ASME SA240 2304 Stainless Steel Plate | SA240 Type 2304 - SHH STEEL

ASME SA240 2304 Stainless Steel Plate | SA240 Type 2304

ASME SA240 2304 (SA240 Type 2304 / UNS S32304) is a lean duplex stainless steel plate offering higher strength than 304/316, good resistance to stress corrosion cracking, and excellent cost-effectiveness. SHH STEEL supplies ASME SA240 2304 as China Mill-Direct Supply with competitive pricing and full mill
Equivalent Grades:
UNS S32304 / EN 1.4362 / JIS SUS329J3L (near) / GB 022Cr23Ni4MoN
Specification:
ASTM A240 / ASME SA-240 — Delivery: Solution Annealed (lean duplex)
Surface:
No.1, 2B, 2D, BA, No.4, HL, 8K Mirror, Hairline
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Material Comparison
Corrosion Resistance
Weldability
Heat Treatment
Surface Finishes
Tolerances
Equivalent Material Grades
Applications
Why Choose SHH STEEL
FAQ
Conclusion

What is ASME SA240 2304 Stainless Steel Plate?

As a professional stainless steel plate supplier and China Mill-Direct Supply / Mill Direct Exporter, SHH STEEL is pleased to present ASME SA240 2304 Stainless Steel Plate, also known as SA240 Type 2304 or UNS S32304.

ASME SA240 Type 2304 is a lean duplex (austenitic-ferritic) stainless steel containing approximately 23% chromium, 4% nickel and nitrogen, with very low molybdenum content. The balanced duplex microstructure delivers significantly higher yield strength than standard austenitic grades such as 304L or 316L (nearly twice the yield strength), combined with good resistance to chloride stress corrosion cracking and adequate pitting resistance for many environments.

Type 2304 offers an attractive combination of mechanical properties, corrosion performance and cost. It is frequently selected as a higher-strength, more economical alternative to 304/304L or 316/316L in applications where the full pitting resistance of molybdenum-bearing duplex grades (such as 2205) is not required. Typical uses include chemical process equipment, pulp & paper, water treatment, storage tanks, structural components and architectural applications.

SHH STEEL supplies ASME SA240 2304 as true Mill Direct Supply, sourcing directly from major Chinese stainless steel mills. This model delivers competitive mill pricing, consistent quality, full heat traceability and shorter lead times. We offer a practical dimensional range and surface finishes suitable for industrial and fabricated applications.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Primary Standard ASME SA240 / SA240M Full compliance
Steel Grade Type 2304 (UNS S32304) Confirmed
Product Form Plate, Sheet Available
Delivery Condition Solution Annealed Standard
Thickness Range 1 mm – 50 mm (thicker available on request) Custom sizes supported
Width Up to 2000–3000 mm Available
Length Up to 12000 mm or cut-to-length Available
Surface Finish No.1, 2B, and others on request Available
Certification EN 10204 3.1 / ASME Mill Test Certificate Available

Chemical Composition

Heat Analysis (Ladle Analysis) according to ASME SA240 Type 2304 (UNS S32304):

Element Content (%)
Carbon (C) ≤ 0.030
Silicon (Si) ≤ 1.00
Manganese (Mn) ≤ 2.50
Phosphorus (P) ≤ 0.040
Sulfur (S) ≤ 0.030
Chromium (Cr) 21.50 – 24.50
Nickel (Ni) 3.00 – 5.50
Molybdenum (Mo) 0.05 – 0.60
Nitrogen (N) 0.05 – 0.20
Copper (Cu) 0.05 – 0.60
Iron (Fe) Balance

Product Analysis (typical permissible variations):

Element Content (%)
Carbon (C) ≤ 0.030
Silicon (Si) ≤ 1.00
Manganese (Mn) ≤ 2.50
Phosphorus (P) ≤ 0.040
Sulfur (S) ≤ 0.030
Chromium (Cr) 21.50 – 24.50
Nickel (Ni) 3.00 – 5.50
Molybdenum (Mo) 0.05 – 0.60
Nitrogen (N) 0.05 – 0.20
Copper (Cu) 0.05 – 0.60

The lean duplex chemistry (high Cr + N, low Ni and very low Mo) produces a balanced austenite-ferrite microstructure that delivers high strength and good stress corrosion cracking resistance at a lower alloy cost than standard duplex 2205.

Mechanical Properties

Room-Temperature Mechanical Properties (Solution Annealed Condition)

Property Value
Tensile Strength ≥ 600 MPa (87 ksi)
Yield Strength (0.2%) ≥ 400 MPa (58 ksi)
Elongation (in 50 mm) ≥ 25%
Hardness ≤ 290 HB

Key Advantage The minimum yield strength of ASME SA240 2304 is approximately twice that of 304L/316L, allowing significant thickness reduction and weight savings in many designs.

Physical Properties

  • Density: approximately 7.80 g/cm³
  • Magnetic: Partially magnetic (duplex microstructure)
  • Thermal Expansion: Lower than austenitic grades

Material Comparison

Grade Structure Yield Strength (min) PREN (approx.) Primary Advantage Typical Preference
SA240 Type 304L Austenitic 170 MPa ≈ 18–20 Excellent formability & weldability General corrosive service
SA240 Type 316L Austenitic 170 MPa ≈ 24 Better pitting resistance Moderate chloride service
SA240 Type 2304 Lean Duplex 400 MPa ≈ 26 High strength + good SCC resistance + lower cost Cost-effective high-strength alternative to 304/316
SA240 Type 2205 Duplex 450 MPa ≥ 35 Higher pitting & crevice corrosion resistance More severe chloride service
SA240 Type 2507 Super Duplex 550 MPa ≥ 40–43 Highest strength & corrosion resistance Seawater / most severe chloride service

ASME SA240 2304 is selected when higher strength and better stress corrosion cracking resistance than 304L/316L are required, while the full pitting resistance of 2205 is not necessary. It is a cost-effective lean duplex solution. For more aggressive chloride environments, astm a240 type 2205 stainless steel sheet plate or astm a240 type 2507 stainless steel sheet plate should be considered. Related austenitic options include astm a240 type 304l stainless steel sheet plate and astm a240 type 316l stainless steel sheet plate.

Corrosion Resistance

ASME SA240 Type 2304 offers good resistance to general corrosion in many chemical environments and significantly better resistance to chloride stress corrosion cracking than austenitic grades 304L and 316L. Its pitting resistance (PREN ≈ 26) is higher than 304L but lower than standard duplex 2205.

It performs well in neutral and alkaline media, many organic acids, and moderate chloride environments. It is not intended for severe seawater or highly aggressive chloride service, where higher-alloy duplex or super duplex grades are preferred.

Weldability

ASME SA240 Type 2304 has good weldability for a duplex stainless steel. Matching lean duplex or 2209-type filler metals are commonly used.

Key points:

  • Heat input and interpass temperature should be controlled (typically interpass ≤ 150°C).
  • Proper shielding is important to maintain the balanced microstructure and corrosion resistance.
  • Post-weld heat treatment is generally not required for most applications.
  • When correctly welded, the joint retains high strength and good corrosion performance.

Heat Treatment

ASME SA240 Type 2304 is supplied in the solution-annealed condition.

Recommended Solution Annealing Parameters

  • Temperature range: 950 – 1050°C (typically 1000 – 1050°C)
  • Holding (soaking) time: – Plates ≤ 25 mm: minimum 15–30 minutes after the section reaches temperature – Plates 25–50 mm: minimum 30–45 minutes – Thicker plates: longer times to ensure uniformity
  • Cooling: Rapid cooling (water quenching preferred) is essential to preserve the balanced duplex microstructure and optimum corrosion resistance. Slow cooling can lead to formation of intermetallic phases that reduce toughness and corrosion performance.

Proper solution annealing and rapid cooling are critical for Type 2304 performance.

Surface Finishes

Finish Description Typical Use / Keywords
No.1 Hot-rolled, annealed and pickled SA240 2304 No.1 – most common for industrial and pressure vessel plate
2B Cold-rolled, annealed, pickled, skin-passed SA240 2304 2B – thinner plates and general fabrication
No.4 Brushed finish SA240 2304 No.4 – when improved surface appearance is required
Special Ground or custom finishes SA240 2304 Special – on request

SHH STEEL regularly supplies ASME SA240 2304 in No.1 and 2B finishes, and can provide other finishes according to project requirements.

Tolerances

Dimensional tolerances for ASME SA240 2304 Stainless Steel Plate conform to ASME SA240 and the general requirements of ASTM A480.

Typical available size range for SA240 2304 plate:

  • Thickness: 1 mm – 50 mm (thicker plates available on request)
  • Width: up to 2000–3000 mm
  • Length: up to 12000 mm or cut-to-length according to customer requirements

Thickness, width, length and flatness tolerances are controlled within standard limits. Tighter tolerances for SA240 2304 plate can be arranged for specific project needs. SHH STEEL provides precise dimensional control for both standard and custom-size SA240 2304 plates.

Equivalent Material Grades

Grade / Designation Standard Notes
SA240 Type 2304 ASME SA240 —
A240 Type 2304 ASTM A240 Essentially identical
UNS S32304 — Unified Numbering System
1.4362 / X2CrNiN23-4 EN 10088-2 European equivalent
Related lean duplex JIS / GB Approximate national equivalents

Related grades frequently evaluated with ASME SA240 2304 include astm a240 type 2205 stainless steel sheet plate, astm a240 type 304l stainless steel sheet plate, astm a240 type 316l stainless steel sheet plate, and astm a240 type 2507 stainless steel sheet plate.

Applications

ASME SA240 Type 2304 is used where higher strength and better stress corrosion cracking resistance than 304/316 are required at an economical cost. Typical applications of SA240 2304 include:

Industry / Sector Typical Components / Equipment (with keywords)
Chemical Processing SA240 2304 tanks, vessels, piping and process equipment
Pulp & Paper SA240 2304 digesters, bleaching equipment and structural parts
Water Treatment & Desalination SA240 2304 tanks, piping and structural components
Storage Tanks SA240 2304 storage and process tanks
Architecture & Construction SA240 2304 structural and cladding components
Food & Beverage SA240 2304 equipment in moderate environments
General Fabrication SA240 2304 high-strength welded structures

Why Choose SHH STEEL

SHH STEEL is a China Mill-Direct Supply and Mill Direct Exporter of stainless steel plate. We maintain long-term strategic cooperation with major Chinese stainless steel mills and supply ASME SA240 Type 2304 with the following advantages:

  • Competitive mill-direct pricing
  • Consistent quality and complete heat traceability
  • Full Mill Test Certificates (EN 10204 3.1 /3.2 ASME)
  • Flexible dimensions and surface finishes (including SA240 2304 No.1 and SA240 2304 2B)
  • Technical support for lean duplex material selection and fabrication
  • Reliable worldwide logistics and export documentation

FAQ

What is the main advantage of SA240 2304 over SA240 304L or 316L?
Type 2304 offers approximately twice the yield strength and significantly better resistance to chloride stress corrosion cracking, while remaining cost-competitive. SHH STEEL recommends 2304 when higher strength and improved SCC resistance are required without the cost of higher-alloy duplex grades.
How does SA240 2304 compare with SA240 2205?
Type 2304 is a lean duplex with lower molybdenum content, offering lower pitting resistance but better economy. Type 2205 provides higher PREN and better performance in more severe chloride environments. SHH STEEL can help select the appropriate grade based on the specific service conditions.
Is ASME SA240 2304 magnetic?
Yes, it is partially magnetic due to its duplex (austenite + ferrite) microstructure. SHH STEEL supplies material that meets this characteristic.
What is the density of SA240 Type 2304?
Approximately 7.80 g/cm³. SHH STEEL provides material certificates confirming physical and mechanical properties.
Can SHH STEEL supply dual-certified ASME SA240 / ASTM A240 Type 2304?
Yes, SHH STEEL commonly supplies dual-certified ASME SA240 / ASTM A240 Type 2304 material.

Conclusion

ASME SA240 2304 Stainless Steel Plate (SA240 Type 2304 / UNS S32304) is a lean duplex stainless steel that delivers high strength, good resistance to stress corrosion cracking and attractive economy. It is an excellent cost-effective alternative to 304L/316L in many chemical, water treatment, pulp & paper and structural applications.

As a professional China Mill-Direct Supply and Mill Direct Exporter, SHH STEEL provides high-quality ASME SA240 Type 2304 plate with competitive pricing, full certification and complete technical support.

Contact SHH STEEL today for stock availability, surface finish options (including SA240 2304 No.1 and SA240 2304 2B), or a competitive quotation.

ASME SA240 2304 Stainless Steel Plate, SA240 Type 2304, SA240 2304, ASME SA240 Type 2304, 2304 stainless steel plate, lean duplex 2304, SA240 2304 supplier

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response