GB/T 3091 Q235B Welded Steel Pipe
What is GB/T 3091 Q235B Welded Steel Pipe?
GB/T 3091-2015 covers welded steel pipes for low-pressure conveyance of water, air, heating steam and gas. Straight-seam high-frequency electric-welded pipe, longitudinal submerged-arc welded (SAWL) pipe and spiral submerged-arc welded (SAWH) pipe are all within the scope. Q235B is the usual carbon grade taken from GB/T 700. This page is a welded-pipe product, not a GB/T 6728 hollow section and not a GB/T 8163 seamless fluids pipe.
The pipe is normally delivered in the as-welded condition. Weld-seam heat treatment or a galvanized finish may be agreed. Outside diameters greater than 508 mm may not be galvanized under the optional clause as written in the standard.
Material, Manufacture and Scope for GB/T 3091 Q235B Welded Pipe
For outside diameters not greater than 219.1 mm the pipe is ordered by nominal size DN and nominal wall thickness, using Table 1. Series 1 diameters are the recommended series. Larger pipes are ordered by outside diameter and wall thickness to GB/T 21835. Usual length is 3 000 mm to 12 000 mm. The theoretical mass formula in clause 4.6.2 is W = 0.0246615(D − t)t kg/m, with density 7.85 kg/dm³.
Each length is subject to a hydrostatic test, or an allowed nondestructive substitute, at a pressure calculated from 60 % of the Table 5 yield, capped at 5.0 MPa. That test is a leak-tightness test for this low-pressure standard, not a design-pressure rating for a high-pressure line.
GB/T 3091 Q235B Chemical Composition (Heat Analysis)
GB/T 3091-2015 does not rewrite the grade chemistry. Clause 5.1.1 sends the heat analysis to GB/T 700 for Q235B. The limits used here are those already verified for Q235B: carbon 0.20 % maximum (0.22 % only with purchaser agreement), silicon 0.35 %, manganese 1.40 %, phosphorus 0.045 %, sulphur 0.045 %, residual chromium, nickel and copper 0.30 % each, and nitrogen 0.008 %. GB/T 700-2006 does not publish a CEV cap for Q235B. Acceptance is by heat analysis unless a product analysis is agreed.
Swipe horizontally to view all dimensions.
GB/T 3091 Q235B Mechanical Properties
Table 5 of GB/T 3091-2015, not the GB/T 700 plate table, governs the finished pipe. For Q235A and Q235B the lower yield ReL is at least 235 MPa for t ≤ 16 mm and 225 MPa for t > 16 mm. The tensile minimum is 370 MPa; the table does not give an upper tensile bound. Minimum elongation is 15 % for D ≤ 168.3 mm and 20 % for D > 168.3 mm. Those elongation figures are lower than the elongation often quoted for Q235B plate, and the plate table must not be pasted onto this pipe page.
For pipes of outside diameter not greater than 60.3 mm tested in full section, elongation is for information only and is not a delivery condition. Bend or flattening tests apply to high-frequency welded pipe by diameter band, and SAW pipe has its own guided-bend rule.
Swipe horizontally to view all dimensions.
GB/T 3091 Q235B Common Sizes: Table A.1 Ordinary and Thickened Walls
The table below is the informative Table A.1 set of ordinary and thickened walls for threaded or grooved ends, using Series 1 outside diameters from DN 6 to DN 200. Masses are calculated with the official formula W = 0.0246615(D − t)t. This is a common-size subset, not a recitation of every GB/T 21835 row, and not a mill stock list. Table 1 also lists a minimum nominal wall for each DN; the contract may specify other walls at or above that minimum. Series 2 and Series 3 diameters exist and must be named if they are wanted.
Swipe horizontally to view all dimensions.
Applications and Service Limits for GB/T 3091 Q235B Welded Pipe
Q235B pipe to GB/T 3091 is used for low-pressure water, air, heating steam and gas lines, and for ordinary mechanical piping where this standard is named. It is not a boiler tube, not a high-pressure process pipe, and not a structural hollow section. Galvanized (zinc-coated) pipe is an agreed finish of the same grade, not a different grade.
Near-Equivalents for GB/T 3091 Q235B Welded Pipe: Not Automatic Substitutes
ASTM A53 Grade B Type E and EN 10255 S195T are often compared in export enquiries, but their tensile tables, chemistry and size series differ. GB/T 8163 Grade 20 is a seamless fluids pipe, not this welded product. A GB/T 700 Q235B hollow section to GB/T 6728 is a structural section, not a 3091 pipe. Do not restamp those certificates as GB/T 3091 Q235B.
Sourcing GB/T 3091 Q235B Welded Steel Pipe from SHH STEEL
Send the DN or outside diameter, the wall (ordinary, thickened or a stated millimetre wall), black or galvanized finish, end finish, length, and the 2015 edition or the edition on the contract. SHH STEEL reviews the grade, the weld process and the certificate before quoting. The Table A.1 sizes are a checked reference, not a warehouse list.
GB/T 3091 Q235B Welded Pipe FAQs
-
Is the tensile requirement 370–500 MPa?
- No. Table 5 of GB/T 3091-2015 gives a tensile minimum of 370 MPa for Q235B. It does not publish an upper bound. Do not paste a 370–500 or 375–500 MPa range from another source onto this certificate.
-
Why is elongation only 15 % for smaller diameters?
- That is the Table 5 rule for D ≤ 168.3 mm. It is a pipe-standard value, not the higher elongation often quoted for Q235B plate in GB/T 700.
-
Is this the same as a Q235B hollow section?
- No. A GB/T 6728 Q235B section is a structural hollow section. GB/T 3091 Q235B is welded pipe for low-pressure fluids.
-
Where do the masses come from?
- From the official formula W = 0.0246615(D − t)t in clause 4.6.2, applied to Table A.1 ordinary and thickened walls.
Conclusion
GB/T 3091-2015 Q235B is welded low-pressure pipe with chemistry from GB/T 700 and mechanicals from Table 5 of the pipe standard: 235 MPa yield up to 16 mm and a 370 MPa tensile minimum. The size table is the Table A.1 ordinary and thickened set with formula masses, not a stock list. Confirm the DN or diameter, the wall, the finish and the certificate on the order.