 22 (550) |
80 |
22 (558.8) |
1.125 (28.58) |
251.05 (373.71) |
| 22 (550) |
— |
22 (558.8) |
1.188 (30.18) |
264.31 (393.44) |
| 22 (550) |
— |
22 (558.8) |
1.25 (31.75) |
277.27 (412.68) |
| 22 (550) |
— |
22 (558.8) |
1.312 (33.32) |
290.15 (431.80) |
| 22 (550) |
100 |
22 (558.8) |
1.375 (34.92) |
303.16 (451.15) |
| 22 (550) |
— |
22 (558.8) |
1.438 (36.53) |
316.08 (470.50) |
| 22 (550) |
— |
22 (558.8) |
1.5 (38.1) |
328.72 (489.25) |
| 22 (550) |
120 |
22 (558.8) |
1.625 (41.28) |
353.94 (526.85) |
| 22 (550) |
140 |
22 (558.8) |
1.875 (47.62) |
403.38 (600.32) |
| 22 (550) |
160 |
22 (558.8) |
2.125 (53.98) |
451.49 (672.03) |
| 24 (600) |
5 |
24 (609.6) |
0.218 (5.54) |
55.42 (82.53) |
| 24 (600) |
10 |
24 (609.6) |
0.25 (6.35) |
63.47 (94.47) |
| 24 (600) |
— |
24 (609.6) |
0.281 (7.14) |
71.25 (106.08) |
| 24 (600) |
— |
24 (609.6) |
0.312 (7.92) |
79.01 (117.52) |
| 24 (600) |
— |
24 (609.6) |
0.344 (8.74) |
86.99 (129.51) |
| 24 (600) |
STD / 20 |
24 (609.6) |
0.375 (9.52) |
94.71 (140.89) |
| 24 (600) |
— |
24 (609.6) |
0.406 (10.31) |
102.40 (152.38) |
| 24 (600) |
— |
24 (609.6) |
0.438 (11.13) |
110.32 (164.27) |
| 24 (600) |
— |
24 (609.6) |
0.469 (11.91) |
117.98 (175.55) |
| 24 (600) |
XS |
24 (609.6) |
0.5 (12.7) |
125.61 (186.95) |
| 24 (600) |
30 |
24 (609.6) |
0.562 (14.27) |
140.81 (209.51) |
| 24 (600) |
— |
24 (609.6) |
0.625 (15.88) |
156.17 (232.52) |
| 24 (600) |
40 |
24 (609.6) |
0.688 (17.48) |
171.45 (255.25) |
| 24 (600) |
— |
24 (609.6) |
0.75 (19.05) |
186.41 (277.44) |
| 24 (600) |
— |
24 (609.6) |
0.812 (20.62) |
201.28 (299.51) |
| 24 (600) |
— |
24 (609.6) |
0.875 (22.22) |
216.31 (321.87) |
| 24 (600) |
— |
24 (609.6) |
0.938 (23.83) |
231.25 (344.25) |
| 24 (600) |
60 |
24 (609.6) |
0.969 (24.61) |
238.57 (355.04) |
| 24 (600) |
— |
24 (609.6) |
1 (25.4) |
245.87 (365.94) |
| 24 (600) |
— |
24 (609.6) |
1.062 (26.97) |
260.41 (387.52) |
| 24 (600) |
— |
24 (609.6) |
1.125 (28.58) |
275.10 (409.52) |
| 24 (600) |
— |
24 (609.6) |
1.188 (30.18) |
289.71 (431.25) |
| 24 (600) |
80 |
24 (609.6) |
1.219 (30.96) |
296.86 (441.80) |
| 24 (600) |
— |
24 (609.6) |
1.25 (31.75) |
304.00 (452.46) |
| 24 (600) |
— |
24 (609.6) |
1.312 (33.32) |
318.21 (473.54) |
| 24 (600) |
— |
24 (609.6) |
1.375 (34.92) |
332.56 (494.90) |
| 24 (600) |
— |
24 (609.6) |
1.438 (36.53) |
346.83 (516.27) |
| 24 (600) |
— |
24 (609.6) |
1.5 (38.1) |
360.79 (536.98) |
| 24 (600) |
100 |
24 (609.6) |
1.531 (38.89) |
367.74 (547.36) |
| 24 (600) |
— |
24 (609.6) |
1.562 (39.67) |
374.66 (557.57) |
| 24 (600) |
120 |
24 (609.6) |
1.812 (46.02) |
429.79 (639.62) |
| 24 (600) |
140 |
24 (609.6) |
2.062 (52.37) |
483.57 (719.68) |
| 24 (600) |
160 |
24 (609.6) |
2.344 (59.54) |
542.64 (807.68) |
| 26 (650) |
— |
26 (660.4) |
0.25 (6.35) |
68.82 (102.42) |
| 26 (650) |
— |
26 (660.4) |
0.281 (7.14) |
77.26 (115.03) |
| 26 (650) |
10 |
26 (660.4) |
0.312 (7.92) |
85.68 (127.44) |
| 26 (650) |
— |
26 (660.4) |
0.344 (8.74) |
94.35 (140.46) |
| 26 (650) |
STD |
26 (660.4) |
0.375 (9.52) |
102.72 (152.81) |
| 26 (650) |
— |
26 (660.4) |
0.406 (10.31) |
111.08 (165.29) |
| 26 (650) |
— |
26 (660.4) |
0.438 (11.13) |
119.69 (178.21) |
| 26 (650) |
— |
26 (660.4) |
0.469 (11.91) |
128.00 (190.47) |
| 26 (650) |
XS / 20 |
26 (660.4) |
0.5 (12.7) |
136.30 (202.86) |
| 26 (650) |
— |
26 (660.4) |
0.562 (14.27) |
152.83 (227.39) |
| 26 (650) |
— |
26 (660.4) |
0.625 (15.88) |
169.54 (252.41) |
| 26 (650) |
— |
26 (660.4) |
0.688 (17.48) |
186.16 (277.15) |
| 26 (650) |
— |
26 (660.4) |
0.75 (19.05) |
202.44 (301.31) |
| 26 (650) |
— |
26 (660.4) |
0.812 (20.62) |
218.64 (325.34) |
| 26 (650) |
— |
26 (660.4) |
0.875 (22.22) |
235.01 (349.71) |
| 26 (650) |
— |
26 (660.4) |
0.938 (23.83) |
251.30 (374.10) |
| 26 (650) |
— |
26 (660.4) |
1 (25.4) |
267.25 (397.77) |