New Products /back


P460NH, P460NH steel plate,P460NH EN10028-3

2011年4月14日 by admin

 

Adopt Standard EN10028-3

Related grades we could supply:

Standard

EN10028-3

Grade

Grade

Grade

Grade

Grade

P275NH

P275NL1

P275NL2

P355N

P355NH

Grade

P355NL1

P355NL2

P460NH

P460NL1

P460NL2

 

P460NH steel grade is a normalized, weldable fine grain steels for pressure purposed. The dimensions and tolerance on dimensions should be according to EN 10028-1.

 

P…N mean the room temperature, P…NH means the elevated temperature quality
P…NL1 means the low temperature quality, P…NL2 means the special low temperature quality.

 

Gangsteel is a large agent of HBIS wuyang mill in China and we are specialized in super thick steel plate. So, we could supply the min order is one steel plate and promise the competitive price in order to enlarge our oversea market.


P460NH Chemical composition cast analysis:

Element

P460NH  Max %

Element

P460NH max %

C

0.20

Cr

0.30

Si

0.60

Cu

0.70

Mn

1.10-1.70

Mo

0.10

P

0.025

Nb

0.05

S

0.015

Ni

0.80

AL

0.020

Ti

0.03

N

0.025

V

0.20

 

P460NH Mechanical properties:

Grade

Type

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-20 degree

P460NH

Normalized

≤ 16

460

570-720

17

30

16> to ≤40

445

570-720

17

30

40> to ≤60

430

570-720

17

30

60> to ≤100

400

540-710

17

30

100> to ≤150

400

540-710

17

30

150> to ≤250

400

540-710

17

30

 

To find more about P460NH or inquiry from our gangsteel, please feel free to contact us by email or calling.

 

Tags: P460NH  P460NH steel plate  P460NH Grade  EN10028-3 P460NH  