ASTM A501 Grade B Steel Hollow Sections | ASTM A501 Steel Hollow Sections - SHH STEEL

ASTM A501 Grade B Steel Hollow Sections

ASTM A501/A501M-21 Grade B is hot-formed welded or seamless carbon steel structural tubing. Tensile strength is 65 ksi [448 MPa] for all walls. Yield is 46, 45, 42.5 or 40 ksi [315, 310, 290 or 280 MPa] by wall-thickness band; do not use a single 50 ksi figure against Table 2. Size tables are a typographical subset, not an A500 list.
Keywords
ASTM A501 Grade B, A501 hot-formed HSS, A501/A501M-21 Grade B, A501 square rectangular round tubing, A501 Grade B hollow section
Equivalent Grades:
Near-equivalents only, not automatic substitutes.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Size Chart
Applications
Comparison
Equivalent Grades
Sourcing
FAQ
Conclusion

What is ASTM A501 Grade B Steel Hollow Section?

ASTM A501/A501M-21 covers black and hot-dipped galvanized hot-formed welded and seamless carbon steel square, round, rectangular, or special-shape structural tubing for welded, riveted, or bolted construction of bridges and buildings, and for general structural purposes. This page is Grade B only. Grades A and C exist in the same specification and are not this product.

Hot-formed A501 tubing is not the same product as cold-formed ASTM A500 Grade B Steel Hollow Sections (HSS). Do not paste an A500 HSS table, an A500 46 ksi yield for all shapes, or an A500 corner-radius practice onto an A501 enquiry. The edition named on the purchase order governs delivery.

Material, Manufacture and Scope for ASTM A501/A501M-21 Grade B

The steel is made by a basic-oxygen or electric-arc-furnace process and may be ingot or strand cast. The finished product is hot-formed welded or seamless tubing. Cold-formed hollow sections belong under A500 or another named standard, not here.

Clause 1.2 of A501/A501M-21 limits square and rectangular flats to 1–16 in. [25–405 mm] with specified wall 0.095–1.0 in. [2.5–25 mm], and rounds to 1–48 in. [25–1220 mm] with specified wall 0.095–4.00 in. [2.5–100 mm]. Clause 1.3 states that the specification covers three grades: A, B and C. This page does not collapse those grades into one number, and it does not use a shorthand 50 ksi yield against Table 2.

ASTM A501 Grade B Chemical Composition (Table 1, Grades B and C)

Table 1 of A501/A501M-21 gives one chemistry block for Grades B and C, distinct from Grade A. Where an ellipsis appears for Grade A manganese, there is no manganese requirement in that Grade A cell; that is not this page. Footnote B allows, for each 0.01 percentage point reduction below the specified carbon maximum, an increase of 0.06 percentage point manganese above the specified maximum, up to 1.60 % by heat analysis and 1.65 % by product analysis.

Swipe horizontally to view all dimensions.

Element Grade B and C heat analysis Grade B and C product analysis Notes
C, max (%) 0.22 0.26 Footnote B permits a manganese increase for each 0.01 percentage point reduction below the carbon maximum.
Mn, max (%) 1.40 1.45 May rise to 1.60 % heat and 1.65 % product under footnote B.
P, max (%) 0.030 0.040 Tighter than the Grade A phosphorus row.
S, max (%) 0.020 0.030 Tighter than the Grade A sulfur row.
Cu, min (%), when copper steel is specified 0.20 0.18 Applies only when copper steel is specified on the order.

ASTM A501 Grade B Mechanical Properties (Table 2)

Table 2 sets Grade B tensile strength at 65 ksi [448 MPa] for all walls. Yield strength falls by wall-thickness band: 46 ksi [315 MPa] up to 1 in., 45 ksi [310 MPa] over 1 in. through 2 in., 42.5 ksi [290 MPa] over 2 in. through 3 in., and 40 ksi [280 MPa] over 3 in. through 4 in. Minimum elongation is 24 %. Impact tests, when required, follow clause 10; they are not required for thicknesses of 0.250 in. [6.3 mm] or less unless specified. Do not replace this table with a single 50 ksi yield, and do not use the A500 Grade B 58 ksi / 46 ksi all-shape row as if it were A501 Grade B.

Swipe horizontally to view all dimensions.

Property Wall thickness Grade B requirement
Tensile strength, min All walls 65 ksi [448 MPa]
Yield strength, min ≤ 1 in. [25 mm] 46 ksi [315 MPa]
Yield strength, min > 1 in. [25 mm] and ≤ 2 in. [50 mm] 45 ksi [310 MPa]
Yield strength, min > 2 in. [50 mm] and ≤ 3 in. [76 mm] 42.5 ksi [290 MPa]
Yield strength, min > 3 in. [76 mm] and ≤ 4 in. [100 mm] 40 ksi [280 MPa]
Elongation, min All walls in Table 2 24 %
Impact energy, min. average / min. single See 10.1 and 10.4; not required for t ≤ 0.250 in. [6.3 mm] unless specified 20 / (see 10.4) ft·lbf [27 J average]

ASTM A501 Grade B Typographical Sizes (Hot-Formed Scope, Sharp-Corner Theoretical Mass)

ASTM A501/A501M-21 produces hot-formed welded and seamless square and rectangular tubing with flats of 1 to 16 in. [25 to 405 mm] and specified wall 0.095 to 1.0 in. [2.5 to 25 mm], and round tubing with outside diameter 1 to 48 in. [25 to 1220 mm] and specified wall 0.095 to 4.00 in. [2.5 to 100 mm]. The tables below are a typographical common-size subset inside that scope. They are not a complete listing of every permitted size, and they are not a warehouse list.

Square and rectangular masses are theoretical sharp-corner values at 7.85 g/cm³ (490 lb/ft³): area = 2 t (H + B − 2 t), mass = 3.403 × area lb/ft. Actual hot-formed corner radii change the mass; do not treat these figures as a weighed delivery mass. Round masses use the plain-end cylindrical estimate W = 10.69(D − t)t lb/ft, the same formula used on this site for pipe, applied here only as a typographical estimate. Do not read these rows as an AISC Manual A500 HSS table, and do not read the round rows as an ASME B36.10 schedule table.

Typographical square sections (sharp-corner theoretical mass)

Swipe horizontally to view all dimensions.

H × B × t (in) H × B × t (mm, converted) Area (in², sharp corner) Mass (lb/ft) Mass (kg/m)
2 × 2 × 0.125 50.8 × 50.8 × 3.17 0.938 3.19 4.75
2.5 × 2.5 × 0.125 63.5 × 63.5 × 3.17 1.188 4.04 6.01
3 × 3 × 0.1875 76.2 × 76.2 × 4.76 2.109 7.18 10.68
4 × 4 × 0.1875 101.6 × 101.6 × 4.76 2.859 9.73 14.48
4 × 4 × 0.25 101.6 × 101.6 × 6.35 3.75 12.76 18.99
5 × 5 × 0.25 127 × 127 × 6.35 4.75 16.16 24.06
6 × 6 × 0.25 152.4 × 152.4 × 6.35 5.75 19.57 29.12
6 × 6 × 0.375 152.4 × 152.4 × 9.52 8.438 28.71 42.73
8 × 8 × 0.25 203.2 × 203.2 × 6.35 7.75 26.37 39.25
8 × 8 × 0.375 203.2 × 203.2 × 9.52 11.438 38.92 57.93
8 × 8 × 0.5 203.2 × 203.2 × 12.7 15 51.05 75.97
10 × 10 × 0.375 254 × 254 × 9.52 14.438 49.13 73.12
10 × 10 × 0.5 254 × 254 × 12.7 19 64.66 96.23
12 × 12 × 0.375 304.8 × 304.8 × 9.52 17.438 59.34 88.31
12 × 12 × 0.5 304.8 × 304.8 × 12.7 23 78.27 116.48
14 × 14 × 0.5 355.6 × 355.6 × 12.7 27 91.88 136.74
16 × 16 × 0.5 406.4 × 406.4 × 12.7 31 105.49 157
16 × 16 × 0.625 406.4 × 406.4 × 15.88 38.438 130.8 194.67

Typographical rectangular sections (sharp-corner theoretical mass)

Swipe horizontally to view all dimensions.

H × B × t (in) H × B × t (mm, converted) Area (in², sharp corner) Mass (lb/ft) Mass (kg/m)
3 × 2 × 0.1875 76.2 × 50.8 × 4.76 1.734 5.9 8.78
4 × 2 × 0.1875 101.6 × 50.8 × 4.76 2.109 7.18 10.68
4 × 3 × 0.25 101.6 × 76.2 × 6.35 3.25 11.06 16.46
5 × 3 × 0.25 127 × 76.2 × 6.35 3.75 12.76 18.99
6 × 3 × 0.25 152.4 × 76.2 × 6.35 4.25 14.46 21.52
6 × 4 × 0.25 152.4 × 101.6 × 6.35 4.75 16.16 24.06
8 × 4 × 0.25 203.2 × 101.6 × 6.35 5.75 19.57 29.12
8 × 6 × 0.375 203.2 × 152.4 × 9.52 9.938 33.82 50.33
10 × 4 × 0.375 254 × 101.6 × 9.52 9.938 33.82 50.33
10 × 6 × 0.375 254 × 152.4 × 9.52 11.438 38.92 57.93
12 × 6 × 0.375 304.8 × 152.4 × 9.52 12.938 44.03 65.52
12 × 8 × 0.5 304.8 × 203.2 × 12.7 19 64.66 96.23
14 × 10 × 0.5 355.6 × 254 × 12.7 23 78.27 116.48
16 × 8 × 0.5 406.4 × 203.2 × 12.7 23 78.27 116.48
16 × 12 × 0.5 406.4 × 304.8 × 12.7 27 91.88 136.74

Typographical round sections (plain-end cylindrical mass estimate)

Swipe horizontally to view all dimensions.

Outside diameter × t (in) OD × t (mm, converted) Mass (lb/ft) Mass (kg/m)
2.875 × 0.203 73 × 5.16 5.8 8.63
3.5 × 0.216 88.9 × 5.49 7.58 11.28
4.5 × 0.237 114.3 × 6.02 10.8 16.07
6.625 × 0.28 168.3 × 7.11 18.99 28.26
8.625 × 0.322 219.1 × 8.18 28.58 42.53
10.75 × 0.365 273.1 × 9.27 40.52 60.3
12.75 × 0.375 323.8 × 9.52 49.61 73.83
14 × 0.375 355.6 × 9.52 54.62 81.28
16 × 0.375 406.4 × 9.52 62.64 93.21
18 × 0.5 457.2 × 12.7 93.54 139.2
20 × 0.5 508 × 12.7 104.23 155.11
24 × 0.5 609.6 × 12.7 125.61 186.92
30 × 0.625 762 × 15.88 196.26 292.07
36 × 0.75 914.4 × 19.05 282.62 420.58

Applications and Service Limits for ASTM A501 Grade B Hollow Sections

A501 Grade B tubing is used in bridges, buildings and general structural work where a hot-formed welded or seamless carbon steel hollow section is specified. Galvanized or black finish, end condition and any required impact test must be stated on the order. The typographical size subset is not a claim that every row is rolled in Grade B on every enquiry.

ASTM A501 Grade B Compared with ASTM A500 Grade B and SA-500 Enquiries

ASTM A500 Grade B Steel Hollow Sections (HSS) is cold-formed HSS to A500/A500M-23, with a single Grade B yield of 46 ksi [315 MPa] for all shapes and a 58 ksi [400 MPa] tensile minimum. A501 Grade B is hot-formed, uses a 65 ksi [448 MPa] tensile minimum, and reduces yield as the wall increases. Those two pages are not substitutes.

An SA-500-named enquiry is handled on a separate companion that uses A500 as its technical basis. That basis is not A501.

Near-Equivalents for ASTM A501 Grade B Hollow Sections: Not Automatic Substitutes

Near-equivalents only, not automatic substitutes. ASTM A500 Grade B or Grade C, EN 10210 hot-finished hollow sections, and EN 10219 cold-formed hollow sections have their own chemistry, forming routes and mechanical tables. Do not treat a certificate from those specifications as A501 Grade B.

Sourcing ASTM A501 Grade B Steel Hollow Sections from SHH STEEL

SHH STEEL reviews the named A501/A501M edition, the Grade B certificate, the hot-formed route and the ordered outside size and wall before quoting. The typographical size tables on this page are not a warehouse list. Name the shape, the outside dimensions, the specified wall and the finish on the enquiry.

FAQ: ASTM A501 Grade B Steel Hollow Sections

Is A501 Grade B the same as A500 Grade B?
No. A501/A501M-21 is hot-formed welded or seamless tubing. A500 is cold-formed HSS. Grade B tensile and yield tables differ, and A500 size tables must not be used as A501 tables.
Why is yield not a single 50 ksi figure?
Table 2 of A501/A501M-21 gives Grade B yield by wall-thickness band: 46, 45, 42.5 and 40 ksi. This page follows that table and does not replace it with a shorthand 50 ksi value.
Are the size tables complete?
No. They are a typographical subset inside the clause 1.2 scope, with theoretical sharp-corner or cylindrical mass clearly labelled. They are not a warehouse list and not an AISC A500 HSS file.

Conclusion

Specify ASTM A501/A501M-21 Grade B as hot-formed structural tubing, with the Table 1 chemistry and the Table 2 tensile, yield-by-wall and 24 % elongation requirements. Do not substitute A500 Grade B documentation or an A500 size table.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X