ASTM A240 304N Stainless Steel Sheet & Plate | Type 304N / SS304N - SHH STEEL

ASTM A240 Type 304N Stainless Steel Sheet & Plate

ASTM A240 Type 304N stainless steel sheet and plate is a nitrogen-strengthened austenitic grade with higher yield and tensile strength than standard 304. It offers excellent corrosion resistance and formability. Globally supplied by SHH STEEL.
Equivalent Grades:
UNS S30451 / EN 1.4315 / JIS SUS 304N1 / GB 06Cr19Ni10N
Product form:
Plate, Sheet, Coil, Strip, Foil, Shim, Circle, Ring
Surface:
No.1, 2B, 2D, BA, No.4, HL, 8K Mirror, Hairline
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Tolerances
Equivalent Material Grade
Supplementary Requirements
Applications
Why Choose SHH STEEL
FAQ
Conclusion

What is ASTM A240 Type 304N Stainless Steel Sheet?

As a production and export expert at SHH STEEL, we are pleased to present our ASTM A240 Type 304N Stainless Steel Sheet and Plate, also known as SS304N or UNS S30451, ASTM A240 304N, ASTM A240 Type 304N, ASTM A240 304N stainless steel plate, ASTM A240 304N sheet, 304N stainless steel plate, 304N stainless steel sheet, SS304N, UNS S30451, 06Cr19Ni10N, 1.4315, SUS304N

This nitrogen-strengthened version of Type 304 is produced under ASTM A240 / ASME SA240 specification. The controlled addition of nitrogen (0.10–0.16%) significantly increases yield and tensile strength while maintaining good ductility, toughness, and corrosion resistance.

ASTM A240 Type 304N is widely used in applications requiring higher mechanical strength than standard 304 without moving to more expensive alloy grades. SHH STEEL supplies ASTM A240 304N stainless steel plate and ASTM A240 304N sheet in thicknesses from 0.5 mm to 100 mm, with widths up to 2500 mm and lengths up to 12000 mm. Custom sizes and various surface finishes are available.

Our material is typically supplied in the annealed condition with full Mill Test Certificates (EN 10204 3.1). Whether you need thin 304N stainless steel sheet for fabrication or thicker 304N stainless steel plate for structural or pressure applications, SHH STEEL provides consistent quality and reliable global supply.

Material Specification of ASTM A240 Type 304N

ASTM A240 Type 304N stainless steel sheet and plate are manufactured in accordance with ASTM A240/A240M and ASME SA240. This specification covers chromium-nickel stainless steel plate, sheet, and strip for pressure vessels and general applications. SHH STEEL offers material in annealed condition with common finishes such as 2B, No.1, BA, and HL.

Specification Element Requirement SHH STEEL Compliance Keywords
Primary Standard ASTM A240 / ASME SA240 Type 304N Full compliance ASTM A240 304N specification
Product Form Sheet & Plate Both available ASTM A240 304N sheet plate
Thickness Range 0.5–100 mm Custom sizes available ASTM A240 304N dimensions
Width / Length Up to 2500 mm / 12000 mm Custom fabrication ASTM A240 304N size options
Surface Finish 2B, No.1, BA, HL Multiple options ASTM A240 304N finish
Heat Treatment Annealed Standard supply condition ASTM A240 304N annealed

ASTM A240 Type 304N Chemical Composition

The chemical composition of ASTM A240 Type 304N is designed with intentional nitrogen addition to increase strength.

Element Content (%) Standard Limit Role Keywords
Carbon (C) ≤0.08 0.08 max Strength and corrosion balance ASTM A240 304N carbon
Manganese (Mn) ≤2.00 2.00 max Deoxidation and strength ASTM A240 304N manganese
Phosphorus (P) ≤0.045 0.045 max Impurity control ASTM A240 304N phosphorus
Sulfur (S) ≤0.030 0.030 max Cleanliness ASTM A240 304N sulfur
Silicon (Si) ≤0.75 0.75 max Deoxidation ASTM A240 304N silicon
Chromium (Cr) 18.00–20.00 18.00–20.00 Corrosion resistance ASTM A240 304N chromium
Nickel (Ni) 8.00–10.50 8.00–10.50 Austenite stability ASTM A240 304N nickel
Nitrogen (N) 0.10–0.16 0.10–0.16 Strengthening element ASTM A240 304N nitrogen

ASTM A240 Type 304N Mechanical Properties

ASTM A240 Type 304N offers higher strength than standard Type 304 due to nitrogen strengthening.

Property Value Test Method Keywords
Tensile Strength ≥550 MPa (80 ksi) ASTM A370 ASTM A240 304N tensile
Yield Strength (0.2% Offset) ≥240 MPa (35 ksi) ASTM A370 ASTM A240 304N yield
Elongation ≥30% ASTM A370 ASTM A240 304N elongation
Hardness ≤217 HB ASTM E10 ASTM A240 304N hardness
Density 8.00 g/cm³ Standard ASTM A240 304N density

Delivery Conditions

SHH STEEL supplies ASTM A240 Type 304N stainless steel sheet and plate primarily in the annealed condition. Common surface finishes include 2B, No.1, BA, and HL. Protective film is available upon request.

Condition Description Keywords
Annealed Standard supply condition ASTM A240 304N annealed
Surface Finish 2B, No.1, BA, HL ASTM A240 304N surface

Tolerances

Dimensional tolerances comply with ASTM A480. Tighter tolerances can be arranged for precision applications.

Equivalent Material Grade

ASTM A240 Type 304N has multiple international and national equivalents. Below is an expanded comparison including Chinese national standards (GB):

Grade Standard Designation Keywords
Type 304N ASTM A240 / ASME SA240 — ASTM A240 304N equivalent
UNS S30451 Unified Numbering System S30451 ASTM A240 304N UNS
1.4315 EN 10088 / EN 10028-7 X5CrNiN19-9 ASTM A240 304N EN
SUS304N1 / SUS304N2 JIS G4304 / G4305 — ASTM A240 304N JIS
06Cr19Ni10N GB/T 20878 / GB/T 4237 / GB/T 3280 S30458 China GB 06Cr19Ni10N
0Cr19Ni9N old China GB — old China GB 0Cr19Ni9N
X5CrNiN19-9 DIN / EN — ASTM A240 304N DIN
304S65 BS — ASTM A240 304N BS

Note:

  • Chinese standards commonly use 06Cr19Ni10N (new designation) and previously 0Cr19Ni9N.
  • It is also referenced under GB/T 24511 (pressure equipment stainless steel plate) and other related Chinese standards for plate, sheet, and strip.

Supplementary Requirements

Additional testing available includes intergranular corrosion testing, ultrasonic examination, product analysis, and elevated temperature mechanical testing upon request.

Applications

Due to its higher strength and good corrosion resistance, ASTM A240 Type 304N stainless steel sheet and plate are used in:

Application Typical Use Keywords
Pressure Vessels Higher-strength vessels and tanks ASTM A240 304N vessel
Chemical Equipment Process equipment requiring higher strength ASTM A240 304N chemical
Structural Components Load-bearing stainless structures ASTM A240 304N structural
Food & Beverage Equipment needing higher mechanical properties ASTM A240 304N food
Nuclear & Industrial Components requiring nitrogen-strengthened austenitic steel ASTM A240 304N industrial

Why Choose SHH STEEL

SHH STEEL is a professional supplier of ASTM A240 Type 304N stainless steel sheet and plate. We offer competitive pricing, flexible custom sizes, multiple surface finishes, and reliable worldwide delivery. All material is supplied with full Mill Test Certificates.

Advantage | Benefit | Keywords —|—|—|— Full Certification | ASTM A240 / ASME SA240 + MTC 3.1 | ASTM A240 304N certified Flexible Supply | Sheet & Plate, custom sizes | ASTM A240 304N custom Global Experience | Export to 50+ countries | ASTM A240 304N trusted supplier

FAQ

What is the main difference between ASTM A240 304 and 304N?
Type 304N contains intentional nitrogen (0.10–0.16%) which significantly increases yield and tensile strength compared with standard Type 304, while maintaining good corrosion resistance and formability.
What is the Chinese equivalent of ASTM A240 Type 304N?
The main Chinese national standard (GB) equivalents are 06Cr19Ni10N (S30458) and the older designation 0Cr19Ni9N.
Is ASTM A240 304N the same as SUS304N1?
Yes, SUS304N1 (and SUS304N2 in some cases) are the Japanese equivalents of ASTM A240 Type 304N / UNS S30451.
What is the density of ASTM A240 Type 304N?
The density is 8.00 g/cm³.

Conclusion

SHH STEEL’s ASTM A240 Type 304N Stainless Steel Sheet and Plate provide higher strength through nitrogen alloying while retaining the excellent corrosion resistance and fabricability of the 304 family. With strict quality control, flexible sizing, expanded equivalent grade support (including Chinese GB standards), and professional global export service, we deliver reliable solutions to customers worldwide.

Contact SHH STEEL today for your ASTM A240 304N requirements.

Keywords Of ASTM A240 Type 304N Stainless Steel Sheet & Plate

ASTM A240 304N, ASTM A240 Type 304N, ASTM A240 304N stainless steel plate, ASTM A240 304N sheet, 304N stainless steel plate, 304N stainless steel sheet, SS304N, UNS S30451, 06Cr19Ni10N, 1.4315, SUS304N1

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X