ISO 630-2 SG250 Steel Plate | SG250 General Structural Plate (Annex B) | ISO 630-2 general structural plate - SHH STEEL

ISO 630-2 SG250 Steel Plate | SG250 General Structural Plate (Annex B)

ISO 630-2 SG250 steel plate is grade SG250 of ISO 630-2:2021 (Edition 3), Annex B, a general-purpose structural steel for plates, wide flats, sections and bars. The purchaser must state the quality (A, B, C or D) and any required delivery condition. SHH STEEL reviews dimensions, inspection documents and official Annex B acceptance before confirming supply.
Keywords
ISO 630-2 SG250 plate, SG250 structural plate, ISO 630-2 Annex B, general-purpose structural steel, SG250 steel plate
Equivalent Grades:
ASTM A36, JIS G3101 SS400, GB/T 700 Q235B (approx.)
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is ISO 630-2 SG250 plate?

ISO 630-2 SG250 is grade SG250 of ISO 630-2:2021 (Edition 3), the international standard for technical delivery conditions for structural steels for general purposes. This grade is covered in Annex B. ISO 630-1 supplies the general technical delivery conditions.

ISO 630-2 specifies eight grades and up to four qualities. Annex A covers S235, S275, S355 and S460. Annex B covers SG205, SG250, SG285 and SG345. Clause 4.3 states that the two annexes are to be regarded separately; each is independent of the other. An Annex A S-grade is not a substitute for this Annex B grade.

Each SG grade is available in up to four qualities: A (no impact testing), B (impact at 20 °C), C (impact at 0 °C) and D (impact at −20 °C). Not every grade is available in every quality. This page is written at grade level; the purchaser must state the quality on the order. Impact energy values sit in Table B.4 and are not transcribed here.

SHH STEEL reviews enquiries against the ordered ISO 630-2:2021 edition, the Annex B grade and quality, and the inspection document. Reconfirm the edition when placing a later order.

Material specification for ISO 630-2 SG250

As of 12 November 2026, ISO 630-2:2021 (Edition 3, April 2021) remains the published edition. It cancels and replaces ISO 630-2:2011 and was technically revised. This page is written to the 2021 edition.

Ordering item Basis
Standard ISO 630-2:2021, Edition 3
General requirements ISO 630-1
Grade SG250 (Annex B)
Quality State A, B, C or D; not all qualities may be available
Product form Reversing-mill plate enquiry; the standard also covers wide flats, sections and bars
Thickness The official scope sets no restriction on nominal thickness for SG205, SG250, SG285 and SG345 for flat products, sections and long products. That is not a stock list.
Delivery condition State a required condition if one is needed; otherwise clause 6.2 leaves it to the manufacturer
Inspection document Specify the document type; see ISO 630-1

Mandatory purchaser information is specified in ISO 630-1. Options include a particular delivery condition, transverse impact testing and special steelmaking. State any option at enquiry.

ASTM A36 plate comparison chemistry (not ISO Table B.1)

Clause 6.3.1 requires the heat analysis of Annex B grades to comply with Table B.1. Clause 6.3.2 refers the permitted deviations for SG205, SG250, SG285 and SG345, relative to the heat analysis, to Table B.2. Those official tables are not in the 2021 preview consulted for this work, and they are not transcribed here as ISO normative rows.

The following figures are related-specification comparison/reference data for ASTM A36, a structural plate in the same yield-strength class. They are not ISO Table B.1 limits. A maximum is not a target addition. Confirm the official ISO Table B.1 and Table B.2 rows before accepting a certificate.

Element Cast / heat analysis, mass %
C ≤0.25 to ≤0.29, depending on thickness
Mn 0.80–1.20, required for thicker plates
P ≤0.030 to ≤0.040
S ≤0.030 to ≤0.050
Si 0.15–0.40, required for thicker plates

The carbon, phosphorus and sulphur windows on the ASTM page vary with product thickness. Those ASTM thickness rules are not ISO Table B.1 rules.

Clause 6.3.3 gives maximum CEV requirements for Annex A grades in Table A.3. That table does not apply to Annex B. Any CEV agreement for an SG grade must be taken from the official Annex B text, not from Table A.3.

ASTM A36 mechanical comparison (not ISO Table B.3)

The designation SG250 identifies a 250 MPa yield-strength class in Annex B. Tensile properties at room temperature shall comply with Table B.3, and Charpy V-notch properties with Table B.4. Those official tables are not in the 2021 preview and are not transcribed here as ISO normative limits.

Quality B is impact-tested at 20 °C, quality C at 0 °C and quality D at −20 °C (clause 4.2). Quality A has no impact test. Those are specified test temperatures, not design temperatures and not impact-energy values. Confirm Table B.4 against the official text. Specimen orientation is longitudinal unless a transverse test is agreed.

The following values are related-specification comparison/reference data. They must not be treated as ISO Table B.3 or Table B.4 limits and must not be used as allowable design stresses.

Property Comparison value
Yield strength, min, ≤200 mm 250 MPa (36 ksi)
Yield strength, min, >200 mm 220 MPa (32 ksi)
Tensile strength 400–550 MPa (58–80 ksi)
Elongation in 200 mm, min 20 %
Elongation in 50 mm, min 23 %

The 250 MPa yield for plates up to 200 mm coincides with the SG250 yield class. JIS SS400 and GB/T 700 Q235B are nearby 245/235 MPa-class plates, not identical ISO grades.

Delivery condition and ordering options for SG250

At the manufacturer’s discretion, clause 6.2 requires products to be delivered in the as-rolled condition, the normalized-rolled condition, the normalized condition, or the thermomechanical processed condition, unless a particular condition is agreed at the time of order. The actual condition shall be recorded on the inspection document.

Clause 8.2.2 sets the Annex B test unit: products of the same form, grade, quality, delivery condition and thickness range as specified in Table B.3, by heat and 50 tonnes or part thereof. By agreement at the time of ordering, two tests by heat may be used. Do not apply the Annex A 60-tonne or 80-tonne rules to this grade.

Weldability and fabrication review for SG250

SG250 is intended, as the standard’s scope describes, for welded or bolted structures in the as-delivered condition. That statement is not a qualified welding procedure. The fabricator must establish consumables, preheat, heat input and any post-weld treatment through the applicable procedure qualification and design requirements.

If a copper range or a silicon control for zinc coating is agreed, say so at enquiry; those options can affect weldability and are Annex-specific where the official text provides them. Confirm any such option against Annex B, not by copying an Annex A note.

Dimensions, surface quality and inspection

Surface condition, internal soundness, dimensions, tolerances and marking refer to ISO 630-1. This preview does not supply the full tolerance schedule; no numeric thickness deviation, flatness allowance or ultrasonic acceptance class is claimed.

State the required nominal dimensions, edge condition, surface restrictions, internal-soundness examination and document type with the enquiry. Identification must remain traceable through cutting, packing and shipment. Dimensional availability remains subject to mill confirmation. The official ‘no thickness restriction’ statement for SG grades is a scope statement, not a promise that every thickness is in stock.

Applications and service limits of SG250

SG250 may be considered for general-purpose welded or bolted structures — frames, members, plates in buildings, bridges and similar construction — where the design specification selects this exact ISO 630-2 Annex B grade and quality. These are intended-use examples, not authorization for a particular load, temperature or construction code.

Impact quality, if required by the project, must be stated. Quality A does not include an impact test. The comparison yield class is not a design allowable.

Compare SG250 with related ISO 630-2 grades

Compare the following published ISO 630-2 Annex A grades by their complete annex rows, quality and project acceptance. Annex A and Annex B are independent. These are related selections within the standard, not interchangeable materials. Other SG grades are not linked here until those product pages are live.

ISO product Classification Review before a grade change
ISO 630-2 S235B Annex A, quality B, 20 °C impact Different annex and a 235 MPa class. Not a substitute for SG250.
ISO 630-2 S275B Annex A, quality B Higher Annex A yield class (275 MPa). Review the complete annex row.
ISO 630-2 S355B Annex A, quality B Higher Annex A yield class. The two annexes are independent.

Related grades and substitution limits for SG250

The heading identifies a comparison topic, not a declaration of interchangeable material. No automatic foreign equivalent or dual certification is offered for SG250.

Product / range Verified relationship or limitation Substitution control
JIS G 3101 SS400 Related 400 MPa tensile-class Japanese structural plate. Yield is thickness-dependent and is not 250 MPa in every band. Engineer approval required; not an automatic equivalent.
GB/T 700 Q235B Related 235 MPa-class Chinese carbon plate. Nearby yield class only. Engineer approval required; not an automatic equivalent.
ISO 630-2 S235B / ISO 630-2 S275B Annex A grades in the same standard. Annex A and Annex B are independent. Engineer approval required; not an automatic equivalent.

Complete specification review and engineer approval are required before substitution. Chemistry, tensile and impact requirements, thickness, delivery condition and the project specification must all be checked.

Why choose SHH STEEL for SG250

SHH STEEL supports specification-led structural-plate purchasing rather than substitution by catalogue name.

  • We quote the requested ISO 630-2:2021 edition, Annex B grade and quality separately from Annex A S-grades and from national-standard plates.
  • Comparison figures on this page are labelled as such; they are not used as unofficial ISO Table B.1 or Table B.3 limits.
  • Delivery condition, impact quality and inspection-document type are reviewed before confirmation.
  • Supply capability, lead time and any additional testing remain subject to quotation confirmation.

Enquiry and supply review for SG250

Send the project material schedule for SG250. SHH STEEL will review the enquiry and identify any clarification needed before confirming the supply route.

Enquiry item Information required
Material identity ISO 630-2:2021 SG250; state the quality (A, B, C or D); identify any proposed dual certification
Dimensions and quantity Product form, nominal thickness, width, length, quantity and cutting drawings
Delivery condition Required condition if one is particular; otherwise clause 6.2 leaves it to the manufacturer
Acceptance values Complete official Annex B chemistry, tensile and impact rows for the ordered edition; say if comparison values are for enquiry only
Inspection document Document type; see ISO 630-1
Destination Delivery place and any packing or marking restrictions

Missing official Table B.1–B.4 figures on this comparison page are not waivers of the standard.

FAQ

Which edition applies to SG250 here?
This page uses ISO 630-2:2021, Edition 3. As of 12 November 2026 (Asia/Shanghai) that edition remains the published text. Reconfirm the edition on the order.
Is SG250 the same as an Annex A S-grade?
No. SG205, SG250, SG285 and SG345 are Annex B grades. S235, S275, S355 and S460 are Annex A. Clause 4.3 requires the two annexes to be regarded separately.
Are chemistry and mechanical numbers ISO normative limits?
No. Official Tables B.1 to B.4 are not in the 2021 preview and are not transcribed as ISO limits. Numeric figures on this page are related-specification comparison/reference data, clearly labelled. Confirm the official ISO rows before supply or design use.
Do I need to specify a quality?
Yes. Qualities A (no impact test), B (20 °C), C (0 °C) and D (−20 °C) are order information. Not every quality is available for every grade. This page does not add a quality suffix to the title.
What should I send for a quotation?
Send ISO 630-2:2021, the grade SG250, the quality, product form and dimensions, the quantity, the delivery condition if a particular condition is required, the inspection-document type and any agreed options. The official Annex B tables must be available for a technical supply commitment.

Request a quotation for ISO 630-2 SG250 plate

Request a SHH STEEL quotation for ISO 630-2:2021 SG250 plate. Send the quality, nominal dimensions, quantity, destination and the project material specification.

Identify any required delivery condition, the inspection-document type and any impact or supplementary tests. If comparison values are being used for enquiry only, say so.

Availability, dimensions, processing, testing and lead time will be confirmed against the enquiry. Related grades are not treated as approved substitutes without engineer review.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    ISO 630-2 S275C Steel Plate | S275C Structural Plate, 0°C Impact | ISO 630-2 Steel - SHH STEEL

    ISO 630-2 S275C Steel Plate | S275C Structural Plate, 0°C Impact

    ISO 630-2 S275C steel plate is grade S275, quality C, of ISO 630-2:2021 (Edition 3), the international standard for technical delivery conditions for structural steels for general purposes. Quality C is impact-tested at 0 °C (clause 4.2). The document applies to reversing-mill plates, wide flats, hot-rolled sections and bars, used in the as-delivered condition and normally intended for welded or bolted structures. Part 2 is not the ISO 630 part that specifies weldable fine-grain structural steels. This page is written to ISO 630-2:2021; confirm that this is the edition on the order. Mechanical-property tables were not inspected for this page; confirm Tables A.4, A.5 and A.6 against the official text.
    View More
    ISO 630-2 S235B Steel Plate | S235B Structural Plate, 20°C Impact | ISO 630-2 Steel - SHH STEEL

    ISO 630-2 S235B Steel Plate | S235B Structural Plate, 20°C Impact

    ISO 630-2 S235B steel plate is grade S235, quality B, of ISO 630-2:2021 (Edition 3), the international standard for technical delivery conditions for structural steels for general purposes. Quality B is impact-tested at 20 °C (clause 4.2). The document applies to reversing-mill plates, wide flats, hot-rolled sections and bars, used in the as-delivered condition and normally intended for welded or bolted structures. Part 2 is not the ISO 630 part that specifies weldable fine-grain structural steels. This page is written to ISO 630-2:2021; confirm that this is the edition on the order. Mechanical-property tables were not inspected for this page; confirm Tables A.4, A.5 and A.6 against the official text.
    View More
    ISO 630-2 S275D Steel Plate | S275D Structural Plate, -20°C Impact | ISO 630-2 Steel - SHH STEEL

    ISO 630-2 S275D Steel Plate | S275D Structural Plate, -20°C Impact

    ISO 630-2 S275D steel plate is grade S275, quality D, of ISO 630-2:2021 (Edition 3), the international standard for technical delivery conditions for structural steels for general purposes. Quality D is impact-tested at −20 °C (clause 4.2). The document applies to reversing-mill plates, wide flats, hot-rolled sections and bars, used in the as-delivered condition and normally intended for welded or bolted structures. Part 2 is not the ISO 630 part that specifies weldable fine-grain structural steels. This page is written to ISO 630-2:2021; confirm that this is the edition on the order. Mechanical-property tables were not inspected for this page; confirm Tables A.4, A.5 and A.6 against the official text.
    View More
    ISO 630-2 S355C Steel Plate | S355C Structural Plate, 0°C Impact | ISO 630-2 Steel - SHH STEEL

    ISO 630-2 S355C Steel Plate | S355C Structural Plate, 0°C Impact

    ISO 630-2 S355C steel plate is grade S355, quality C, of ISO 630-2:2021 (Edition 3), the international standard for technical delivery conditions for structural steels for general purposes. Quality C is impact-tested at 0 °C (clause 4.2). The document applies to reversing-mill plates, wide flats, hot-rolled sections and bars, used in the as-delivered condition and normally intended for welded or bolted structures. Part 2 is not the ISO 630 part that specifies weldable fine-grain structural steels. This page is written to ISO 630-2:2021; confirm that this is the edition on the order. Mechanical-property tables were not inspected for this page; confirm Tables A.4, A.5 and A.6 against the official text.
    View More
    ISO 630-2 S355B Steel Plate | S355B Structural Plate, 20°C Impact | ISO 630-2 Steel - SHH STEEL

    ISO 630-2 S355B Steel Plate | S355B Structural Plate, 20°C Impact

    ISO 630-2 S355B steel plate is grade S355, quality B, of ISO 630-2:2021 (Edition 3), the international standard for technical delivery conditions for structural steels for general purposes. Quality B is impact-tested at 20 °C (clause 4.2). The document applies to reversing-mill plates, wide flats, hot-rolled sections and bars, used in the as-delivered condition and normally intended for welded or bolted structures. Part 2 is not the ISO 630 part that specifies weldable fine-grain structural steels. This page is written to ISO 630-2:2021; confirm that this is the edition on the order. Mechanical-property tables were not inspected for this page; confirm Tables A.4, A.5 and A.6 against the official text.
    View More
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X