JIS G 3452 SGP Carbon Steel Pipe
What is JIS G 3452 SGP Carbon Steel Pipe?
JIS G 3452 is the Japanese industrial standard for carbon steel pipes for ordinary piping, often called gas pipe in Japanese practice. The 2026 edition still has only one grade symbol: SGP. The product is a welded or forge-welded pipe, not a seamless pipe, and it is not JIS G 3444 carbon steel pipe for general structure. Those two JIS leaves must stay on separate pages.
Black pipe is uncoated; white pipe is zinc-coated. The drawing notation SGP-ZN may be used to mark white pipe on documents, but that suffix is not applied as a product stamp. Absence of -ZN on the pipe itself does not prove that the length is black.
Material, Manufacture and Scope for JIS G 3452 SGP Pipe
Manufacture is electric-resistance welding (E) or forge welding (B), with finish symbols H (hot-finished), C (cold-finished) or G (as electric-resistance welded). Hot-finished and as-welded pipe are usually delivered without heat treatment. Cold-finished pipe is annealed after manufacture. A hydrostatic test at a lower limit of 2.5 MPa, or an allowed ultrasonic or eddy-current substitute, is required. The standard is written for ordinary piping, not for high-pressure service and not for structural hollow sections.
JIS G 3452 SGP Chemical Composition
JIS G 3452:2026 specifies only phosphorus and sulphur, each 0.040 % maximum on the heat analysis. Carbon, silicon and manganese are not specified. The grade is controlled by the 290 N/mm² tensile minimum and the process tests, not by a carbon number. Other alloying elements may be added if necessary. Published ‘typical carbon’ figures for SGP are not a standard limit and are not used here.
Swipe horizontally to view all dimensions.
JIS G 3452 SGP Mechanical Properties
The tensile minimum for SGP is 290 N/mm² (MPa). There is no specified yield minimum in the grade table. Elongation depends on the test piece and direction, as in the table below. For nominal sizes 32A and smaller, the elongation limits are not a delivery condition, although the result is recorded and a limit may be agreed. Flattening to two-thirds of the outside diameter shall not crack the test piece. A 90° bend over an inside radius of six times the outside diameter may be specified in place of flattening for sizes 50A and smaller.
Swipe horizontally to view all dimensions.
JIS G 3452 SGP Common Sizes and Plain-End Masses
The table below is a typographical common-size subset of SGP pipe, from 10A to 500A, with plain-end masses as published in a 2025 mill handbook and checked with W = 0.0246615(D − t)t. Published masses that are already rounded to three significant figures were kept when they match the formula. This is not a complete JIS size dump and not a stock list. Japanese outside diameters (for example 21.7 mm at 15A) must not be replaced by ISO 21.3 mm sizes without being named.
Swipe horizontally to view all dimensions.
Applications and Service Limits for JIS G 3452 SGP Pipe
SGP is used for ordinary water, air, gas and general piping, including galvanized white pipe where a zinc coating is ordered. It is not JIS G 3454 pressure piping, not JIS G 3444 structural pipe, and not a hollow section. Do not treat the 290 MPa tensile minimum as a 235 MPa or 355 MPa structural grade.
Near-Equivalents for JIS G 3452 SGP Pipe: Not Automatic Substitutes
EN 10255 S195T and GB/T 3091 Q235B are often compared with SGP in export work, but their chemistry tables and tensile minima differ, and their diameter series are not identical. JIS G 3444 STK400 is a structural pipe with its own tensile and yield table. JIS G 3454 STPG370 is a pressure pipe that may be seamless or ERW and is not this ordinary-piping standard.
Sourcing JIS G 3452 SGP Carbon Steel Pipe from SHH STEEL
Send the nominal size, black or white (galvanized) finish, end finish, length, the manufacturing symbol if it matters, and the JIS G 3452 edition on the contract. The 2026 edition should be named when it is the governing text. SHH STEEL reviews the grade symbol, the finish and the certificate before quoting.
JIS G 3452 SGP Pipe FAQs
-
Is SGP the same as JIS G 3444?
- No. JIS G 3452 SGP is ordinary piping. JIS G 3444 is carbon steel pipe for general structure, with its own grade symbols and mechanical table. They must not be merged.
-
Does SGP specify a carbon content?
- No. The 2026 standard specifies only phosphorus and sulphur at 0.040 % maximum. Carbon, silicon and manganese are not specified. The tensile minimum is 290 MPa.
-
What is white pipe?
- White pipe is zinc-coated SGP. Black pipe is uncoated. The document notation SGP-ZN may mark white pipe on drawings, but it is not a product stamp.
-
Is there more than one SGP grade?
- No. JIS G 3452 has a single grade symbol, SGP.
Conclusion
JIS G 3452 SGP is the single-grade carbon steel pipe for ordinary piping, with phosphorus and sulphur limited to 0.040 % and a 290 MPa tensile minimum. The size table is a typographical common set with formula-checked plain-end masses, not a stock list and not a JIS G 3444 structural-pipe page. Confirm the size, the black or white finish and the edition on the order.