(S)A240 S31753, (S)A240 TP 317LN, S31753 Stainless Plate, TP317LN

2015年7月30日 by admin

 

(S)A240 S31753, (S)A240 TP 317LN, S31753 Stainless Plate, TP317LN
 
Gangsteel Stainless Factory is the large manufacturer to supply (S)A240 S31753, (S)A240 TP 317LN,
S31753 Stainless Plate, TP317LN as per ASTM, ASME, JIS , EN, UNS Specs. We have about 3000tons
each thickness and size stainless plates and large warehouse. If you have any requirement for
stainless plate in competitive price and faster delivery time, please contact us.
 
Tags: A240 S31753, (S)A240 S31753, S31753 Stainless plate,SS317LN, A240 317LN, SA240 317LN,TP317LN
 
What forms of A240 S31753 Stainless Steel are available at UNITEDSTEEL?
1). Stainless steel Plate & Sheet & Strip & Coil
Supply Dimensions: Thk: 0.8--100mm  Wd: 500-- 2500mm Lgth: 1000--12000mm
Surface Finish: 2B, BA, No.1, etc.
2). Pipe & Tube
3). Stainless Section Bar
4). Weld Wire
 (S)A240 S31753 Chemical Composition, max %

C
Mn
P
S
Si
Cr
0.03
2.00
0.045
0.030
0.75
18.0-20.0
Ni
Mo
N
Cu
Others
11.0-15.0
3.00-4.00
0.10-0.22
 
 

(S)A240 S31753 Mechanical Properties

Grade
Tensile Str., min, MPa
0.2% Yield Str., min, MPa
E.L in 50mm, min %
max HRB
(S)A240 S31753
550
240
40
95

 
                                                                                                                                                                              
Gangsteel Stainless Factory is the large manufacturer for ASTM, ASME, JIS, EN, UNS Stainless plate
and sheet. We have about 3000tons each thickness and size stainless plates and large warehouse.
 
If any requirement for stainless plate in competitive price and faster delivery time, please contact us.
 
Other related Stainless Plate For (S)A240                                                                                     

Tags: SA240 S31753  SA240 TP 317LN  S31753 Stainless Plate  TP317LN  

0 Comments, 0 Trackbacks