ASTM A738 Grade E Steel Plate | A738 Gr.E Heat-Treated Vessel Plate | ASTM A738 Steel - SHH STEEL

ASTM A738 Grade E Steel Plate | A738 Gr.E Heat-Treated Vessel Plate

ASTM A738 Grade E is a heat-treated carbon-manganese-silicon steel plate for welded pressure vessels in moderate and lower temperature service, to ASTM A738/A738M-19(2026). It is the 90 ksi [620 MPa] strength level, with a tensile strength of 90–110 ksi [620–760 MPa] in the thinnest band. SHH STEEL produces and exports this plate to the ordered thickness and tests.
Equivalent Grades:
Code companion: ASME SA-738 Grade E. Related: ASTM A537. Not automatic substitutes.
Heat Treatment
Quenched and tempered; temper 595 °C minimum.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is ASTM A738 Grade E steel plate?

ASTM A738 Grade E is a heat-treated carbon-manganese-silicon steel plate to ASTM A738/A738M, Standard Specification for Pressure Vessel Plates, Heat-Treated, Carbon-Manganese-Silicon Steel, for Moderate and Lower Temperature Service. It is intended for welded pressure vessels. Grade E is the 90 ksi [620 MPa] minimum tensile strength level of the specification.

The current listing is A738/A738M-19(2026): the 2019 specification, reapproved in 2026 and published on 1 February 2026. A reapproval carries the 2019 technical content forward. The specification has five grades, A, B, C, D and E, at four strength levels: 75 ksi [515 MPa], 85 ksi [585 MPa], 80 ksi [550 MPa] and 90 ksi [620 MPa] minimum.

For ASME Code work the related specification is SA-738/SA-738M; the 2023 Code edition states it is identical with A738/A738M-19. The related Code page is ASME SA738 Grade E. A certificate to one designation does not automatically satisfy an order written to the other.

SHH STEEL produces and exports ASTM A738 Grade E plate as a producer, exporter and mill agent, to the thickness, heat treatment, supplementary requirements and inspection document written on the enquiry. The grade sits in our ASTM A738 range under Nuclear-Grade Steel Plates. The other grades are ASTM A738 Grade A, ASTM A738 Grade B, ASTM A738 Grade C, ASTM A738 Grade D.

Material specification for ASTM A738 Grade E

The table summarises the specification items for this grade. Sizes are agreed per order; no stock range is implied.

Parameter Detail
Specification ASTM A738/A738M-19(2026)
Grade Grade E, 90 ksi [620 MPa] strength level
Product form Heat-treated C-Mn-Si plate for welded pressure vessels, moderate and lower temperature service
General requirements ASTM A20/A20M; where A738 conflicts with A20/A20M, A738 prevails
Steelmaking Killed steel meeting the fine austenitic grain size requirement of A20/A20M
Heat treatment Quenched and tempered in all thicknesses. Minimum tempering temperature 1100 °F [595 °C].
Thickness (scope) 2 in. [50 mm] (maximum permitted nominal thickness)
Units Inch-pound (A738) or SI (A738M), used independently
Our supply We produce and export ASTM A738 Grade E plate to the order

Chemical composition of ASTM A738 Grade E

Heat and product analyses shall meet Table 1 of A738/A738M for Grade E, unless modified by Supplementary Requirement S17, Vacuum Carbon-Deoxidized Steel, of A20/A20M. Carbon, phosphorus, sulfur, titanium, boron and aluminum limits apply to both heat and product analysis.

Element Grade E heat analysis, % Grade E product analysis, %
Carbon, max 0.12 0.12
Manganese 1.10–1.60 1.02–1.72
Phosphorus, max 0.015 0.015
Sulfur, max 0.006 0.006
Silicon 0.15–0.50 0.13–0.55
Copper, max 0.35 0.38
Nickel, max 0.70 0.73
Chromium, max 0.30 0.34
Molybdenum, max 0.35 0.38
Vanadium, max 0.09 0.10
Niobium (columbium), max 0.05 0.06
Niobium plus vanadium, max 0.12 0.13
Boron, max 0.0007 0.0007
Aluminum, min 0.020 total or 0.015 acid soluble 0.020 total or 0.015 acid soluble
Titanium Only by agreement, 0.006–0.03 by heat analysis; aluminum minimum then does not apply Report if used

For Grade E, each 0.01 percentage point reduction below the carbon maximum permits a 0.06 percentage point increase above the manganese maximum, up to 1.85 % by heat analysis and 1.99 % by product analysis.

Niobium and columbium are interchangeable names for the same element.

Mechanical properties of ASTM A738 Grade E

Tension tests follow A20/A20M and Table 2 of A738/A738M. For nominal thicknesses of 3/4 in. [20 mm] and under, the 1.5 in. [40 mm] wide rectangular specimen may be used with elongation measured in 2 in. [50 mm].

Nominal thickness Tensile strength, ksi [MPa] Yield strength, min, ksi [MPa] Elongation in 2 in. [50 mm], min, %
1.5 in. [40 mm] and under 90–110 [620–760] 75 [515] 20
Over 1.5 to 2.0 in. [40 to 50 mm] 90–110 [620–760] 75 [515] 20

Elongation is subject to the A20/A20M adjustments. Charpy V-notch impact testing is Supplementary Requirement S5 and applies only when ordered. Nonmandatory Appendix X1 lists, for information, the guarantees generally available: 20 ft·lbf [27 J] at −50 °F [−45 °C] longitudinal and 20 ft·lbf [27 J] at −20 °F [−30 °C] transverse. Conformance to those values is a matter of agreement on the order.

Heat treatment and delivery condition of ASTM A738 Grade E

Quenched and tempered in all thicknesses. When plates are tempered, the minimum tempering temperature is 1100 °F [595 °C].

  • Supplementary requirements listed by the specification include S1 vacuum treatment, S2 product analysis, S3 simulated post-weld heat treatment of mechanical test coupons, S4 additional tension test, S5 Charpy V-notch impact test, S6 drop-weight test (0.625 in. [16 mm] and over), S9 magnetic particle examination, S12 ultrasonic examination to A578/A578M and S20 maximum carbon equivalent for weldability
  • Supplementary requirements apply only when stated on the purchase order
  • Plates are supplied in the heat-treated condition stated on the certificate

Welding ASTM A738 Grade E plate

A738 plates are intended for welded pressure vessels. ASTM A738 Grade E is a carbon-manganese-silicon steel with very low carbon, low phosphorus and sulfur and controlled microalloying, so weldability is generally good with a qualified procedure. For quenched and tempered plate, control heat input and keep any post-weld heat treatment below the tempering temperature.

Where the vessel will be stress relieved, order S3 simulated post-weld heat treatment so the certificate reflects the fabricated condition. S20 can be used to set a maximum carbon equivalent when the fabricator needs it.

Dimensions, thickness limits and examination

Permitted variations in dimensions and mass, quality and repair of defects, and marking follow ASTM A20/A20M.

Item Requirement
Thickness, width, length, flatness ASTM A20/A20M permitted variations for the ordered size
Thickness limit 2 in. [50 mm] (maximum permitted nominal thickness)
Ultrasonic examination S12, A578/A578M, only when ordered
Magnetic particle examination S9, only when ordered

Applications and specification limits

ASTM A738 Grade E plate is used for shells, heads and other pressure parts of welded vessels in moderate and lower temperature service, where a heat-treated C-Mn-Si plate with the Grade E strength level is specified.

Listing this specification in our ASTM A738 range under the Nuclear-Grade Steel Plates family is a catalogue grouping only. It is not a nuclear qualification, an RCC-M qualification or an ASME Section III certification of SHH STEEL, of the mill or of any heat. Where plate is intended for nuclear construction, the Code edition, material organisation and quality-system rules, fracture-toughness testing and project chemistry limits must be written on the purchase order and confirmed before acceptance.

  • Thickness: 2 in. [50 mm] (maximum permitted nominal thickness)
  • Low-temperature impact properties must be ordered (S5); they are not a base requirement
  • Design stresses come from the construction code named on the order

Compare ASTM A738 Grade E with related vessel plates

Within A738 the grade must match the drawing. Grades differ in strength level, chemistry and thickness limit, so one grade cannot be stamped as another because a test result is high. Related C-Mn-Si specifications look similar but are written to different requirements.

Grade Strength level / family Tensile strength (thinnest range) Thickness limit Relation
ASTM A738 Grade E 90 ksi [620 MPa] 90–110 [620–760] 2 in. [50 mm] (maximum permitted nominal thickness) This page
ASTM A738 Grade A 75 ksi [515 MPa] 75–95 [515–655] 6 in. [150 mm] (current practice) Different grade; not a substitute
ASTM A738 Grade B 85 ksi [585 MPa] 85–102 [585–705] 4 in. [100 mm] (current practice) Different grade; not a substitute
ASTM A738 Grade C 80 ksi [550 MPa] 80–100 [550–690] 6 in. [150 mm] (current practice) Different grade; not a substitute
ASTM A738 Grade D 85 ksi [585 MPa] 85–105 [585–724] 1.5 in. [40 mm] (maximum permitted nominal thickness) Different grade; not a substitute
ASTM A537 Class 1 Heat-treated C-Mn-Si, own specification Per A537 Per A537 Related family; not a substitute
ASTM A537 Class 2 QT C-Mn-Si, own specification Per A537 Per A537 Related family; not a substitute
ASTM A516 Grade 70 Carbon steel, own specification Per A516 Per A516 Different specification

Equivalent and related grades for ASTM A738 Grade E

Equivalents below are engineering judgement only and are not automatic substitutes. Any equivalence must be approved by the designer or code authority for the project.

Region Grade Note
USA (ASME) ASME SA738 Grade E Code companion; SA-738 in the 2023 Code is identical with A738/A738M-19
Related ASTM ASTM A537 Class 1 Heat-treated C-Mn-Si plate in a similar strength range; engineering judgement only
Europe EN 10028-6 quenched and tempered fine-grain steels (plain text) Different chemistry and test basis; engineering judgement only
Japan JIS G3115 / JIS G3126 vessel steels of a similar strength (plain text) Different specification basis; engineering judgement only

Why choose SHH STEEL for ASTM A738 Grade E

  • SHH STEEL produces and exports ASTM A738 Grade E heat-treated plate as a producer, exporter and mill agent
  • We check chemistry and Table 2 thickness bands against A738/A738M before quoting
  • We keep ASTM A738 and ASME SA-738 designations distinct and quote dual certification only when confirmed
  • We do not present the Nuclear-Grade Steel Plates listing as a nuclear qualification
  • We match supplementary tests and the inspection document to the order

How to enquire for ASTM A738 Grade E

Item What to state
Specification ASTM A738/A738M-19(2026), Grade E
Size Thickness, width, length and quantity
Heat treatment Quenched and tempered
Supplementary requirements For example S3 simulated PWHT, S5 Charpy V-notch with temperature and energy, S12 ultrasonic, S20 carbon equivalent
Documentation Inspection document required, for example EN 10204 3.1 or 3.2

Cutting and other processing can be added when written on the order.

FAQ

What is ASTM A738 Grade E?
A heat-treated C-Mn-Si pressure vessel plate to A738/A738M-19(2026) at the 90 ksi [620 MPa] strength level, for welded vessels in moderate and lower temperature service.
How is it heat treated?
Quenched and tempered in all thicknesses. Minimum tempering temperature is 1100 °F [595 °C].
What thickness does the specification allow?
2 in. [50 mm] (maximum permitted nominal thickness). Actual sizes are agreed per order.
Is impact testing included?
No. Charpy V-notch testing is Supplementary Requirement S5. Appendix X1 lists 20 ft·lbf [27 J] at −50 °F [−45 °C] longitudinal and −20 °F [−30 °C] transverse as generally available guarantees, only by agreement.
Is A738 the same as ASME SA-738?
SA-738 in the 2023 Code is identical with A738/A738M-19. For Code work order the SA designation; dual certification must be confirmed on the order.

Request a quotation

Contact SHH STEEL for a quotation for ASTM A738 Grade E heat-treated pressure vessel plate. Please send the specification and edition, grade, thickness, width, length, quantity, delivery destination and preferred delivery schedule so we can review your production and export requirements.

If your design also names ASME SA738 Grade E or another C-Mn-Si vessel plate, send the specification set with your enquiry so dual certification and differences can be reviewed.

State any supplementary requirements, simulated post-weld heat treatment, impact testing, ultrasonic examination and the inspection document required, so they are agreed before the order is placed.

For a detailed quotation, email your material specification, drawing, quantity and delivery requirements to our team.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X