JIS G 3444 STK400 Carbon Steel Pipe
What is JIS G 3444 STK400 Carbon Steel Pipe?
JIS G 3444 is the Japanese industrial standard for carbon steel tubes for general structural purposes. STK400 is the usual grade, named for a 400 N/mm2 tensile minimum, with a 235 N/mm2 minimum yield. The standard allows electric-resistance-welded, hot electric-resistance-welded, arc-welded and seamless tubes; the manufacturing process has to be named on the order. This page is filed under the JIS G 3444 welded-pipe term in the catalogue, but a seamless STK400 tube is still a G 3444 product when it is made and certified that way.
STK400 is a structural tube, not JIS G 3452 SGP ordinary piping and not JIS G 3454 STPG370 pressure piping. Those leaves stay on their own pages.
Material, Manufacture and Scope for JIS G 3444 STK400
G 3444 also lists STK290, STK490, STK500 and STK540. This page is confined to STK400. A flattening test to 2/3 of the outside diameter applies; a bend test may replace flattening, when specified, on tubes of 50 mm outside diameter or less. For arc-welded tube over 350 mm outside diameter, a weld-tensile requirement of 400 N/mm2 minimum applies. The ordered edition of JIS G 3444 governs acceptance.
JIS G 3444 STK400 Chemical Composition
STK400 carbon is 0.25 % maximum, with phosphorus 0.040 % maximum and sulphur 0.040 % maximum. Silicon and manganese are not specified for this grade. Do not copy the silicon or manganese caps from STK490, STK500 or STK540 onto an STK400 certificate, and do not invent a ‘typical carbon’ figure in place of the 0.25 % maximum.
Swipe horizontally to view all dimensions.
JIS G 3444 STK400 Mechanical Properties
Minimum tensile strength is 400 N/mm2 and minimum yield is 235 N/mm2. Minimum elongation is 23 % on a No. 11 or No. 12 longitudinal test piece, and 18 % on a No. 5 transverse test piece for outside diameters of 200 mm and over. These are not the STK490 (490 / 315) or STK540 (540 / 390) figures, and they are not JIS G 3452 SGP piping properties.
Swipe horizontally to view all dimensions.
JIS G 3444 STK400 Common Sizes: Typographical Handbook Subset
The table below is a typographical subset of standard STK outside diameters and walls, with theoretical masses checked against W = 0.02466 (D − t) t kg/m. It is not a complete JIS G 3444 size listing and not a mill stock list. Other diameters and walls may be quoted when they are named on the order.
Swipe horizontally to view all dimensions.
Applications and Service Limits for JIS G 3444 STK400
STK400 tubes are used in building frames, towers, piling, supports, scaffolding and other general structures where this grade is named. The grade is not a pressure-piping specification and not a cold-formed hollow-section standard such as JIS G 3466. If the project needs a fluid-service pipe or a higher-tensile STK grade, that product has to be ordered as such.
Near-Equivalents for JIS G 3444 STK400: Not Automatic Substitutes
STK290 is a lower-tensile grade in the same standard, and STK490 / STK540 are higher-tensile grades with their own chemistry. EN 10219 S235JRH and GB/T 6728 Q235B are neighbouring structural hollow products, not restamps of STK400. JIS G 3452 SGP and ASTM A53 are piping specifications, not this structural tube standard.
Sourcing JIS G 3444 STK400 Carbon Steel Pipe from SHH STEEL
Send the manufacturing process (ERW, hot ERW, arc-welded or seamless), the outside diameter and wall, the length, and the JIS G 3444 edition. Name STK400 explicitly. Do not use a G 3452 or G 3454 term for this page. SHH STEEL reviews the process, the grade and the certificate before quoting. The size table is a typographical reference, not a warehouse list.
JIS G 3444 STK400 FAQs
-
Is STK400 only a welded pipe?
- No. JIS G 3444 allows ERW, hot ERW, arc-welded and seamless tubes. The process has to be named on the order. This page is filed under the welded-pipe term, but that filing does not forbid a seamless certificate.
-
Are silicon and manganese limited?
- Not for STK400. Only carbon (0.25 % max), phosphorus (0.040 % max) and sulphur (0.040 % max) are specified. Do not copy STK490 silicon or manganese caps onto this grade.
-
Is this the same as JIS G 3452 SGP?
- No. SGP is ordinary piping. STK400 is a general-structure tube with a specified 235 N/mm2 yield. The certificates are not interchangeable.
-
Is the size table complete?
- No. It is a typographical handbook subset with masses checked at W = 0.02466 (D - t) t, not a complete standard list and not a stock list.
Conclusion
JIS G 3444 STK400 is the usual general-structure carbon steel tube grade, with 400 N/mm2 tensile and 235 N/mm2 yield, and with silicon and manganese unspecified. Name the manufacturing process as well as the grade. The size table is a typographical subset with formula-checked masses, not a stock list.