Q500D quenched tempered Steel plate

2013年12月11日 by admin

 

Q500D quenched tempered Steel plate, GB/T 16270 Q500D
 
 
GB/T 16270-2009 Q500D High strength structural steel plates in the quenched and tempered condition
Q500D Chemical requirement 

Grade
Chemical requirement or element Max %
 
C
Si
Mn
P
S
Cu
Cr
Ni
Mo
B
V
Nb
Ti
Q500D
0.2
0.8
1.7
0.025
0.015
0.5
1.5
2
0.7
0.005
0.12
0.06
0.05

 
Q500D Property in tensile and yield strength, and impact test requirement

Grade
Property
Impact test
Q500D
Yield Mpa Min
Tensile Mpa
Elongation
Min J
Thickness mm
Thickness mm
Degree
50
50-100
100-150
50
50-100
10-150
%
0
-20
-40
-60
500
480
440
590-770
540-720
17
 
47
 
 

 
HENAN GANG IRON AND STEEL CO.,LTD Supply Q500D in about 3000tons stock for many thickness and sizes. If you have requirement for stock or new Q500D requirement, please feel free to contact us or email to us by admin@gangsteel.com
 