ASME SA-36 Round, Square and Flat Steel Bars
What are ASME SA-36 Round, Square and Flat Steel Bars?
ASME SA-36/SA-36M, as printed in ASME BPVC Section II, Part A, 2023, is marked identical with ASTM Specification A36/A36M-19. Scope 1.1 covers carbon steel shapes, plates and bars of structural quality. This page is for bars only: rounds, squares and flats. It is not the live ASTM A36 bar page, and it is not an SA-36 angle, channel, W-shape or S-shape page.
An ordinary ASTM A36 certificate is not an SA-36 certificate. The SA designation is used when the order needs the ASME materials listing. The Code edition on the order governs; a later ASTM A36 year is not automatically the SA text in the 2023 book.
Material, Manufacture and Scope for ASME SA-36 Steel Bars
The steel shall be killed. Structural products furnished to this specification shall conform to the current edition of Specification A6/A6M for the product ordered, unless a conflict exists, in which case SA-36 prevails. Supplementary requirements apply only when specified. Clause 8.2 provides that bars, other than flats, less than 1/2 in. [12.5 mm] in thickness or diameter need not be tension-tested by the manufacturer, provided the chemical composition used is appropriate for obtaining the tensile properties in Table 2. That exemption is stated, not replaced by an invented test method.
ASME SA-36 Bar Chemical Composition (Heat Analysis)
The figures below are the bar columns of Table 3 (bars, and plates 15 in. [380 mm] and under in width), not the shapes column and not the wide-plate columns. Carbon maxima rise with thickness from 0.26 % through 0.29 %. Manganese has no specified requirement up to 3/4 in. [20 mm] inclusive, and is 0.60-0.90 % above that. Phosphorus is 0.04 % maximum, sulfur 0.05 % maximum and silicon 0.40 % maximum. Copper is 0.20 % minimum only when copper steel is specified. Do not copy the shapes-column manganese rule, or a plate-width carbon split, onto a bar order.
Swipe horizontally to view all dimensions.
ASME SA-36 Bar Mechanical Properties
Table 2 requires 58-80 ksi [400-550 MPa] tensile strength, a 36 ksi [250 MPa] minimum yield point, 20 % minimum elongation in 8 in. [200 mm], and 23 % minimum elongation in 2 in. [50 mm] for bars. The 23 % figure is the plates-and-bars elongation, not the 21 % shapes column. The 32 ksi reduction is for plates over 8 in. thick only and does not apply to bars. Charpy testing is not required unless specified.
Swipe horizontally to view all dimensions.
ASME SA-36 Common Bar Sizes: Rounds, Squares and Flats
The tables below are the same common typographical merchant-bar sizes already verified on the ASTM A36 bar page, with theoretical masses at 490 lb/ft3. They are not a complete A6 bar list and not a mill stock list. Preferred sizes remain those named on the order. Rounds below 1/2 in. diameter fall under the clause 8.2 tension-test exemption described above unless the purchaser requires a test.
Swipe horizontally to view all dimensions.
Common square bars
Swipe horizontally to view all dimensions.
Common flat bars
Swipe horizontally to view all dimensions.
Applications and Service Limits for ASME SA-36 Steel Bars
SA-36 bars are used in general structural fabrication, fixtures and details where the order names the ASME listing. A Section II, Part A listing is not by itself permission under every construction Code part or every pressure service. SA-36 is not SA-516, and it is not a quenched-and-tempered alloy bar. Do not treat an A36 bar as SA-36 unless both the marking and the certificate say so.
Near-Equivalents for ASME SA-36 Steel Bars: Not Automatic Substitutes
ASTM A36/A36M-19 is the text adopted as identical in the 2023 SA-36 specification, but an A36 certificate is not automatically an SA-36 certificate. EN 10025-2 S235JR and S275JR bars, and GB/T 700 Q235B, follow different tables. SA-36 shapes use the shapes chemistry column, not the bar columns on this page.
Sourcing ASME SA-36 Steel Bars from SHH STEEL
Send the form, the size, the length, and the BPVC Section II, Part A edition required, and name SA-36/SA-36M explicitly. Do not use the ASTM A36 bar term, or an SA-36 shape term, for this page. SHH STEEL reviews the form, the Code edition and the certificate before quoting. The size tables are a typographical reference, not a warehouse list.
ASME SA-36 Steel Bar FAQs
-
Is SA-36 the same as ASTM A36?
- The 2023 SA-36/SA-36M text is identical with A36/A36M-19, but an ordinary A36 certificate is not an SA-36 certificate. Name the SA designation and the Code edition when that listing is required.
-
Which chemistry column applies to bars?
- The bar columns of Table 3, which split carbon and manganese by thickness. Do not use the shapes column or the wide-plate columns on a bar order.
-
Must every small bar be tension-tested?
- Clause 8.2 allows the manufacturer to omit tension tests on bars, other than flats, under 1/2 in. thickness or diameter if the chemistry is appropriate for Table 2. Flats are not in that exemption.
-
Does this page cover SA-36 shapes?
- No. Shapes have a different chemistry column and a different elongation line. Use the matching SA-36 shape page, once published, for those products.
Conclusion
ASME SA-36 bars follow the 2023 Section II, Part A text, identical with A36/A36M-19, and use the bar columns of Table 3 with 36 ksi yield and 58-80 ksi tensile strength. An ordinary A36 certificate is not SA-36. Confirm the form, the size, the Code edition and the certificate on the order.