CNS 13812 SN490B Equal and Unequal Steel Angles
What is CNS 13812 SN490B Steel Angle?
CNS 13812 SN490B steel angle is a hot-rolled building-structure angle whose material grade is SN490B under CNS 13812. The same SN family is specified in JIS G 3136:2022. SN marks a building-structure steel, 490 is the tensile-strength class (490–610 N/mm²), and B is the quality with a 27 J impact requirement at 0 °C when testing applies. Related qualities on this page are SN400B, SN400YB and SN490YB.
These bars are filed under steel angle profiles in the steel structural profiles category. The designation is A×A×t, A×B×t or A×B×t1×t2, for example 75×75×9, 150×100×12 or 200×90×9×14. They are not GB/T 706 or European sections of a similar millimetre size, and they are not JIS G 3106 SM490 bars, even when the same JIS G 3192 size table is used.
This page covers Equal and Unequal Steel Angles in CNS 13812 SN490B. The Equal Leg Steel Angles and Unequal Leg Steel Angles follow CNS 1490 or JIS G 3192, as named on the order; the material standard does not by itself define the dimensions.
Material, Dimensions and the SN Quality Family
The purchase order and the inspection document should name CNS 13812 or JIS G 3136 and its edition, the full quality symbol, the dimensional standard (CNS 1490 or JIS G 3192), the designation (A×A×t, A×B×t or A×B×t1×t2), and the inspection document type.
CNS 13812 SN490B Equal Leg Steel Angles
The tables are the complete tabulated standard series in JIS G 3192:2024: Table 8 equal-leg (40 sizes, 25×25×3 to 250×250×35), Table 9 unequal-leg (13 sizes, 90×75×9 to 150×100×15), and Table 10 unequal-leg unequal-thickness (7 sizes, 200×90×9×14 to 400×100×13×18). Name CNS 1490 or JIS G 3192 as the dimensional standard actually required. A published mill production band such as 25–100 mm is a mill range, not a complete standard table, and is not used here as a size list. Governing thickness for the material tables is ordinarily the leg t, or the thicker leg t2 on Table 10.
Equal-leg angles (Table 8)
Swipe horizontally to view all dimensions.
CNS 13812 SN490B Unequal Leg Steel Angles
Unequal-leg angles (Table 9)
Swipe horizontally to view all dimensions.
Unequal-leg unequal-thickness angles (Table 10)
Swipe horizontally to view all dimensions.
SN490B and Related SN Chemical Composition
The figures below are heat-analysis maxima as reprinted from CNS 13812 (JIS G 3136:2022). Boron is shown as less than 0.0008%. Carbon equivalent and Pcm are the tabulated maxima; the calculation in the ordered edition of the standard governs, and no formula is invented here. For SN490B the catalog reprints two Ceq maxima, 0.44 and 0.46, in two thickness bands; the 40 mm split is clear for SN490YB (0.44 then 0.46) and is not forced onto SN490B on this page. The edition named on the order governs the applicable band.
Swipe horizontally to view all dimensions.
SN490B Mechanical Properties: Yield, Tensile and 0 °C Impact
The mechanical values below are those reprinted for section steels with a flange thickness of 6 mm to 40 mm. They are not extended above 40 mm on this page. For H-sections with a web thinner than 9 mm, the upper yield limit in the range columns does not apply, and the yield-ratio maximum is 85% rather than 80%. Thickness for these tables is the flange thickness of the finished section unless the order names another location.
Review bars with a leg length under 40 mm (the Table 8 25×25 and 30×30 families) against the annex of the ordered edition; numeric annex values are not restated here.
Swipe horizontally to view all dimensions.
Impact results are the mean of three tests at 0 °C, 27 J, for the B and YB qualities in this table.
Delivery Conditions, Inspection and Identification
The inspection document should identify CNS 13812 (or JIS G 3136) and its edition, the full quality symbol, the dimensional standard and designation, heat analysis, Ceq or Pcm, and tensile and impact results against the governing thickness. A plate or H-beam certificate does not, by itself, identify a steel angle.
Weldability of SN490B Steel Angles
SN steels are specified as building-structure steels with a published Ceq and Pcm. Preheat and consumable choice should use the certified heat analysis, the certified Ceq or Pcm, the actual thickness and the joint design.
CNS 1490 or JIS G 3192 Shape Tolerances and Theoretical Mass
Shape, mass and tolerances belong to the dimensional standard named on the order, ordinarily CNS 1490 or JIS G 3192. Mass in the size table is the published theoretical figure. Millimetre tolerance tables are not reproduced here.
Applications and Service Limits
SN490B steel angles are used in building frames and bracing where a Taiwanese or Japanese SN 490-class building-structure grade and a 0 °C impact test are specified. They are not a silent substitute for an SM490 angle or for a GB/T 706 or European section of similar size.
SN490B Compared with SN400YB and SM490
The comparisons below are an orientation only; they are not automatic substitutes.
Near-Equivalents: Not Automatic Substitutes
A near-equivalent is a starting point for a discussion, not a licence to swap certificates. If a project names SN490B or SN490YB, keep that quality letter and the dimensional standard on the order.
Sourcing SN490B Steel Angles from SHH STEEL
SHH STEEL supplies CNS 13812 SN490B steel angles, and the related SN400 and SN490YB qualities, against a named designation list, the material edition and the inspection document type. Enquiries should state the A×A×t, A×B×t or A×B×t1×t2 designations, the quality letter, whether CNS 1490 or JIS G 3192 is required, cut lengths or mill lengths, and any processing.
The size table is the standard series, not a claim that every designation is rolled in every quality. Once the list is clear, a quotation can be prepared against the stated edition and certificate.
SN490B Steel Angle FAQs
-
Is SN490B the same as SN400YB or SM490?
- No. SN490B is a 490 N/mm² tensile-class building-structure grade with a 0 °C / 27 J impact test. SN400YB is a 400 N/mm² class with a yield window. SM490 is a JIS G 3106 welded-structure grade, not an SN grade.
-
Do the mechanical tables apply above 40 mm?
- The tabulated mechanical values on this page are those reprinted for finished sections with a flange or leg thickness of 6 mm to 40 mm. Values above 40 mm are not invented here.
-
Is a 25–100 mm mill band the complete size table?
- No. A mill production band is not a standard series. This page lists the complete tabulated JIS G 3192 series as reference dimensions. The order should name the designations actually required.
-
Which material edition is used on this page?
- The numeric tables follow the CNS 13812 / JIS G 3136:2022 reprint in the mill catalog used for this page. The edition named on the order governs.
Request a Quotation for CNS 13812 SN490B Steel Angle
CNS 13812 SN490B steel angle is a building-structure angle in the 490–610 N/mm² tensile class, with a 27 J impact requirement at 0 °C. Nominate the A×A×t, A×B×t or A×B×t1×t2 designation, the quality letter, CNS 13812 or JIS G 3136 and the dimensional standard on the order, and the inspection document type. Send the size list, quality, edition, certificate type and any processing notes; SHH STEEL will review the package and quote accordingly.