Q460F quenched tempered Steel plate, GB/T 16270 Q460F
 
 
 
GB/T 16270-2009 Q460F High strength structural steel plates in the quenched and tempered condition
 
Q460F Chemical requirement 

Grade
Chemical requirement or element Max %
 
C
Si
Mn
P
S
Cu
Cr
Ni
Mo
B
V
Nb
Ti
Q460F
0.2
0.8
1.70
0.020
0.010
0.5
1.5
2.0
0.7
0.005
0.12
0.06
0.05

 
 
Q460F Property in tensile and yield strength, and impact test requirement

Grade
Property
Impact test
Q460F
Yield Mpa Min
Tensile Mpa
Elongation
Min J
Thickness mm
Thickness mm
Degree
50
50-100
100-150
50
50-100
10-150
%
0
-20
-40
-60
460
440
400
550-720
500-670
17
 
 
 
34

 
 