GB/T 8162 Grade 20 Seamless Steel Pipe
What is GB/T 8162 Grade 20 Seamless Steel Pipe?
GB/T 8162 is the Chinese national standard for seamless steel tubes for structural use. Grade 20 is the usual quality-carbon grade. The pipe is pierced and rolled from a solid billet. It is not a GB/T 8163 fluid-service seamless pipe and not a GB/T 3091 welded pipe. Those two leaves stay on their own pages, even though the grade name ’20’ also appears on GB/T 8163.
The ordered edition should be named on the contract; the chemistry and tensile figures on this page follow the 2018 edition as corroborated from the standard’s mechanical table and its reference to GB/T 699 for heat analysis.
Material, Manufacture and Scope for GB/T 8162 Grade 20 Seamless Pipe
For quality carbon steels, GB/T 8162-2018 requires the grade and the heat analysis to conform to GB/T 699. Grade 20 chemistry on this page is therefore the GB/T 699-2015 grade 20 row, not the tighter phosphorus, sulphur and copper limits written into GB/T 8163-2018 for fluid pipe. Dimensions follow the ordinary seamless-pipe size system used with this standard; masses on this page are computed with W = 0.0246615(D − t)t kg/m.
GB/T 8162 Grade 20 Chemical Composition (Heat Analysis)
Heat analysis for grade 20 is carbon 0.17-0.23 %, silicon 0.17-0.37 %, manganese 0.35-0.65 %, phosphorus 0.035 % maximum, sulphur 0.035 % maximum, chromium 0.25 % maximum, nickel 0.30 % maximum and copper 0.25 % maximum. Do not replace the 0.035 % phosphorus and sulphur, or the 0.25 % copper, with the 0.030 % / 0.20 % figures used on the GB/T 8163 Grade 20 page. Those are fluid-pipe limits.
Swipe horizontally to view all dimensions.
GB/T 8162 Grade 20 Mechanical Properties
GB/T 8162-2018 requires a tensile strength of at least 410 MPa, with no upper bound tabulated for this grade in that standard, and a minimum elongation of 20 %. Lower yield is banded by nominal wall: 245 MPa for walls of 16 mm and under, 235 MPa above 16 mm through 30 mm, and 225 MPa above 30 mm. Do not paste the single 245 MPa yield and the 410-530 MPa tensile range of GB/T 8163 Grade 20 onto this structural-pipe certificate.
Swipe horizontally to view all dimensions.
GB/T 8162 Grade 20 Common Sizes: Typographical Subset with Formula Masses
The table below is a typographical common-size subset of Series 1 outside diameters and preferred walls, with theoretical masses from W = 0.0246615(D − t)t. It is not a complete GB/T 17395 listing and not a mill stock list. Other walls and Series 2 diameters may be available when they are named on the order.
Swipe horizontally to view all dimensions.
Applications and Service Limits for GB/T 8162 Grade 20 Seamless Pipe
Grade 20 structural seamless pipe is used for frames, mechanical parts, supports and general construction where a structural seamless tube is named. It is not, by itself, a fluid-conveying specification. If the line is for water, oil or gas under GB/T 8163, that standard and its tensile range have to be named. The grade is not a pressure-vessel steel and not a hollow-section standard such as GB/T 6728.
Near-Equivalents for GB/T 8162 Grade 20 Seamless Pipe: Not Automatic Substitutes
GB/T 8163 Grade 20 shares the grade name but uses a tighter phosphorus and sulphur limit and a single-band 245 MPa yield with a 410-530 MPa tensile range. GB/T 699 Grade 20 is the bar (and chemistry-source) standard, not a pipe standard. ASTM A53 or A106 and JIS G 3444 STK400 are neighbouring products, not automatic substitutes.
Sourcing GB/T 8162 Grade 20 Seamless Steel Pipe from SHH STEEL
Send the outside diameter, the wall, the length, the delivery condition, and the GB/T 8162 edition. Name grade 20 and the structural-pipe standard explicitly. Do not use the GB/T 8163 term for this page. SHH STEEL reviews the grade and the certificate before quoting. The size table is a typographical reference, not a warehouse list.
GB/T 8162 Grade 20 Seamless Pipe FAQs
-
How does this differ from GB/T 8163 Grade 20?
- 8162 is structural pipe: tensile is 410 MPa minimum with no tabulated upper bound, and yield is banded by wall thickness. 8163 is fluid pipe: tensile is 410-530 MPa and yield is a single 245 MPa minimum, with tighter phosphorus, sulphur and copper limits.
-
Where does the chemistry come from?
- GB/T 8162-2018 requires quality carbon grades to follow GB/T 699. The row on this page is GB/T 699-2015 grade 20, including phosphorus and sulphur at 0.035 % maximum.
-
Is a 410-530 MPa tensile range required?
- Not in GB/T 8162. That range belongs to GB/T 8163 Grade 20 and must not be pasted onto this certificate.
-
Is the size table complete?
- No. It is a typographical common-size subset with formula masses, not a complete dimensional listing and not a stock list.
Conclusion
GB/T 8162 Grade 20 is structural seamless pipe whose heat analysis follows GB/T 699 and whose tensile strength is 410 MPa minimum, with yield banded by wall thickness. It is not GB/T 8163 fluid pipe. Confirm the standard, the wall band, the size and the certificate on the order.