EN 10025-3 S355nl 250mm Thickness passed LR approval in 2011-10-15.  That is a new project in super thickness project in gangsteel.

Gangsteel cooperated with HBIS wuyang mill in Electroslag remelting technology to produce EN 10025-3 S355NL 250mm. 

We have got the satisfactory results in property of steel plate:

Yield strength is 413Mpa,
Tensile strenth is 539Mpa
Elongtation is 28% }
CEQ is   0.44%
-40 Test result is   194Mpa, 269Mpa, 294Mpa.

All of property of S355nl Have passed LR inspection of China

It broke donw our mill record in S355nl steel grade.