New Products /back


S355NL EN10025-3 S355NL steel plate

2011年4月5日 by admin

S355NL steel plate

Adopt standard: EN10025-3

 

Sell steel grade: S275N S355N S420N S460N, S275NL, S355NL, S420NL, S460NL steel plate

 

S355NL steel plate

 

S355N steel is a structural steel grade. S means structural steel, 355 means min yield strength for thickness less 16mm expressed in Mpa, NL mean the delivery condition.

 

Compare the S275N/s275NL, S355NL steel has a more yield and tensile strength. The equal grade of S355NL is S355ML.

 

Gangsteel could provide max thickness to 350mm by using ingot. Max width 3800mm, we also could do the UT test, impact test, Chemical analysis, mechanical test, and Simulated may treatment according to our customer requirement.

 

 

About S355NL steel detail informationplease refer to technical date in following.

 

The Chemical is max composition of product analysis:

 

Grade

C %

Si %

Mn %

P %

S %

V %

AL %

Cr %

S355NL

0.180

0.500

0.9-1.65

0.025

0.020

0.120

0.020

0.300

Cu %

Mo %

Nb %

Ni %

Ti %

N %

 

 

0.550

0.100

0.050

0.300

0.050

0.015

 

 

 

 

The mechanical properties steel plate

 

 

Grade

Thickness(mm)

Min Yield (Mpa)

Tensile(MPa)

Elongation(%)

Min Impact Energy

S355NL

8mm-100mm

235Map-275Mpa

470-630Mpa

22%

-50

27J

101mm-200mm

285Mpa-315Mpa

450-600Mpa

21%

-50

27J

201mm-250mm

275Mpa-285Mpa

450-600Mpa

21%

-50

27J

The min impact energy is longitudinal energy

 

 

 

 

For more information in quality certificate or inquiry in competitive official quotation, please contact us by email.

 

 

Tags: s355nl  s355nl steel  s355n  