P355N steel grade is a normalized, weldable fine grain steels for pressure purposed. The dimensions and tolerance on dimensions should be according to EN 10028-1.

 

P…N mean the room temperature, P…NH means the elevated temperature quality
P…NL1 means the low temperature quality, P…NL2 means the special low temperature quality.

 

Gangsteel is a large agent of HBIS wuyang mill in China and we are specialized in super thick steel plate. So, we could supply the min order is one steel plate and promise the competitive price in order to enlarge our oversea market.


P355N Chemical composition cast analysis:

Element

P355N  Max %

Element

P355N max %

C

0.18

Cr

0.30

Si

0.50

Cu

0.30

Mn

1.10-1.70

Mo

0.08

P

0.025

Nb

0.050

S

0.015

Ni

0.50

AL

0.020

Ti

0.03

N

0.012

V

0.01

 

P355N Mechanical properties:

Grade

Type

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-20 degree

P355N

Normalized

≤ 16

355

490-630

22

30

16> to ≤40

345

490-630

22

30

40> to ≤60

335

490-630

22

30

60> to ≤100

315

470-610

21

30

100> to ≤150

305

460-600

21

30

150> to ≤250

295

450-590

21

30

 