ASME SA-106 Grade B Seamless Steel Pipe

ASME SA-106 Grade B is seamless carbon steel pipe for high-temperature service, as printed in ASME BPVC Section II, Part A, 2023. That text is identical with ASTM A106/A106M-19a. Grade B tensile strength is 60 ksi (415 MPa) and yield is 35 ksi (240 MPa). An A106 certificate is not SA-106. SHH STEEL reviews the Code edition and certificate before quoting.
Keywords
ASME SA-106 Grade B pipe, SA-106 Grade B seamless, SA-106/SA-106M Grade B, BPVC SA-106 pipe, SA106 Grade B
Equivalent Grades:
Near-equivalents only, not automatic substitutes.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Size Chart
Applications
Equivalent Grades
Sourcing
FAQ
Conclusion

What is ASME SA-106 Grade B Seamless Steel Pipe?

ASME SA-106/SA-106M, as printed in ASME BPVC Section II, Part A, 2023, is marked identical with ASTM Specification A106/A106M-19a. The specification covers seamless carbon steel pipe for high-temperature service in NPS 1/8 to NPS 48 [DN 6 to DN 1200], with nominal (average) wall thickness as given in ASME B36.10M, or other dimensions that still meet the specification. This page is Grade B only. It is not the live ASTM A106 Grade B page, and it is not SA-53 or SA-106 Grade A or Grade C.

An ordinary ASTM A106 certificate is not an SA-106 certificate. The SA designation is used when the order needs the ASME materials listing. The Code edition on the order governs; a later ASTM A106 year is not automatically the SA text in the 2023 book.

Material, Manufacture and Scope for ASME SA-106 Grade B Pipe

Pipe ordered under this specification shall be suitable for bending, flanging and similar forming operations, and for welding, with a welding procedure suited to the grade and the service. Graphitization in high-temperature service is a known consideration and is not dismissed here. Supplementary requirements apply only when they are stated on the order. The Grade B chemistry and tensile figures below are the values already verified for A106 Grade B on this site and adopted in the 19a text printed as SA-106 in the 2023 book; they are not taken from a later ASTM year.

ASME SA-106 Grade B Chemical Composition (Heat Analysis)

Grade B heat analysis is carbon 0.30 % maximum, manganese 0.29-1.06 %, phosphorus 0.035 % maximum, sulfur 0.035 % maximum and silicon 0.10 % minimum, with chromium, copper and nickel each 0.40 % maximum, molybdenum 0.15 % maximum, vanadium 0.08 % maximum, and a 1 % combined cap on Cr+Cu+Mo+Ni+V. A manganese/carbon trade-off footnote applies in the adopted text and must be read from that table rather than invented here. Do not copy Grade A or Grade C carbon and manganese windows onto a Grade B order.

Swipe horizontally to view all dimensions.

Element Grade B
Carbon, max 0.30 (see the manganese trade-off note)
Manganese 0.29-1.06 (see the carbon trade-off note)
Phosphorus, max 0.035
Sulfur, max 0.035
Silicon, min 0.10
Chromium, max 0.40
Copper, max 0.40
Molybdenum, max 0.15
Nickel, max 0.40
Vanadium, max 0.08
Cr+Cu+Mo+Ni+V 1 % combined

ASME SA-106 Grade B Mechanical Properties

Grade B minimum tensile strength is 60 ksi [415 MPa] and minimum yield is 35 ksi [240 MPa]. Basic minimum elongations are 30 % longitudinal and 16.5 % transverse on a full-section or transverse-strip specimen, and 22 % longitudinal and 12 % transverse on a standard 2 in. round specimen. Hydrostatic or non-destructive examination follows the specification as ordered. These figures are not Grade A or Grade C values.

Swipe horizontally to view all dimensions.

Property Grade B
Tensile strength, min 60 ksi [415 MPa]
Yield strength, min 35 ksi [240 MPa]
Elongation, full-section / transverse-strip basic min, longitudinal 30 %
Elongation, full-section / transverse-strip basic min, transverse 16.5 %
Elongation, standard round 2 in. specimen, longitudinal 22 %
Elongation, standard round 2 in. specimen, transverse 12 %

ASME SA-106 Grade B Common Sizes: ASME B36.10 Table 2-1

Dimensions and theoretical masses below follow the same ASME B36.10-2022 Table 2-1 typographical subset already verified on the ASTM A106 Grade B page. They are not a mill stock list. Other walls may be furnished when they still comply with the specification. Masses are the standard pipe formula used with that table; the ordered wall and the ordered NPS still govern.

Swipe horizontally to view all dimensions.

NPS (DN) Schedule / identification Outside diameter, in (mm) Wall thickness, in (mm) Plain-end mass, lb/ft (kg/m)
1/8 (6) 10 0.405 (10.29) 0.049 (1.24) 0.19 (0.28)
1/8 (6) 30 0.405 (10.29) 0.057 (1.45) 0.21 (0.32)
1/8 (6) STD / 40 0.405 (10.29) 0.068 (1.73) 0.24 (0.37)
1/8 (6) XS / 80 0.405 (10.29) 0.095 (2.41) 0.31 (0.47)
1/8 (6) 160 0.405 (10.29) 0.124 (3.15) 0.37 (0.55)
1/8 (6) XXS 0.405 (10.29) 0.19 (4.83) 0.44 (0.65)
1/4 (8) 10 0.54 (13.72) 0.065 (1.65) 0.33 (0.49)
1/4 (8) 30 0.54 (13.72) 0.073 (1.85) 0.36 (0.54)
1/4 (8) STD / 40 0.54 (13.72) 0.088 (2.24) 0.43 (0.63)
1/4 (8) XS / 80 0.54 (13.72) 0.119 (3.02) 0.54 (0.80)
1/4 (8) 160 0.54 (13.72) 0.145 (3.68) 0.61 (0.91)
1/4 (8) XXS 0.54 (13.72) 0.238 (6.05) 0.77 (1.14)
3/8 (10) 10 0.675 (17.14) 0.065 (1.65) 0.42 (0.63)
3/8 (10) 30 0.675 (17.14) 0.073 (1.85) 0.47 (0.70)
3/8 (10) STD / 40 0.675 (17.14) 0.091 (2.31) 0.57 (0.84)
3/8 (10) XS / 80 0.675 (17.14) 0.126 (3.2) 0.74 (1.10)
3/8 (10) 160 0.675 (17.14) 0.158 (4.01) 0.87 (1.30)
3/8 (10) XXS 0.675 (17.14) 0.252 (6.4) 1.14 (1.70)
1/2 (15) 5 0.84 (21.34) 0.065 (1.65) 0.54 (0.80)
1/2 (15) 10 0.84 (21.34) 0.083 (2.11) 0.67 (1.00)
1/2 (15) 30 0.84 (21.34) 0.095 (2.41) 0.76 (1.13)
1/2 (15) STD / 40 0.84 (21.34) 0.109 (2.77) 0.85 (1.27)
1/2 (15) XS / 80 0.84 (21.34) 0.147 (3.73) 1.09 (1.62)
1/2 (15) 160 0.84 (21.34) 0.188 (4.78) 1.31 (1.95)
3/4 (20) 5 1.05 (26.67) 0.065 (1.65) 0.68 (1.02)
3/4 (20) 10 1.05 (26.67) 0.083 (2.11) 0.86 (1.28)
3/4 (20) 30 1.05 (26.67) 0.095 (2.41) 0.97 (1.44)
3/4 (20) STD / 40 1.05 (26.67) 0.113 (2.87) 1.13 (1.68)
3/4 (20) XS / 80 1.05 (26.67) 0.154 (3.91) 1.48 (2.19)
3/4 (20) 160 1.05 (26.67) 0.219 (5.56) 1.95 (2.89)
3/4 (20) XXS 1.05 (26.67) 0.308 (7.82) 2.44 (3.64)
1 (25) 5 1.315 (33.4) 0.065 (1.65) 0.87 (1.29)
1 (25) 10 1.315 (33.4) 0.109 (2.77) 1.41 (2.09)
1 (25) 30 1.315 (33.4) 0.114 (2.9) 1.46 (2.18)
1 (25) STD / 40 1.315 (33.4) 0.133 (3.38) 1.68 (2.50)
1 (25) XS / 80 1.315 (33.4) 0.179 (4.55) 2.17 (3.24)
1 (25) 160 1.315 (33.4) 0.25 (6.35) 2.85 (4.24)
1 (25) XXS 1.315 (33.4) 0.358 (9.09) 3.66 (5.45)
1-1/4 (32) 5 1.66 (42.16) 0.065 (1.65) 1.11 (1.65)
1-1/4 (32) 10 1.66 (42.16) 0.109 (2.77) 1.81 (2.69)
1-1/4 (32) 30 1.66 (42.16) 0.117 (2.97) 1.93 (2.87)
1-1/4 (32) STD / 40 1.66 (42.16) 0.14 (3.56) 2.27 (3.39)
1-1/4 (32) XS / 80 1.66 (42.16) 0.191 (4.85) 3.00 (4.46)
1-1/4 (32) 160 1.66 (42.16) 0.25 (6.35) 3.77 (5.61)
1-1/4 (32) XXS 1.66 (42.16) 0.382 (9.7) 5.22 (7.76)
1-1/2 (40) 5 1.9 (48.26) 0.065 (1.65) 1.28 (1.90)
1-1/2 (40) 10 1.9 (48.26) 0.109 (2.77) 2.09 (3.11)
1-1/2 (40) 30 1.9 (48.26) 0.125 (3.18) 2.37 (3.54)
1-1/2 (40) STD / 40 1.9 (48.26) 0.145 (3.68) 2.72 (4.05)
1-1/2 (40) XS / 80 1.9 (48.26) 0.2 (5.08) 3.63 (5.41)
1-1/2 (40) 160 1.9 (48.26) 0.281 (7.14) 4.86 (7.24)
1-1/2 (40) XXS 1.9 (48.26) 0.4 (10.16) 6.41 (9.55)
2 (50) 5 2.375 (60.32) 0.065 (1.65) 1.61 (2.39)
2 (50) — 2.375 (60.32) 0.083 (2.11) 2.03 (3.03)
2 (50) 10 2.375 (60.32) 0.109 (2.77) 2.64 (3.93)
2 (50) 30 2.375 (60.32) 0.125 (3.18) 3.01 (4.48)
2 (50) — 2.375 (60.32) 0.141 (3.58) 3.37 (5.01)
2 (50) STD / 40 2.375 (60.32) 0.154 (3.91) 3.66 (5.44)
2 (50) — 2.375 (60.32) 0.172 (4.37) 4.05 (6.03)
2 (50) — 2.375 (60.32) 0.188 (4.78) 4.40 (6.55)
2 (50) XS / 80 2.375 (60.32) 0.218 (5.54) 5.03 (7.48)
2 (50) — 2.375 (60.32) 0.25 (6.35) 5.68 (8.45)
2 (50) — 2.375 (60.32) 0.281 (7.14) 6.29 (9.36)
2 (50) 160 2.375 (60.32) 0.344 (8.74) 7.47 (11.12)
2 (50) XXS 2.375 (60.32) 0.436 (11.07) 9.04 (13.45)
2-1/2 (65) 5 2.875 (73.02) 0.083 (2.11) 2.48 (3.69)
2-1/2 (65) — 2.875 (73.02) 0.109 (2.77) 3.22 (4.80)
2-1/2 (65) 10 2.875 (73.02) 0.12 (3.05) 3.53 (5.26)
2-1/2 (65) — 2.875 (73.02) 0.125 (3.18) 3.67 (5.48)
2-1/2 (65) — 2.875 (73.02) 0.141 (3.58) 4.12 (6.13)
2-1/2 (65) — 2.875 (73.02) 0.156 (3.96) 4.53 (6.74)
2-1/2 (65) — 2.875 (73.02) 0.172 (4.37) 4.97 (7.40)
2-1/2 (65) 30 2.875 (73.02) 0.188 (4.78) 5.40 (8.04)
2-1/2 (65) STD / 40 2.875 (73.02) 0.203 (5.16) 5.80 (8.64)
2-1/2 (65) — 2.875 (73.02) 0.216 (5.49) 6.14 (9.14)
2-1/2 (65) — 2.875 (73.02) 0.25 (6.35) 7.02 (10.44)
2-1/2 (65) XS / 80 2.875 (73.02) 0.276 (7.01) 7.67 (11.41)
2-1/2 (65) 160 2.875 (73.02) 0.375 (9.52) 10.02 (14.91)
2-1/2 (65) XXS 2.875 (73.02) 0.552 (14.02) 13.71 (20.40)
3 (80) 5 3.5 (88.9) 0.083 (2.11) 3.03 (4.52)
3 (80) — 3.5 (88.9) 0.109 (2.77) 3.95 (5.88)
3 (80) 10 3.5 (88.9) 0.12 (3.05) 4.34 (6.46)
3 (80) — 3.5 (88.9) 0.125 (3.18) 4.51 (6.72)
3 (80) — 3.5 (88.9) 0.141 (3.58) 5.06 (7.53)
3 (80) — 3.5 (88.9) 0.156 (3.96) 5.58 (8.30)
3 (80) — 3.5 (88.9) 0.172 (4.37) 6.12 (9.11)
3 (80) 30 3.5 (88.9) 0.188 (4.78) 6.66 (9.92)
3 (80) STD / 40 3.5 (88.9) 0.216 (5.49) 7.58 (11.29)
3 (80) — 3.5 (88.9) 0.25 (6.35) 8.69 (12.93)
3 (80) — 3.5 (88.9) 0.281 (7.14) 9.67 (14.40)
3 (80) XS / 80 3.5 (88.9) 0.3 (7.62) 10.26 (15.27)
3 (80) 160 3.5 (88.9) 0.438 (11.13) 14.34 (21.35)
3 (80) XXS 3.5 (88.9) 0.6 (15.24) 18.60 (27.68)
3-1/2 (90) 5 4 (101.6) 0.083 (2.11) 3.48 (5.18)
3-1/2 (90) — 4 (101.6) 0.109 (2.77) 4.53 (6.75)
3-1/2 (90) 10 4 (101.6) 0.12 (3.05) 4.98 (7.41)
3-1/2 (90) — 4 (101.6) 0.125 (3.18) 5.18 (7.72)
3-1/2 (90) — 4 (101.6) 0.141 (3.58) 5.82 (8.65)
3-1/2 (90) — 4 (101.6) 0.156 (3.96) 6.41 (9.54)
3-1/2 (90) — 4 (101.6) 0.172 (4.37) 7.04 (10.48)
3-1/2 (90) 30 4 (101.6) 0.188 (4.78) 7.66 (11.41)
3-1/2 (90) STD / 40 4 (101.6) 0.226 (5.74) 9.12 (13.57)
3-1/2 (90) — 4 (101.6) 0.25 (6.35) 10.02 (14.92)
3-1/2 (90) — 4 (101.6) 0.281 (7.14) 11.17 (16.63)
3-1/2 (90) XS / 80 4 (101.6) 0.318 (8.08) 12.52 (18.64)
4 (100) 5 4.5 (114.3) 0.083 (2.11) 3.92 (5.84)
4 (100) — 4.5 (114.3) 0.109 (2.77) 5.12 (7.62)
4 (100) 10 4.5 (114.3) 0.12 (3.05) 5.62 (8.37)
4 (100) — 4.5 (114.3) 0.125 (3.18) 5.85 (8.71)
4 (100) — 4.5 (114.3) 0.141 (3.58) 6.57 (9.78)
4 (100) — 4.5 (114.3) 0.156 (3.96) 7.24 (10.78)
4 (100) — 4.5 (114.3) 0.172 (4.37) 7.96 (11.85)
4 (100) 30 4.5 (114.3) 0.188 (4.78) 8.67 (12.91)
4 (100) — 4.5 (114.3) 0.203 (5.16) 9.32 (13.89)
4 (100) — 4.5 (114.3) 0.219 (5.56) 10.02 (14.91)
4 (100) STD / 40 4.5 (114.3) 0.237 (6.02) 10.80 (16.08)
4 (100) — 4.5 (114.3) 0.25 (6.35) 11.36 (16.91)
4 (100) — 4.5 (114.3) 0.281 (7.14) 12.67 (18.87)
4 (100) — 4.5 (114.3) 0.312 (7.92) 13.97 (20.78)
4 (100) XS / 80 4.5 (114.3) 0.337 (8.56) 15.00 (22.32)
4 (100) 120 4.5 (114.3) 0.438 (11.13) 19.02 (28.32)
4 (100) 160 4.5 (114.3) 0.531 (13.49) 22.53 (33.54)
4 (100) XXS 4.5 (114.3) 0.674 (17.12) 27.57 (41.03)

NPS 5 through 12 (119 rows).

Swipe horizontally to view all dimensions.

NPS (DN) Schedule / identification Outside diameter, in (mm) Wall thickness, in (mm) Plain-end mass, lb/ft (kg/m)
5 (125) 5 5.563 (141.3) 0.083 (2.11) 4.86 (7.24)
5 (125) 5 5.563 (141.3) 0.109 (2.77) 6.36 (9.46)
5 (125) 5 5.563 (141.3) 0.125 (3.18) 7.27 (10.83)
5 (125) 10 5.563 (141.3) 0.134 (3.4) 7.78 (11.56)
5 (125) 5 5.563 (141.3) 0.156 (3.96) 9.02 (13.41)
5 (125) 5 5.563 (141.3) 0.188 (4.78) 10.80 (16.09)
5 (125) 5 5.563 (141.3) 0.219 (5.56) 12.51 (18.61)
5 (125) STD / 40 5.563 (141.3) 0.258 (6.55) 14.63 (21.77)
5 (125) 5 5.563 (141.3) 0.281 (7.14) 15.87 (23.62)
5 (125) 5 5.563 (141.3) 0.312 (7.92) 17.51 (26.05)
5 (125) 5 5.563 (141.3) 0.344 (8.74) 19.19 (28.57)
5 (125) XS / 80 5.563 (141.3) 0.375 (9.52) 20.80 (30.94)
5 (125) 120 5.563 (141.3) 0.5 (12.7) 27.06 (40.28)
5 (125) 160 5.563 (141.3) 0.625 (15.88) 32.99 (49.12)
5 (125) XXS 5.563 (141.3) 0.75 (19.05) 38.59 (57.43)
6 (150) — 6.625 (168.28) 0.083 (2.11) 5.80 (8.65)
6 (150) 5 6.625 (168.28) 0.109 (2.77) 7.59 (11.31)
6 (150) — 6.625 (168.28) 0.125 (3.18) 8.69 (12.95)
6 (150) 10 6.625 (168.28) 0.134 (3.4) 9.30 (13.83)
6 (150) — 6.625 (168.28) 0.141 (3.58) 9.77 (14.54)
6 (150) — 6.625 (168.28) 0.156 (3.96) 10.79 (16.05)
6 (150) — 6.625 (168.28) 0.172 (4.37) 11.87 (17.66)
6 (150) — 6.625 (168.28) 0.188 (4.78) 12.94 (19.27)
6 (150) — 6.625 (168.28) 0.203 (5.16) 13.94 (20.76)
6 (150) — 6.625 (168.28) 0.219 (5.56) 15.00 (22.31)
6 (150) — 6.625 (168.28) 0.25 (6.35) 17.04 (25.36)
6 (150) STD / 40 6.625 (168.28) 0.28 (7.11) 18.99 (28.26)
6 (150) — 6.625 (168.28) 0.312 (7.92) 21.06 (31.32)
6 (150) — 6.625 (168.28) 0.344 (8.74) 23.10 (34.39)
6 (150) — 6.625 (168.28) 0.375 (9.52) 25.05 (37.27)
6 (150) XS / 80 6.625 (168.28) 0.432 (10.97) 28.60 (42.56)
6 (150) — 6.625 (168.28) 0.5 (12.7) 32.74 (48.73)
6 (150) 120 6.625 (168.28) 0.562 (14.27) 36.43 (54.20)
6 (150) — 6.625 (168.28) 0.625 (15.88) 40.09 (59.68)
6 (150) 160 6.625 (168.28) 0.719 (18.26) 45.39 (67.56)
6 (150) — 6.625 (168.28) 0.75 (19.05) 47.10 (70.11)
6 (150) XXS 6.625 (168.28) 0.864 (21.95) 53.21 (79.21)
6 (150) — 6.625 (168.28) 0.875 (22.22) 53.78 (80.04)
8 (200) 5 8.625 (219.08) 0.109 (2.77) 9.92 (14.78)
8 (200) — 8.625 (219.08) 0.125 (3.18) 11.36 (16.93)
8 (200) 10 8.625 (219.08) 0.148 (3.76) 13.41 (19.97)
8 (200) — 8.625 (219.08) 0.156 (3.96) 14.12 (21.01)
8 (200) — 8.625 (219.08) 0.188 (4.78) 16.96 (25.26)
8 (200) — 8.625 (219.08) 0.203 (5.16) 18.28 (27.22)
8 (200) — 8.625 (219.08) 0.219 (5.56) 19.68 (29.28)
8 (200) 20 8.625 (219.08) 0.25 (6.35) 22.38 (33.31)
8 (200) 30 8.625 (219.08) 0.277 (7.04) 24.72 (36.81)
8 (200) — 8.625 (219.08) 0.312 (7.92) 27.73 (41.24)
8 (200) STD / 40 8.625 (219.08) 0.322 (8.18) 28.58 (42.55)
8 (200) — 8.625 (219.08) 0.344 (8.74) 30.45 (45.34)
8 (200) — 8.625 (219.08) 0.375 (9.52) 33.07 (49.20)
8 (200) 60 8.625 (219.08) 0.406 (10.31) 35.67 (53.08)
8 (200) — 8.625 (219.08) 0.438 (11.13) 38.33 (57.08)
8 (200) XS / 80 8.625 (219.08) 0.5 (12.7) 43.43 (64.64)
8 (200) — 8.625 (219.08) 0.562 (14.27) 48.44 (72.08)
8 (200) 100 8.625 (219.08) 0.594 (15.09) 51.00 (75.91)
8 (200) — 8.625 (219.08) 0.625 (15.88) 53.45 (79.58)
8 (200) 120 8.625 (219.08) 0.719 (18.26) 60.77 (90.43)
8 (200) — 8.625 (219.08) 0.75 (19.05) 63.14 (93.97)
8 (200) 140 8.625 (219.08) 0.812 (20.62) 67.82 (100.92)
8 (200) XXS 8.625 (219.08) 0.875 (22.22) 72.49 (107.88)
8 (200) 160 8.625 (219.08) 0.906 (23.01) 74.76 (111.26)
8 (200) — 8.625 (219.08) 1 (25.4) 81.51 (121.32)
10 (250) 5 10.75 (273) 0.134 (3.4) 15.21 (22.61)
10 (250) 10 10.75 (273) 0.156 (3.96) 17.67 (26.27)
10 (250) 10 10.75 (273) 0.165 (4.19) 18.67 (27.78)
10 (250) 10 10.75 (273) 0.188 (4.78) 21.23 (31.62)
10 (250) 10 10.75 (273) 0.203 (5.16) 22.89 (34.08)
10 (250) 10 10.75 (273) 0.219 (5.56) 24.65 (36.67)
10 (250) 20 10.75 (273) 0.25 (6.35) 28.06 (41.76)
10 (250) 10 10.75 (273) 0.279 (7.09) 31.23 (46.49)
10 (250) 30 10.75 (273) 0.307 (7.8) 34.27 (51.01)
10 (250) 10 10.75 (273) 0.344 (8.74) 38.27 (56.96)
10 (250) STD / 40 10.75 (273) 0.365 (9.27) 40.52 (60.29)
10 (250) 10 10.75 (273) 0.438 (11.13) 48.28 (71.88)
10 (250) XS / 60 10.75 (273) 0.5 (12.7) 54.79 (81.53)
10 (250) 10 10.75 (273) 0.562 (14.27) 61.21 (91.05)
10 (250) 80 10.75 (273) 0.594 (15.09) 64.49 (95.98)
10 (250) 10 10.75 (273) 0.625 (15.88) 67.65 (100.69)
10 (250) 100 10.75 (273) 0.719 (18.26) 77.10 (114.71)
10 (250) 10 10.75 (273) 0.812 (20.62) 86.26 (128.34)
10 (250) 120 10.75 (273) 0.844 (21.44) 89.38 (133.01)
10 (250) 10 10.75 (273) 0.875 (22.22) 92.37 (137.42)
10 (250) 10 10.75 (273) 0.938 (23.83) 98.39 (146.43)
10 (250) XXS / 140 10.75 (273) 1 (25.4) 104.23 (155.10)
10 (250) 160 10.75 (273) 1.125 (28.58) 115.75 (172.27)
10 (250) 10 10.75 (273) 1.25 (31.75) 126.94 (188.90)
10 (250) 10 10.75 (273) 1.375 (34.92) 137.80 (205.03)
10 (250) 10 10.75 (273) 1.438 (36.53) 143.15 (213.03)
12 (300) 5 12.75 (323.8) 0.156 (3.96) 21.00 (31.24)
12 (300) — 12.75 (323.8) 0.172 (4.37) 23.13 (34.43)
12 (300) 10 12.75 (323.8) 0.18 (4.57) 24.19 (35.98)
12 (300) — 12.75 (323.8) 0.188 (4.78) 25.25 (37.61)
12 (300) — 12.75 (323.8) 0.203 (5.16) 27.23 (40.55)
12 (300) — 12.75 (323.8) 0.219 (5.56) 29.34 (43.64)
12 (300) 20 12.75 (323.8) 0.25 (6.35) 33.41 (49.71)
12 (300) — 12.75 (323.8) 0.281 (7.14) 37.46 (55.76)
12 (300) — 12.75 (323.8) 0.312 (7.92) 41.48 (61.70)
12 (300) 30 12.75 (323.8) 0.33 (8.38) 43.81 (65.19)
12 (300) — 12.75 (323.8) 0.344 (8.74) 45.62 (67.91)
12 (300) STD 12.75 (323.8) 0.375 (9.52) 49.61 (73.79)
12 (300) 40 12.75 (323.8) 0.406 (10.31) 53.57 (79.71)
12 (300) — 12.75 (323.8) 0.438 (11.13) 57.65 (85.82)
12 (300) XS 12.75 (323.8) 0.5 (12.7) 65.48 (97.44)
12 (300) 60 12.75 (323.8) 0.562 (14.27) 73.22 (108.93)
12 (300) — 12.75 (323.8) 0.625 (15.88) 81.01 (120.59)
12 (300) 80 12.75 (323.8) 0.688 (17.48) 88.71 (132.05)
12 (300) — 12.75 (323.8) 0.75 (19.05) 96.21 (143.17)
12 (300) — 12.75 (323.8) 0.812 (20.62) 103.63 (154.17)
12 (300) 100 12.75 (323.8) 0.844 (21.44) 107.42 (159.87)
12 (300) — 12.75 (323.8) 0.875 (22.22) 111.08 (165.26)
12 (300) — 12.75 (323.8) 0.938 (23.83) 118.44 (176.29)
12 (300) XXS / 120 12.75 (323.8) 1 (25.4) 125.61 (186.92)
12 (300) — 12.75 (323.8) 1.062 (26.97) 132.69 (197.43)
12 (300) 140 12.75 (323.8) 1.125 (28.58) 139.81 (208.08)
12 (300) — 12.75 (323.8) 1.25 (31.75) 153.67 (228.68)
12 (300) 160 12.75 (323.8) 1.312 (33.32) 160.42 (238.69)
12 (300) — 12.75 (323.8) 1.375 (34.92) 167.20 (248.78)
12 (300) — 12.75 (323.8) 1.5 (38.1) 180.39 (268.44)

NPS 14 through 26 (203 rows).

Swipe horizontally to view all dimensions.

NPS (DN) Schedule / identification Outside diameter, in (mm) Wall thickness, in (mm) Plain-end mass, lb/ft (kg/m)
14 (350) 5 14 (355.6) 0.156 (3.96) 23.09 (34.34)
14 (350) — 14 (355.6) 0.188 (4.78) 27.76 (41.36)
14 (350) — 14 (355.6) 0.203 (5.16) 29.94 (44.59)
14 (350) — 14 (355.6) 0.21 (5.33) 30.96 (46.04)
14 (350) — 14 (355.6) 0.219 (5.56) 32.26 (48.00)
14 (350) 10 14 (355.6) 0.25 (6.35) 36.75 (54.69)
14 (350) — 14 (355.6) 0.281 (7.14) 41.21 (61.36)
14 (350) 20 14 (355.6) 0.312 (7.92) 45.65 (67.91)
14 (350) — 14 (355.6) 0.344 (8.74) 50.22 (74.76)
14 (350) STD / 30 14 (355.6) 0.375 (9.52) 54.62 (81.25)
14 (350) — 14 (355.6) 0.406 (10.31) 59.00 (87.79)
14 (350) 40 14 (355.6) 0.438 (11.13) 63.50 (94.55)
14 (350) — 14 (355.6) 0.469 (11.91) 67.84 (100.95)
14 (350) XS 14 (355.6) 0.5 (12.7) 72.16 (107.40)
14 (350) — 14 (355.6) 0.562 (14.27) 80.73 (120.12)
14 (350) 60 14 (355.6) 0.594 (15.09) 85.13 (126.72)
14 (350) — 14 (355.6) 0.625 (15.88) 89.36 (133.04)
14 (350) — 14 (355.6) 0.688 (17.48) 97.91 (145.76)
14 (350) 80 14 (355.6) 0.75 (19.05) 106.23 (158.11)
14 (350) — 14 (355.6) 0.812 (20.62) 114.48 (170.34)
14 (350) — 14 (355.6) 0.875 (22.22) 122.77 (182.69)
14 (350) 100 14 (355.6) 0.938 (23.83) 130.98 (194.98)
14 (350) — 14 (355.6) 1 (25.4) 138.97 (206.84)
14 (350) — 14 (355.6) 1.062 (26.97) 146.88 (218.58)
14 (350) 120 14 (355.6) 1.094 (27.79) 150.93 (224.66)
14 (350) — 14 (355.6) 1.125 (28.58) 154.84 (230.49)
14 (350) 140 14 (355.6) 1.25 (31.75) 170.37 (253.58)
14 (350) 160 14 (355.6) 1.406 (35.71) 189.29 (281.72)
14 (350) — 14 (355.6) 2 (50.8) 256.56 (381.85)
14 (350) — 14 (355.6) 2.125 (53.98) 269.76 (401.52)
14 (350) — 14 (355.6) 2.2 (55.88) 277.51 (413.04)
14 (350) — 14 (355.6) 2.5 (63.5) 307.34 (457.43)
16 (400) 5 16 (406.4) 0.165 (4.19) 27.93 (41.56)
16 (400) — 16 (406.4) 0.188 (4.78) 31.78 (47.34)
16 (400) — 16 (406.4) 0.203 (5.16) 34.28 (51.06)
16 (400) — 16 (406.4) 0.219 (5.56) 36.95 (54.96)
16 (400) 10 16 (406.4) 0.25 (6.35) 42.09 (62.65)
16 (400) — 16 (406.4) 0.281 (7.14) 47.22 (70.30)
16 (400) 20 16 (406.4) 0.312 (7.92) 52.32 (77.83)
16 (400) — 16 (406.4) 0.344 (8.74) 57.57 (85.71)
16 (400) STD / 30 16 (406.4) 0.375 (9.52) 62.64 (93.18)
16 (400) — 16 (406.4) 0.406 (10.31) 67.68 (100.71)
16 (400) — 16 (406.4) 0.438 (11.13) 72.86 (108.49)
16 (400) — 16 (406.4) 0.469 (11.91) 77.87 (115.87)
16 (400) XS / 40 16 (406.4) 0.5 (12.7) 82.85 (123.31)
16 (400) — 16 (406.4) 0.562 (14.27) 92.75 (138.00)
16 (400) — 16 (406.4) 0.625 (15.88) 102.72 (152.94)
16 (400) 60 16 (406.4) 0.656 (16.66) 107.60 (160.13)
16 (400) — 16 (406.4) 0.688 (17.48) 112.62 (167.66)
16 (400) — 16 (406.4) 0.75 (19.05) 122.27 (181.98)
16 (400) — 16 (406.4) 0.812 (20.62) 131.84 (196.18)
16 (400) 80 16 (406.4) 0.844 (21.44) 136.74 (203.54)
16 (400) — 16 (406.4) 0.875 (22.22) 141.48 (210.52)
16 (400) — 16 (406.4) 0.938 (23.83) 151.03 (224.83)
16 (400) — 16 (406.4) 1 (25.4) 160.35 (238.66)
16 (400) 100 16 (406.4) 1.031 (26.19) 164.98 (245.57)
16 (400) — 16 (406.4) 1.062 (26.97) 169.59 (252.37)
16 (400) — 16 (406.4) 1.125 (28.58) 178.89 (266.30)
16 (400) — 16 (406.4) 1.188 (30.18) 188.11 (280.01)
16 (400) 120 16 (406.4) 1.219 (30.96) 192.61 (286.66)
16 (400) — 16 (406.4) 1.25 (31.75) 197.10 (293.35)
16 (400) 140 16 (406.4) 1.438 (36.53) 223.85 (333.21)
16 (400) 160 16 (406.4) 1.594 (40.49) 245.48 (365.38)
16 (400) — 16 (406.4) 1.75 (44.45) 266.58 (396.77)
18 (450) 5 18 (457.2) 0.165 (4.19) 31.46 (46.81)
18 (450) — 18 (457.2) 0.188 (4.78) 35.80 (53.33)
18 (450) — 18 (457.2) 0.219 (5.56) 41.63 (61.93)
18 (450) 10 18 (457.2) 0.25 (6.35) 47.44 (70.60)
18 (450) — 18 (457.2) 0.281 (7.14) 53.23 (79.25)
18 (450) 20 18 (457.2) 0.312 (7.92) 58.99 (87.75)
18 (450) — 18 (457.2) 0.344 (8.74) 64.93 (96.66)
18 (450) STD 18 (457.2) 0.375 (9.52) 70.65 (105.11)
18 (450) — 18 (457.2) 0.406 (10.31) 76.36 (113.63)
18 (450) 30 18 (457.2) 0.438 (11.13) 82.23 (122.44)
18 (450) — 18 (457.2) 0.469 (11.91) 87.89 (130.79)
18 (450) XS 18 (457.2) 0.5 (12.7) 93.54 (139.22)
18 (450) 40 18 (457.2) 0.562 (14.27) 104.76 (155.88)
18 (450) — 18 (457.2) 0.625 (15.88) 116.09 (172.83)
18 (450) — 18 (457.2) 0.688 (17.48) 127.32 (189.56)
18 (450) 60 18 (457.2) 0.75 (19.05) 138.30 (205.84)
18 (450) — 18 (457.2) 0.812 (20.62) 149.20 (222.01)
18 (450) — 18 (457.2) 0.875 (22.22) 160.18 (238.36)
18 (450) 80 18 (457.2) 0.938 (23.83) 171.08 (254.68)
18 (450) — 18 (457.2) 1 (25.4) 181.73 (270.48)
18 (450) — 18 (457.2) 1.062 (26.97) 192.29 (286.15)
18 (450) — 18 (457.2) 1.125 (28.58) 202.94 (302.10)
18 (450) 100 18 (457.2) 1.156 (29.36) 208.15 (309.78)
18 (450) — 18 (457.2) 1.188 (30.18) 213.51 (317.82)
18 (450) — 18 (457.2) 1.25 (31.75) 223.82 (333.13)
18 (450) 120 18 (457.2) 1.375 (34.92) 244.37 (363.66)
18 (450) 140 18 (457.2) 1.562 (39.67) 274.48 (408.48)
18 (450) 160 18 (457.2) 1.781 (45.24) 308.79 (459.62)
20 (500) 5 20 (508) 0.188 (4.78) 39.82 (59.32)
20 (500) 20 20 (508) 0.219 (5.56) 46.31 (68.89)
20 (500) 10 20 (508) 0.25 (6.35) 52.78 (78.56)
20 (500) 20 20 (508) 0.281 (7.14) 59.23 (88.19)
20 (500) 20 20 (508) 0.312 (7.92) 65.66 (97.68)
20 (500) 20 20 (508) 0.344 (8.74) 72.28 (107.61)
20 (500) STD / 20 20 (508) 0.375 (9.52) 78.67 (117.03)
20 (500) 20 20 (508) 0.406 (10.31) 85.04 (126.54)
20 (500) 20 20 (508) 0.438 (11.13) 91.59 (136.38)
20 (500) 20 20 (508) 0.469 (11.91) 97.92 (145.71)
20 (500) XS / 30 20 (508) 0.5 (12.7) 104.23 (155.13)
20 (500) 20 20 (508) 0.562 (14.27) 116.78 (173.75)
20 (500) 40 20 (508) 0.594 (15.09) 123.23 (183.43)
20 (500) 20 20 (508) 0.625 (15.88) 129.45 (192.73)
20 (500) 20 20 (508) 0.688 (17.48) 142.03 (211.45)
20 (500) 20 20 (508) 0.75 (19.05) 154.34 (229.71)
20 (500) 60 20 (508) 0.812 (20.62) 166.56 (247.84)
20 (500) 20 20 (508) 0.875 (22.22) 178.89 (266.20)
20 (500) 20 20 (508) 0.938 (23.83) 191.14 (284.54)
20 (500) 20 20 (508) 1 (25.4) 203.11 (302.30)
20 (500) 80 20 (508) 1.031 (26.19) 209.06 (311.19)
20 (500) 20 20 (508) 1.062 (26.97) 215.00 (319.94)
20 (500) 20 20 (508) 1.125 (28.58) 227.00 (337.91)
20 (500) 20 20 (508) 1.188 (30.18) 238.91 (355.63)
20 (500) 20 20 (508) 1.25 (31.75) 250.55 (372.90)
20 (500) 100 20 (508) 1.281 (32.54) 256.34 (381.55)
20 (500) 20 20 (508) 1.312 (33.32) 262.10 (390.05)
20 (500) 20 20 (508) 1.375 (34.92) 273.76 (407.41)
20 (500) 120 20 (508) 1.5 (38.1) 296.65 (441.52)
20 (500) 140 20 (508) 1.75 (44.45) 341.41 (508.15)
20 (500) 160 20 (508) 1.969 (50.01) 379.53 (564.85)
22 (550) 5 22 (558.8) 0.188 (4.78) 43.84 (65.31)
22 (550) — 22 (558.8) 0.219 (5.56) 50.99 (75.86)
22 (550) 10 22 (558.8) 0.25 (6.35) 58.13 (86.51)
22 (550) — 22 (558.8) 0.281 (7.14) 65.24 (97.14)
22 (550) — 22 (558.8) 0.312 (7.92) 72.34 (107.60)
22 (550) — 22 (558.8) 0.344 (8.74) 79.64 (118.56)
22 (550) STD / 20 22 (558.8) 0.375 (9.52) 86.69 (128.96)
22 (550) — 22 (558.8) 0.406 (10.31) 93.72 (139.46)
22 (550) — 22 (558.8) 0.438 (11.13) 100.96 (150.33)
22 (550) — 22 (558.8) 0.469 (11.91) 107.95 (160.63)
22 (550) XS / 30 22 (558.8) 0.5 (12.7) 114.92 (171.04)
22 (550) — 22 (558.8) 0.562 (14.27) 128.79 (191.63)
22 (550) — 22 (558.8) 0.625 (15.88) 142.81 (212.62)
22 (550) — 22 (558.8) 0.688 (17.48) 156.74 (233.35)
22 (550) — 22 (558.8) 0.75 (19.05) 170.37 (253.58)
22 (550) — 22 (558.8) 0.812 (20.62) 183.92 (273.68)
22 (550) 60 22 (558.8) 0.875 (22.22) 197.60 (294.03)
22 (550) — 22 (558.8) 0.938 (23.83) 211.19 (314.39)
22 (550) — 22 (558.8) 1 (25.4) 224.49 (334.12)
22 (550) — 22 (558.8) 1.062 (26.97) 237.70 (353.73)
22 (550) 80 22 (558.8) 1.125 (28.58) 251.05 (373.71)
22 (550) — 22 (558.8) 1.188 (30.18) 264.31 (393.44)
22 (550) — 22 (558.8) 1.25 (31.75) 277.27 (412.68)
22 (550) — 22 (558.8) 1.312 (33.32) 290.15 (431.80)
22 (550) 100 22 (558.8) 1.375 (34.92) 303.16 (451.15)
22 (550) — 22 (558.8) 1.438 (36.53) 316.08 (470.50)
22 (550) — 22 (558.8) 1.5 (38.1) 328.72 (489.25)
22 (550) 120 22 (558.8) 1.625 (41.28) 353.94 (526.85)
22 (550) 140 22 (558.8) 1.875 (47.62) 403.38 (600.32)
22 (550) 160 22 (558.8) 2.125 (53.98) 451.49 (672.03)
24 (600) 5 24 (609.6) 0.218 (5.54) 55.42 (82.53)
24 (600) 10 24 (609.6) 0.25 (6.35) 63.47 (94.47)
24 (600) — 24 (609.6) 0.281 (7.14) 71.25 (106.08)
24 (600) — 24 (609.6) 0.312 (7.92) 79.01 (117.52)
24 (600) — 24 (609.6) 0.344 (8.74) 86.99 (129.51)
24 (600) STD / 20 24 (609.6) 0.375 (9.52) 94.71 (140.89)
24 (600) — 24 (609.6) 0.406 (10.31) 102.40 (152.38)
24 (600) — 24 (609.6) 0.438 (11.13) 110.32 (164.27)
24 (600) — 24 (609.6) 0.469 (11.91) 117.98 (175.55)
24 (600) XS 24 (609.6) 0.5 (12.7) 125.61 (186.95)
24 (600) 30 24 (609.6) 0.562 (14.27) 140.81 (209.51)
24 (600) — 24 (609.6) 0.625 (15.88) 156.17 (232.52)
24 (600) 40 24 (609.6) 0.688 (17.48) 171.45 (255.25)
24 (600) — 24 (609.6) 0.75 (19.05) 186.41 (277.44)
24 (600) — 24 (609.6) 0.812 (20.62) 201.28 (299.51)
24 (600) — 24 (609.6) 0.875 (22.22) 216.31 (321.87)
24 (600) — 24 (609.6) 0.938 (23.83) 231.25 (344.25)
24 (600) 60 24 (609.6) 0.969 (24.61) 238.57 (355.04)
24 (600) — 24 (609.6) 1 (25.4) 245.87 (365.94)
24 (600) — 24 (609.6) 1.062 (26.97) 260.41 (387.52)
24 (600) — 24 (609.6) 1.125 (28.58) 275.10 (409.52)
24 (600) — 24 (609.6) 1.188 (30.18) 289.71 (431.25)
24 (600) 80 24 (609.6) 1.219 (30.96) 296.86 (441.80)
24 (600) — 24 (609.6) 1.25 (31.75) 304.00 (452.46)
24 (600) — 24 (609.6) 1.312 (33.32) 318.21 (473.54)
24 (600) — 24 (609.6) 1.375 (34.92) 332.56 (494.90)
24 (600) — 24 (609.6) 1.438 (36.53) 346.83 (516.27)
24 (600) — 24 (609.6) 1.5 (38.1) 360.79 (536.98)
24 (600) 100 24 (609.6) 1.531 (38.89) 367.74 (547.36)
24 (600) — 24 (609.6) 1.562 (39.67) 374.66 (557.57)
24 (600) 120 24 (609.6) 1.812 (46.02) 429.79 (639.62)
24 (600) 140 24 (609.6) 2.062 (52.37) 483.57 (719.68)
24 (600) 160 24 (609.6) 2.344 (59.54) 542.64 (807.68)
26 (650) — 26 (660.4) 0.25 (6.35) 68.82 (102.42)
26 (650) — 26 (660.4) 0.281 (7.14) 77.26 (115.03)
26 (650) 10 26 (660.4) 0.312 (7.92) 85.68 (127.44)
26 (650) — 26 (660.4) 0.344 (8.74) 94.35 (140.46)
26 (650) STD 26 (660.4) 0.375 (9.52) 102.72 (152.81)
26 (650) — 26 (660.4) 0.406 (10.31) 111.08 (165.29)
26 (650) — 26 (660.4) 0.438 (11.13) 119.69 (178.21)
26 (650) — 26 (660.4) 0.469 (11.91) 128.00 (190.47)
26 (650) XS / 20 26 (660.4) 0.5 (12.7) 136.30 (202.86)
26 (650) — 26 (660.4) 0.562 (14.27) 152.83 (227.39)
26 (650) — 26 (660.4) 0.625 (15.88) 169.54 (252.41)
26 (650) — 26 (660.4) 0.688 (17.48) 186.16 (277.15)
26 (650) — 26 (660.4) 0.75 (19.05) 202.44 (301.31)
26 (650) — 26 (660.4) 0.812 (20.62) 218.64 (325.34)
26 (650) — 26 (660.4) 0.875 (22.22) 235.01 (349.71)
26 (650) — 26 (660.4) 0.938 (23.83) 251.30 (374.10)
26 (650) — 26 (660.4) 1 (25.4) 267.25 (397.77)

NPS 28 through 48 (209 rows).

Swipe horizontally to view all dimensions.

NPS (DN) Schedule / identification Outside diameter, in (mm) Wall thickness, in (mm) Plain-end mass, lb/ft (kg/m)
28 (700) — 28 (711.2) 0.25 (6.35) 74.16 (110.38)
28 (700) — 28 (711.2) 0.281 (7.14) 83.26 (123.97)
28 (700) 10 28 (711.2) 0.312 (7.92) 92.35 (137.36)
28 (700) — 28 (711.2) 0.344 (8.74) 101.70 (151.41)
28 (700) STD 28 (711.2) 0.375 (9.52) 110.74 (164.74)
28 (700) — 28 (711.2) 0.406 (10.31) 119.76 (178.21)
28 (700) — 28 (711.2) 0.438 (11.13) 129.05 (192.16)
28 (700) — 28 (711.2) 0.469 (11.91) 138.03 (205.39)
28 (700) XS / 20 28 (711.2) 0.5 (12.7) 146.99 (218.77)
28 (700) — 28 (711.2) 0.562 (14.27) 164.84 (245.26)
28 (700) 30 28 (711.2) 0.625 (15.88) 182.90 (272.30)
28 (700) — 28 (711.2) 0.688 (17.48) 200.87 (299.05)
28 (700) — 28 (711.2) 0.75 (19.05) 218.48 (325.17)
28 (700) — 28 (711.2) 0.812 (20.62) 236.00 (351.17)
28 (700) — 28 (711.2) 0.875 (22.22) 253.72 (377.55)
28 (700) — 28 (711.2) 0.938 (23.83) 271.36 (403.96)
28 (700) — 28 (711.2) 1 (25.4) 288.63 (429.59)
28 (700) — 28 (711.2) 1.062 (26.97) 305.82 (455.10)
30 (750) 5 30 (762) 0.25 (6.35) 79.51 (118.34)
30 (750) — 30 (762) 0.281 (7.14) 89.27 (132.92)
30 (750) 10 30 (762) 0.312 (7.92) 99.02 (147.29)
30 (750) — 30 (762) 0.344 (8.74) 109.06 (162.36)
30 (750) STD 30 (762) 0.375 (9.52) 118.76 (176.67)
30 (750) — 30 (762) 0.406 (10.31) 128.44 (191.12)
30 (750) — 30 (762) 0.438 (11.13) 138.42 (206.10)
30 (750) — 30 (762) 0.469 (11.91) 148.06 (220.32)
30 (750) XS / 20 30 (762) 0.5 (12.7) 157.68 (234.68)
30 (750) — 30 (762) 0.562 (14.27) 176.86 (263.14)
30 (750) 30 30 (762) 0.625 (15.88) 196.26 (292.20)
30 (750) — 30 (762) 0.688 (17.48) 215.58 (320.95)
30 (750) — 30 (762) 0.75 (19.05) 234.51 (349.04)
30 (750) — 30 (762) 0.812 (20.62) 253.36 (377.01)
30 (750) — 30 (762) 0.875 (22.22) 272.43 (405.38)
30 (750) — 30 (762) 0.938 (23.83) 291.41 (433.81)
30 (750) — 30 (762) 1 (25.4) 310.01 (461.41)
30 (750) — 30 (762) 1.062 (26.97) 328.53 (488.88)
30 (750) — 30 (762) 1.125 (28.58) 347.26 (516.93)
30 (750) — 30 (762) 1.188 (30.18) 365.90 (544.68)
30 (750) — 30 (762) 1.25 (31.75) 384.17 (571.79)
32 (800) — 32 (813) 0.25 (6.35) 84.85 (126.32)
32 (800) — 32 (813) 0.281 (7.14) 95.28 (141.90)
32 (800) 10 32 (813) 0.312 (7.92) 105.69 (157.25)
32 (800) — 32 (813) 0.344 (8.74) 116.41 (173.35)
32 (800) STD 32 (813) 0.375 (9.52) 126.78 (188.64)
32 (800) — 32 (813) 0.406 (10.31) 137.12 (204.09)
32 (800) — 32 (813) 0.438 (11.13) 147.78 (220.10)
32 (800) — 32 (813) 0.469 (11.91) 158.08 (235.29)
32 (800) XS / 20 32 (813) 0.5 (12.7) 168.37 (250.65)
32 (800) — 32 (813) 0.562 (14.27) 188.87 (281.09)
32 (800) 30 32 (813) 0.625 (15.88) 209.62 (312.17)
32 (800) 40 32 (813) 0.688 (17.48) 230.29 (342.94)
32 (800) — 32 (813) 0.75 (19.05) 250.55 (373.00)
32 (800) — 32 (813) 0.812 (20.62) 270.72 (402.94)
32 (800) — 32 (813) 0.875 (22.22) 291.14 (433.33)
32 (800) — 32 (813) 0.938 (23.83) 311.47 (463.78)
32 (800) — 32 (813) 1 (25.4) 331.39 (493.35)
32 (800) — 32 (813) 1.062 (26.97) 351.23 (522.80)
32 (800) — 32 (813) 1.125 (28.58) 371.31 (552.88)
32 (800) — 32 (813) 1.188 (30.18) 391.30 (582.64)
32 (800) — 32 (813) 1.25 (31.75) 410.90 (611.72)
34 (850) — 34 (864) 0.25 (6.35) 90.20 (134.31)
34 (850) — 34 (864) 0.281 (7.14) 101.29 (150.88)
34 (850) 10 34 (864) 0.312 (7.92) 112.36 (167.21)
34 (850) — 34 (864) 0.344 (8.74) 123.77 (184.34)
34 (850) STD 34 (864) 0.375 (9.52) 134.79 (200.61)
34 (850) — 34 (864) 0.406 (10.31) 145.80 (217.06)
34 (850) — 34 (864) 0.438 (11.13) 157.14 (234.10)
34 (850) — 34 (864) 0.469 (11.91) 168.11 (250.27)
34 (850) XS / 20 34 (864) 0.5 (12.7) 179.06 (266.63)
34 (850) — 34 (864) 0.562 (14.27) 200.89 (299.04)
34 (850) 30 34 (864) 0.625 (15.88) 222.99 (332.14)
34 (850) 40 34 (864) 0.688 (17.48) 245.00 (364.92)
34 (850) — 34 (864) 0.75 (19.05) 266.58 (396.96)
34 (850) — 34 (864) 0.812 (20.62) 288.08 (428.88)
34 (850) — 34 (864) 0.875 (22.22) 309.84 (461.28)
34 (850) — 34 (864) 0.938 (23.83) 331.52 (493.75)
34 (850) — 34 (864) 1 (25.4) 352.77 (525.30)
34 (850) — 34 (864) 1.062 (26.97) 373.94 (556.73)
34 (850) — 34 (864) 1.125 (28.58) 395.36 (588.83)
34 (850) — 34 (864) 1.188 (30.18) 416.70 (620.60)
34 (850) — 34 (864) 1.25 (31.75) 437.62 (651.65)
36 (900) — 36 (914) 0.25 (6.35) 95.54 (142.14)
36 (900) — 36 (914) 0.281 (7.14) 107.30 (159.68)
36 (900) 10 36 (914) 0.312 (7.92) 119.03 (176.97)
36 (900) — 36 (914) 0.344 (8.74) 131.12 (195.12)
36 (900) STD 36 (914) 0.375 (9.52) 142.81 (212.35)
36 (900) — 36 (914) 0.406 (10.31) 154.48 (229.77)
36 (900) — 36 (914) 0.438 (11.13) 166.51 (247.82)
36 (900) — 36 (914) 0.469 (11.91) 178.14 (264.96)
36 (900) XS / 20 36 (914) 0.5 (12.7) 189.75 (282.29)
36 (900) — 36 (914) 0.562 (14.27) 212.90 (316.63)
36 (900) 30 36 (914) 0.625 (15.88) 236.35 (351.73)
36 (900) — 36 (914) 0.688 (17.48) 259.71 (386.47)
36 (900) 40 36 (914) 0.75 (19.05) 282.62 (420.45)
36 (900) — 36 (914) 0.812 (20.62) 305.44 (454.30)
36 (900) — 36 (914) 0.875 (22.22) 328.55 (488.68)
36 (900) — 36 (914) 0.938 (23.83) 351.57 (523.14)
36 (900) — 36 (914) 1 (25.4) 374.15 (556.62)
36 (900) — 36 (914) 1.062 (26.97) 396.64 (589.98)
36 (900) — 36 (914) 1.125 (28.58) 419.42 (624.07)
36 (900) — 36 (914) 1.188 (30.18) 442.10 (657.81)
36 (900) — 36 (914) 1.25 (31.75) 464.35 (690.80)
38 (950) — 38 (965) 0.312 (7.92) 125.70 (186.94)
38 (950) — 38 (965) 0.344 (8.74) 138.47 (206.11)
38 (950) STD 38 (965) 0.375 (9.52) 150.83 (224.33)
38 (950) — 38 (965) 0.406 (10.31) 163.16 (242.74)
38 (950) — 38 (965) 0.438 (11.13) 175.87 (261.82)
38 (950) — 38 (965) 0.469 (11.91) 188.17 (279.94)
38 (950) XS 38 (965) 0.5 (12.7) 200.44 (298.26)
38 (950) — 38 (965) 0.562 (14.27) 224.92 (334.58)
38 (950) — 38 (965) 0.625 (15.88) 249.71 (371.70)
38 (950) — 38 (965) 0.688 (17.48) 274.42 (408.46)
38 (950) — 38 (965) 0.75 (19.05) 298.65 (444.41)
38 (950) — 38 (965) 0.812 (20.62) 322.80 (480.24)
38 (950) — 38 (965) 0.875 (22.22) 347.26 (516.62)
38 (950) — 38 (965) 0.938 (23.83) 371.63 (553.11)
38 (950) — 38 (965) 1 (25.4) 395.53 (588.57)
38 (950) — 38 (965) 1.062 (26.97) 419.35 (623.90)
38 (950) — 38 (965) 1.125 (28.58) 443.47 (660.01)
38 (950) — 38 (965) 1.188 (30.18) 467.50 (695.77)
38 (950) — 38 (965) 1.25 (31.75) 491.07 (730.74)
40 (1000) 40 40 (1016) 0.312 (7.92) 132.37 (196.90)
40 (1000) 40 40 (1016) 0.344 (8.74) 145.83 (217.11)
40 (1000) STD 40 (1016) 0.375 (9.52) 158.85 (236.30)
40 (1000) 40 40 (1016) 0.406 (10.31) 171.84 (255.71)
40 (1000) 40 40 (1016) 0.438 (11.13) 185.24 (275.82)
40 (1000) 40 40 (1016) 0.469 (11.91) 198.19 (294.92)
40 (1000) XS 40 (1016) 0.5 (12.7) 211.13 (314.23)
40 (1000) 40 40 (1016) 0.562 (14.27) 236.93 (352.53)
40 (1000) 40 40 (1016) 0.625 (15.88) 263.07 (391.67)
40 (1000) 40 40 (1016) 0.688 (17.48) 289.13 (430.45)
40 (1000) 40 40 (1016) 0.75 (19.05) 314.69 (468.37)
40 (1000) 40 40 (1016) 0.812 (20.62) 340.16 (506.17)
40 (1000) 40 40 (1016) 0.875 (22.22) 365.97 (544.57)
40 (1000) 40 40 (1016) 0.938 (23.83) 391.68 (583.08)
40 (1000) 40 40 (1016) 1 (25.4) 416.91 (620.51)
40 (1000) 40 40 (1016) 1.062 (26.97) 442.05 (657.82)
40 (1000) 40 40 (1016) 1.125 (28.58) 467.52 (695.96)
40 (1000) 40 40 (1016) 1.188 (30.18) 492.90 (733.73)
40 (1000) 40 40 (1016) 1.25 (31.75) 517.80 (770.67)
42 (1050) — 42 (1067) 0.344 (8.74) 153.18 (228.10)
42 (1050) STD 42 (1067) 0.375 (9.52) 166.86 (248.27)
42 (1050) — 42 (1067) 0.406 (10.31) 180.52 (268.67)
42 (1050) — 42 (1067) 0.438 (11.13) 194.60 (289.82)
42 (1050) — 42 (1067) 0.469 (11.91) 208.22 (309.90)
42 (1050) XS 42 (1067) 0.5 (12.7) 221.82 (330.21)
42 (1050) — 42 (1067) 0.625 (15.88) 276.44 (411.64)
42 (1050) — 42 (1067) 0.688 (17.48) 303.84 (452.43)
42 (1050) — 42 (1067) 0.75 (19.05) 330.72 (492.33)
42 (1050) — 42 (1067) 0.812 (20.62) 357.52 (532.11)
42 (1050) — 42 (1067) 0.938 (23.83) 411.74 (613.05)
42 (1050) — 42 (1067) 1 (25.4) 438.29 (652.46)
42 (1050) — 42 (1067) 1.062 (26.97) 464.76 (691.75)
42 (1050) — 42 (1067) 1.125 (28.58) 491.57 (731.91)
42 (1050) — 42 (1067) 1.188 (30.18) 518.30 (771.69)
42 (1050) — 42 (1067) 1.25 (31.75) 544.52 (810.60)
44 (1100) — 44 (1118) 0.344 (8.74) 160.54 (239.09)
44 (1100) STD 44 (1118) 0.375 (9.52) 174.88 (260.25)
44 (1100) — 44 (1118) 0.406 (10.31) 189.20 (281.64)
44 (1100) — 44 (1118) 0.438 (11.13) 203.97 (303.82)
44 (1100) — 44 (1118) 0.469 (11.91) 218.25 (324.88)
44 (1100) XS 44 (1118) 0.5 (12.7) 232.51 (346.18)
44 (1100) — 44 (1118) 0.562 (14.27) 260.97 (388.42)
44 (1100) — 44 (1118) 0.625 (15.88) 289.80 (431.62)
44 (1100) — 44 (1118) 0.688 (17.48) 318.55 (474.42)
44 (1100) — 44 (1118) 0.75 (19.05) 346.76 (516.29)
44 (1100) — 44 (1118) 0.812 (20.62) 374.88 (558.04)
44 (1100) — 44 (1118) 0.875 (22.22) 403.38 (600.46)
44 (1100) — 44 (1118) 0.938 (23.83) 431.79 (643.03)
44 (1100) — 44 (1118) 1 (25.4) 459.67 (684.41)
44 (1100) — 44 (1118) 1.125 (28.58) 515.63 (767.85)
44 (1100) — 44 (1118) 1.188 (30.18) 543.70 (809.65)
44 (1100) — 44 (1118) 1.25 (31.75) 571.25 (850.54)
46 (1150) — 46 (1168) 0.344 (8.74) 167.89 (249.87)
46 (1150) STD 46 (1168) 0.375 (9.52) 182.90 (271.99)
46 (1150) — 46 (1168) 0.406 (10.31) 197.88 (294.35)
46 (1150) — 46 (1168) 0.438 (11.13) 213.33 (317.54)
46 (1150) — 46 (1168) 0.469 (11.91) 228.27 (339.56)
46 (1150) XS 46 (1168) 0.5 (12.7) 243.20 (361.84)
46 (1150) — 46 (1168) 0.562 (14.27) 272.98 (406.02)
46 (1150) — 46 (1168) 0.625 (15.88) 303.16 (451.20)
46 (1150) — 46 (1168) 0.688 (17.48) 333.26 (495.97)
46 (1150) — 46 (1168) 0.75 (19.05) 362.79 (539.78)
46 (1150) — 46 (1168) 0.812 (20.62) 392.24 (583.47)
46 (1150) — 46 (1168) 0.875 (22.22) 422.09 (627.86)
46 (1150) — 46 (1168) 0.938 (23.83) 451.85 (672.41)
46 (1150) — 46 (1168) 1 (25.4) 481.05 (715.73)
46 (1150) — 46 (1168) 1.062 (26.97) 510.17 (758.92)
46 (1150) — 46 (1168) 1.125 (28.58) 539.68 (803.09)
46 (1150) — 46 (1168) 1.188 (30.18) 569.10 (846.86)
46 (1150) — 46 (1168) 1.25 (31.75) 597.97 (889.69)
48 (1200) — 48 (1219) 0.344 (8.74) 175.25 (260.86)
48 (1200) STD 48 (1219) 0.375 (9.52) 190.92 (283.96)
48 (1200) — 48 (1219) 0.406 (10.31) 206.56 (307.32)
48 (1200) — 48 (1219) 0.438 (11.13) 222.70 (331.54)
48 (1200) — 48 (1219) 0.469 (11.91) 238.30 (354.54)
48 (1200) XS 48 (1219) 0.5 (12.7) 253.89 (377.81)
48 (1200) — 48 (1219) 0.562 (14.27) 285.00 (423.97)
48 (1200) — 48 (1219) 0.625 (15.88) 316.52 (471.17)
48 (1200) — 48 (1219) 0.688 (17.48) 347.97 (517.95)
48 (1200) — 48 (1219) 0.75 (19.05) 378.83 (563.74)
48 (1200) — 48 (1219) 0.812 (20.62) 409.61 (609.40)
48 (1200) — 48 (1219) 0.875 (22.22) 440.80 (655.81)
48 (1200) — 48 (1219) 0.938 (23.83) 471.90 (702.38)
48 (1200) — 48 (1219) 1 (25.4) 502.43 (747.67)
48 (1200) — 48 (1219) 1.062 (26.97) 532.88 (792.84)
48 (1200) — 48 (1219) 1.125 (28.58) 563.73 (839.04)
48 (1200) — 48 (1219) 1.188 (30.18) 594.50 (884.82)
48 (1200) — 48 (1219) 1.25 (31.75) 624.70 (929.62)

Applications and Service Limits for ASME SA-106 Grade B Seamless Pipe

SA-106 Grade B is used for high-temperature steam, boiler and process lines where the order names the ASME listing. A Section II, Part A listing is not by itself permission under every construction Code part. The applicable construction Code, allowable-stress table and edition still have to be checked. Do not treat an A106 Grade B pipe as SA-106 unless both the marking and the certificate say so, and do not treat SA-53 as this product.

Near-Equivalents for ASME SA-106 Grade B: Not Automatic Substitutes

ASTM A106/A106M-19a is the text adopted as identical in the 2023 SA-106 specification, but an A106 certificate is not automatically an SA-106 certificate. ASTM A53 Type S Grade B and ASME SA-53 are different listings. EN 10216-1 P235TR1 and JIS G 3454 STPG370 are neighbouring seamless products, not restamps. SA-106 Grade A and Grade C stay on their own enquiries.

Sourcing ASME SA-106 Grade B Seamless Steel Pipe from SHH STEEL

Send the NPS or diameter, the wall or schedule, the length, and the BPVC Section II, Part A edition required, and name SA-106 Grade B explicitly. Do not use the ASTM A106 term, or an SA-53 term, for this page. SHH STEEL reviews the grade, the Code edition and the certificate before quoting. The size table is a typographical reference, not a warehouse list.

ASME SA-106 Grade B FAQs

Is SA-106 the same as ASTM A106?
The 2023 SA-106/SA-106M text is identical with A106/A106M-19a, but an ordinary A106 certificate is not an SA-106 certificate. Name the SA designation and the Code edition when that listing is required.
Why 19a and not 19?
The 2023 Section II, Part A title page of SA-106/SA-106M states that it is identical with A106/A106M-19a. A later or earlier ASTM year is not assumed to be that adopted text.
Is this the same as SA-53?
No. SA-53 is a different Section II listing for welded and seamless pipe, and a 2023 SA-53 pack is not issued from this work. Do not treat the two designations as interchangeable.
Are the sizes a stock list?
No. They are the typographical B36.10 subset already used on the ASTM A106 Grade B page, not a warehouse list.

Conclusion

ASME SA-106 Grade B follows the 2023 Section II, Part A text, identical with A106/A106M-19a, with 60 ksi tensile and 35 ksi yield. An A106 certificate is not SA-106. Confirm the size, the Code edition and the certificate on the order.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X