EN 10025-2 S355JR Round, Square and Flat Steel Bars

EN 10025-2 S355JR, steel number 1.0045, is supplied here as round, square and flat bars. Minimum yield is 355 MPa up to 16 mm, with 470–630 MPa tensile strength and 27 J at +20 °C. Size tables are common metric sizes with theoretical masses at 7.85 g/cm³, not a beam table. SHH STEEL reviews the form, grade and certificate before quoting.
Keywords
EN 10025-2 S355JR bars, S355JR round bar, S355JR flat bar, 1.0045 steel bar, S355JR square bar
Equivalent Grades:
Near-equivalents only, not automatic substitutes.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Size Chart
Applications
Equivalent Grades
Sourcing
FAQ
Conclusion

What are EN 10025-2 S355JR Round, Square and Flat Steel Bars?

EN 10025-2 S355JR is a non-alloy structural steel, steel number 1.0045, with a 355 MPa minimum yield up to 16 mm and a JR impact quality of 27 J at +20 °C. This page is for bars: rounds, squares and flats. It is not the live S355JR angle, channel, I-beam or H-beam page, and those shape tables must not be copied here. The material standard is EN 10025-2. Preferred dimensions are those of EN 10060 for rounds, EN 10059 for squares and EN 10058 for flats.

An S355JR plate, an HEA, or an L-shape of a similar millimetre size is a different product. The bar certificate has to name the bar form and the dimensional standard actually used.

Material, Manufacture and Scope for EN 10025-2 S355JR Steel Bars

The chemistry and mechanical tables on this page are the long-product values already verified for S355JR on this site. They apply to bars as long products. JR quality is supplied with the usual non-specific or specific inspection choices of EN 10025-2; the 27 J at +20 °C requirement is the JR mark, not a J0 or J2 result. Delivery condition follows the standard (usually +AR, +N or +M as ordered).

EN 10025-2 S355JR Chemical Composition and Carbon Equivalent for Bars

For S355JR long products the ladle-analysis carbon maximum is 0.24 % in all three thickness columns up to 100 mm; carbon above 100 mm is subject to agreement. Do not copy the tighter 0.22 % figure used for S355J0 or S355J2 at t > 30 mm onto an S355JR bar order. Silicon is 0.55 % maximum, manganese 1.60 %, phosphorus 0.040 %, sulphur 0.040 %, nitrogen 0.012 % and copper 0.55 %. The nitrogen maximum does not apply if total aluminium is at least 0.020 %, or if sufficient other nitrogen-binding elements are present and reported. Maximum CEV is 0.45 % for t ≤ 30 mm and 0.47 % for 30 mm < t ≤ 140 mm.

Swipe horizontally to view all dimensions.

Element or item S355JR long products, ladle analysis
Carbon, max, all three thickness columns up to 100 mm 0.24 %
Silicon, max 0.55 %
Manganese, max 1.60 %
Phosphorus, max 0.040 %
Sulphur, max 0.040 %
Nitrogen, max 0.012 % (see the aluminium / N-binding footnote)
Copper, max 0.55 %
CEV, max, t ≤ 30 mm 0.45 %
CEV, max, 30 mm < t ≤ 140 mm 0.47 %

EN 10025-2 S355JR Mechanical Properties for Steel Bars

Minimum yield ReH is 355 MPa up to 16 mm, then 345, 335, 325, 315 and 295 MPa in the usual thickness bands up to 150 mm. Tensile strength Rm is 470–630 MPa up to 100 mm and 450–600 MPa for 100 mm < t ≤ 150 mm. Minimum elongation is 22 % up to 40 mm, then 21, 20 and 18 % as the table shows. The impact requirement is 27 J at +20 °C. These values are for the material standard; they are not a substitute for a beam or angle size table.

Swipe horizontally to view all dimensions.

Nominal thickness t (mm) ReH min (MPa) Rm (MPa) A min (%)
t ≤ 16 355 470–630 22
16 < t ≤ 40 345 470–630 22
40 < t ≤ 63 335 470–630 21
63 < t ≤ 80 325 470–630 20
80 < t ≤ 100 315 470–630 20
100 < t ≤ 150 295 450–600 18

EN 10025-2 S355JR Common Bar Sizes: Metric Rounds, Squares and Flats

The tables below are common typographical metric bar sizes, not a complete EN 10060, EN 10059 or EN 10058 listing and not a mill stock list. They are also not IPE, IPN, HE or L-shape tables. Theoretical mass is computed at a density of 7.85 g/cm³: M = 0.006165 d² kg/m for rounds, and M = 0.00785 a b kg/m for squares and flats, with dimensions in millimetres. Preferred sizes on an order should still be taken from the dimensional standard named in the contract.

Round bars (29 common diameters).

Swipe horizontally to view all dimensions.

Diameter d (mm) Theoretical mass (kg/m)
10 0.617
12 0.888
16 1.578
18 1.997
20 2.466
22 2.984
25 3.853
28 4.833
30 5.548
32 6.313
36 7.99
40 9.86
45 12.48
50 15.41
56 19.33
60 22.19
63 24.47
70 30.21
80 39.46
90 49.94
100 61.65
110 74.6
120 88.78
130 104.19
140 120.83
150 138.71
160 157.82
180 199.75
200 246.6

Square bars (12 common sides).

Swipe horizontally to view all dimensions.

Side a (mm) Theoretical mass (kg/m)
10 0.785
12 1.13
16 2.01
20 3.14
25 4.906
30 7.065
40 12.56
50 19.62
60 28.26
70 38.46
80 50.24
100 78.5

Flat bars (35 common thickness × width combinations).

Swipe horizontally to view all dimensions.

Thickness × width (mm) Theoretical mass (kg/m)
5 × 20 0.785
5 × 30 1.177
5 × 40 1.57
5 × 50 1.962
6 × 20 0.942
6 × 30 1.413
6 × 40 1.884
6 × 50 2.355
6 × 60 2.826
8 × 20 1.256
8 × 30 1.884
8 × 40 2.512
8 × 50 3.14
8 × 80 5.024
10 × 20 1.57
10 × 30 2.355
10 × 40 3.14
10 × 50 3.925
10 × 80 6.28
10 × 100 7.85
12 × 30 2.826
12 × 40 3.768
12 × 50 4.71
12 × 80 7.536
12 × 100 9.42
16 × 40 5.024
16 × 50 6.28
16 × 80 10.05
16 × 100 12.56
20 × 40 6.28
20 × 50 7.85
20 × 80 12.56
20 × 100 15.7
25 × 50 9.812
25 × 80 15.7
25 × 100 19.62

Applications and Service Limits for EN 10025-2 S355JR Steel Bars

S355JR bars are used for fixtures, pins, general fabrications, machined parts and structural details where a 355 MPa non-alloy bar is named. The grade is not a pressure-vessel steel and not a quenched-and-tempered alloy bar. A colder impact quality (J0 or J2) or a different form (plate, angle, beam) has to be ordered as that product.

Near-Equivalents for EN 10025-2 S355JR Steel Bars: Not Automatic Substitutes

S235JR is a lower-strength JR grade in the same standard. S355J0 and S355J2 use colder impact qualities and, at some thicknesses, a tighter carbon limit. ASTM A36 and ASTM A572 Grade 50 bars follow different chemistry and tensile tables. GB/T 1591 Q355B is a Chinese grade, not a restamp of S355JR. ASME SA designations are not inferred here.

Sourcing EN 10025-2 S355JR Steel Bars from SHH STEEL

Send the form (round, square or flat), the diameter or the thickness and width, the length, the delivery condition, and the EN 10025-2 edition. Name S355JR explicitly. Do not use an H-beam or angle term for this page. SHH STEEL reviews the form, the grade and the certificate before quoting. The size tables are a typographical reference, not a warehouse list.

EN 10025-2 S355JR Steel Bar FAQs

Are these the same tables as the S355JR H-beam or angle pages?
No. The material grade is the same, but this page is for bars. Beam, channel and angle size tables must not be copied onto a bar certificate.
What dimensional standards apply?
Preferred dimensions are EN 10060 for rounds, EN 10059 for squares and EN 10058 for flats. The tables here are a common typographical subset, not a complete listing.
Is S355JR carbon 0.22 %?
No. For S355JR long products the carbon maximum is 0.24 % in the usual thickness columns. The 0.22 % figure belongs to S355J0 / S355J2 at t > 30 mm and must not be pasted here.
Is an SA-36 or SA-572 bar implied?
No. ASME SA designations are used only when the named BPVC Section II, Part A edition can be quoted. That inference is not made here.

Conclusion

EN 10025-2 S355JR bars are the 355 MPa, 27 J at +20 °C long-product grade of steel number 1.0045, supplied as rounds, squares and flats. The size tables are common typographical metric sizes with theoretical masses at 7.85 g/cm³, not a beam table and not a stock list. Confirm the form, the size, the edition and the certificate on the order.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X