BV A420 Chemical composition heat analysis

Element
BV A420 Max %
Element
BV A420  max %
C
0.21
Ni
2.0
Mn
1.70
Mo
1.0
Si
 0.10-0.55
    Al
 0.015 min
S
0.035
    Nb
0.06
P
0.035
V
0.10
Cu
1.5
Ti
0.20
     Cr
2.0
N
0.020

   
 
 
 
 
BV A420 Mechanical properties,            longitudinal min impact energy

Grade
Thickness
Yield Strength
Tensile Strength
Elongation
Impact Energy
(mm)
MPa (min)
MPa
% (min)
(KV J) (min)
 
 
 
 
0 degree
BV A420
8-260
420
530-680
18
28J

 
Note: the impact energy under less 150mm thickness
 
 