Q500E quenched tempered Steel plate,
2013年12月11日 by admin
Q500E quenched tempered Steel plate, GB/T 16270 Q500E
GB/T 16270-2009 Q500E High strength structural steel plates in the quenched and tempered condition
Q500E Chemical requirement
Grade | Chemical requirement or element Max % | ||||||||||||
| C | Si | Mn | P | S | Cu | Cr | Ni | Mo | B | V | Nb | Ti |
Q500E | 0.2 | 0.8 | 1.7 | 0.02 | 0.010 | 0.5 | 1.5 | 2 | 0.7 | 0.005 | 0.12 | 0.06 | 0.05 |
Q500E Property in tensile and yield strength, and impact test requirement
Grade | Property | Impact test | |||||||||
Q500E | Yield Mpa Min | Tensile Mpa | Elongation | Min J | |||||||
Thickness mm | Thickness mm | Degree | |||||||||
50 | 50-100 | 100-150 | 50 | 50-100 | 10-150 | % | 0 | -20 | -40 | -60 | |
500 | 480 | 440 | 590-770 | 540-720 | 17 | | | 34 | |
HENAN GANG IRON AND STEEL CO.,LTD Supply Q500E in about 3000tons stock for many thickness and sizes. If you have requirement for stock or new Q500E requirement, please feel free to contact us or email to us by admin@gangsteel.com
0 Comments, 0 Trackbacks