ASME SA387 Grade 2 Class 1 (SA387 Gr 2 Cl 1) Steel Plate
What is ASME SA387 Grade 2 Class 1?
ASME SA387 Grade 2 Class 1 (SA387 Gr 2 Cl 1) alloy steel plates are an entry-level chrome-moly grade in the ASME SA387 specification. While higher classes like Class 2 offer quenched and tempered properties for greater strength, Class 1 is normalized, providing tensile strength (415–585 MPa) and yield strength (minimum 240 MPa) with good creep resistance.
The plates are manufactured using normalizing heat treatment, which improves ductility and toughness at elevated temperatures, making them suitable for boilers, pressure vessels, and petrochemical equipment under moderate high-heat conditions.
SHH STEEL supplies ASME SA387 Grade 2 Class 1 plates in a wide size range from 6mm to 100mm thickness, up to 4600mm width, and up to 12000mm length, meeting both ASME Section VIII pressure vessel code and customer-specific requirements.
Material Specification
As a production and export expert at SHH STEEL, we can confirm that ASME SA387 Grade 2 Class 1 alloy steel plates are governed by ASME SA387/SA387M, the standard for pressure vessel plates, alloy steel, chromium-molybdenum.
This specification outlines requirements for normalized plates for elevated temperature service, ensuring suitability for welded pressure vessels and boilers. SHH STEEL complies fully with this standard, providing plates in normalized conditions to optimize mechanical properties.
The specification supports thicknesses from 6mm to 100mm, widths up to 4600mm, and lengths to 12000mm, with custom dimensions available for vessel designs. Ultrasonic examination per ASME SA-578 Class 1 detects laminations, guaranteeing defect-free material, while dual certification with ASTM A387 Gr 2 Cl 1 or EN 10028-2 is offered for international compatibility.
This makes our ASME SA387 Gr 2 Cl 1 plates a reliable choice for global buyers, supported by mill test certificates for complete traceability.
| Specification Element | Requirement | SHH STEEL Compliance | Keywords |
| Primary Standard | ASME SA387/SA387M | ASME Section VIII | SA387 Gr 2 Cl 1 specification |
| Thickness Range | 6mm-100mm (custom) | Mill Test Certificate | SA387 Gr 2 Cl 1 dimensions |
| Width/Length | Up to 4600mm / 12000mm | Custom fabrication available | SA387 Gr 2 Cl 1 size options |
| Ultrasonic Testing | No laminations >0.25% thickness | Class 1 per ASME SA-578 | SA387 Gr 2 Cl 1 inspection |
| Heat Treatment | Normalized | 900-950°C furnace control | SA387 Gr 2 Cl 1 heat treat |
Chemical Composition
At SHH STEEL, we ensure the chemical composition of ASME SA387 Grade 2 Class 1 is tightly controlled per ASME SA387/SA387M to guarantee elevated temperature stability and weldability.
The maximum carbon content is 0.17%, preventing brittleness, while manganese (0.55-0.80%) and silicon (0.15-0.40%) enhance strength and deoxidation. Phosphorus and sulfur are capped at 0.025% each to minimize cracking, chromium (0.50-0.80%) and molybdenum (0.45-0.60%) provide creep resistance.
Our testing per ASME SA-350 maintains a Carbon Equivalent (CE) ≤0.45 per AWS D1.1. Melt analysis (heat analysis) and product analysis differ slightly with tolerances. Melt analysis is stricter for ladle chemistry, while product analysis allows variation for finished plates.
This ensures consistency, making ASME SA387 Gr 2 Cl 1 plates a reliable choice for buyers searching for “ASME SA387 Gr 2 Cl 1 chemical composition.”
| Element | Melt Analysis (%) | Product Analysis (%) | Standard Limit | Test Method | Role | Keywords |
| Carbon (C) | 0.05-0.17 | 0.04-0.18 | 0.17 max | ASME SA-350 | Strength without brittleness | SA387 Gr 2 Cl 1 carbon |
| Manganese (Mn) | 0.55-0.80 | 0.50-0.88 | 0.55-0.80 | ASME SA-350 | Toughness, hardenability | SA387 Gr 2 Cl 1 manganese |
| Phosphorus (P) | ≤0.025 | ≤0.025 | 0.025 max | ASME SA-350 | Reduces brittleness | SA387 Gr 2 Cl 1 phosphorus |
| Sulfur (S) | ≤0.025 | ≤0.025 | 0.025 max | ASME SA-350 | Improves weldability | SA387 Gr 2 Cl 1 sulfur |
| Silicon (Si) | 0.15-0.40 | 0.13-0.45 | 0.15-0.40 | ASME SA-350 | Deoxidation, fluidity | SA387 Gr 2 Cl 1 silicon |
| Chromium (Cr) | 0.50-0.80 | 0.46-0.85 | 0.50-0.80 | ASME SA-350 | Corrosion resistance | SA387 Gr 2 Cl 1 chromium |
| Molybdenum (Mo) | 0.45-0.60 | 0.40-0.65 | 0.45-0.60 | ASME SA-350 | Creep resistance | SA387 Gr 2 Cl 1 molybdenum |
Mechanical Properties
As a production and export expert at SHH STEEL, we can assure you that ASME SA387 Grade 2 Class 1 pressure vessel steel plates deliver strong mechanical properties, tested per ASME SA-370 for tensile/yield, ASME SA-23 for impact, and ASME SA-466 for fatigue.
With a minimum yield strength of 240 MPa and tensile range of 415-585 MPa, these plates support moderate load-bearing capacity, while 22% elongation ensures ductility for forming. The impact energy of 27J typical prevents brittle failure, and the modulus of elasticity (200 GPa) provides structural stability.
The fatigue limit (200 MPa est.) varies with surface finish, optimized by our grinding process. This makes ASME SA387 Gr 2 Cl 1 plates a reliable choice for buyers searching for “ASME SA387 Gr 2 Cl 1 mechanical properties.”
| Property | Value | Test Method | Temperature (°C) | Thickness Effect | Keywords |
| Tensile Strength | 415-585 MPa | ASME SA-370 | Ambient | -5% >100mm | SA387 Gr 2 Cl 1 tensile |
| Yield Strength | 240 MPa (min) | ASME SA-370 | Ambient | Stable to 100mm | SA387 Gr 2 Cl 1 yield |
| Elongation | 22% (min) | ASME SA-370 | Ambient | 20-24% (6-25mm) | SA387 Gr 2 Cl 1 elongation |
| Impact Energy | 27J typical | ASME SA-23 | Ambient | All thicknesses | SA387 Gr 2 Cl 1 impact |
| Modulus of Elasticity | 200 GPa | ASME SA-111 | Ambient | Constant | SA387 Gr 2 Cl 1 modulus |
| Fatigue Limit | 200 MPa (est.) | ASME SA-466 | Ambient | Varies with surface | SA387 Gr 2 Cl 1 fatigue |
Heat Treatment
SHH STEEL provides ASME SA387 Gr 2 Cl 1 plates in normalized condition as standard, heated to 900-950°C and air-cooled to improve toughness for elevated temperature applications.
| Factor | Value/Condition | Standard | Recommended | Keywords |
| Heat Treatment | Normalized at 900-950°C | ASME SA387 | Standard condition | SA387 Gr 2 Cl 1 heat treat |
Delivery
Plates are delivered with as-rolled or stress-relieved options for flexibility, including heat numbers for traceability. Our global shipping ensures timely delivery, with 3-7 days to Asia for standard orders.
| Factor | Value/Condition | Standard | Recommended | Keywords |
| Delivery Condition | Normalized | ASME SA-20 | Transit 3-7 days Asia | SA387 Gr 2 Cl 1 delivery |
Tolerances
We maintain strict tolerances per ASME SA-20: thickness ±1.5mm for <40mm and ±2.0mm for thicker up to 100mm; width/length ±10mm (or ±5mm custom); flatness 3mm per meter. EN 10029 Class B available for European compatibility.
| Factor | Value/Condition | Standard | Recommended | Keywords |
| Thickness Tolerance (<40mm) | ±1.5mm | ASME SA-20 | 6-40mm | SA387 Gr 2 Cl 1 tolerance |
| Flatness | 3mm per meter | ASME SA-20 | All | SA387 Gr 2 Cl 1 flatness |
Weldability
ASME SA387 Gr 2 Cl 1 is weldable with low CE ≤0.45. Preheat at 150-200°C for >25mm to avoid cracking; PWHT at 620-650°C for stress relief. Use GTAW/SMAW/GMAW with E7018 filler for 90-95% efficiency per ASME Section IX. Low sulfur reduces hot shortness, and 22% elongation ensures ductility. Testing includes bend tests (ASTM E190) for 3t radius and ultrasonic for weld integrity per ASTM A435.
| Weldability Factor | Value/Condition | Standard | Recommended Process | Keywords |
| Carbon Equivalent (CE) | ≤0.45 | AWS D1.1 | GTAW, SMAW | SA387 Gr 2 Cl 1 weldability |
| Preheating (°C) | 150-200 (>25mm) | ASME Section IX | GMAW | SA387 Gr 2 Cl 1 welding |
| PWHT (°C) | 620-650 | ASME SA-20 | All | SA387 Gr 2 Cl 1 heat treat |
| Filler Metal | E7018 | AWS A5.1 | SMAW | SA387 Gr 2 Cl 1 welding rod |
| Bend Test Radius (mm) | 3t (t=thickness) | ASTM E190 | All | SA387 Gr 2 Cl 1 bend test |
Equivalent Grades
Global equivalents for ASME SA387 Gr 2 Cl 1 facilitate international projects, offering similar tensile and yield properties for pressure vessel use. For example, 13CrMo4-5 (EN 10028-2) is a European equivalent with 440-590 MPa tensile and 290 MPa yield, suitable for boilers in EU regulations. SCMV2 (JIS G4103) serves Japanese applications with 735 MPa tensile and 415 MPa yield, ideal for high-strength vessels. 15CrMoR (GB/T 1591) is the Chinese standard equivalent, providing 440-590 MPa tensile and 245 MPa yield for cost-effective high-temperature equipment in Asian markets. These equivalents ensure cross-compatibility, allowing buyers to substitute ASME SA387 Gr 2 Cl 1 plates seamlessly in global supply chains.
| Grade | Standard | Tensile (MPa) | Yield (MPa) | Elongation (%) | Impact (J @ -20°C) | Keywords |
| SA387 Gr 2 Cl 1 | ASME SA-387/SA-387M | 415-585 | 240 | 22 | 27 | SA387 Gr 2 Cl 1 equivalent |
| 13CrMo4-5 | EN 10028-2 | 440-590 | 290 | 22 | 27 | SA387 Gr 2 Cl 1 EN grade |
| SCMV2 | JIS G4103 | 735 | 415 | 15 | 27 | SA387 Gr 2 Cl 1 JIS grade |
| 15CrMoR | GB/T 1591 | 440-590 | 245 | 20 | 27 | SA387 Gr 2 Cl 1 GB grade |
| A387 Gr.5 Cl.1 | ASTM A387 | 515-690 | 310 | 19 | 34 | SA387 Gr 2 Cl 1 alternative |
| A516 Gr.60 | ASTM A516 | 415-550 | 220 | 21 | 27 | SA387 Gr 2 Cl 1 similar alt |
Supplementary Requirements
Supplementary requirements for ASME SA387 Gr 2 Cl 1 pressure vessel steel plates enhance performance for specialized applications. They offer buyers tailored options.
These include ultrasonic testing (Class 1 per ASTM A435 for no laminations >0.25% thickness). Charpy impact at -50°C (27J min per ASTM A20 for cold service) is another. Heat analysis per heat number (ASTM E350 for traceability) ensures quality. Product analysis allows ±0.02% tolerance on elements. Shot blasting to Sa 2.5 (50-100μm profile per ISO 8501-1) is available for surface preparation.
SHH STEEL provides these to meet stringent needs. Buyers search for “SA387 Gr 2 Cl 1 supplementary requirements.”
| Requirement | Detail | Standard | Test Frequency | Applicable Thickness (mm) | Keywords |
| Ultrasonic Testing | Class 1, no laminations | ASTM A435 | Full plate | 6-100 | SA387 Gr 2 Cl 1 ultrasonic |
| Charpy Impact | -50°C, 27J min | ASTM A20 | Per heat | 6-100 | SA387 Gr 2 Cl 1 cold impact |
| Heat Analysis | Per heat number | ASTM E350 | Each batch | All | SA387 Gr 2 Cl 1 analysis |
| Product Analysis | ±0.02% tolerance | ASTM E350 | Sample per lot | All | SA387 Gr 2 Cl 1 product test |
| Shot Blasting | Sa 2.5, 50-100μm profile | ISO 8501-1 | On request | 6-50 | SA387 Gr 2 Cl 1 blasting |
Applications
ASME SA387 Gr 2 Cl 1 pressure vessel steel plates are versatile for elevated-temperature and pressure environments. They have good toughness and formability.
| Application | Temperature (°C) | Pressure (bar) | Thickness (mm) | Standard Compliance | Keywords |
| Pressure Vessels | Up to 450 | 300 | 20-100 | ASME Section VIII | SA387 Gr 2 Cl 1 vessels |
| Boilers | Up to 450 | 200 | 10-50 | ASME Section I | SA387 Gr 2 Cl 1 boilers |
| Heat Exchangers | Up to 400 | 150 | 6-30 | TEMA Standards | SA387 Gr 2 Cl 1 heat exchange |
| Storage Tanks | Up to 350 | 100 | 30-80 | API 650 | SA387 Gr 2 Cl 1 tanks |
| Steam Drums | Up to 450 | 250 | 20-60 | ASME Section VIII | SA387 Gr 2 Cl 1 steam drums |
Details: Pressure vessels benefit from 415-585 MPa tensile at 450°C. Boilers handle 450°C with 22% elongation for forming. Heat exchangers use 6-30mm plates for 150 bar at 400°C. Storage tanks leverage 30-80mm for 100 bar at 350°C per API 650. Steam drums utilize 20-60mm plates for 250 bar at 450°C, per ASME Section VIII for efficient steam generation.
Why Choose SHH STEEL
SHH STEEL offers ASME and ASTM-certified SA387 Gr 2 Cl 1 plates. We provide custom thicknesses up to 300mm. Heat treatments are tailored to your project. Our 15-year track record includes zero defect deliveries to 50+ countries. This is backed by SGS verification and mill test certificates.
| Advantage | Benefit | Keywords |
| Expert Certification | ASME Section VIII compliant | SA387 Gr 2 Cl 1 certified |
| Custom Fabrication | Up to 300mm thickness | SA387 Gr 2 Cl 1 custom |
| Proven Reliability | 50+ countries, zero rejects | SA387 Gr 2 Cl 1 trusted supplier |
FAQ
-
What is ASME SA387 Grade 2 Class 1 used for?
- ASME SA387 Grade 2 Class 1 is widely used for moderate-temperature pressure vessels, boilers, and heat exchangers in power generation and petrochemical industries. It handles temperatures up to 450°C and pressures to 300 bar, with 415-585 MPa tensile strength ensuring reliability. SHH STEEL supplies these for welded constructions per ASME Section VIII Division 1.
-
What is the difference between SA387 Gr 2 Cl 1 and SA387 Gr 2 Cl 2?
- SA387 Gr 2 Cl 1 is normalized with 240 MPa yield for standard service, while Gr 2 Cl 2 is quenched and tempered with 310 MPa yield for higher strength. SHH STEEL recommends Gr 2 Cl 1 for moderate loads.
-
What is the chemical composition of SA387 Gr 2 Cl 1?
- The composition includes C 0.05-0.17%, Mn 0.55-0.80%, P ≤0.025%, S ≤0.025%, Si 0.15-0.40%, Cr 0.50-0.80%, Mo 0.45-0.60%, tested per ASME SA-350. This alloyed formula ensures creep resistance with CE ≤0.45 (AWS D1.1). SHH STEEL provides MTCs with full analysis for traceability.
-
Is SA387 Gr 2 Cl 1 weldable?
- Yes, SA387 Gr 2 Cl 1 is highly weldable with low carbon (0.05-0.17%) and preheating at 150-200°C for >25mm thicknesses. Use E7018 filler (AWS A5.1) for 90% joint efficiency per ASME Section IX. PWHT at 620-650°C reduces stress, validated by bend tests per ASTM E190.
-
What is the density of SA387 Gr 2 Cl 1
- The density is 7.85 g/cm³, standard for alloy steel, aiding weight calculations in vessel design. Hardness is 143-217 HB (ASME SA-18), balancing wear resistance for high-temperature use.
-
What is the equivalent of ASME SA387 Gr 2 Cl 1 in EN standards?
- The closest EN equivalent is 13CrMo4-5 (EN 10028-2), with 440-590 MPa tensile and 290 MPa yield, suitable for EU boilers. SHH STEEL provides dual-certified plates for seamless transitions.
-
What is the maximum thickness for SA387 Gr 2 Cl 1?
- Standard thickness is 100mm, with custom options up to 300mm available. Normalized at 900-950°C per ASME SA-20, these plates are ideal for moderate-temperature vessels, with ultrasonic testing per ASME SA-578 ensuring no laminations for structural integrity.
Conclusion
SHH STEEL’s ASME SA387 Gr 2 Cl 1 Pressure Vessel Steel Plates provide unmatched strength and reliability for elevated-temperature pressure vessels and boilers. With precise tolerances, superior weldability, and global equivalents, we offer customized solutions. Trust SHH STEEL for your steel needs.