(S)A240 S31703, (S)A240 TP 317L, S31703 Stainless Plate, TP317L
2015年7月30日 by admin
(S)A240 S31703, (S)A240 TP 317L, S31703 Stainless Plate, TP317L
Gangsteel Stainless Factory is the large manufacturer to supply (S)A240 S31703, (S)A240 TP 317L,
S31703 Stainless Plate, TP317L as per ASTM, ASME, JIS , EN, UNS Specs. We have about 3000tons
each thickness and size stainless plates and large warehouse. If you have any requirement for
stainless plate in competitive price and faster delivery time, please contact us.
Tags: A240 S31703, (S)A240 S31703, S31703 Stainless plate,SS317L, A240 317L, SA240 317L,TP317L
What forms of A240 S31703 Stainless Steel are available at UNITEDSTEEL?
1). Stainless steel Plate & Sheet & Strip & Coil
Supply Dimensions: Thk: 0.8--100mm Wd: 500-- 2500mm Lgth: 1000--12000mm
Surface Finish: 2B, BA, No.1, etc.
2). Pipe & Tube
3). Stainless Section Bar
4). Weld Wire
(S)A240 S31703 Chemical Composition, max %
C | Mn | P | S | Si | Cr |
0.03 | 2.00 | 0.045 | 0.030 | 0.75 | 18.0-20.0 |
Ni | Mo | N | Cu | Others | |
11.0-15.0 | 3.00-4.00 | 0.10 | | |
(S)A240 S31703 Mechanical Properties
Grade | Tensile Str., min, MPa | 0.2% Yield Str., min, MPa | E.L in 50mm, min % | max HRB |
(S)A240 S31703 | 515 | 205 | 40 | 95 |
Gangsteel Stainless Factory is the large manufacturer for ASTM, ASME, JIS, EN, UNS Stainless plate
and sheet. We have about 3000tons each thickness and size stainless plates and large warehouse.
If any requirement for stainless plate in competitive price and faster delivery time, please contact us.