EN 10025-2 S235JR Round, Square and Flat Steel Bars

EN 10025-2 S235JR, steel number 1.0038, is supplied here as round, square and flat bars. Minimum yield is 235 MPa up to 16 mm, with 360-510 MPa tensile strength and 27 J at +20 C. Size tables are common metric sizes with theoretical masses at 7.85 g/cm3, not a beam table. SHH STEEL reviews the form, grade and certificate before quoting.
Keywords
EN 10025-2 S235JR bars, S235JR round bar, S235JR flat bar, 1.0038 steel bar, S235JR square bar
Equivalent Grades:
Near-equivalents only, not automatic substitutes.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Size Chart
Applications
Equivalent Grades
Sourcing
FAQ
Conclusion

What are EN 10025-2 S235JR Round, Square and Flat Steel Bars?

EN 10025-2 S235JR is a non-alloy structural steel, steel number 1.0038, with a 235 MPa minimum yield up to 16 mm and a JR impact quality of 27 J at +20 C. This page is for bars: rounds, squares and flats. It is not the live S235JR angle, channel, I-beam or H-beam page, and those shape tables must not be copied here. The material standard is EN 10025-2. Preferred dimensions are those of EN 10060 for rounds, EN 10059 for squares and EN 10058 for flats.

An S235JR plate, an IPE, or an L-shape of a similar millimetre size is a different product. The bar certificate has to name the bar form and the dimensional standard actually used.

Material, Manufacture and Scope for EN 10025-2 S235JR Steel Bars

The chemistry and mechanical tables on this page are the long-product values already verified for S235JR on this site. They apply to bars as long products. JR quality is the 27 J at +20 C mark, not a J0 or J2 result, and not a 355 MPa grade. Delivery condition follows the standard (usually +AR, +N or +M as ordered). The edition named on the order governs acceptance.

EN 10025-2 S235JR Chemical Composition and Carbon Equivalent for Bars

For S235JR long products the ladle-analysis carbon maximum is 0.17 % up to 40 mm and 0.20 % above 40 mm; carbon above 100 mm is subject to agreement. There is no general silicon maximum in the long-product table. Do not invent a 0.55 % silicon cap from S355JR, and do not paste a flat-product 0.035 % phosphorus default onto a bar order unless that is what was agreed. Manganese is 1.40 % maximum, phosphorus 0.040 %, sulphur 0.040 %, nitrogen 0.012 % and copper 0.55 %. The nitrogen maximum does not apply if total aluminium is at least 0.020 %, or if sufficient other nitrogen-binding elements are present and reported. Maximum CEV is 0.35 % up to 40 mm and 0.38 % for 40 mm < t <= 140 mm. By agreement, silicon may be set at 0.14-0.25 % and phosphorus at <= 0.035 % for hot-dip galvanizing category B.

Swipe horizontally to view all dimensions.

Element or item S235JR long products, ladle analysis
Carbon, max, t <= 16 mm 0.17 %
Carbon, max, 16 mm < t <= 40 mm 0.17 %
Carbon, max, t > 40 mm 0.20 % (above 100 mm, carbon is subject to agreement)
Silicon No general maximum
Manganese, max 1.40 %
Phosphorus, max 0.040 %
Sulphur, max 0.040 %
Nitrogen, max 0.012 % (see the aluminium / N-binding footnote)
Copper, max 0.55 %
CEV, max, t <= 40 mm 0.35 %
CEV, max, 40 mm < t <= 140 mm 0.38 %

EN 10025-2 S235JR Mechanical Properties for Steel Bars

Minimum yield ReH is 235 MPa up to 16 mm, then 225 MPa to 40 mm, 215 MPa through 100 mm, and 195 MPa for 100 mm < t <= 150 mm. Tensile strength Rm is 360-510 MPa up to 100 mm and 350-500 MPa for 100 mm < t <= 150 mm. Minimum elongation is 26 % up to 40 mm, then 25, 24 and 22 % as the table shows. The impact requirement is 27 J at +20 C. These values are for the material standard; they are not a substitute for a beam or angle size table.

Swipe horizontally to view all dimensions.

Nominal thickness t (mm) ReH min (MPa) Rm (MPa) A min (%)
t <= 16 235 360-510 26
16 < t <= 40 225 360-510 26
40 < t <= 63 215 360-510 25
63 < t <= 80 215 360-510 24
80 < t <= 100 215 360-510 24
100 < t <= 150 195 350-500 22

EN 10025-2 S235JR Common Bar Sizes: Metric Rounds, Squares and Flats

The tables below are common typographical metric bar sizes, not a complete EN 10060, EN 10059 or EN 10058 listing and not a mill stock list. They are also not IPE, IPN, HE or L-shape tables. Theoretical mass is computed at a density of 7.85 g/cm3: M = 0.006165 d2 kg/m for rounds, and M = 0.00785 a b kg/m for squares and flats, with dimensions in millimetres. Preferred sizes on an order should still be taken from the dimensional standard named in the contract.

Round bars (29 common diameters).

Swipe horizontally to view all dimensions.

Diameter d (mm) Theoretical mass (kg/m)
10 0.617
12 0.888
16 1.578
18 1.997
20 2.466
22 2.984
25 3.853
28 4.833
30 5.548
32 6.313
36 7.99
40 9.86
45 12.48
50 15.41
56 19.33
60 22.19
63 24.47
70 30.21
80 39.46
90 49.94
100 61.65
110 74.6
120 88.78
130 104.19
140 120.83
150 138.71
160 157.82
180 199.75
200 246.6

Square bars (12 common sides).

Swipe horizontally to view all dimensions.

Side a (mm) Theoretical mass (kg/m)
10 0.785
12 1.13
16 2.01
20 3.14
25 4.906
30 7.065
40 12.56
50 19.62
60 28.26
70 38.46
80 50.24
100 78.5

Flat bars (35 common thickness x width combinations).

Swipe horizontally to view all dimensions.

Thickness x width (mm) Theoretical mass (kg/m)
5 x 20 0.785
5 x 30 1.177
5 x 40 1.57
5 x 50 1.962
6 x 20 0.942
6 x 30 1.413
6 x 40 1.884
6 x 50 2.355
6 x 60 2.826
8 x 20 1.256
8 x 30 1.884
8 x 40 2.512
8 x 50 3.14
8 x 80 5.024
10 x 20 1.57
10 x 30 2.355
10 x 40 3.14
10 x 50 3.925
10 x 80 6.28
10 x 100 7.85
12 x 30 2.826
12 x 40 3.768
12 x 50 4.71
12 x 80 7.536
12 x 100 9.42
16 x 40 5.024
16 x 50 6.28
16 x 80 10.05
16 x 100 12.56
20 x 40 6.28
20 x 50 7.85
20 x 80 12.56
20 x 100 15.7
25 x 50 9.812
25 x 80 15.7
25 x 100 19.62

Applications and Service Limits for EN 10025-2 S235JR Steel Bars

S235JR bars are used for fixtures, pins, general fabrications, machined parts and ordinary structural details where a 235 MPa non-alloy bar is named. The grade is not a pressure-vessel steel and not a quenched-and-tempered alloy bar. A colder impact quality (J0 or J2), a higher yield (S275JR or S355JR), or a different form (plate, angle, beam) has to be ordered as that product.

Near-Equivalents for EN 10025-2 S235JR Steel Bars: Not Automatic Substitutes

S275JR and S355JR are higher-strength JR grades in the same standard. S235J0 and S235J2 use colder impact qualities. ASTM A36 bars follow a different chemistry table and a 36 ksi yield. GB/T 700 Q235B is a Chinese grade, not a restamp of S235JR. ASME SA designations are not inferred here except where a named BPVC edition can be quoted on a separate page.

Sourcing EN 10025-2 S235JR Steel Bars from SHH STEEL

Send the form (round, square or flat), the diameter or the thickness and width, the length, the delivery condition, and the EN 10025-2 edition. Name S235JR explicitly. Do not use an H-beam, I-beam or angle term for this page. SHH STEEL reviews the form, the grade and the certificate before quoting. The size tables are a typographical reference, not a warehouse list.

EN 10025-2 S235JR Steel Bar FAQs

Are these the same tables as the S235JR I-beam or angle pages?
No. The material grade is the same, but this page is for bars. Beam, channel and angle size tables must not be copied onto a bar certificate.
What dimensional standards apply?
Preferred dimensions are EN 10060 for rounds, EN 10059 for squares and EN 10058 for flats. The tables here are a common typographical subset, not a complete listing.
Is the silicon maximum 0.55 %?
No. S235JR long products have no general silicon maximum in the ladle-analysis table. The 0.55 % figure belongs to other grades such as S355JR and must not be pasted here.
Is this the same as the S355JR bar page?
No. S355JR is a 355 MPa grade with a different carbon, manganese and tensile table. Do not treat an S235JR bar certificate as S355JR.

Conclusion

EN 10025-2 S235JR bars are the 235 MPa, 27 J at +20 C long-product grade of steel number 1.0038, supplied as rounds, squares and flats. The size tables are common typographical metric sizes with theoretical masses at 7.85 g/cm3, not a beam table and not a stock list. Confirm the form, the size, the edition and the certificate on the order.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X