RCC-M M3307 Austenitic Stainless Steel Plates | RCC-M M3307 Procurement Specification
What is RCC-M M3307?
RCC-M M3307 Austenitic Stainless Steel Plates refers to Part Procurement Specification M3307 of RCC-M, the AFCEN code of design and construction rules for mechanical components of PWR nuclear islands. M3307 is titled Class 1, 2 and 3 austenitic stainless steel plates. It is not a standalone ISO or ASTM style product standard and not a commercial grade-by-grade standard; it sets procurement requirements for plates that will be used in RCC-M components.
RCC-M is issued in editions; AFCEN’s latest is the 2024 edition (the fourteenth), after the 2022, 2020 and 2018 editions. The applicable M3307 text is the one in the RCC-M edition and addenda named in the equipment specification. In RCC-M material lists, M3307 is referenced for parts such as plate for fabricated parts and heads of auxiliary tanks, fittings and orifice plates in stainless auxiliary piping, and austenitic stainless plate for supports.
AFCEN RCC-M Errata 008 (January 2025, applying to the 2018 and 2020 editions, Annex ZY 350) lists M3307 among the procurement specifications whose procurement is compliant with the ESPN technical-qualification essential safety requirement without a specific technical qualification file. That is a property of the code text, not a qualification of any supplier.
Important: M3307 is a procurement specification inside the AFCEN RCC-M code. Neither the specification nor this page, nor its listing in our Nuclear-Grade Steel Plates range, is a nuclear, RCC-M or ASME Section III qualification of SHH STEEL, of a mill or of a given heat. Supply to RCC-M requires the code edition, component class, material organisation, surveillance and inspection arrangements written on the purchase order and accepted by the purchaser.
SHH STEEL supplies austenitic stainless plate for enquiries written to RCC-M M3307 as a producer, exporter and mill agent, and reviews the edition, grade and requirements before quoting. The specification is listed in our RCC-M M3307 range under Nuclear-Grade Steel Plates.
Nature of the M3307 specification
The items below describe the nature of the specification. Values are not reproduced because they depend on the RCC-M edition and are confirmed from the cited text on each order.
| Parameter | Detail |
|---|---|
| Specification | AFCEN RCC-M, Section II, Part Procurement Specification M3307, Class 1, 2 and 3 austenitic stainless steel plates |
| Edition | As named on the purchase order (RCC-M 2024 is AFCEN’s latest edition) |
| Steel family | Austenitic chromium-nickel stainless steels, with and without molybdenum, in normal and low-carbon versions |
| Component classes | RCC-M Class 1, 2 and 3 components, as stated in the specification title |
| Related sheet specification | M3307 Bis covers Class 2 and 3 austenitic stainless steel sheets |
| Grade list, chemistry, mechanical, impact, NDE | Per the M3307 text in the cited edition; confirmed per order, not reproduced here |
| Sizes | Per the order; no stock range implied |
Chemical composition under M3307
M3307 sets its own chemistry for each grade, which can be tighter than commercial standards, for example on carbon, cobalt and other residual elements relevant to nuclear service. Material databases associate AFCEN designations such as Z2 CN 18-10, Z6 CN 18-10, Z2 CND 17-12 and Z6 CND 17-12, and controlled-nitrogen variants, with M3307 across editions. The grade list and limits must be read from the edition on the purchase order.
| Item | How it is set |
|---|---|
| Grades | Per M3307 in the cited RCC-M edition |
| Heat and product analysis limits | Per M3307 tables; not reproduced on this page |
| Residual elements (for example cobalt) | Per M3307 and the equipment specification |
| Reporting | As the specification and the order require |
We do not publish M3307 numbers taken from commercial summaries. Send the edition and grade, and the values are checked against that text before quotation.
Mechanical properties under M3307
Room-temperature and elevated-temperature tensile requirements, any impact requirements and the test sampling plan are those of M3307 in the cited edition, together with RCC-M Section II general rules.
| Property | Requirement |
|---|---|
| Tensile and yield strength | Per M3307, edition on the order |
| Elevated-temperature tensile | Per M3307 where specified |
| Impact testing | Per M3307 where specified |
| Intergranular corrosion and other tests | Per M3307 and the order |
Delivery condition of M3307 plates
Austenitic stainless plates are normally delivered in the solution-annealed condition with a descaled surface. The heat-treatment parameters, surface condition and cleanliness requirements for M3307 plates are those of the cited specification and the RCC-M fabrication rules.
- Condition: per M3307, normally solution annealed and quenched
- Surface: per M3307 and the order
- Marking and traceability: per M3307 and RCC-M Section II
Welding austenitic M3307 plates
Austenitic 18-10 and 17-12 stainless steels are readily weldable. Low-carbon grades limit sensitisation in the heat-affected zone. For RCC-M components, welding procedures, filler materials and welder qualifications follow RCC-M Section IV and the equipment specification, not this page.
Dimensions and examination
Dimensional tolerances and non-destructive examination for M3307 plates are those of the specification and the order. Ultrasonic and surface examination requirements are confirmed against the cited edition.
| Item | Requirement |
|---|---|
| Thickness, width, length, flatness | Per M3307 and the order |
| Non-destructive examination | Per M3307 and the order |
Where M3307 plate is referenced
In RCC-M material lists, M3307 plate is referenced for items such as auxiliary tank shells and heads, fittings and orifice plates in stainless auxiliary piping, and stainless plate for supports. The equipment specification decides whether M3307 applies to a given part.
Important: M3307 is a procurement specification inside the AFCEN RCC-M code. Neither the specification nor this page, nor its listing in our Nuclear-Grade Steel Plates range, is a nuclear, RCC-M or ASME Section III qualification of SHH STEEL, of a mill or of a given heat. Supply to RCC-M requires the code edition, component class, material organisation, surveillance and inspection arrangements written on the purchase order and accepted by the purchaser.
Compare RCC-M M3307 with commercial stainless plate standards
Commercial austenitic plate standards cover similar chemistries but not the RCC-M procurement requirements. A commercial certificate does not satisfy an M3307 order on its own.
| Specification | Nature | Relation to M3307 |
|---|---|---|
| RCC-M M3307 | Nuclear code procurement specification | This page |
| ASTM A240 Type 304L | Commercial ASTM plate standard | Similar low-carbon Cr-Ni chemistry; not a substitute |
| ASTM A240 Type 316L | Commercial ASTM plate standard | Similar low-carbon Cr-Ni-Mo chemistry; not a substitute |
| EN 10028-7 1.4307 X2CrNi18-9 | European pressure-vessel stainless plate | Similar chemistry; not a substitute |
| EN 10028-7 1.4404 X2CrNiMo17-12-2 | European pressure-vessel stainless plate | Similar chemistry; not a substitute |
Near commercial chemistries for M3307 grades
The table gives nearest commercial chemistries by engineering judgement only. They are not automatic substitutes and do not carry RCC-M requirements.
| AFCEN-style designation (examples) | Near commercial chemistry | Note |
|---|---|---|
| Z2 CN 18-10 | EN 10028-7 1.4307 X2CrNi18-9, ASME SA240 304L | Low-carbon Cr-Ni; engineering judgement only |
| Z6 CN 18-10 | EN 10028-7 1.4301 X5CrNi18-10 | Cr-Ni; engineering judgement only |
| Z2 CND 17-12 | EN 10028-7 1.4404 X2CrNiMo17-12-2, ASME SA240 316L | Low-carbon Cr-Ni-Mo; engineering judgement only |
| Z6 CND 17-12 | EN 10028-7 1.4401 X5CrNiMo17-12-2 | Cr-Ni-Mo; engineering judgement only |
Why choose SHH STEEL for M3307 enquiries
- SHH STEEL reviews RCC-M M3307 enquiries as a producer, exporter and mill agent
- We read the cited RCC-M edition and grade before quoting, instead of using generic numbers
- We state clearly that the listing is not a nuclear qualification
- We match documentation and third-party inspection to the order
How to enquire for RCC-M M3307 plates
| Item | What to state |
|---|---|
| Code | RCC-M edition and addenda, M3307, component class |
| Grade | AFCEN designation required |
| Size | Thickness, width, length and quantity |
| Inspection | Surveillance, third-party inspection and documents required |
We confirm feasibility after reviewing the specification text.
FAQ
-
What is RCC-M M3307?
- An AFCEN RCC-M Section II procurement specification titled Class 1, 2 and 3 austenitic stainless steel plates, used for PWR mechanical components.
-
Is M3307 a commercial product standard?
- No. It is a code procurement specification. The grades and requirements come from the RCC-M edition named on the order.
-
Does this page mean SHH STEEL is RCC-M qualified?
- No. Neither the specification nor this listing is a nuclear, RCC-M or ASME Section III qualification of SHH STEEL, a mill or a heat.
-
What does AFCEN Errata 008 say about M3307?
- It lists M3307 among procurements compliant with the ESPN technical-qualification requirement without a specific qualification file. That concerns the code, not any supplier.
-
What should an enquiry include?
- The RCC-M edition, M3307, component class, AFCEN grade, sizes, quantity and the inspection and documentation arrangements.
Request a quotation
Contact SHH STEEL for a quotation for RCC-M M3307 austenitic stainless steel plates. Please send the specification and edition, grade, thickness, width, length, quantity, delivery destination and preferred delivery schedule so we can review your production and export requirements.
State the RCC-M edition and addenda, component class, AFCEN grade and the surveillance and inspection arrangements.
State any supplementary requirements, simulated post-weld heat treatment, impact testing, ultrasonic examination and the inspection document required, so they are agreed before the order is placed.
For a detailed quotation, email your material specification, drawing, quantity and delivery requirements to our team.
Contact: admin@steelspecs.com