GB/T 699 Grade 20 Round, Square and Flat Steel Bars
What are GB/T 699 Grade 20 Steel Bars?
GB/T 699 is the Chinese national standard for quality carbon structural steel. Grade 20 (often written 20 or 20#) is named for a nominal 0.20 % carbon content. This page is for bars: rounds, squares and flats. It is not a GB/T 8162 or GB/T 8163 seamless-pipe page, and a pipe certificate must not be used as a bar certificate, or the other way around.
The grade is widely used for shafts, pins, carburized parts, bolts and general machine details. The dimensional standard actually used (for example a hot-rolled bar dimensional standard named on the order) has to appear on the certificate together with GB/T 699 and the grade.
Material, Manufacture and Scope for GB/T 699 Grade 20 Steel Bars
The chemistry and the normalized tensile figures on this page follow GB/T 699-2015. The edition named on the order governs acceptance. Mechanical properties in Table 2 of that edition are determined on a 25 mm sample blank in the normalized condition and apply to bars up to 80 mm. For bars over 80 mm up to 250 mm, elongation may be 2 percentage points lower and reduction of area 5 percentage points lower. Where there is no distinct yield, ReL may be replaced by Rp0.2. Delivery may be as-rolled, normalized or otherwise as ordered; the hardness cap below is for material not heat treated.
GB/T 699 Grade 20 Chemical Composition (Heat Analysis)
Heat analysis for grade 20 is carbon 0.17-0.23 %, silicon 0.17-0.37 %, manganese 0.35-0.65 %, phosphorus 0.035 % maximum, sulphur 0.035 % maximum, chromium 0.25 % maximum, nickel 0.30 % maximum and copper 0.25 % maximum. Do not replace these phosphorus, sulphur or copper limits with the tighter 0.030 % / 0.20 % figures used in GB/T 8163 Grade 20 pipe. Those pipe limits belong to the pipe standard, not to this bar grade.
Swipe horizontally to view all dimensions.
GB/T 699 Grade 20 Mechanical Properties for Steel Bars
For normalized 25 mm sample blanks, on bars up to 80 mm, the minima are 410 MPa tensile strength, 245 MPa lower yield, 25 % elongation and 55 % reduction of area. Maximum hardness in the not-heat-treated delivery state is 156 HBW. Do not paste the thickness-banded yields of GB/T 8162 structural pipe, or the 410-530 MPa tensile range of GB/T 8163 fluid pipe, onto a GB/T 699 bar certificate.
Swipe horizontally to view all dimensions.
GB/T 699 Grade 20 Common Bar Sizes: Metric Rounds, Squares and Flats
The tables below are common typographical metric bar sizes, not a complete dimensional-standard listing and not a mill stock list. Theoretical mass is computed at a density of 7.85 g/cm3: M = 0.006165 d2 kg/m for rounds, and M = 0.00785 a b kg/m for squares and flats, with dimensions in millimetres. Preferred sizes on an order should still be taken from the dimensional standard named in the contract.
Round bars (29 common diameters).
Swipe horizontally to view all dimensions.
Square bars (12 common sides).
Swipe horizontally to view all dimensions.
Flat bars (35 common thickness x width combinations).
Swipe horizontally to view all dimensions.
Applications and Service Limits for GB/T 699 Grade 20 Steel Bars
Grade 20 bars are used for lightly loaded shafts, pins, bolts, carburized bushes and general welded or machined details. The grade is a quality carbon steel, not a pressure-vessel steel and not a quenched-and-tempered alloy bar. Through-hardening is not the usual route; carburizing is the common way to harden a wear surface. A pipe, a plate or a higher-carbon GB/T 699 grade has to be ordered as that product.
Near-Equivalents for GB/T 699 Grade 20 Steel Bars: Not Automatic Substitutes
ASTM A108 1018 is a cold-finished chemistry grade with a different carbon window and no default tensile minima. JIS S20C and SAE 1020 are neighbouring low-carbon designations, not automatic substitutes. GB/T 8162 Grade 20 and GB/T 8163 Grade 20 are seamless-pipe standards that use the same grade name with different mechanical tables. ASME SA designations are not inferred here.
Sourcing GB/T 699 Grade 20 Steel Bars from SHH STEEL
Send the form (round, square or flat), the diameter or the thickness and width, the length, the delivery condition, and the GB/T 699 edition. Name grade 20 explicitly. Do not use a pipe term for this page. SHH STEEL reviews the form, the grade and the certificate before quoting. The size tables are a typographical reference, not a warehouse list.
GB/T 699 Grade 20 Steel Bar FAQs
-
Is this the same as GB/T 8162 or GB/T 8163 Grade 20 pipe?
- No. Those are seamless-pipe standards. This page is for bars under GB/T 699. Chemistry of 8162 refers back to GB/T 699, but the pipe mechanical tables are different and must not be mixed.
-
Do the tensile figures apply to as-rolled bars?
- The 410 MPa / 245 MPa / 25 % / 55 % figures are for a normalized 25 mm sample blank on bars up to 80 mm. Name the delivery condition on the order. The 156 HBW cap is for material not heat treated.
-
What happens above 80 mm?
- For bars over 80 mm up to 250 mm, elongation may be 2 percentage points lower and reduction of area 5 percentage points lower. Confirm the size band on the certificate.
-
Is SAE 1020 an automatic substitute?
- No. The grades sit in the same low-carbon family, but they are not automatic substitutes. Dual certification is possible only when the delivered bar meets every requirement of each named standard.
Conclusion
GB/T 699 Grade 20 bars are the quality carbon grade with carbon 0.17-0.23 %, supplied as rounds, squares and flats. Normalized blank properties up to 80 mm are 410 MPa tensile, 245 MPa yield, 25 % elongation and 55 % reduction of area. The size tables are common typographical metric sizes, not a stock list. Confirm the form, the size, the edition and the certificate on the order.