New Products /back


EN10025-6 S690QL,S690QL Grade,S690QL steel plate,S690QL

2011年3月30日 by admin

EN10025-6 S690QL,S690QL Grade,S690QL steel plate,S690QL

 

Adopt standard:  S690QL steel EN 10025-6

Sell steel grade: S690Q steel plate, S690QL steel plate, S690QL1 steel plate

 

S690QL steel plate

 

S690QL is good weld ability, -40 temperature impact test in 30J in quenched and tempered steel.

 

 

The symbol S is for structural steel, 690 for the minimum yield strength in thickness under 50mm.

Q mean the delivery condition in quenched and tempered.

S690QL could be through the -40 temperature impact and the energy is 30J.

 

 

Gangsteel could supply EN 10025-6 S690QL plates directly from our mill. Besides that we also have many stock in hand in large thickness. Gangsteel sincerely hope new and old customers come to enquiry our steel plates.

 

 

About S690QL detail informationplease refer to technical date in following.

 

The Chemical is max composition of product analysis:

Grade

C

Si

Mn

P

S

N

B

Cr

S690QL

0.200

0.800

1.700

0.020

0.010

0.015

0.005

1.500

Cu

Mo

Nb

Ni

Ti

V

Zr

 

0.500

0.700

0.060

2.000

0.050

0.120

0.150

 

 

 

The mechanical properties at ambient temperature for quenched and tempered steel plate

Grade

Thickness

Min Yield

Tensile

Elongation

Min Impact Energy

S690QL

8mm-50mm

Min 690Mpa

770-940Mpa

14%

-40

Min 30J

51mm-100mm

Min 650Mpa

760-930Mpa

14%

-40

Min 30J

101mm-150mm

Min 630Mpa

710-900Mpa

14%

-40

Min 30J

 

For more information in MTC or consult us to get a competitive price, please contact us soon.

 

EN10025-6 S690QL,S690QL Grade,S690QL steel plate,S690QL

 

Tags: EN10025-6 S690QL  S690QL Grade  S690QL steel plate  S690QL  

0 Comments, 0 Trackbacks