Q460D quenched tempered Steel plate, GB/T 16270 Q460D
 
 
 
GB/T 16270-2009 Q460D High strength structural steel plates in the quenched and tempered condition
 
Q460D Chemical requirement 

Grade
Chemical requirement or element Max %
 
C
Si
Mn
P
S
Cu
Cr
Ni
Mo
B
V
Nb
Ti
Q460D
0.2
0.8
1.70
0.025
0.015
0.5
1.5
2.0
0.7
0.005
0.12
0.06
0.05

 
 
Q460D Property in tensile and yield strength, and impact test requirement

Grade
Property
Impact test
Q460D
Yield Mpa Min
Tensile Mpa
Elongation
Min J
Thickness mm
Thickness mm
Degree
50
50-100
100-150
50
50-100
10-150
%
0
-20
-40
-60
460
440
400
550-720
500-670
17
 
47
 
 

 
 
HENAN GANG IRON AND STEEL CO.,LTD Supply Q460D in about 3000tons stock for many thickness and sizes. If you have requirement for stock or new Q460D requirement, please feel free to contact us or send email to us admin@gangsteel.com
 