EN 10210-1 S355J2H Hot Finished Steel Hollow Sections from SHH STEEL

EN 10210-1 S355J2H Hot Finished Steel Hollow Sections

EN 10210-1 S355J2H is a hot-finished structural hollow section in steel number 1.0576. In the usual thickness band the specified minimum yield is 355 MPa, with 27 J impact at −20 °C. Size tables reprint a formula-checked limited range from EN 10210-2:2006 Annex B, not a cold-formed EN 10219 mass list. SHH STEEL reviews the grade, size and certificate before quoting.
Keywords
EN 10210-1 S355J2H, S355J2H hollow section, hot finished HSS, 1.0576 steel, EN 10210-2 sizes
Equivalent Grades:
Near-equivalents only, not automatic substitutes.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Available Sizes (433 verified EN 10210-2 Annex B sizes)
Applications
Equivalent Grades
Sourcing
FAQ
Conclusion

What are EN 10210-1 S355J2H Hot Finished Steel Hollow Sections?

EN 10210-1 S355J2H is a hot-finished structural hollow section in non-alloy quality steel number 1.0576. The product may be square, rectangular or circular. The J2 quality requires a 27 J Charpy verification at −20 °C, and J2 / K2 qualities are supplied with specific inspection. In the thickness band most often ordered, the specified minimum yield strength is 355 MPa. This page is for the hot-finished EN 10210 family, not for cold-formed EN 10219-1 S355J2H, and the two certificates must not be mixed.

Hot finishing changes the corner geometry of square and rectangular sections. For the same designated size and thickness, the EN 10210-2 calculation radii (external 1.5T, internal 1.0T) give a different mass from an EN 10219-2 cold-formed section. A 100 × 100 × 5 section is 14.7 kg/m in the EN 10210-2 Annex B table and about 14.4 kg/m under the cold-formed rules. That difference is a reason to keep the families apart on an enquiry.

Material, Manufacture and Scope for EN 10210-1 S355J2H Hollow Sections

EN 10210-1:2006 is the technical delivery standard. Dimensions, tolerances and sectional properties are those of EN 10210-2. Non-alloy hollow sections shall conform to Annex A; S355J2H is a fully killed (FF) grade in Table A.1. Qualities JR, J0, J2 and K2 are delivered hot finished. Seamless and welded manufacture are both permitted. Welded sections made by a continuous process shall not include the strip-joining welds in the finished length, except as the standard allows.

Fine-grain grades such as S355NH belong to Annex B and are a different designation. Some current mill programmes are offered as S355NH rather than S355J2H. That is not a silent substitute: the chemistry table, inspection route and delivery condition differ, and the certificate has to name the grade that was actually produced.

EN 10210-1 S355J2H Chemical Composition and Carbon Equivalent

Table A.1 of EN 10210-1:2006 sets these maximum cast-analysis limits for S355J2H, in percent: carbon 0.22 for both the t ≤ 40 mm and the 40 mm < t ≤ 120 mm columns, silicon 0.55, manganese 1.60, phosphorus 0.030 and sulphur 0.030. The grade is fully killed with nitrogen-binding elements (FF). The nitrogen maximum used for FN grades does not apply to this FF grade.

Table A.2 sets the maximum carbon equivalent, based on the cast analysis, at 0.45 % for t ≤ 16 mm, 0.47 % for 16 mm < t ≤ 40 mm, 0.50 % for 40 mm < t ≤ 65 mm and 0.53 % for 65 mm < t ≤ 120 mm. The CEV formula is the standard IIW expression given in clause 6.5.1. Product-analysis deviations, when a product analysis is required, follow Table 1 of the standard, not a copied EN 10219 table.

Swipe horizontally to view all dimensions.

Item S355J2H (1.0576), cast analysis
Carbon, max, t ≤ 40 mm and 40 mm < t ≤ 120 mm 0.22 % in both columns
Silicon, max 0.55 %
Manganese, max 1.60 %
Phosphorus, max 0.030 %
Sulphur, max 0.030 %
Deoxidation FF, fully killed with nitrogen-binding elements
CEV, max, t ≤ 16 mm 0.45 %
CEV, max, 16 mm < t ≤ 40 mm 0.47 %
CEV, max, 40 mm < t ≤ 65 mm 0.50 %
CEV, max, 65 mm < t ≤ 120 mm 0.53 %

EN 10210-1 S355J2H Mechanical Properties: Yield, Tensile, Elongation and Impact

Table A.3 of EN 10210-1:2006 gives the following longitudinal values for S355J2H, which shares the S355 tensile and elongation columns with S355J0H and S355K2H. Minimum yield ReH is 355 MPa for t ≤ 16 mm, 345 MPa for 16 mm < t ≤ 40 mm, 335 MPa for 40 mm < t ≤ 63 mm, 325 MPa for 63 mm < t ≤ 80 mm, 315 MPa for 80 mm < t ≤ 100 mm and 295 MPa for 100 mm < t ≤ 120 mm. Tensile strength Rm is 510–680 MPa for t ≤ 3 mm, 470–630 MPa for 3 mm < t ≤ 100 mm and 450–600 MPa for 100 mm < t ≤ 120 mm. Minimum elongation A is 22 % up to 40 mm, 21 % up to 63 mm, 20 % up to 100 mm and 18 % up to 120 mm. Transverse elongation is 2 % lower.

The impact requirement is 27 J at −20 °C. For J2 quality this test is part of specific inspection, not an option. Do not treat an S355J0H result (27 J at 0 °C, and only when Option 1.3 is specified) as a substitute for S355J2H.

Swipe horizontally to view all dimensions.

Specified thickness t (mm) ReH min (MPa) Rm (MPa) A min, longitudinal (%)
t ≤ 16 355 510–680 (t ≤ 3) / 470–630 (3 < t ≤ 100) 22 (t ≤ 40)
16 < t ≤ 40 345 470–630 22
40 < t ≤ 63 335 470–630 21
63 < t ≤ 80 325 470–630 20 (t ≤ 100)
80 < t ≤ 100 315 470–630 20
100 < t ≤ 120 295 450–600 18

EN 10210-1 S355J2H Common Sizes: Limited Range from EN 10210-2:2006 Annex B

The tables below reprint the limited range of standard sizes in EN 10210-2:2006 Annex B for circular, square and rectangular hollow sections. Each listed mass and area has been recomputed with the Annex A formulae (circular: M = 0.785A; square and rectangular: calculation radii ro = 1.5T and ri = 1.0T) and kept only where the published listing matches. This is the standard’s own limited range, not a recitation of every size a mill can roll, and it is not a warehouse stock list. Elliptical sections in Table B.4 are omitted here. Not every thickness is available from every mill.

Square hollow sections (106 sizes).

Swipe horizontally to view all dimensions.

Designation (mm) Side B (mm) Wall t (mm) Area (cm²) Mass M (kg/m)
40 × 40 × 2.6 40 2.6 3.82 3
40 × 40 × 3.2 40 3.2 4.6 3.61
40 × 40 × 4 40 4 5.59 4.39
40 × 40 × 5 40 5 6.73 5.28
50 × 50 × 2.6 50 2.6 4.86 3.81
50 × 50 × 3.2 50 3.2 5.88 4.62
50 × 50 × 4 50 4 7.19 5.64
50 × 50 × 5 50 5 8.73 6.85
50 × 50 × 6.3 50 6.3 10.6 8.31
60 × 60 × 2.6 60 2.6 5.9 4.63
60 × 60 × 3.2 60 3.2 7.16 5.62
60 × 60 × 4 60 4 8.79 6.9
60 × 60 × 5 60 5 10.7 8.42
60 × 60 × 6.3 60 6.3 13.1 10.3
60 × 60 × 8 60 8 16 12.5
70 × 70 × 3.2 70 3.2 8.4 6.63
70 × 70 × 4 70 4 10.4 8.15
70 × 70 × 5 70 5 12.7 9.99
70 × 70 × 6.3 70 6.3 15.6 12.3
70 × 70 × 8 70 8 19.2 15
80 × 80 × 3.2 80 3.2 9.72 7.63
80 × 80 × 4 80 4 12 9.41
80 × 80 × 5 80 5 14.7 11.6
80 × 80 × 6.3 80 6.3 18.1 14.2
80 × 80 × 8 80 8 22.4 17.5
90 × 90 × 4 90 4 13.6 10.7
90 × 90 × 5 90 5 16.7 13.1
90 × 90 × 6.3 90 6.3 20.7 16.2
90 × 90 × 8 90 8 25.6 20.1
100 × 100 × 4 100 4 15.2 11.9
100 × 100 × 5 100 5 18.7 14.7
100 × 100 × 6.3 100 6.3 23.2 18.2
100 × 100 × 8 100 8 28.8 22.6
100 × 100 × 10 100 10 34.9 27.4
120 × 120 × 5 120 5 22.7 17.8
120 × 120 × 6.3 120 6.3 28.2 22.2
120 × 120 × 8 120 8 35.2 27.6
120 × 120 × 10 120 10 42.9 33.7
120 × 120 × 12.5 120 12.5 52.1 40.9
140 × 140 × 5 140 5 26.7 21
140 × 140 × 6.3 140 6.3 33.3 26.1
140 × 140 × 8 140 8 41.6 32.6
140 × 140 × 10 140 10 50.9 40
140 × 140 × 12.5 140 12.5 62.1 48.7
150 × 150 × 5 150 5 28.7 22.6
150 × 150 × 6.3 150 6.3 35.8 28.1
150 × 150 × 8 150 8 44.8 35.1
150 × 150 × 10 150 10 54.9 43.1
150 × 150 × 12.5 150 12.5 67.1 52.7
150 × 150 × 14.2 150 14.2 75 58.9
150 × 150 × 16 150 16 83 65.2
160 × 160 × 5 160 5 30.7 24.1
160 × 160 × 6.3 160 6.3 38.3 30.1
160 × 160 × 8 160 8 48 37.6
160 × 160 × 10 160 10 58.9 46.3
160 × 160 × 12.5 160 12.5 72.1 56.6
160 × 160 × 14.2 160 14.2 80.7 63.3
160 × 160 × 16 160 16 89.4 70.2
180 × 180 × 5 180 5 34.7 27.3
180 × 180 × 6.3 180 6.3 43.3 34
180 × 180 × 8 180 8 54.4 42.7
180 × 180 × 10 180 10 66.9 52.5
180 × 180 × 12.5 180 12.5 82.1 64.4
180 × 180 × 14.2 180 14.2 92 72.2
180 × 180 × 16 180 16 102 80.2
200 × 200 × 5 200 5 38.7 30.4
200 × 200 × 6.3 200 6.3 48.4 38
200 × 200 × 8 200 8 60.8 47.7
200 × 200 × 10 200 10 74.9 58.8
200 × 200 × 12.5 200 12.5 92.1 72.3
200 × 200 × 14.2 200 14.2 103 81.1
200 × 200 × 16 200 16 115 90.3
220 × 220 × 6.3 220 6.3 53.4 41.9
220 × 220 × 8 220 8 67.2 52.7
220 × 220 × 10 220 10 82.9 65.1
220 × 220 × 12.5 220 12.5 102 80.1
220 × 220 × 14.2 220 14.2 115 90.1
220 × 220 × 16 220 16 128 100
250 × 250 × 6.3 250 6.3 61 47.9
250 × 250 × 8 250 8 76.8 60.3
250 × 250 × 10 250 10 94.9 74.5
250 × 250 × 12.5 250 12.5 117 91.9
250 × 250 × 14.2 250 14.2 132 103
250 × 250 × 16 250 16 147 115
260 × 260 × 6.3 260 6.3 63.5 49.9
260 × 260 × 8 260 8 80 62.8
260 × 260 × 10 260 10 98.9 77.7
260 × 260 × 12.5 260 12.5 122 95.8
260 × 260 × 14.2 260 14.2 137 108
260 × 260 × 16 260 16 153 120
300 × 300 × 6.3 300 6.3 74 57.8
300 × 300 × 8 300 8 93 72.8
300 × 300 × 10 300 10 115 90.2
300 × 300 × 12.5 300 12.5 142 112
300 × 300 × 14.2 300 14.2 160 126
300 × 300 × 16 300 16 179 141
350 × 350 × 8 350 8 109 85.4
350 × 350 × 10 350 10 135 106
350 × 350 × 12.5 350 12.5 167 131
350 × 350 × 14.2 350 14.2 189 148
350 × 350 × 16 350 16 211 166
400 × 400 × 10 400 10 155 122
400 × 400 × 12.5 400 12.5 192 151
400 × 400 × 14.2 400 14.2 217 170
400 × 400 × 16 400 16 243 191
400 × 400 × 20 400 20 300 235

Rectangular hollow sections (112 sizes).

Swipe horizontally to view all dimensions.

Designation (mm) H (mm) B (mm) Wall t (mm) Area (cm²) Mass M (kg/m)
50 × 30 × 2.6 50 30 2.6 3.82 3
50 × 30 × 3.2 50 30 3.2 4.6 3.61
50 × 30 × 4 50 30 4 5.59 4.39
50 × 30 × 5 50 30 5 6.73 5.28
60 × 40 × 2.6 60 40 2.6 4.86 3.81
60 × 40 × 3.2 60 40 3.2 5.88 4.62
60 × 40 × 4 60 40 4 7.19 5.64
60 × 40 × 5 60 40 5 8.73 6.85
60 × 40 × 6.3 60 40 6.3 10.6 8.31
80 × 40 × 3.2 80 40 3.2 7.16 5.62
80 × 40 × 4 80 40 4 8.79 6.9
80 × 40 × 5 80 40 5 10.7 8.42
80 × 40 × 6.3 80 40 6.3 13.1 10.3
80 × 40 × 8 80 40 8 16 12.5
90 × 50 × 3.2 90 50 3.2 8.44 6.63
90 × 50 × 4 90 50 4 10.4 8.15
90 × 50 × 5 90 50 5 12.7 9.99
90 × 50 × 6.3 90 50 6.3 15.6 12.3
90 × 50 × 8 90 50 8 19.2 15
100 × 50 × 3.2 100 50 3.2 9.08 7.13
100 × 50 × 4 100 50 4 11.2 8.78
100 × 50 × 5 100 50 5 13.7 10.8
100 × 50 × 6.3 100 50 6.3 16.9 13.3
100 × 50 × 8 100 50 8 20.8 16.3
100 × 60 × 3.2 100 60 3.2 9.72 7.63
100 × 60 × 4 100 60 4 12 9.41
100 × 60 × 5 100 60 5 14.7 11.6
100 × 60 × 6.3 100 60 6.3 18.1 14.2
100 × 60 × 8 100 60 8 22.4 17.5
120 × 60 × 4 120 60 4 13.6 10.7
120 × 60 × 5 120 60 5 16.7 13.1
120 × 60 × 6.3 120 60 6.3 20.7 16.2
120 × 60 × 8 120 60 8 25.6 20.1
120 × 60 × 10 120 60 10 30.9 24.3
120 × 80 × 4 120 80 4 15.2 11.9
120 × 80 × 5 120 80 5 18.7 14.7
120 × 80 × 6.3 120 80 6.3 23.2 18.2
120 × 80 × 8 120 80 8 28.8 22.6
120 × 80 × 10 120 80 10 34.9 27.4
140 × 80 × 4 140 80 4 16.8 13.2
140 × 80 × 5 140 80 5 20.7 16.3
140 × 80 × 6.3 140 80 6.3 25.7 20.2
140 × 80 × 8 140 80 8 32 25.1
140 × 80 × 10 140 80 10 38.9 30.6
150 × 100 × 4 150 100 4 19.2 15.1
150 × 100 × 5 150 100 5 23.7 18.6
150 × 100 × 6.3 150 100 6.3 29.5 23.1
150 × 100 × 8 150 100 8 36.8 28.9
150 × 100 × 10 150 100 10 44.9 35.3
150 × 100 × 12.5 150 100 12.5 54.6 42.8
160 × 80 × 4 160 80 4 18.4 14.4
160 × 80 × 5 160 80 5 22.7 17.8
160 × 80 × 6.3 160 80 6.3 28.2 22.2
160 × 80 × 8 160 80 8 35.2 27.6
160 × 80 × 10 160 80 10 42.9 33.7
160 × 80 × 12.5 160 80 12.5 52.1 40.9
180 × 100 × 4 180 100 4 21.6 16.9
180 × 100 × 5 180 100 5 26.7 21
180 × 100 × 6.3 180 100 6.3 33.3 26.1
180 × 100 × 8 180 100 8 41.6 32.6
180 × 100 × 10 180 100 10 50.9 40
180 × 100 × 12.5 180 100 12.5 62.1 48.7
200 × 100 × 4 200 100 4 23.2 18.2
200 × 100 × 5 200 100 5 28.7 22.6
200 × 100 × 6.3 200 100 6.3 35.8 28.1
200 × 100 × 8 200 100 8 44.8 35.1
200 × 100 × 10 200 100 10 54.9 43.1
200 × 100 × 12.5 200 100 12.5 67.1 52.7
200 × 100 × 16 200 100 16 83 65.2
200 × 120 × 6.3 200 120 6.3 38.3 30.1
200 × 120 × 8 200 120 8 48 37.6
200 × 120 × 10 200 120 10 58.9 46.3
200 × 120 × 12.5 200 120 12.5 72.1 56.6
250 × 150 × 6.3 250 150 6.3 48.4 38
250 × 150 × 8 250 150 8 60.8 47.7
250 × 150 × 10 250 150 10 74.9 58.8
250 × 150 × 12.5 250 150 12.5 92.1 72.3
250 × 150 × 14.2 250 150 14.2 103 81.1
250 × 150 × 16 250 150 16 115 90.3
260 × 180 × 6.3 260 180 6.3 53.4 41.9
260 × 180 × 8 260 180 8 67.2 52.7
260 × 180 × 10 260 180 10 82.9 65.1
260 × 180 × 12.5 260 180 12.5 102 80.1
260 × 180 × 14.2 260 180 14.2 115 90.1
260 × 180 × 16 260 180 16 128 100
300 × 200 × 6.3 300 200 6.3 61 47.9
300 × 200 × 8 300 200 8 76.8 60.3
300 × 200 × 10 300 200 10 94.9 74.5
300 × 200 × 12.5 300 200 12.5 117 91.9
300 × 200 × 14.2 300 200 14.2 132 103
300 × 200 × 16 300 200 16 147 115
350 × 250 × 6.3 350 250 6.3 73.6 57.8
350 × 250 × 8 350 250 8 92.8 72.8
350 × 250 × 10 350 250 10 115 90.2
350 × 250 × 12.5 350 250 12.5 142 112
350 × 250 × 14.2 350 250 14.2 160 126
350 × 250 × 16 350 250 16 179 141
400 × 200 × 8 400 200 8 92.8 72.8
400 × 200 × 10 400 200 10 115 90.2
400 × 200 × 12.5 400 200 12.5 142 112
400 × 200 × 14.2 400 200 14.2 160 126
400 × 200 × 16 400 200 16 179 141
450 × 250 × 8 450 250 8 109 85.4
450 × 250 × 10 450 250 10 135 106
450 × 250 × 12.5 450 250 12.5 167 131
450 × 250 × 14.2 450 250 14.2 189 148
450 × 250 × 16 450 250 16 211 166
500 × 300 × 10 500 300 10 155 122
500 × 300 × 12.5 500 300 12.5 192 151
500 × 300 × 14.2 500 300 14.2 217 170
500 × 300 × 16 500 300 16 243 191
500 × 300 × 20 500 300 20 300 235

Circular hollow sections (215 sizes).

CHS up to 168.3 mm (52 sizes).

Swipe horizontally to view all dimensions.

D × t (mm) Outside diameter D (mm) Wall t (mm) Area (cm²) Mass M (kg/m)
21.3 × 2.3 21.3 2.3 1.37 1.08
21.3 × 2.6 21.3 2.6 1.53 1.2
21.3 × 3.2 21.3 3.2 1.82 1.43
26.9 × 2.3 26.9 2.3 1.78 1.4
26.9 × 2.6 26.9 2.6 1.98 1.56
26.9 × 3.2 26.9 3.2 2.38 1.87
33.7 × 2.6 33.7 2.6 2.54 1.99
33.7 × 3.2 33.7 3.2 3.07 2.41
33.7 × 4 33.7 4 3.73 2.93
42.4 × 2.6 42.4 2.6 3.25 2.55
42.4 × 3.2 42.4 3.2 3.94 3.09
42.4 × 4 42.4 4 4.83 3.79
48.3 × 2.6 48.3 2.6 3.73 2.93
48.3 × 3.2 48.3 3.2 4.53 3.56
48.3 × 4 48.3 4 5.57 4.37
48.3 × 5 48.3 5 6.8 5.34
60.3 × 2.6 60.3 2.6 4.71 3.7
60.3 × 3.2 60.3 3.2 5.74 4.51
60.3 × 4 60.3 4 7.07 5.55
60.3 × 5 60.3 5 8.69 6.82
76.1 × 2.6 76.1 2.6 6 4.71
76.1 × 3.2 76.1 3.2 7.33 5.75
76.1 × 4 76.1 4 9.06 7.11
76.1 × 5 76.1 5 11.2 8.77
88.9 × 3.2 88.9 3.2 8.62 6.76
88.9 × 4 88.9 4 10.7 8.38
88.9 × 5 88.9 5 13.2 10.3
88.9 × 6.3 88.9 6.3 16.3 12.8
101.6 × 3.2 101.6 3.2 9.89 7.77
101.6 × 4 101.6 4 12.3 9.63
101.6 × 5 101.6 5 15.2 11.9
101.6 × 6.3 101.6 6.3 18.9 14.8
101.6 × 8 101.6 8 23.5 18.5
101.6 × 10 101.6 10 28.8 22.6
114.3 × 3.2 114.3 3.2 11.2 8.77
114.3 × 4 114.3 4 13.9 10.9
114.3 × 5 114.3 5 17.2 13.5
114.3 × 6.3 114.3 6.3 21.4 16.8
114.3 × 8 114.3 8 26.7 21
114.3 × 10 114.3 10 32.8 25.7
139.7 × 4 139.7 4 17.1 13.4
139.7 × 5 139.7 5 21.2 16.6
139.7 × 6.3 139.7 6.3 26.4 20.7
139.7 × 8 139.7 8 33.1 26
139.7 × 10 139.7 10 40.7 32
139.7 × 12.5 139.7 12.5 50 39.2
168.3 × 4 168.3 4 20.6 16.2
168.3 × 5 168.3 5 25.7 20.1
168.3 × 6.3 168.3 6.3 32.1 25.2
168.3 × 8 168.3 8 40.3 31.6
168.3 × 10 168.3 10 49.7 39
168.3 × 12.5 168.3 12.5 61.2 48

CHS over 168.3 mm up to 406.4 mm (65 sizes).

Swipe horizontally to view all dimensions.

D × t (mm) Outside diameter D (mm) Wall t (mm) Area (cm²) Mass M (kg/m)
177.8 × 5 177.8 5 27.1 21.3
177.8 × 6.3 177.8 6.3 33.9 26.6
177.8 × 8 177.8 8 42.7 33.5
177.8 × 10 177.8 10 52.7 41.4
177.8 × 12.5 177.8 12.5 64.9 51
193.7 × 5 193.7 5 29.6 23.3
193.7 × 6.3 193.7 6.3 37.1 29.1
193.7 × 8 193.7 8 46.7 36.6
193.7 × 10 193.7 10 57.7 45.3
193.7 × 12.5 193.7 12.5 71.2 55.9
193.7 × 14.2 193.7 14.2 80.1 62.9
193.7 × 16 193.7 16 89.3 70.1
219.1 × 5 219.1 5 33.6 26.4
219.1 × 6.3 219.1 6.3 42.1 33.1
219.1 × 8 219.1 8 53.1 41.6
219.1 × 10 219.1 10 65.7 51.6
219.1 × 12.5 219.1 12.5 81.1 63.7
219.1 × 14.2 219.1 14.2 91.4 71.8
219.1 × 16 219.1 16 102 80.1
219.1 × 20 219.1 20 125 98.2
244.5 × 5 244.5 5 37.6 29.5
244.5 × 6.3 244.5 6.3 47.1 37
244.5 × 8 244.5 8 59.4 46.7
244.5 × 10 244.5 10 73.7 57.8
244.5 × 12.5 244.5 12.5 91.1 71.5
244.5 × 14.2 244.5 14.2 102.7 80.6
244.5 × 16 244.5 16 115 90.2
244.5 × 20 244.5 20 141 110.7
244.5 × 25 244.5 25 172 135
273 × 5 273 5 42.1 33
273 × 6.3 273 6.3 52.8 41.4
273 × 8 273 8 66.6 52.3
273 × 10 273 10 82.6 64.9
273 × 12.5 273 12.5 102 80.3
273 × 14.2 273 14.2 115 90.6
273 × 16 273 16 129 101
273 × 20 273 20 159 125
273 × 25 273 25 195 153
323.9 × 5 323.9 5 50.1 39.3
323.9 × 6.3 323.9 6.3 62.9 49.3
323.9 × 8 323.9 8 79.4 62.3
323.9 × 10 323.9 10 98.6 77.4
323.9 × 12.5 323.9 12.5 122 96
323.9 × 14.2 323.9 14.2 138 108.5
323.9 × 16 323.9 16 155 121
323.9 × 20 323.9 20 191 150
323.9 × 25 323.9 25 235 184
355.6 × 6.3 355.6 6.3 69.1 54.3
355.6 × 8 355.6 8 87.4 68.6
355.6 × 10 355.6 10 109 85.2
355.6 × 12.5 355.6 12.5 135 106
355.6 × 14.2 355.6 14.2 152 120
355.6 × 16 355.6 16 171 134
355.6 × 20 355.6 20 211 166
355.6 × 25 355.6 25 260 204
406.4 × 6.3 406.4 6.3 79.2 62.2
406.4 × 8 406.4 8 100 78.6
406.4 × 10 406.4 10 125 97.8
406.4 × 12.5 406.4 12.5 155 121
406.4 × 14.2 406.4 14.2 175 137
406.4 × 16 406.4 16 196 154
406.4 × 20 406.4 20 243 191
406.4 × 25 406.4 25 300 235
406.4 × 30 406.4 30 355 278
406.4 × 40 406.4 40 460 361

CHS over 406.4 mm (98 sizes).

Swipe horizontally to view all dimensions.

D × t (mm) Outside diameter D (mm) Wall t (mm) Area (cm²) Mass M (kg/m)
457 × 6.3 457 6.3 89.2 70
457 × 8 457 8 113 88.6
457 × 10 457 10 140 110
457 × 12.5 457 12.5 175 137
457 × 14.2 457 14.2 198 155
457 × 16 457 16 222 174
457 × 20 457 20 275 216
457 × 25 457 25 339 266
457 × 30 457 30 402 316
457 × 40 457 40 524 411
508 × 6.3 508 6.3 99.3 77.9
508 × 8 508 8 126 98.6
508 × 10 508 10 156 123
508 × 12.5 508 12.5 195 153
508 × 14.2 508 14.2 220 173
508 × 16 508 16 247 194
508 × 20 508 20 307 241
508 × 25 508 25 379 298
508 × 30 508 30 451 354
508 × 40 508 40 588 462
508 × 50 508 50 719 565
610 × 6.3 610 6.3 119 93.8
610 × 8 610 8 151 119
610 × 10 610 10 188 148
610 × 12.5 610 12.5 235 184
610 × 14.2 610 14.2 266 209
610 × 16 610 16 299 234
610 × 20 610 20 371 291
610 × 25 610 25 459 361
610 × 30 610 30 547 429
610 × 40 610 40 716 562
610 × 50 610 50 880 691
711 × 6.3 711 6.3 139 109
711 × 8 711 8 177 139
711 × 10 711 10 220 173
711 × 12.5 711 12.5 274 215
711 × 14.2 711 14.2 311 244
711 × 16 711 16 349 274
711 × 20 711 20 434 341
711 × 25 711 25 539 423
711 × 30 711 30 642 504
711 × 40 711 40 843 662
711 × 50 711 50 1038 815
711 × 60 711 60 1227 963
762 × 6.3 762 6.3 150 117
762 × 8 762 8 190 149
762 × 10 762 10 236 185
762 × 12.5 762 12.5 294 231
762 × 14.2 762 14.2 334 262
762 × 16 762 16 375 294
762 × 20 762 20 466 366
762 × 25 762 25 579 454
762 × 30 762 30 690 542
762 × 40 762 40 907 712
762 × 50 762 50 1118 878
813 × 8 813 8 202 159
813 × 10 813 10 252 198
813 × 12.5 813 12.5 314 247
813 × 14.2 813 14.2 356 280
813 × 16 813 16 401 314
813 × 20 813 20 498 391
813 × 25 813 25 619 486
813 × 30 813 30 738 579
914 × 8 914 8 228 179
914 × 10 914 10 284 223
914 × 12.5 914 12.5 354 278
914 × 14.2 914 14.2 401 315
914 × 16 914 16 451 354
914 × 20 914 20 562 441
914 × 25 914 25 698 548
914 × 30 914 30 833 654
1016 × 8 1016 8 253 199
1016 × 10 1016 10 316 248
1016 × 12.5 1016 12.5 394 309
1016 × 14.2 1016 14.2 447 351
1016 × 16 1016 16 503 395
1016 × 20 1016 20 626 491
1016 × 25 1016 25 778 611
1016 × 30 1016 30 929 729
1067 × 10 1067 10 332 261
1067 × 12.5 1067 12.5 414 325
1067 × 14.2 1067 14.2 470 369
1067 × 16 1067 16 528 415
1067 × 20 1067 20 658 516
1067 × 25 1067 25 818 642
1067 × 30 1067 30 977 767
1168 × 10 1168 10 364 286
1168 × 12.5 1168 12.5 454 356
1168 × 14.2 1168 14.2 515 404
1168 × 16 1168 16 579 455
1168 × 20 1168 20 721 566
1168 × 25 1168 25 898 705
1219 × 10 1219 10 380 298
1219 × 12.5 1219 12.5 474 372
1219 × 14.2 1219 14.2 537 422
1219 × 16 1219 16 605 475
1219 × 20 1219 20 753 591
1219 × 25 1219 25 938 736

Applications and Service Limits for EN 10210-1 S355J2H Hollow Sections

Hot-finished S355J2H sections are used in building frames, trusses, columns, bridges and general structural work where a 355 MPa class and a −20 °C impact quality are specified in a hot-finished hollow section. The grade is a structural product, not a pressure-pipe grade and not a boiler tube. Suitability for galvanizing, exact length and any option for corner-region testing have to be written on the order when they are required.

Do not substitute a cold-formed EN 10219-1 S355J2H section, an ASTM A500 HSS, or a GB/T 6728 section on the same certificate. Those products have their own corner-radius rules, tensile tables and inspection routes.

Near-Equivalents for EN 10210-1 S355J2H Hollow Sections: Not Automatic Substitutes

EN 10219-1 S355J2H is the cold-formed counterpart in the same steel number 1.0576. It is not hot-finished, and its mass for a square or rectangular size will usually differ. EN 10210-1 S355J0H uses the same yield class but verifies impact at 0 °C, and that test is only run when Option 1.3 is specified. S355NH is a fine-grain normalized grade in Annex B, not a restamp of S355J2H. ASTM A500 or A1085 HSS, and GB/T 6728 sections, follow different specifications.

Sourcing EN 10210-1 S355J2H Hot Finished Steel Hollow Sections from SHH STEEL

Send the shape, the designated size and thickness, the length, the EN 10210-1 edition, and whether a Declaration of Performance is required. Name S355J2H explicitly if the −20 °C quality and specific inspection are needed. SHH STEEL reviews the grade, the hot-finished family, the size and the certificate wording before quoting. The Annex B tables above are a checked dimensional reference, not a claim of warehouse stock.

EN 10210-1 S355J2H Hollow Section FAQs

Is EN 10210-1 S355J2H the same as EN 10219-1 S355J2H?
No. Both can use steel number 1.0576, but EN 10210 is hot-finished and EN 10219 is cold-formed. Square and rectangular masses differ because the calculation corner radii differ. They must be ordered as the family the design names.
Where do the masses on this page come from?
From EN 10210-2:2006 Annex B, recomputed with the Annex A formulae. For square and rectangular sections the calculation radii are ro = 1.5T and ri = 1.0T. Only rows that match the published listing are shown.
Can S355NH be supplied instead of S355J2H?
Not automatically. S355NH is a fine-grain normalized grade in Annex B, with its own chemistry and delivery condition. Some mill programmes are offered as S355NH. Name the grade the design requires and read the certificate.
Is the impact test optional for S355J2H?
No. J2 quality is supplied with specific inspection, and the 27 J at −20 °C requirement is part of Table A.3. For JR and J0 qualities the impact test is verified only when Option 1.3 is specified.

Conclusion

EN 10210-1 S355J2H is the hot-finished 355 MPa hollow section of steel number 1.0576, with 27 J impact at −20 °C and specific inspection. The size tables reprint a formula-checked limited range from EN 10210-2:2006 Annex B. They are not a cold-formed EN 10219 mass list and not a stock list. Confirm the family, the grade, the edition, the size and the certificate on the order.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X