GB/T 700 Q235B Steel Hollow Sections (GB/T 6728-2025)
What is a GB/T 700 Q235B Steel Hollow Section (GB/T 6728-2025)?
A GB/T 700 Q235B steel hollow section on this page is a cold-formed closed square (SHS), rectangular (RHS) or circular (CHS) section whose steel grade is quality B of GB/T 700, and whose dimensions, mass calculation and technical delivery follow GB/T 6728-2025. The 2025 edition, published 29 August 2025 and implemented 1 March 2026, replaces GB/T 6728-2017 and absorbs GB/T 6723-2017. It is the dimensional and technical-delivery standard for the section, not the steel-grade standard. The Q235B name still marks a 235 N/mm² yield class and quality B in GB/T 700-2006; the formed section also has to meet the product yield class 235 line in GB/T 6728-2025 Table 25.
Closed sections are normally produced on a continuous roll-forming line from cold-rolled or hot-rolled plate or strip, then welded. Wall thickness 18 mm and above may use a two-stage forming route. Longitudinal high-frequency welding, longitudinal submerged-arc welding or spiral submerged-arc welding may be used. The standard also covers continuous hot-dip galvanized sections, but it does not apply to sections that are cold-formed and welded from already-galvanized sheet or strip.
Material, Manufacture and the Two Standards for Q235B Hollow Sections
Keep the two documents distinct on the order. GB/T 700-2006 states ladle chemistry, the thickness-dependent yield and tensile table, and the +20 °C impact rule for Q235B. GB/T 6728-2025 states section sizes, Annex A masses, Annex B wall-thickness deviations, length and straightness, galvanizing mass, and, new in this edition, product mechanicals in Table 25. Clause 6.5 of the 2025 text requires the starting product and the section to conform to the named material standard on the order. Other grades may be supplied only by agreement and must be stated in the contract.
Usual mill length for closed sections is 4000–12000 mm. Ordinary cut-length tolerance is +50/0 mm; precision cut length is +5/0 mm up to 6000 mm and +10/0 mm above that, per Table 21. Closed-section straightness is not more than 2 mm per metre and not more than 0.15 % of total length. When the section is delivered to theoretical mass, the lot tolerance in clause 6.4 is −6 % to +10 % where the total of the side lengths is not more than 1600 mm, and −4 % to +6 % above that.
GB/T 700 Q235B Hollow-Section Sizes: Verified Common Subset of GB/T 6728-2025 Tables 1–3
This page lists 625 verified closed-section sizes (216 square, 321 rectangular and 88 circular). Area was recomputed with GB/T 6728-2025 Annex A, and only typographical rows whose published area matches that formula are shown. Corner radius in the square and rectangular formula is 2.0t for t ≤ 6 mm, 2.5t for 6 mm < t ≤ 10 mm, and 3.0t above 10 mm. Circular area uses A = π(D² − d²)/400 cm² with d = D − 2t.
The size tables below are a formula-checked subset of GB/T 6728-2025 Tables 1 (square), 2 (rectangular) and 3 (circular). Each listed size uses a typographical designation and a preferred wall thickness whose published area matches the Annex A formula. Theoretical mass is computed as M = 0.785A (kg/m, with A in cm²). These tables are not a complete recitation of every row in the 2025 standard. Order against the edition on the contract, and do not treat a withdrawn 2017 table as a 2025 size list.
Verified common square sizes from GB/T 6728-2025 Table 1 (formula-checked subset, not every published row)
216 verified SHS rows are listed below, grouped by size.
20–90 mm square (66 sizes)
Swipe horizontally to view all dimensions.
95–160 mm square (53 sizes)
Swipe horizontally to view all dimensions.
170–300 mm square (49 sizes)
Swipe horizontally to view all dimensions.
320–1200 mm square (48 sizes)
Swipe horizontally to view all dimensions.
Verified common rectangular sizes from GB/T 6728-2025 Table 2 (formula-checked subset, not every published row)
321 verified RHS rows are listed below, grouped by size.
H 30–80 mm rectangular (74 sizes)
Swipe horizontally to view all dimensions.
H 90–150 mm rectangular (75 sizes)
Swipe horizontally to view all dimensions.
H 160–250 mm rectangular (59 sizes)
Swipe horizontally to view all dimensions.
H 260–400 mm rectangular (53 sizes)
Swipe horizontally to view all dimensions.
H 450–1000 mm rectangular (60 sizes)
Swipe horizontally to view all dimensions.
Verified common circular sizes from GB/T 6728-2025 Table 3 (formula-checked subset, not every published row)
88 verified CHS rows are listed below, grouped by size.
Outside diameter up to 165 mm (31 sizes)
Swipe horizontally to view all dimensions.
Outside diameter 219.1–1219 mm (57 sizes)
Swipe horizontally to view all dimensions.
GB/T 700 Q235B Chemical Composition (Heat Analysis) for Hollow Sections
Ladle analysis for Q235B is taken from GB/T 700-2006, which remains the grade standard. GB/T 6728-2025 clause 6.5 sends chemistry back to that document (and to the other material standards it names). The concession that carbon, manganese and silicon need not be delivery conditions if mechanicals are guaranteed applies to grade A, not to quality B.
Swipe horizontally to view all dimensions.
Mechanical Properties: GB/T 6728-2025 Table 25 Class 235 and GB/T 700 Table 2
For the cold-formed section, GB/T 6728-2025 Table 25 now specifies a product yield class. A Q235B enquiry that is sold to the 2025 section standard is checked against class 235: minimum yield 235 MPa, tensile 370–560 MPa, and minimum elongation 24 %. That tensile range is not the 370–500 MPa band in GB/T 700-2006 Table 2. Both documents have to be satisfied when both are named on the order; one table does not replace the other.
Table 25 footnote: for sections not larger than 60 mm × 60 mm (including equal-perimeter circular and rectangular sections), or with a flat-width to thickness ratio not greater than 14, the elongation on a 12.5 mm wide tensile specimen may be 3 percentage points lower.
Swipe horizontally to view all dimensions.
GB/T 700-2006 Table 2 remains the starting-steel mechanical table for Q235B. Yield falls with thickness; tensile strength stays 370–500 MPa through 200 mm. For sections and bars, tensile and bend specimens are longitudinal. For t > 100 mm, the lower tensile limit may be reduced by 20 N/mm². These figures describe the GB/T 700 product, not Table 25.
Swipe horizontally to view all dimensions.
Impact testing of 6728 sections 6 mm and thicker is optional by agreement; when it is required, results follow the raw-material standard. Under GB/T 700, Q235B has a 27 J longitudinal requirement at +20 °C for thickness not less than 12 mm (or diameter not less than 16 mm). For Q235B thinner than 25 mm the test may be omitted from inspection if the supplier guarantees conformity and the purchaser agrees. That is a waiver of inspection, not a deletion of the requirement, and it is a GB/T 700 rule, not a 6728 default.
Delivery, Inspection and Identification of Q235B GB/T 6728-2025 Hollow Sections
Orders should name both standards, the grade and quality (Q235B), the shape (SHS, RHS or CHS), the designation or the side lengths, outside diameter and wall, the length and cutting class, the weld process if it matters, and whether delivery is to theoretical or actual mass. If a zinc coating is required, state the mass and whether both the inner and outer surfaces are to be coated. Closed galvanized sections are hot-dip galvanized; unless otherwise agreed, coating mass is not less than 200 g/m² on each of the inner and outer surfaces (clause 6.11.2).
Inspection and batching follow GB/T 6728-2025 clauses 7 and 8, with retest rules including those added for zinc-coating mass. The quality certificate should identify the 2025 edition when that is the ordered document, and should not quietly cite a withdrawn 2017 table.
Weldability and Surface Condition of Q235B Cold-Formed Hollow Sections
Q235B is a weldable carbon structural steel, but GB/T 700 does not publish a CEV cap, and the 6728 product is a cold-formed, usually welded, closed section. Procedure qualification, including work on the longitudinal weld and the cold-formed corners, belongs on the order when the application needs it. Surface quality and weld quality are set in clauses 6.9 and 6.10 of GB/T 6728-2025. Laser or plasma cutting, where used, must follow the 2025 provisions added in clause 6.3. Do not assume that a galvanized surface is part of the supply unless it is specified.
Dimensional Tolerances and Theoretical Mass for Q235B GB/T 6728-2025 Hollow Sections
Wall-thickness deviations changed in the 2025 edition and must be read from Annex B, not from a 2017 carry-over. Length, straightness and theoretical-mass lot tolerances are summarised in the material section above. Circular sections also have an out-of-roundness requirement in Table 24. Theoretical masses in the size tables are Annex A values; they are the calculation basis for a theoretical-mass order, not a substitute for weighing when actual mass is specified.
Wall-thickness permitted deviations are taken from GB/T 6728-2025 Annex B Table B.1, as recovered from the 2025 text. Values are plus or minus, in millimetres. Arbitration measurement is 50 mm from the end. Square sections use five positions (Fig. B.1, average); rectangular sections use five positions (Fig. B.2, average); circular sections use three positions (Fig. B.3, average), excluding the weld and HAZ. The recovered table starts at the >1.50–2.00 mm band. A possible thinner first band was not recovered as clean text, so deviations for walls 1.50 mm and under are not stated here.
Swipe horizontally to view all dimensions.
Applications and Service Limits for GB/T 700 Q235B Steel Hollow Sections
Q235B hollow sections are used in general building frames, trusses, light columns, purlins, fences, agricultural structures and similar fabricated work where a 235 MPa yield class and quality B are specified. They are not a pressure-vessel or fire-resistant grade by default, and they are not automatically a low-temperature grade: quality B impact, when tested, is at +20 °C. Where a 0 °C or −20 °C test, a higher yield class, or a weathering or bridge steel is required, specify that grade and standard instead of assuming a substitution.
GB/T 700 Q235B Hollow Sections Compared with Q355B, S235JRH and A500
Q355B in the same 6728-2025 size family is a different material standard (GB/T 1591) and a different Table 25 class (355, tensile 470–680 MPa). S235JRH under EN 10219-1 is a frequent comparison in export enquiries, but it carries its own chemistry, impact and dimensional standard. ASTM A500 Grade B or Grade C HSS use imperial yield and tensile figures and AISC designations. None of those comparisons is an automatic substitute. The certificate has to name the standard actually produced.
Near-Equivalents for GB/T 700 Q235B Hollow Sections: Not Automatic Substitutes
The line below the keywords is limited to a one-line caution. Detail belongs in this table.
Swipe horizontally to view all dimensions.
Sourcing GB/T 700 Q235B Steel Hollow Sections from SHH STEEL
SHH STEEL reviews the ordered grade, the 6728-2025 size and wall, the weld process, length and any galvanizing requirement before quoting. Send the designation or the measured sides and thickness, the length, the certificate text you need, and whether delivery is to theoretical or actual mass. The tables on this page are a verified subset; sizes that are in the 2025 standard but not listed here can still be discussed against the official table on the contract.
Q235B Hollow Section FAQs
-
Is GB/T 6728-2025 the steel grade standard for Q235B?
- No. GB/T 6728-2025 is the dimensional and technical-delivery standard for the cold-formed section. Q235B chemistry and the Table 2 mechanicals come from GB/T 700-2006. The formed section also has to meet Table 25 class 235 when the 2025 edition is named.
-
Are the size tables on this page the complete 2025 list?
- No. They are a formula-checked subset of Tables 1–3: typographical sizes and preferred walls whose published area matches Annex A. Rows that did not meet that check, including several rectangular pages with poor OCR, are omitted rather than guessed.
-
Why is the Table 25 tensile range 370–560 MPa when GB/T 700 quotes 370–500 MPa?
- They are different tables. Table 25 is the 2025 product yield-class requirement for the cold-formed section. GB/T 700 Table 2 is the starting-steel table. When both standards are on the order, both ranges have to be considered; they are not interchangeable.
-
Can a 2017 hollow-section size chart be used for a 2025 order?
- No. The 2025 preface states that section sizes were added and that wall-thickness deviations changed. Withdrawn 2017 tables must not be written as if they were 2025 sizes.
-
Is impact testing mandatory on every Q235B hollow section?
- Not automatically. Under 6728-2025, impact testing of sections 6 mm and thicker is optional by agreement, and then follows GB/T 700. Quality B is a +20 °C, 27 J grade when the test applies, with the GB/T 700 inspection waiver for thickness under 25 mm only when the supplier guarantees conformity and the purchaser agrees.
Conclusion
Specify Q235B hollow sections by both GB/T 700-2006 and GB/T 6728-2025, and read Table 25 class 235 together with the GB/T 700 chemistry and Table 2 mechanicals. Use the formula-checked size subset on this page as a verified working list, not as a claim that every 2025 row has been reproduced. SHH STEEL will check grade, shape, wall and certificate wording against the ordered edition before issuing a quotation.