(S)A240 S31700, (S)A240 TP 317, S31700 Stainless Plate, TP317

2015年7月30日 by admin

 

(S)A240 S31700, (S)A240 TP 317, S31700 Stainless Plate, TP317
 
Gangsteel Stainless Factory is the large manufacturer to supply (S)A240 S31700, (S)A240 TP 317,
S31700 Stainless Plate, TP317 as per ASTM, ASME, JIS , EN, UNS Specs. We have about 3000tons
each thickness and size stainless plates and large warehouse. If you have any requirement for
stainless plate in competitive price and faster delivery time, please contact us.
 
Tags: A240 S31700, (S)A240 S31700, S31700 Stainless plate,SS317, A240 317, SA240 317,TP317
 
What forms of A240 S31700 Stainless Steel are available at UNITEDSTEEL?
1). Stainless steel Plate & Sheet & Strip & Coil
Supply Dimensions: Thk: 0.8--100mm  Wd: 500-- 2500mm Lgth: 1000--12000mm
Surface Finish: 2B, BA, No.1, etc.
2). Pipe & Tube
3). Stainless Section Bar
4). Weld Wire
 (S)A240 S31700 Chemical Composition, max %

C
Mn
P
S
Si
Cr
0.08
2.00
0.045
0.030
0.75
18.0-20.0
Ni
Mo
N
Cu
Others
11.0-15.0
3.00-4.00
0.10
 
 

(S)A240 S31700 Mechanical Properties

Grade
Tensile Str., min, MPa
0.2% Yield Str., min, MPa
E.L in 50mm, min %
max HRB
(S)A240 S31700
515
205
35
95

 
                                                                                                                                                                              
Gangsteel Stainless Factory is the large manufacturer for ASTM, ASME, JIS, EN, UNS Stainless plate
and sheet. We have about 3000tons each thickness and size stainless plates and large warehouse.
 
If any requirement for stainless plate in competitive price and faster delivery time, please contact us.
 
Other related Stainless Plate For (S)A240                                                          

Tags: SA240 S31700  SA240 TP 317  S31700 Stainless Plate  TP317  

0 Comments, 0 Trackbacks