(S)A240 S31635, (S)A240 TP 316Ti, S31635 Stainless Plate, TP316Ti
2015年7月30日 by admin
(S)A240 S31635, (S)A240 TP 316Ti, S31635 Stainless Plate, TP316Ti
Gangsteel Stainless Factory is the large manufacturer to supply (S)A240 S31635, (S)A240 TP 316Ti,
S31635 Stainless Plate, TP316Ti as per ASTM, ASME, JIS , EN, UNS Specs. We have about 3000tons
each thickness and size stainless plates and large warehouse. If you have any requirement for
stainless plate in competitive price and faster delivery time, please contact us.
Tags: A240 S31635, (S)A240 S31635, S31635 Stainless plate,SS316Ti, A240 316Ti, SA240 316Ti,TP316Ti
What forms of A240 S31635 Stainless Steel are available at UNITEDSTEEL?
1). Stainless steel Plate & Sheet & Strip & Coil
Supply Dimensions: Thk: 0.8--100mm Wd: 500-- 2500mm Lgth: 1000--12000mm
Surface Finish: 2B, BA, No.1, etc.
2). Pipe & Tube
3). Stainless Section Bar
4). Weld Wire
(S)A240 S31635 Chemical Composition, max %
C | Mn | P | S | Si | Cr |
0.08 | 2.00 | 0.045 | 0.030 | 0.75 | 16.0-18.0 |
Ni | Mo | N | Cu | Others | |
10.0-14.0 | 2.00-3.00 | 0.10-0.16 | | Ti: 5×(C+N) min, 0.70 max |
(S)A240 S31635 Mechanical Properties
Grade | Tensile Str., min, MPa | 0.2% Yield Str., min, MPa | E.L in 50mm, min % | max HRB |
(S)A240 S31635 | 515 | 205 | 40 | 95 |
Gangsteel Stainless Factory is the large manufacturer for ASTM, ASME, JIS, EN, UNS Stainless plate
and sheet. We have about 3000tons each thickness and size stainless plates and large warehouse.
If any requirement for stainless plate in competitive price and faster delivery time, please contact us.
Other related Stainless Plate For (S)A240
Tags: SA240 S31635 SA240 TP 316Ti S31635 Stainless Plate TP316Ti
0 Comments, 0 Trackbacks