GB/T 8163 Grade 20 Seamless Steel Pipe

GB/T 8163 Grade 20 is seamless steel pipe for ordinary liquid service. Cast analysis is carbon 0.17–0.23 %, with a tensile range of 410–530 MPa and a 245 MPa minimum yield. Impact testing is not specified for this grade. Size tables are a typographical common subset with formula masses. SHH STEEL reviews the grade and certificate before quoting.
Keywords
GB/T 8163 Grade 20, 20# seamless pipe, 8163 steel pipe, Grade 20 seamless, fluid seamless pipe
Equivalent Grades:
Near-equivalents only, not automatic substitutes.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Size Chart (114 typographical common sizes)
Applications
Equivalent Grades
Sourcing
FAQ
Conclusion

What is GB/T 8163 Grade 20 Seamless Steel Pipe?

GB/T 8163 is the Chinese national standard for seamless steel pipes for ordinary liquid service. Grade 20 (often written 20 or 20#) is the usual carbon grade, named for a nominal 0.20 % carbon content. The pipe is pierced and rolled from a solid billet; it is not a welded GB/T 3091 pipe and not a GB/T 8162 structural seamless pipe. Those two GB leaves must stay on separate pages.

Hot-rolled or hot-expanded pipe may be delivered as rolled or heat-treated. Cold-drawn or cold-rolled pipe is delivered annealed or high-temperature tempered. The ordered edition should be named on the contract; the chemistry and tensile figures on this page follow the 2018 edition as restated in corroborated grade data.

Material, Manufacture and Scope for GB/T 8163 Grade 20 Seamless Pipe

The standard also lists grades 10, Q345, Q390, Q420 and Q460. This page is confined to grade 20. Dimensions follow the ordinary seamless-pipe size system used with this standard; masses on this page are computed with W = 0.0246615(D − t)t kg/m. Flattening, flaring and bend tests apply in the diameter and thickness bands set out in the standard, with a flattening coefficient a = 0.07 for grade 20.

GB/T 8163 Grade 20 Chemical Composition (Cast Analysis)

Cast analysis for grade 20, in percent, is carbon 0.17–0.23, silicon 0.17–0.37, manganese 0.35–0.65, phosphorus 0.030 maximum, sulphur 0.030 maximum, chromium 0.25 maximum, nickel 0.30 maximum and copper 0.20 maximum. These 2018 figures must not be replaced by older 0.035 % phosphorus or sulphur limits from a withdrawn edition. Product-analysis deviations, when a product analysis is agreed, follow GB/T 222 as applied by the pipe standard.

Swipe horizontally to view all dimensions.

Element Cast analysis, % by mass
Carbon 0.17–0.23
Silicon 0.17–0.37
Manganese 0.35–0.65
Phosphorus, max 0.030
Sulphur, max 0.030
Chromium, max 0.25
Nickel, max 0.30
Copper, max 0.20

GB/T 8163 Grade 20 Mechanical Properties

In the delivery condition, longitudinal tensile properties for grade 20 are a tensile range of 410–530 MPa, a lower yield of at least 245 MPa, and a minimum elongation of 20 %. An impact test is not specified for grade 20 in GB/T 8163. Do not paste thickness-banded yields from GB/T 699 bar or from another pipe standard onto this certificate unless that document is actually named on the order.

Swipe horizontally to view all dimensions.

Property Grade 20, longitudinal, delivery condition
Tensile strength Rm 410–530 MPa
Lower yield ReL, min 245 MPa
Elongation A, min 20 %
Impact test Not specified for grade 20 in GB/T 8163

GB/T 8163 Grade 20 Common Sizes: Typographical Subset with Formula Masses

The table below is a typographical common-size subset of Series 1 outside diameters and preferred walls, with theoretical masses from W = 0.0246615(D − t)t. It is not a complete GB/T 17395 or GB/T 21835 listing and not a mill stock list. Other walls and Series 2 diameters may be available when they are named on the order.

Swipe horizontally to view all dimensions.

Outside diameter D (mm) Wall t (mm) Theoretical mass (kg/m)
21.3 2.6 1.199
21.3 3.2 1.428
21.3 4 1.707
21.3 5 2.01
26.9 2.6 1.558
26.9 3.2 1.87
26.9 4 2.259
26.9 5 2.7
26.9 6.3 3.201
33.7 2.6 1.994
33.7 3.2 2.407
33.7 4 2.93
33.7 5 3.539
33.7 6.3 4.257
33.7 8 5.07
42.4 2.6 2.552
42.4 3.2 3.094
42.4 4 3.788
42.4 5 4.612
42.4 6.3 5.609
42.4 8 6.787
42.4 10 7.99
48.3 2.6 2.93
48.3 3.2 3.559
48.3 4 4.37
48.3 5 5.339
48.3 6.3 6.525
48.3 8 7.951
48.3 10 9.445
60.3 2.6 3.7
60.3 3.2 4.506
60.3 4 5.554
60.3 5 6.819
60.3 6.3 8.39
60.3 8 10.32
60.3 10 12.4
60.3 12.5 14.74
76.1 2.6 4.713
76.1 3.2 5.753
76.1 4 7.112
76.1 5 8.767
76.1 6.3 10.84
76.1 8 13.44
76.1 10 16.3
76.1 12.5 19.61
88.9 2.6 5.534
88.9 3.2 6.763
88.9 4 8.375
88.9 5 10.35
88.9 6.3 12.83
88.9 8 15.96
88.9 10 19.46
88.9 12.5 23.55
114.3 2.6 7.162
114.3 3.2 8.768
114.3 4 10.88
114.3 5 13.48
114.3 6.3 16.78
114.3 8 20.97
114.3 10 25.72
114.3 12.5 31.38
139.7 2.6 8.791
139.7 3.2 10.77
139.7 4 13.39
139.7 5 16.61
139.7 6.3 20.73
139.7 8 25.98
139.7 10 31.99
139.7 12.5 39.21
168.3 2.6 10.62
168.3 3.2 13.03
168.3 4 16.21
168.3 5 20.14
168.3 6.3 25.17
168.3 8 31.63
168.3 10 39.04
168.3 12.5 48.03
219.1 4 21.22
219.1 5 26.4
219.1 6.3 33.06
219.1 8 41.65
219.1 10 51.57
219.1 12.5 63.69
273 4 26.54
273 5 33.05
273 6.3 41.44
273 8 52.28
273 10 64.86
273 12.5 80.3
323.9 5 39.32
323.9 6.3 49.34
323.9 8 62.32
323.9 10 77.41
323.9 12.5 95.99
355.6 5 43.23
355.6 6.3 54.27
355.6 8 68.58
355.6 10 85.23
355.6 12.5 105.77
406.4 5 49.5
406.4 6.3 62.16
406.4 8 78.6
406.4 10 97.76
406.4 12.5 121.43
457 5 55.73
457 6.3 70.02
457 8 88.58
457 10 110.24
457 12.5 137.03
508 5 62.02
508 6.3 77.95
508 8 98.65
508 10 122.81
508 12.5 152.75

Applications and Service Limits for GB/T 8163 Grade 20 Seamless Pipe

Grade 20 pipe is used for ordinary water, oil and general fluid lines in plant and building work. It is not a boiler or high-pressure hydrogen tube, not GB/T 8162 structural pipe, and not an ASTM A106 or EN 10216-1 certificate. Those products have their own chemistry, tensile and inspection rules.

Near-Equivalents for GB/T 8163 Grade 20 Seamless Pipe: Not Automatic Substitutes

ASTM A106 Grade B and ASTM A53 Grade B Type S are often compared in export enquiries, but they use different chemistry footnotes, tensile units and inspection routes. EN 10216-1 P235TR1 is a European pressure-tube grade, not a restamp of 20#. GB/T 699 grade 20 is a bar steel, not this pipe standard. GB/T 8162 must not be used as a silent substitute for 8163, or the other way around.

Sourcing GB/T 8163 Grade 20 Seamless Steel Pipe from SHH STEEL

Send the outside diameter, the wall, hot-finished or cold-finished delivery, length, and the GB/T 8163 edition on the contract. Name grade 20 explicitly, and do not tick the GB/T 8162 structural-pipe term for this page. SHH STEEL reviews the grade, the process and the certificate before quoting.

GB/T 8163 Grade 20 Seamless Pipe FAQs

Is this the same as GB/T 8162?
No. GB/T 8163 is seamless pipe for ordinary liquid service. GB/T 8162 is structural seamless pipe. They are separate leaves and must not be merged.
Is an impact test required?
No. An impact test is not specified for grade 20 in GB/T 8163. Other designations in the same standard may have impact qualities.
Does yield fall with thickness?
The corroborated 2018 tensile table used here gives a single 245 MPa minimum yield and a 410–530 MPa tensile range. Do not paste a thickness-banded yield from another standard onto this certificate.
Are the size tables complete?
No. They are a typographical common subset with formula masses, not a complete dimensional standard dump and not a stock list.

Conclusion

GB/T 8163 Grade 20 is seamless pipe for ordinary liquid service, with carbon 0.17–0.23 %, a 410–530 MPa tensile range and a 245 MPa yield minimum. The size table is a typographical common subset with formula masses, not a stock list and not a GB/T 8162 page. Confirm the diameter, the wall, the delivery condition and the edition on the order.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X