EN 10255 S195T Welded Steel Pipe
What is EN 10255 S195T Welded Steel Pipe?
EN 10255:2004 specifies non-alloy steel tubes suitable for welding and threading, in specified outside diameters from 10.2 mm to 165.1 mm (thread sizes 1/8 to 6). The only steel name in the standard is S195T, steel number 1.0026. The tubes may be used for fluid conveyance and for other applications. The standard allows both welded (W) and seamless (S) manufacture. This page is filed under welded steel pipes and is confined to the welded product. A seamless EN 10255 enquiry belongs on a seamless-pipe order, not on this leaf.
The usual series are Medium (M) and Heavy (H) in Table 2. Types L, L1 and L2, with different designated thicknesses, are listed in Annex B and are not reprinted here. The product is not a structural hollow section under EN 10219 and is not EN 10216-1 pressure tube.
Material, Manufacture and Scope for EN 10255 S195T Welded Pipe
The purchaser states whether the tube is welded or seamless, the specified outside diameter or the thread size R, and the wall thickness or the series (M or H) or type. Threaded ends, sockets, suitability for galvanizing to EN ISO 1461 or EN 10240, and other options in clause 5.2 are order entries, not automatic features of the grade. For welded tubes the wall-thickness tolerance on the M and H series is ±10 %, and the mass tolerance on bundles of 10 tonnes or more is ±7.5 %.
The tubes shall be suitable for cold bending and threading. The behaviour in a later weld depends on the steel and on the welding procedure, as the note to Table 1 records.
EN 10255 S195T Chemical Composition and Mechanical Properties
Table 1 of EN 10255:2004 sets the cast analysis and the mechanical properties in one place. For S195T the maxima are carbon 0.20 %, manganese 1.40 %, phosphorus 0.035 % and sulphur 0.030 %. Upper yield strength ReH is at least 195 MPa, tensile strength Rm is 320–520 MPa, and minimum elongation A is 20 %. Do not replace the official 320–520 MPa tensile range with a narrower range from an older national gas-list tube sheet.
Swipe horizontally to view all dimensions.
EN 10255 S195T Sizes: Medium and Heavy Series from Table 2
The table below reprints the specified outside diameters, medium and heavy walls, and plain-end masses from EN 10255:2004 Table 2. Threaded-and-socketed masses in the same table are omitted here; they are heavier than the plain-end figures. This is the official Table 2 range, not a mill stock list. Types L, L1 and L2 remain in Annex B if the order names them.
Swipe horizontally to view all dimensions.
Applications and Service Limits for EN 10255 S195T Welded Pipe
S195T tube is used for ordinary water, gas and general engineering lines that are welded or threaded, including installations that still refer to older medium and heavy gas-list series. It is not a structural hollow section, not EN 10216-1 pressure tube, and not a boiler tube. Galvanizing, thread form and socket type have to be stated when they are required.
Near-Equivalents for EN 10255 S195T Welded Pipe: Not Automatic Substitutes
ISO 65 is often mentioned with this diameter series, but this site does not treat an ISO 65 leaf as a substitute page. ASTM A53 Grade B ERW and GB/T 3091 Q235B are higher-strength welded pipes with different chemistry and mechanical tables. EN 10219 hollow sections and EN 10216-1 seamless pressure tubes are different product families.
Sourcing EN 10255 S195T Welded Steel Pipe from SHH STEEL
Send the manufacturing route (welded), the DN or thread size, the series (M or H) or a stated wall, plain or threaded ends, any coating, the length, and the edition on the contract. SHH STEEL reviews the type letter, the series and the certificate before quoting. The Table 2 listing is a checked reference, not a warehouse list.
EN 10255 S195T Welded Pipe FAQs
-
Does EN 10255 allow seamless tube?
- Yes. The standard covers welded (W) and seamless (S) tube. This page is confined to the welded product under the welded-pipe category. A seamless enquiry should be ordered as seamless.
-
What is the difference between medium and heavy series?
- Table 2 assigns a thicker wall and a higher plain-end mass to the heavy series at each specified outside diameter. The order should name the series or the wall, not only the diameter.
-
Is S195T the same as Grade B?
- No. S195T has a 195 MPa yield minimum and a 320–520 MPa tensile range. ASTM A53 Grade B is a 35 ksi [240 MPa] / 60 ksi [415 MPa] grade with a different chemistry table.
-
Are light series tubes included?
- Types L, L1 and L2 are in Annex B of EN 10255:2004 and are not reprinted in the Table 2 medium and heavy listing on this page.
Conclusion
EN 10255 S195T is the 195 MPa non-alloy tube of steel number 1.0026, written for welding and threading in 10.2 mm to 165.1 mm outside diameter. This page covers the welded product and reprints official Table 2 medium and heavy plain-end sizes. Confirm the type, the series, the ends and the certificate on the order.