ASTM A108 1018 Cold Finished Steel Bars

ASTM A108 1018 is a cold-finished carbon steel bar specified first by chemistry. Grade 1018 carbon is 0.15-0.20 % with manganese 0.60-0.90 %, from the A29 composition used by A108. A108 does not set tensile or yield minima unless the order adds a mechanical requirement. SHH STEEL reviews the grade, finish and certificate before quoting.
Keywords
ASTM A108 1018 bars, 1018 cold finished bar, A108 1018 round bar, 1018 CF steel bar, AISI 1018 bar
Equivalent Grades:
Near-equivalents only, not automatic substitutes.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Size Chart
Applications
Equivalent Grades
Sourcing
FAQ
Conclusion

What are ASTM A108 1018 Cold Finished Steel Bars?

ASTM A108 is the specification for cold-finished carbon and alloy steel bars. Grade 1018 is the usual low-carbon designation taken from the ASTM A29/A29M composition tables that A108 uses. This page is chemistry-first: 1018 is accepted on composition unless the purchase order also invokes a mechanical-property requirement. Published mill ‘typical’ tensile figures are not specification minima and are not tabulated here.

The product is a cold-finished bar, not a hot-rolled A36 bar and not a GB/T 699 Grade 20 bar. A different A108 grade, a hot-rolled 1018, or a bar ordered only to A29, is a different enquiry.

Material, Manufacture and Scope for ASTM A108 1018 Bars

A108 covers cold-finished bars in a range of carbon and alloy grades. This page is confined to 1018. The usual finishing routes are cold drawing, turning, grinding or polishing, or a combination named on the order. General requirements and the grade chemistry come from the A29 (and related) documents referenced by A108. The A108 edition named on the order governs acceptance. Heat treatment, when required, has to be stated; it is not implied by the grade name.

ASTM A108 1018 Chemical Composition (Heat Analysis)

Grade 1018 heat analysis is carbon 0.15-0.20 %, manganese 0.60-0.90 %, phosphorus 0.040 % maximum and sulfur 0.050 % maximum. These are the A29 limits used for 1018 when the bar is furnished to A108. Silicon is not given a general maximum in that 1018 composition row and is not invented here. Do not replace this carbon window with the 0.17-0.23 % range of GB/T 699 Grade 20, or with ASTM A36 bar carbon limits.

Swipe horizontally to view all dimensions.

Element Grade 1018 heat analysis (ASTM A29 chemistry used by A108)
Carbon 0.15-0.20 %
Manganese 0.60-0.90 %
Phosphorus, max 0.040 %
Sulfur, max 0.050 %

ASTM A108 1018 Mechanical Properties: Chemistry-First, No Default Tensile Minima

By default, ASTM A108 1018 is supplied to chemistry. The specification does not set a minimum tensile strength, yield strength or elongation for 1018 unless the purchaser requires mechanical properties (for example by a supplementary requirement or by another specification named on the order). This page therefore does not publish a tensile or yield minimum, and it does not treat catalogue ‘typical’ strengths as acceptance values. If the project needs a guaranteed yield or tensile result, that requirement has to be written on the enquiry.

ASTM A108 1018 Common Cold-Finished Round Sizes

A108 does not prescribe a closed list of diameters. The table below is a typographical subset of common inch cold-finished rounds, not a complete mill programme and not a stock list. Theoretical mass is computed at 490 lb/ft3 as W = 2.670 d2 lb/ft, with d in inches (kg/m = lb/ft x 1.48816). Squares, hexagons and other finishes may be quoted when they are named on the order. Preferred sizes remain those actually ordered.

Round bars (20 common inch diameters).

Swipe horizontally to view all dimensions.

Diameter (in) d (in) d (mm) Theoretical mass (lb/ft) Theoretical mass (kg/m)
1/4 0.25 6.35 0.167 0.249
5/16 0.312 7.938 0.261 0.388
3/8 0.375 9.525 0.375 0.558
7/16 0.438 11.112 0.511 0.76
1/2 0.5 12.7 0.667 0.993
9/16 0.562 14.287 0.845 1.257
5/8 0.625 15.875 1.043 1.552
3/4 0.75 19.05 1.502 2.235
7/8 0.875 22.225 2.044 3.04
1 1 25.4 2.67 3.97
1-1/8 1.125 28.575 3.38 5.03
1-1/4 1.25 31.75 4.17 6.21
1-3/8 1.375 34.925 5.05 7.52
1-1/2 1.5 38.1 6.01 8.94
1-3/4 1.75 44.45 8.18 12.17
2 2 50.8 10.68 15.89
2-1/4 2.25 57.15 13.52 20.12
2-1/2 2.5 63.5 16.69 24.84
2-3/4 2.75 69.85 20.19 30.05
3 3 76.2 24.03 35.76

Applications and Service Limits for ASTM A108 1018 Cold Finished Bars

1018 cold-finished bars are used for pins, shafts, fixtures, studs and general machined parts where a low-carbon, close-finish bar is named. The grade is not a pressure-vessel steel and not an automatic substitute for A36, 1045, or a heat-treated alloy bar. Weldability is generally good for this carbon range, but the welding procedure still has to suit the part and the finish.

Near-Equivalents for ASTM A108 1018 Bars: Not Automatic Substitutes

SAE 1018 and UNS G10180 describe the same chemistry family, but an A108 product is a cold-finished bar to that specification. GB/T 699 Grade 20 and JIS S20C are neighbouring low-carbon grades with their own mechanical tables. ASTM A36 is a structural grade with required tensile properties and a different chemistry table. ASME SA designations are not inferred here.

Sourcing ASTM A108 1018 Cold Finished Steel Bars from SHH STEEL

Send the finish, the diameter (or across-flats size), the length, and whether any mechanical test is required, together with the A108 edition. Name 1018 explicitly. Do not use a hot-rolled A36 or a GB/T 699 term for this page. SHH STEEL reviews the grade, the finish and the certificate before quoting. The size table is a typographical reference, not a warehouse list.

ASTM A108 1018 Steel Bar FAQs

Does A108 1018 have a minimum tensile strength?
Not by default. The grade is accepted on chemistry unless the purchase order requires mechanical properties. Typical mill values are not used as minima on this page.
Is 1018 the same as A36 bar?
No. A36 is a structural specification with required tensile and yield values and a different chemistry table. A108 1018 is a cold-finished chemistry grade.
Where do the carbon limits come from?
From the ASTM A29/A29M 1018 composition used by A108: carbon 0.15-0.20 %, manganese 0.60-0.90 %, phosphorus 0.040 % max and sulfur 0.050 % max.
Are the diameters a complete A108 list?
No. A108 does not prescribe a closed size table. The rounds shown are a common typographical subset with theoretical masses, not a stock list.

Conclusion

ASTM A108 1018 is a cold-finished carbon steel bar specified first by chemistry, with carbon 0.15-0.20 % and manganese 0.60-0.90 %. No tensile or yield minimum is published here because the specification does not set one unless the order adds that requirement. Confirm the finish, the size, the edition and any mechanical test on the enquiry.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X