NV F36|DNV F36 steel plate
2013年8月8日 by admin
Gangsteel is specialized in supplying extra high strength steel plate in Grade F36 approved by DNV, ABS, RINA, LR, GL, BV, CCS, NK and KR.
For more information of DNV Grade F36 steel plate, please check them in following:
DNV Steel Plate Grade | ||||
General Strength | ||||
High Strength | ||||
Extra Strength | ||||
Our mill could produce size in the following:
Thickness: 6mm to 240mm,
Width: 1500mm to 4020mm
Length: 3000mm to 27000mm.
Steel Services: Cutting, Painting, Pretreatment, Ultrasonic Test, Third Party Inspection, and so on.
Gangsteel exported DNV F36 steel material directly from our mill in the competitive price from sales department. Each plate has the Mill Certificate Test EN10204 3.2 Version.
DNV GRADE F36 Chemical composition heat analysis:
NV F36 high Strength Chemical Composition | |||||||
Grade | The Element Max (%) | ||||||
C | Si | Mn | P | S | Al | N | |
0.16 | 0.10-0.50 | 0.9-1.6 | 0.025 | 0.025 | 0.015-0.08 | 0.009 | |
Nb | V | Ti | Cu | Cr | Ni | Mo | |
0.02-0.05 | 0.05-0.10 | 0.02 | 0.35 | 0.20 | 0.80 | 0.08 |
Crack Sensitivity: Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
NV F36 high general strength property | |||||||
Grade | | Mechanical Property | Charpy V Impact Test | ||||
Thickness | Yield | Tensile | Elongation | Degree | Energy 1 | Energy 2 | |
mm | Min Mpa | Mpa | Min % | -60 | J | J | |
t≤50 | 355 | 490-620 | 21% | 24 | 34 | ||
50<t≤70 | 355 | 490-620 | 21% | 27 | 41 | ||
70<t≤150 | 355 | 490-620 | 21% | 34 | 50 | ||
Note: Energy 1 is transverse impact test, Energy 2 is longitudinal |
Boiler steel plates| Alloy steel plates| High strength plate| Carbon steel plate| Stainless steel plate
Equivalent steel grade of NV F36 | |||||||
AB/F36 | GL-F36 | LR/F36 | BV/F36 | CCS/F36 | K F36 | R F36 | RI/F36 |