Q460E quenched tempered Steel plate

2013年12月11日 by admin

 

Q460E quenched tempered Steel plate, GB/T 16270 Q460E
 
 
 
GB/T 16270-2009 Q460E High strength structural steel plates in the quenched and tempered condition
 
Q460E Chemical requirement 

Grade
Chemical requirement or element Max %
 
C
Si
Mn
P
S
Cu
Cr
Ni
Mo
B
V
Nb
Ti
Q460E
0.2
0.8
1.70
0.020
0.010
0.5
1.5
2.0
0.7
0.005
0.12
0.06
0.05

 
 
Q460E Property in tensile and yield strength, and impact test requirement

Grade
Property
Impact test
Q460E
Yield Mpa Min
Tensile Mpa
Elongation
Min J
Thickness mm
Thickness mm
Degree
50
50-100
100-150
50
50-100
10-150
%
0
-20
-40
-60
460
440
400
550-720
500-670
17
 
 
34
 

 
 
HENAN GANG IRON AND STEEL CO.,LTD Supply Q460E in about 3000tons stock for many thickness and sizes. If you have requirement for stock or new Q460E requirement, please feel free to contact us or send email to us admin@gangsteel.com
 