ASME SA240 UNS S30200 (Type 302) stainless steel plate at SHH STEEL warehouse

ASME SA240 UNS S30200 Stainless Steel Plate

ASME SA240 UNS S30200 stainless steel plate: UNS S30200 (Type 302) is a higher-carbon 18-8 austenitic grade, supplied as plate, sheet and strip to ASME SA-240 / ASTM A240 (C ≤ 0.15 %, Cr 17.0–19.0 %, Ni 8.0–10.0 %; minimum yield 205 MPa). SHH STEEL advises on grade selection and dual certification and supplies mill-direct plate with third-party inspection, small-lot consolidation and in-house processing.
Keywords
ASME SA240 UNS S30200, SA240 S30200 plate, UNS S30200 stainless steel plate, SA-240 Type 302 plate, S30200 sheet supplier
Equivalent Grades:
EN 1.4310 X10CrNi18-8; JIS SUS302; GB/T 12Cr18Ni9 (S30210) (nearest; limits differ)
Share:
Overview
Specification
Chemical Composition
Mechanical Properties
Key Characteristics
Equivalent Grades
Related Grades
Applications
Sizes and Supply Forms
Fabrication
Testing and Certificates
Buyer Concerns
Supply Notes
FAQ
Conclusion

What is ASME SA240 UNS S30200 stainless steel plate?

UNS S30200 (Type 302) is the older, higher-carbon (≤ 0.15 %) version of the 18-8 austenitic steels, with 17.0–19.0 % chromium and 8.0–10.0 % nickel. It has the same minimum tensile and yield levels as Type 304. Its higher permitted carbon makes it more prone to sensitization during welding, so most welded fabrication has moved to S30400 or S30403.

This page sets out the SA-240 requirements for UNS S30200 (Type 302) plate, sheet and strip, the nearest EN, JIS and GB/T grades, typical sizes and the documents that come with each shipment. SHH STEEL supplies S30200 plate mill-direct from long-term Chinese mill partners and advises buyers on grade selection, dual certification and inspection before the order is placed.

SA-240 and A240 coverage of UNS S30200

ASME SA-240/SA-240M is the ASME Boiler and Pressure Vessel Code (Section II, Part A) adoption of ASTM A240/A240M, the specification for chromium, chromium-nickel and chromium-manganese-nickel stainless steel plate, sheet and strip for pressure vessels and general applications. General requirements such as ordering information, heat treatment, dimensional tolerances, finish, testing and certification come from ASTM A480/A480M.

UNS S30200 (Type 302) appears in Table 1 (chemistry) and Table 2 (mechanical properties) of the specification. For ASME Code construction, order and certify to SA-240 for the Code edition named in the design; most mills issue dual ASTM A240 / ASME SA-240 certificates. Allowable stresses are not part of SA-240 and come from ASME Section II, Part D.

UNS S30200 chemical composition (heat analysis, %)

Heat analysis limits for UNS S30200 (Type 302), in percent by mass (maximum unless a range or minimum is shown), from ASTM A240/A240M Table 1:

Grade C Mn P S Si Cr Ni N
UNS S30200 0.15 2.00 0.045 0.030 0.75 17.0–19.0 8.0–10.0 0.10

Product (check) analysis tolerances follow ASTM A480/A480M.

UNS S30200 mechanical properties (annealed)

Room-temperature tensile and hardness requirements for UNS S30200 (Type 302) in the annealed condition (ASTM A240/A240M Table 2):

Condition / thickness Tensile strength, min Yield strength 0.2 %, min Elongation in 50 mm, min Hardness, max Cold bend
All thicknesses 515 MPa [75 ksi] 205 MPa [30 ksi] 40 % 201 HBW / 92 HRBW not required

Yield strength is the 0.2 % offset value; 1 % offset yield can be reported when ordered under Supplementary Requirement S3, and Charpy impact tests under Supplementary Requirement S1.

Bend tests are not required for austenitic or duplex grades.

Key characteristics of UNS S30200 (Type 302)

UNS S30200 (Type 302) is a higher-carbon 18-8 austenitic grade. The points that matter most when specifying it:

  • Minimum tensile 515 MPa and yield 205 MPa, with hardness up to 201 HBW.
  • Carbon up to 0.15 % increases the risk of chromium-carbide precipitation in weld heat-affected zones.
  • Good spring properties after cold working.
  • Silicon maximum is 0.75 %, the same as for Type 304.

UNS S30200 equivalent grades: EN, JIS and GB/T

The grades below are the nearest equivalents of UNS S30200 (Type 302) in other standards. They are cross-references, not identical specifications: element ranges and minimum properties differ, so dual certification is only possible when one heat meets every standard named on the order.

Standard Nearest grade Note
EN EN 1.4310 X10CrNi18-8 nearest (lower Ni)
JIS JIS SUS302 nearest
GB/T GB/T 4237 12Cr18Ni9 (S30210) nearest

UNS S30200 (Type 302) compared with related grades

Grades buyers most often compare with UNS S30200 (Type 302):

All grades in this series are listed under ASME SA240/SA240M stainless steel plate and ASTM A240/A240M stainless steel plate.

Applications of SA240 UNS S30200 plate

Typical uses of UNS S30200 (Type 302) plate, sheet and strip:

  • Spring and formed parts made from sheet or strip
  • Trim and appliance components
  • Replacement parts for older equipment designed for Type 302
  • General non-welded fabrications

The final choice should always be checked against the service medium, temperature and design code; SHH STEEL can share mill corrosion data and reference projects on request.

UNS S30200 (Type 302) sizes, finishes and supply forms

Size ranges below are typical mill capabilities for UNS S30200 (Type 302), not limits set by the specification; actual availability depends on the mill campaign and is confirmed at quotation.

Item Typical supply range
Product forms Cold rolled sheet and strip are the most common forms; plate is available against mill production.
Width 1000, 1219, 1250, 1500, 1800, 2000 mm; wider plate by mill
Length 2000, 2438, 3000, 6000 mm, coil, or cut to size
Surface finish No.1 (hot rolled, annealed and pickled) for plate; 2B, 2D or BA for cold rolled sheet; No.4 / HL polishing on request
Tolerances ASTM A480/A480M, or tighter by agreement

For weight estimates, plate weight (kg) ≈ thickness (mm) × width (m) × length (m) × density, with density about 7.9–8.0 g/cm³ for this grade family. The mill certificate weight governs invoicing.

Forming, welding and heat treatment of UNS S30200

Annealed plate forms well by bending, rolling and pressing; austenitic steels work-harden, so allow for higher forming forces than for carbon steel.

Welding by GTAW, GMAW, SMAW or SAW with a matching or suitable austenitic filler is standard. Clean the joint, control heat input and interpass temperature, and remove heat tint by pickling or brushing to restore corrosion resistance.

Heat treatment (solution annealing) and its cooling requirements follow ASTM A480/A480M. Re-anneal after severe cold work if the part must return to the annealed properties.

Testing, inspection and certificates for S30200 plate

Each heat is tested to SA-240 / A240 and ASTM A480/A480M: heat analysis, tension tests and hardness, plus the surface and dimensional checks for the product form.

Mill test certificates to EN 10204 3.1 are standard. EN 10204 3.2 certificates with third-party witness (TUV, ABS, CCS, BV, DNV, LR or an inspector named by the buyer) can be arranged, together with optional tests such as PMI, intergranular corrosion, ultrasonic testing and Charpy impact (Supplementary Requirement S1).

Common buyer concerns and SHH STEEL solutions

The concerns below come up most often when buyers source UNS S30200 (Type 302) plate from China, together with how SHH STEEL deals with each one.

Buyer Concern SHH STEEL Solution
Fake material or certificates Each heat can be checked by TUV, ABS, CCS or another class society as third-party witness, and partner laboratories run PMI, chemical and mechanical tests against the order. Third-party witness and EN 10204 3.2 certificates available.
Unsafe deposit TT and LC are both accepted, including TT + LC combinations. For large projects the buyer can sign directly with the mill, and SHH STEEL handles coordination and documents for a small service fee.
Small orders below mill MOQ Small quantities are consolidated with other customers’ orders of the same grade and thickness, so even lots below the mill MOQ are rolled as genuine mill production with full traceability.
Slow delivery Dedicated staff chase the mill delivery schedule and report progress at melting, rolling, heat treatment, testing and packing, so delays are seen early.
Processing needs Our own workshop provides cutting, bevelling, machining to drawings and surface pretreatment as value-added services, so plates arrive ready for fabrication.

How to order UNS S30200 plate from SHH STEEL

To quote quickly, please send: specification and edition (name ASME SA-240 (with Code edition) or ASTM A240, and the UNS number); thickness, width and length or a cutting list; quantity; finish; inspection document (3.1 or 3.2) and any third-party inspector; supplementary tests; and delivery terms.

SHH STEEL works as a sourcing and supply partner with long-term mill relationships. We help select the grade, check dual-certification options, consolidate small lots, follow production at the mill and process plates in our own workshop before shipment. Payment by TT or LC is accepted.

FAQ

What is the difference between S30200 and S30400?
The main difference is carbon. S30200 allows up to 0.15 % C and S30400 up to 0.08 % C, and the nickel and chromium ranges differ slightly. For welded parts S30400 or S30403 is usually preferred.
Is SA240 302 still available?
Yes, but mills roll it less often than 304. Small quantities are usually supplied from planned production or replaced by an approved alternative with the buyer’s agreement.
Can 304 be certified as 302?
Only if the heat meets every S30200 limit in Table 1 and Table 2. Dual marking needs a heat analysis that fits both grades, and the buyer should approve it.
Where can I buy ASME SA240 UNS S30200 plate in small quantities?
SHH STEEL consolidates small orders of S30200 with other customers’ orders of the same grade, so lots below the mill MOQ can still be placed against mill production. Cut-to-size pieces can be supplied from our workshop.
What certificates come with S30200 stainless steel plate?
Plates are supplied with EN 10204 3.1 mill test certificates to SA-240 / A240. Third-party witness and EN 10204 3.2 certificates available, issued with TUV, ABS, CCS or another nominated inspector.
What is the lead time for S30200 plate from China?
Lead time depends on the mill rolling schedule, thickness and the tests ordered, and is confirmed with the quotation. Dedicated SHH STEEL staff follow the mill schedule and report progress until shipment.

Conclusion

ASME SA240 UNS S30200 Stainless Steel Plate is ordered as UNS S30200 (Type 302), a higher-carbon 18-8 austenitic grade. Specify the standard and edition, the UNS number, the inspection document and any supplementary tests on the order so the certificate can be checked line by line. Contact SHH STEEL for a quotation, mill-direct supply and processing to your drawings.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X