BV Grade FH36 Steel Plate: High-Strength Shipbuilding Steel Supplier| SHH STEEL

BV Grade FH36 Steel Plate

BV Grade FH36 steel plates are high-strength, ideal for shipbuilding and offshore structures in extreme cold. With 490-630 MPa tensile and 355 MPa yield, widely supplied globally by SHH STEEL.
Specification:
BV Rules for Building and Classing Steel Vessels, Part 2, for shipbuilding and marine applications
Dimensions:
5-100mm thick, 3000mm max wide, 12000mm max long;
Hardness/Density:
BV FH36 Hardness 140-200 HB, Density 7.85 g/cm³
Equivalent Material:
ABS FH36, LR FH36, DNV NV F36, GL-F36
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Price / Cost
Tolerances
Difference VS others
Equivalent
Supplementary
Applications
Why Choose Us
FAQ
Conclusion

General Description

When it comes to building tough ships and offshore platforms that can handle freezing cold and heavy loads, BV Grade FH36 steel plate is a top pick.

This high-strength steel is made for extreme marine conditions, offering great toughness in super cold weather, easy welding, and good resistance to rust from saltwater. It’s part of the “FH” family, which means it’s built for high performance in freezing temps.

At SHH STEEL, we make and send out BV FH36 plates that follow strict Bureau Veritas (BV) rules. These plates are often used in ship hulls, decks, and other parts for vessels in polar areas.

What makes BV Grade FH36 special? It keeps its strength even at -60°C, helping ships stay safe and last longer in icy seas. If you’re in shipbuilding or engineering, knowing about BV FH36 steel plate can help you choose the right material for your project.

Material Specification

BV Grade FH36 is classified as a high-strength steel under BV rules, in the “FH” group for better tensile and extreme cold toughness.

It’s usually hot-rolled and can use thermo-mechanical controlled processing (TMCP) to get a fine structure that boosts its qualities. It follows BV Rules for the Classification of Steel Ships, perfect for ships in very cold waters.

At SHH STEEL, every BV FH36 plate is certified and ready for worldwide use.

Thickness and Sizes Available

We offer BV FH36 steel plates in different sizes for ship projects in cold areas. This range helps with custom builds and cuts down waste.

Here’s a quick table summary:

Dimension Type Range/Details
Thickness 5 mm to 100 mm
Width Up to 3000 mm
Length Up to 12000 mm
Custom Options Available for cuts and shapes

Need exact sizes for your BV/FH36 plates? Our experts can tailor them to your designs.

Chemical Composition

The mix in BV FH36 steel plate is set for strength and cold resistance.

Elements are controlled to skip problems like breaking or bad welds. Low phosphorus and sulfur stop cracks.

BV sets limits by ladle (melt) analysis and product (final) checks. Here’s the usual setup:

At SHH STEEL, we test batches to match specs for trusty BV FH36 marine grade steel.

Element Ladle Analysis (Max % unless range) Product Analysis (Max % unless range)
Carbon (C) ≤ 0.16 ≤ 0.18
Manganese (Mn) 0.90 – 1.60 0.85 – 1.65
Silicon (Si) ≤ 0.50 ≤ 0.55
Phosphorus (P) ≤ 0.025 ≤ 0.030
Sulfur (S) ≤ 0.025 ≤ 0.030
Aluminum (Al) ≥ 0.015 (acid soluble) ≥ 0.010
Niobium (Nb) 0.02 – 0.05 0.02 – 0.05
Vanadium (V) 0.05 – 0.10 0.05 – 0.10

Note: Traces like copper or chromium may add for better rust fight.

Mechanical Properties

BV FH36 steel plate has strong features for heavy loads in freezing ship work.

It has high yield to fight bending, solid tensile for lasting power, and good stretch for shaping without snaps.

It also passes impact tests at -60°C for tough in ice-cold. These help BV Grade FH36 handle waves, bumps, and wear in polar.

See the table for key properties:

Property Value/Requirement
Yield Strength (min) 355 MPa
Tensile Strength 490 – 630 MPa
Elongation (min) 21% (in 200 mm)
Charpy V-Notch Impact 34 J (longitudinal) at -60°C

Vs. basic steels, BV/FH36 gives top performance for cold marine jobs.

Delivery Conditions

At SHH STEEL, we deliver BV FH36 steel plates ready for your needs.

Main states: normalized rolling (heat to 900°C, air cool) for better toughness.

For thick plates, thermo-mechanical controlled processing (TMCP) mixes rolling and cooling for strength without weld loss.

Plates include BV cert, with MTC per EN 10204 3.1 or 3.2, proving spec match.

Packed with waterproof and wood crates.

Times 15-30 days, rush options. Global shipping.

Special needs? Tell us early.

Delivery Condition Description
Normalized Heated and air-cooled for uniformity
TMCP Controlled rolling and cooling for enhanced strength

Price / Cost in China Market

China’s steel prices for BV FH36 vary by raw costs and demand.

Now, expect $550-$750 per ton for standard. Thin lower, thick higher from processing.

Trends and BV cert add 10-20%. SHH STEEL fair prices, bulk deals.

Quote for BV Grade FH36 – quality saves on fixes long-term.

Tolerances

Fit is key in ships for easy joins. BV FH36 from SHH STEEL follows BV/EN 10029 for sizes/flat.

Prevents warps. New gear to hit specs, inspect each.

Tighter needs? Talk to us.

Table of usual tolerances:

Tolerance Type Specification/Details
Thickness For <25 mm: +0.3 mm / -0.3 mm; For 25-40 mm: +0.4 mm / -0.3 mm; Up for thicker
Width +20 mm / -0 mm
Length +50 mm / -0 mm
Flatness Max 6 mm per meter
Squareness Max 10 mm deviation

Prepares BV/FH36 for exact builds.

Difference VS others

To pick the right steel, compare BV FH36 with BV AH36, BV DH36, BV EH36, BV FH40. They differ in cold resistance and strength.

BV FH36 for extreme cold with high strength.

Property BV AH36 BV DH36 BV EH36 BV FH40 BV FH36
Yield Strength (min MPa) 355 355 355 390 355
Tensile Strength (MPa) 490-620 490-620 490-620 510-650 490-620
Impact Test Temp (°C) 0 -20 -40 -60 -60
Toughness (Charpy J min) 34 34 34 41 34
Typical Use High stress Cold high Arctic high Extreme cold high Extreme cold high
Cost Relative Medium-High Medium-High High Higher High

BV Grade FH36 optimal for extreme cold high-stress.

Equivalent Material Grade

BV FH36 has world matches for sourcing.

These have like chemistry and properties, ok with approvals. Good for global builds.

SHH STEEL supplies BV FH36 or equals for your rules.

Here’s a table of common equivalents:

Classification Society Equivalent Grade
Lloyd’s Register (LR) FH36
American Bureau of Shipping (ABS) FH36
Det Norske Veritas (DNV) NV F36
Germanischer Lloyd (GL) F36
Registro Italiano Navale (RINA) FH36
China Classification Society (CCS) FH36
Nippon Kaiji Kyokai (NK) FH36
Korean Register (KR) FH36

Supplementary Requirements

To boost performance, BV FH36 can have extras like Z-testing (Z25 or Z35) for better through-thickness strength, reducing tear risks in welds.

We also do ultrasonic checks to spot hidden flaws and fine-grain treatments for extra toughness.

For welded parts, simulated post-weld heat treatment is available. Specify these when ordering from SHH STEEL for premium shipbuilding steel.

Applications

BV FH36 steel plate is versatile in extreme cold marine work. It’s key for ship hulls that take ice hits, like in icebreakers.

In offshore setups, it builds platforms and legs that stand up to arctic waves. Other uses: barges in polar areas, ferries in icy waters, and coast wind farms in freezing spots.

Its strength and cold resistance make it ideal for long sea exposure. SHH STEEL has delivered BV Grade FH36 for many successful projects.

Why Choose Us

Pick SHH STEEL for BV FH36 steel plates because we’re pros in making and shipping them from China.

Our modern factories ensure top quality at good prices. We offer expert help from start to finish, including tech advice and fast global shipping.

With exports to 50+ countries and full BV certs, we’re reliable. Plus, we focus on green methods. Trust us for strong, dependable marine steel plate.

FAQ

What is the difference between BV FH36 and BV EH36 steel plates?
BV FH36 and EH36 are both high-strength steels with 355 MPa yield and 490-620 MPa tensile, but FH36 is impact-tested at -60°C for extreme cold toughness, while EH36 is at -40°C. FH36 is better for polar regions to avoid brittleness, but EH36 suffices for less severe arctic conditions. Both weld well, but choose based on temperature requirements.
What are the chemical composition requirements for BV FH36 marine grade steel?
BV FH36 limits carbon to 0.16%, manganese between 0.90-1.60%, silicon up to 0.50%, phosphorus and sulfur to 0.025% each for good weldability and toughness. Aluminum is min 0.015% for grain refinement, with niobium 0.02-0.05% and vanadium 0.05-0.10%. Check the MTC for your batch's exact ladle or product analysis.
How does BV FH36 steel perform in low-temperature environments compared to other grades?
BV FH36 performs excellently at -60°C with 34J impact, making it superior for extreme cold; compared to EH36 (-40°C) or DH36 (-20°C), it's better for polar routes, while AH36 (0°C) is for milder conditions. It's a staple for ice-class ships.
What are the typical applications and uses of BV Grade FH36 steel plate in shipbuilding?
BV Grade FH36 is typically used for hulls, decks, and bulkheads in ice-class vessels due to its high strength and cold toughness. It's also ideal for offshore platforms, risers, and marine gear in freezing waters. It handles fatigue and salt well, making vessels safer.
Is BV FH36 steel plate suitable for welding, and what precautions should be taken?
Yes, BV FH36 is highly weldable with methods like SMAW or GMAW. For thicker plates (over 50mm), preheat to 100-150°C to prevent cracking, use low-hydrogen electrodes. Post-weld heat treatment may be optional but follow BV guidelines for strong, defect-free joints.

Conclusion

BV FH36 steel plate is a powerhouse in the shipbuilding world, offering unmatched strength, reliability, and value for extreme cold applications.

From its precise specifications to versatile applications, it’s clear why this marine grade is a top pick for professionals. As your dedicated SHH STEEL supplier, we’re here to provide premium BV Grade FH36 tailored to your needs. Ready to elevate your next project? Reach out today for expert advice and unbeatable service.

 

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *



    Related Products

    +86 18939509537
    sale@steelspecs.com
    +86 021-62716097
    Shenghonghe: Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *



      X