Q500C quenched tempered Steel plate, GB/T 16270 Q500C
GB/T 16270-2009 Q500C High strength structural steel plates in the quenched and tempered condition
Q500C Chemical requirement
Grade | Chemical requirement or element Max % | ||||||||||||
| C | Si | Mn | P | S | Cu | Cr | Ni | Mo | B | V | Nb | Ti |
Q500C | 0.2 | 0.8 | 1.7 | 0.025 | 0.015 | 0.5 | 1.5 | 2 | 0.7 | 0.005 | 0.12 | 0.06 | 0.05 |
Q500C Property in tensile and yield strength, and impact test requirement
Grade | Property | Impact test | |||||||||
Q500C | Yield Mpa Min | Tensile Mpa | Elongation | Min J | |||||||
Thickness mm | Thickness mm | Degree | |||||||||
50 | 50-100 | 100-150 | 50 | 50-100 | 10-150 | % | 0 | -20 | -40 | -60 | |
500 | 480 | 440 | 590-770 | 540-720 | 17 | 47 | | | |
HENAN GANG IRON AND STEEL CO.,LTD Supply Q500C in about 3000tons stock for many thickness and sizes. If you have requirement for stock or new Q500C requirement, please feel free to contact us or email to us by admin@gangsteel.com