JIS G 3466 STKR400 Steel Hollow Sections | JIS G 3466 Steel Hollow Sections - SHH STEEL

JIS G 3466 STKR400 Steel Hollow Sections

JIS G 3466:2025 STKR400 is carbon steel square and rectangular hollow section. Heat analysis limits carbon to 0.25 % and phosphorus and sulfur to 0.040 %; silicon and manganese are unrestricted. Minimum tensile strength is 400 N/mm² and minimum yield is 245 N/mm². Elongation is 23 % on a No. 5 piece, reduced 1.5 % per millimetre below 8 mm wall.
Keywords
JIS G 3466 STKR400, STKR400 hollow section, G3466 square rectangular tube, STKR400 carbon steel section, JIS G3466 STKR400 sizes
Equivalent Grades:
Near-equivalents only, not automatic substitutes.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Size Chart
Applications
Equivalent Grades
Sourcing
FAQ
Conclusion

What is JIS G 3466 STKR400 Steel Hollow Section?

JIS G 3466 STKR400 is carbon steel square and rectangular hollow section for general structural use. The values on this page follow JIS G 3466:2025, dual-sourced from a JISC-verified public recitation and a September 2025 mill handbook extract that agree on the STKR400 limits used here. The edition named on the purchase order governs delivery.

STKR490 is a second grade in the same standard, with higher strength, and is not this product. Circular hollow sections are outside the square-and-rectangular scope of this page.

Material, Manufacture and Scope for JIS G 3466 STKR400

G 3466 covers carbon steel square and rectangular tubes for general structure. The forming route and any required weld test must follow the named edition and the order. This page does not recast STKR400 as an EN 10219, EN 10210, ASTM A500 or ASTM A501 product.

JIS G 3466 STKR400 Chemical Composition (Heat Analysis)

STKR400 limits carbon to 0.25 % and phosphorus and sulfur to 0.040 % on heat analysis. Silicon and manganese are unrestricted in the STKR400 row used here; do not invent maxima for those two elements.

Swipe horizontally to view all dimensions.

Element Heat-analysis limit (mass %) Notes
C, max 0.25 STKR400 in JIS G 3466:2025.
Si Unrestricted in the STKR400 row used here No silicon maximum is stated for STKR400 in the sources compared for this page.
Mn Unrestricted in the STKR400 row used here No manganese maximum is stated for STKR400 in the sources compared for this page.
P, max 0.040 —
S, max 0.040 —

JIS G 3466 STKR400 Mechanical Properties

Minimum tensile strength is 400 N/mm² and minimum yield strength is 245 N/mm². Minimum elongation is 23 % on a No. 5 test piece for walls of 8 mm and thicker. For walls thinner than 8 mm, that 23 % value is reduced by 1.5 percentage points for each millimetre of wall below 8 mm. Do not apply the STKR490 mechanical row to this grade.

Swipe horizontally to view all dimensions.

Property Requirement for STKR400
Tensile strength, min 400 N/mm²
Yield strength, min 245 N/mm²
Elongation, min, No. 5 test piece, wall ≥ 8 mm 23 %
Elongation, wall < 8 mm The 23 % No. 5 value is reduced by 1.5 percentage points for each millimetre of wall thickness below 8 mm, in the 2025 text used here.

JIS G 3466 STKR400 Typographical Square and Rectangular Sizes

JIS G 3466 does not, on this page, receive a complete official size annex transcription. The tables are a typographical common-size subset of square and rectangular carbon steel sections, with theoretical sharp-corner mass at 7.85 g/cm³: M = 0.0157 t (A + B − 2t) kg/m. Actual corner radii specified or produced under G 3466 change the mass. These rows are not a mill stock list, and they are not an EN 10219 or ASTM A500 HSS table.

Typographical square sections (STKR400 enquiries)

Swipe horizontally to view all dimensions.

A × B × t (mm) Theoretical sharp-corner mass (kg/m)
50 × 50 × 2.3 3.44
50 × 50 × 3.2 4.7
60 × 60 × 3.2 5.71
75 × 75 × 3.2 7.21
100 × 100 × 3.2 9.73
100 × 100 × 4.5 13.49
125 × 125 × 4.5 17.03
150 × 150 × 4.5 20.56
150 × 150 × 6 27.13
200 × 200 × 6 36.55
200 × 200 × 9 53.98
250 × 250 × 6 45.97
250 × 250 × 9 68.11
300 × 300 × 9 82.24
300 × 300 × 12 108.52

Typographical rectangular sections (STKR400 enquiries)

Swipe horizontally to view all dimensions.

A × B × t (mm) Theoretical sharp-corner mass (kg/m)
75 × 45 × 3.2 5.71
100 × 50 × 3.2 7.21
100 × 50 × 4.5 9.96
125 × 75 × 4.5 13.49
150 × 100 × 4.5 17.03
150 × 100 × 6 22.42
200 × 100 × 6 27.13
200 × 150 × 6 31.84
250 × 150 × 6 36.55
250 × 150 × 9 53.98
300 × 200 × 9 68.11
300 × 200 × 12 89.68

Applications and Service Limits for JIS G 3466 STKR400 Hollow Sections

STKR400 is used for general structural square and rectangular tubes. It is not automatically a substitute for EN 10219 or ASTM A500 Grade B, even where some tensile figures look close. Outside size, wall and length must be stated on the order.

Near-Equivalents for JIS G 3466 STKR400: Not Automatic Substitutes

Near-equivalents only, not automatic substitutes. STKR490 is a different grade in G 3466. ASTM A500, ASTM A501, EN 10219 and EN 10210 hollow sections have their own chemistry, forming routes and size systems. Do not treat a certificate from those specifications as STKR400.

Sourcing JIS G 3466 STKR400 Steel Hollow Sections from SHH STEEL

SHH STEEL reviews the named JIS G 3466 edition, the STKR400 certificate and the ordered outside size and wall before quoting. The typographical size tables on this page are not a warehouse list.

FAQ: JIS G 3466 STKR400 Steel Hollow Sections

Is STKR400 the same as STKR490?
No. STKR490 is a higher-strength grade in JIS G 3466 and would need its own product page. This page is STKR400 only.
Which edition is used on this page?
JIS G 3466:2025, dual-sourced from a JISC-verified recitation and a September 2025 mill handbook extract that agree on the STKR400 limits used here. The edition named on the order governs delivery.
Are the size tables an official annex?
No. They are a typographical common-size subset with theoretical sharp-corner mass clearly labelled. They are not a warehouse list.

Conclusion

Specify JIS G 3466:2025 STKR400 as square or rectangular carbon steel hollow section, with the 0.25 % carbon maximum and the 400 / 245 N/mm² mechanical minima. Do not substitute STKR490 or an A500 or EN 10219 certificate without a written agreement.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *