EN 10216-1 P235TR1 is seamless non-alloy steel tube for pressure purposes, steel number 1.0254, with room-temperature properties. Minimum yield is 235 MPa up to 16 mm, with a tensile range of 360–500 MPa. Impact testing is not required for the TR1 quality. Size tables are a typographical common subset with formula masses. SHH STEEL reviews the quality and certificate before quoting.
Keywords
EN 10216-1 P235TR1, P235TR1 seamless pipe, 1.0254 steel tube, EN 10216 TR1, pressure seamless pipe
Equivalent Grades:
Near-equivalents only, not automatic substitutes.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Size Chart (114 typographical common sizes)
Applications
Equivalent Grades
Sourcing
FAQ
Conclusion

What is EN 10216-1 P235TR1 Seamless Steel Pipe?

EN 10216-1 specifies seamless non-alloy steel tubes for pressure purposes with specified room-temperature properties. P235TR1, steel number 1.0254, is the usual 235 MPa TR1 quality. TR1 is supplied with a 2.2 test report unless a different document is agreed; impact testing is not required. TR2 is a different quality, with product-analysis and impact options, and must be named if it is wanted. This is a seamless pressure tube, not a welded EN 10217 tube and not a structural hollow section.

The mechanical figures on this page are taken from Table 4 of EN 10216-1:2002+A1:2004. Chemistry is the corroborated P235TR1 cast-analysis set used with that standard. Purchasers who order the 2013 edition should name that edition on the contract and read the certificate against it.

Material, Manufacture and Scope for EN 10216-1 P235TR1 Seamless Pipe

Preferred dimensions are selected from EN 10220. A typical mill range is 10.2 mm to 711 mm outside diameter with walls from about 1.6 mm to 100 mm, subject to the producer. Outside-diameter and wall-thickness tolerances follow the T/D bands in the standard, not an ASME B36.10 footnote. A hydrostatic leak-tightness test, or an allowed electromagnetic substitute, is required; the hydrostatic test is not a strength test.

Footnote e of Table 4 notes that TR1 grades are unlikely to support the essential requirements of the Pressure Equipment Directive unless other criteria are taken into account. Where PED essential requirements apply, the purchaser should consider TR2 or another named quality, not assume that a TR1 certificate is sufficient.

EN 10216-1 P235TR1 Chemical Composition (Cast Analysis)

Cast analysis maxima for P235TR1 are carbon 0.16 %, silicon 0.35 %, manganese 1.20 %, phosphorus 0.025 %, sulphur 0.020 %, chromium, nickel and copper 0.30 % each, molybdenum 0.08 %, niobium 0.01 %, vanadium 0.02 % and titanium 0.04 %. Aluminium, boron and nitrogen are not specified for this TR1 quality. A carbon-equivalent maximum is not published for P235TR1 in the sources used here, and one is not invented on this page. Product-analysis deviations, when they apply, follow Table 3 of the standard and are written for TR2 unless otherwise agreed.

Swipe horizontally to view all dimensions.

Element P235TR1 (1.0254), cast analysis, max unless noted
Carbon 0.16 %
Silicon 0.35 %
Manganese 1.20 %
Phosphorus 0.025 %
Sulphur 0.020 %
Chromium / Nickel / Copper, each 0.30 %
Molybdenum 0.08 %
Niobium 0.01 %
Vanadium 0.02 %
Titanium 0.04 %
Aluminium, boron, nitrogen Not specified for TR1

EN 10216-1 P235TR1 Mechanical Properties

Table 4 requires a minimum upper yield ReH of 235 MPa for T ≤ 16 mm, 225 MPa for 16 mm < T ≤ 40 mm and 215 MPa for 40 mm < T ≤ 60 mm. Properties above 60 mm are subject to agreement. Tensile strength Rm is 360–500 MPa. Minimum elongation is 25 % longitudinal and 23 % transverse. Impact energy is not specified for P235TR1; the 0 °C and −10 °C columns in Table 4 apply to TR2 qualities. Do not treat a P235TR2 impact result as automatic on a TR1 certificate.

Swipe horizontally to view all dimensions.

Property Value
ReH, min, T ≤ 16 mm 235 MPa
ReH, min, 16 mm < T ≤ 40 mm 225 MPa
ReH, min, 40 mm < T ≤ 60 mm 215 MPa
Rm 360–500 MPa
Elongation A, min, longitudinal / transverse 25 % / 23 %
Impact KV Not required for TR1

EN 10216-1 P235TR1 Common Sizes: Typographical Subset with Formula Masses

The table below is a typographical common-size subset of Series 1 outside diameters and preferred walls, with theoretical masses from W = 0.0246615(D − t)t. Dimensions should be selected from EN 10220 on the order. This is not a complete EN 10220 list and not a mill stock list. It is also not an ASME B36.10 A106 table, even where some diameters coincide.

Swipe horizontally to view all dimensions.

Outside diameter D (mm) Wall t (mm) Theoretical mass (kg/m)
21.3 2.6 1.199
21.3 3.2 1.428
21.3 4 1.707
21.3 5 2.01
26.9 2.6 1.558
26.9 3.2 1.87
26.9 4 2.259
26.9 5 2.7
26.9 6.3 3.201
33.7 2.6 1.994
33.7 3.2 2.407
33.7 4 2.93
33.7 5 3.539
33.7 6.3 4.257
33.7 8 5.07
42.4 2.6 2.552
42.4 3.2 3.094
42.4 4 3.788
42.4 5 4.612
42.4 6.3 5.609
42.4 8 6.787
42.4 10 7.99
48.3 2.6 2.93
48.3 3.2 3.559
48.3 4 4.37
48.3 5 5.339
48.3 6.3 6.525
48.3 8 7.951
48.3 10 9.445
60.3 2.6 3.7
60.3 3.2 4.506
60.3 4 5.554
60.3 5 6.819
60.3 6.3 8.39
60.3 8 10.32
60.3 10 12.4
60.3 12.5 14.74
76.1 2.6 4.713
76.1 3.2 5.753
76.1 4 7.112
76.1 5 8.767
76.1 6.3 10.84
76.1 8 13.44
76.1 10 16.3
76.1 12.5 19.61
88.9 2.6 5.534
88.9 3.2 6.763
88.9 4 8.375
88.9 5 10.35
88.9 6.3 12.83
88.9 8 15.96
88.9 10 19.46
88.9 12.5 23.55
114.3 2.6 7.162
114.3 3.2 8.768
114.3 4 10.88
114.3 5 13.48
114.3 6.3 16.78
114.3 8 20.97
114.3 10 25.72
114.3 12.5 31.38
139.7 2.6 8.791
139.7 3.2 10.77
139.7 4 13.39
139.7 5 16.61
139.7 6.3 20.73
139.7 8 25.98
139.7 10 31.99
139.7 12.5 39.21
168.3 2.6 10.62
168.3 3.2 13.03
168.3 4 16.21
168.3 5 20.14
168.3 6.3 25.17
168.3 8 31.63
168.3 10 39.04
168.3 12.5 48.03
219.1 4 21.22
219.1 5 26.4
219.1 6.3 33.06
219.1 8 41.65
219.1 10 51.57
219.1 12.5 63.69
273 4 26.54
273 5 33.05
273 6.3 41.44
273 8 52.28
273 10 64.86
273 12.5 80.3
323.9 5 39.32
323.9 6.3 49.34
323.9 8 62.32
323.9 10 77.41
323.9 12.5 95.99
355.6 5 43.23
355.6 6.3 54.27
355.6 8 68.58
355.6 10 85.23
355.6 12.5 105.77
406.4 5 49.5
406.4 6.3 62.16
406.4 8 78.6
406.4 10 97.76
406.4 12.5 121.43
457 5 55.73
457 6.3 70.02
457 8 88.58
457 10 110.24
457 12.5 137.03
508 5 62.02
508 6.3 77.95
508 8 98.65
508 10 122.81
508 12.5 152.75

Applications and Service Limits for EN 10216-1 P235TR1 Seamless Pipe

P235TR1 is used for ordinary pressure piping at room-temperature design conditions where this Part 1 quality is named. It is not a high-temperature Part 2 grade, not a stainless Part 5 grade, and not ASTM A106 Grade B. Where the Pressure Equipment Directive’s essential requirements apply, TR1 may not be the right quality.

Near-Equivalents for EN 10216-1 P235TR1 Seamless Pipe: Not Automatic Substitutes

P235TR2 uses the same yield and tensile table but adds impact and tighter inspection options. ASTM A106 Grade B and GB/T 8163 Grade 20 are often compared in export work, yet their chemistry and tensile ranges differ. EN 10255 S195T is a welding-and-threading tube, not this pressure-tube standard. ASME SA designations are not inferred here.

Sourcing EN 10216-1 P235TR1 Seamless Steel Pipe from SHH STEEL

Send the outside diameter, the wall, the length, the EN 10216-1 edition, and whether TR1 is really the required quality. If a 3.1 certificate or an impact test is needed, say so, and consider whether TR2 is the correct enquiry. SHH STEEL reviews the quality, the edition and the certificate before quoting.

EN 10216-1 P235TR1 Seamless Pipe FAQs

Is P235TR1 the same as P235TR2?
No. Both share the 235 MPa yield class and the 360–500 MPa tensile range, but TR2 has impact and tighter inspection options. TR1 does not require an impact test.
Which edition is used on this page?
Mechanicals are from Table 4 of EN 10216-1:2002+A1:2004. The ordered edition, often 2013 in current enquiries, should be named on the contract and checked on the certificate.
Is this an ASME SA-106 pipe?
No. An SA designation is used only when the named BPVC Section II, Part A edition lists it. That inference is not made here.
Are the size tables a complete EN 10220 list?
No. They are a typographical common subset with formula masses, not a complete listing and not a stock list.

Conclusion

EN 10216-1 P235TR1 is seamless non-alloy pressure tube of steel number 1.0254, with a 235 MPa yield up to 16 mm and a 360–500 MPa tensile range. Impact testing is not required for TR1. The size table is a typographical common subset with formula masses, not a stock list. Confirm the quality, the edition and the certificate on the order.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X