EN10025-6 S690QL1,S690QL1 Grade,S690QL1 steel plate,S690QL1

 
Adopt standard: S690QL1 steel EN 10025-6
Sell steel grade: S690Q steel plate, S690QL steel plate, S690QL1 steel plate
 
S690QL1 steel plate
 
S690QL1 is good weld-ability, -60 temperature impact test in 30J in quenched and tempered steel.
 
The symbol S is for structural steel, 690 for the minimum yield strength in thickness under 50mm.
Q mean the delivery condition in quenched and tempered.
S690QL1 steel could be through the -60 temperature impact and the energy is 30J, which could be used in lower temperature environment.
 
 
Gangsteel exported EN 10025-6 S690QL1 steel plates directly from our mill. Besides, we also have stock in hand in large thickness of S690QL1 steel. Gangsteel sincerely hope customer could come to our mill and factory to inspect our quality and ability in manufacture for our long cooperation.
 
About S690QL1 detail information, please consult technical date in following.
 
The Chemical is max composition of product analysis:

Grade
C %
Si %
Mn %
P %
S %
N %
B %
Cr %
S690QL1
0.200
0.800
1.700
w
0.010
0.015
0.005
1.500
Cu %
Mo %
Nb %
Ni %
Ti %
V %
Zr %
 
0.500
0.700
0.060
2.000
0.050
0.120
0.150
 

 
 
The mechanical properties at ambient temperature for quenched and tempered steel plate
 

Grade
Thick
Min Yield
Tensile
Elongation
Min Impact Energy
S690QL1
8mm-50mm
Min 690Mpa
770-940Mpa
14%
-60
Min 30J
51mm-100mm
Min 650Mpa
760-930Mpa
14%
-60
Min 30J
101mm-150mm
Min 630Mpa
710-900Mpa
14%
-60
Min 30J

 
 
 
For more information in MTC or consult us to get a competitive price, Please feel free to contact us. Gangsteel will use our specialized knowledge, perfected service and fastest delivery to build our long cooperation in business.
 
EN10025-6 S690QL1,S690QL1 Grade,S690QL1 steel plate,S690QL1
 
 

Tags: S690QL1  S690QL1 Grade  S690QL1 steel plate  S690QL  EN10025-6  

0 Comments, 0 Trackbacks